Abstract
The limited quantum yield of strained monolayer transition metal dichalcogenides grown by vapor-phase methods and during transfer-based stacking poses a fundamental challenge for their optoelectronic applications. Here, we introduce the concept of "entropy engineering" as a transformative strategy to selectively enhance light-matter interactions through controlled electron-phonon coupling. We unveil how tailored entropy introduced via precise selenium doping or interfacial van der Waals proximity can significantly amplify radiative recombination from momentum-dark excitons in WS2 monolayers. Notably, we discover that slight selenium doping drastically enhances the photoluminescence (PL) of WS2 under strain. While both undoped and heavily doped WS2 suffer from strong PL quenching owing to the direct-to-indirect bandgap transition, lightly Se-doped samples exhibit an order-of-magnitude increase in emission intensity. This counterintuitive boost is traced to doping-induced structural disorder, which intensifies electron-phonon interactions and unlocks efficient phonon-assisted emission from otherwise non-radiative indirect excitons. Moreover, we demonstrate that van der Waals coupling to adjacent Se-doped layers can impart interfacial entropy and further augment PL via proximity effects. Our work highlights entropy engineering via controlled doping as a powerful strategy for activating high-efficiency light emission in atomically thin semiconductors.
Two-dimensional transition metal dichalcogenides (TMDs) have attracted considerable research interest, both for fundamental studies of novel physical phenomena and for applications ranging from nanoelectronics and nanophotonics to sensing and actuation at the nanoscale[1, 2, 3, 4, 5, 6]. In particular, monolayer semiconductor TMDs exhibit a direct bandgap and strong light–matter interactions, offering great potential for photonics and optoelectronics[2, 3, 4, 5, 6]. Nevertheless, despite advances in vapor-phase deposition for large-area synthesis[7, 8, 9, 10], these monolayers often suffer from non-ideal photoluminescence (PL) intensity and quality. Key limiting factors include their atomic thickness, high defect density, strain, and structural disorder. Notably, strain—introduced during either growth or subsequent transfer and stacking processes[11]—can trigger a direct-to-indirect bandgap transition[12, 13]. Semiconductors with an indirect bandgap usually leading to strong PL quenching and low quantum yield because electrons and holes located in different valleys. Intervalley excitons are momentum-dark since photons cannot provide the required momentum necessary for an indirect recombination[14, 15, 16, 17, 18, 19, 20]. Furthermore, dark excitons are highly interesting for TMD research, as they can lie energetically below bright excitons and hence have a significant impact on nonequilibrium dynamics as well as optical response of these materials[15, 16, 17, 18, 19, 20]. Consequently, enhancing the quantum efficiency of momentum-dark intervalley excitons in strain-induced indirect-gap TMDs thus represents a critical challenge for their practical use in high-performance photonics and optoelectronics.
Here, we report an unconventional and counterintuitive strategy based on entropy engineering—using slight selenium (Se) doping and interfacial van der Waals proximity in strained monolayers—to enhance electron–phonon coupling, leading to an orders-of-magnitude increase in PL radiation. Previous studies[21, 22, 23, 24, 25, 26] have primarily focused on modulating the Se doping ratio in alloys to achieve composition-tunable electronic and optical properties, while the effect of structural disorder induced by Se doping on electron–phonon coupling has remained unexplored. In this work, we systematically compare the PL characteristics of pure , lightly Se-doped (Se-), and heavily Se-doped (alloyed). Under strain, both undoped and alloys exhibit severely suppressed quantum efficiency due to direct-to-indirect bandgap transition. In contrast, although Se- also transitions to an indirect bandgap under strain, it exhibits strong electron–phonon coupling, which significantly enhances radiative recombination from momentum-dark indirect excitons via phonon-assisted intervalley charge transfer and multi-phonon participation. Our findings reveal that the radiative recombination of indirect excitons is highly susceptible to entropy modulation. The disorder introduced by light Se doping in both phonon and electronic structures facilitates strong electron–phonon coupling, enabling tunable enhancement of indirect exciton radiation by orders of magnitude. Furthermore, we observe that a van der Waals heterostructure composed of Se- and pure exhibits a pronounced proximity-enhanced luminescence at the interface. This effect unveils a novel mechanism whereby interlayer van der Waals contact modulates system disorder, thereby enhancing electron–phonon coupling and indirect exciton radiation. Our results not only demonstrate a new approach to enhance the light emission efficiency in TMDs but also highlight the profound role of disorder in mediating electron–phonon interactions, offering fresh physical insights and motivating new theoretical explorations.
The Se- flakes were synthesized on substrates via conventional two-step atmospheric-pressure chemical vapor deposition (CVD) with a rapid cooling process employed to introduce tensile strain into the as-synthesized material (see Fig. S1 and Methods for details). Obviously, such a method generally does not allow precise control over the doping concentration of Se or its spatial distribution. In our experiments, triangular flakes are typically observed, wherein the Se-WS region is situated at the center of the triangle, surrounded by intrinsic WS along the outer region, thereby forming an in-plane lateral heterostructure (Figure 1a). Such structure indicate that the growth process initially forms small WSe domains, and the subsequent introduction of sulfur replaces the selenium in the existing WSe domains (sulfurization), while simultaneously promoting the lateral epitaxial growth of WS along the edges of the domains. Figure 1b shows two typical Raman spectra obtained from the pure WS and the Se-WS regions under 532 nm excitation, represented by the black and red curves respectively, both exhibiting distinct characteristic peaks of intrinsic WS monolayer (See Fig. S2 and S3 for more experimental results and detail discussion). The Raman spectra exhibit resonance features, and apart from peaks due to the Brillouin zone center optical phonons, various second-order peaks emerge throughout the 100–450 cm frequency range (See Fig. S4 for detail discussion of various Raman modes). The most prominent modes in both spectra exhibit the following shared features: a double-resonance Raman scattering peak involving two longitudinal acoustic phonons (2LA) at 350 cm, and zone-center optical phonons corresponding to in-plane (E) and out-of-plane (A) vibrations at 354 cm and 418 cm, respectively. Mechanical strain alters interatomic distances, thereby shifting phonon frequencies through modifications in lattice dynamics, which can be monitored via Raman spectroscopy. Generally, the A mode exhibits a weak response to in-plane strain, whereas the E mode shows a more pronounced shift due to its vibrational direction being within the plane where strain is applied. In previous studies[27, 28, 29, 30, 31], the strain magnitude has often been quantified using the frequency separation () between the E and A peaks. In our as-grown WS flakes, is measured to be approximately 64 cm, compared to a reported value of 62 cm for transferred WS where strain is released[27, 28]. Based on this difference, the residual strain in our as-grown lateral heterostructure is globally estimated to be around 0.5% to 1%. In addition to strain information, Raman spectroscopy can also reveal doping characteristics. The primary spectral difference between the two regions lies in the emergence of two characteristic peaks at approximately 376 cm and 396 cm (Figure 1b), which are exclusively observed in the Se-WS region. These peaks are attributed to disorder-activated vibrational modes, tentatively assigned to in-plane (E) and out-of-plane (A) vibrations of S–W–Se[21, 32, 33] (See Fig. S4 for detail discussion).

Figure 1. Optical characterization and energy band structure in /Se- lateral heterostructure. a, Schematic diagram of a monolayer /Se- lateral heterostructure under biaxial strain . The yellow and purple dashed boxes indicate the contour of the whole monolayer and the interface of the /Se- lateral heterostructure, respectively. b, Raman spectra obtained from pure (marked by black star in Fig. S2a), and Se- (marked by red star in Fig. S2a), respectively. Inset: Zoom-in of the Raman spectra in the range from 330 to 423 . c, PL spectra obtained from pure (marked by black star in Fig. S2a), and Se- (marked by red star in Fig. S2a), respectively. d and e, the calculated electronic band structures of and the Se- (Se doping concentration of 2.08%) monolayer under application of biaxial strain (). The application of strain induces a direct-to-indirect bandgap transition in both and Se- monolayer. f, Sketch of direct and indirect decay channels for excitons showing the underlying scattering processes in the excitonic center-of mass dispersion (right) and the corresponding PL signals (left).
These Raman characterization results are consistent with the formation of a lateral WS/Se-WS heterostructure, as schematically illustrated in Figure 1a. To further evaluate the Se doping concentration and its influence on the band structure and excitonic properties, we performed PL measurements (Figure 1c). Both the Se-WS and pure WS regions exhibit PL emission at nearly identical energies, comparable to previously reported[27, 28, 29, 30, 31] peak positions for intrinsic WS. This suggests a low Se doping concentration in the Se-WS region, estimated to be less than 5% (We aimed to estimate a conservative upper limit; the actual doping level is likely even lower.). Moreover, the PL signal from the pure WS region is notably weak, comparable in intensity to that of the bilayer region, and exhibits a double-peak feature with energy difference meV (additional PL results are provided in Fig. S2c). These observations suggest that the applied strain induces a transition from direct to indirect bandgap in , leading to strong PL quenching. To validate this hypothesis, we conducted first-principles calculations. As shown in Figure 1d and 1e, both pure and Se- (Se doping concentration of 2.08%) undergo a direct-to-indirect bandgap transition under biaxial strain of 1% (see Figs. S5 and S6 for details and discussion of the first-principles calculations). Similar to bilayer TMDs[34, 35, 36, 37, 38], as shown in Figure 1f, photoexcitation initially creates direct excitons at the K-points. These subsequently undergo rapid phonon-assisted relaxation to the lower-energy indirect band edges, forming momentum-mismatched indirect excitons. Radiative recombination of these indirect excitons requires a slow, phonon-mediated second-order process to conserve momentum, resulting in low quantum efficiency. Nevertheless, thermal population of the higher-energy direct states can also produce a weaker direct emission, giving rise to a higher-energy emission peak alongside the dominant low-energy indirect peak, thereby resulting in a characteristic dual-peak PL spectrum. Remarkably, however, under the same strain conditions, the Se- region exhibits highly efficient PL—showing an order-of-magnitude enhancement compared to the undoped region (See Fig. S3 for more experimental results of additional sample)—despite undergoing a similar direct-to-indirect bandgap transition.
To investigate the underlying mechanism of Se- maintains efficient luminescence under strain, we performed Raman and PL measurements on another sample grown by the same method. Figure 2a shows an optical image of a composition-graded monolayer, which exhibits a well-faceted regular triangular shape with a distinct color gradation from the center to the edge. Both Raman and PL spectra, as functions of spatial position, clearly demonstrate the composition gradient within the sample: pure is located at the outermost edge, while the Se doping concentration gradually increases toward the center (Figure 2b and Figure 2c). For clarity, the sample can be divided into three distinct regions: the outermost region consisting of pure , the central region with a higher Se doping concentration for alloy, and an intermediate region exhibiting slight Se doping in . As shown in Figure 2d, both pure and the alloy exhibit weak luminescence intensity due to the strain-induced direct-to-indirect bandgap transition (see Fig. S7 for the first-principles calculations of alloy), whereas the region with slight Se-doped demonstrates highly efficient PL intensity. A sublinear relationship widely used for ternary alloy semiconductors[33]: , where is the composition ratio of Se/(S + Se) and is the bowing factor (The value of is given as 0.154[33], , ). It can be estimated that a significant enhancement in PL intensity occurs only when the doping concentration is less than 15% (with a predicted lower limit of 1.900 eV, see Fig. S4 for detail discussion).
Figure 2. Raman and PL characterization of composition-graded WSSe monolayer. a, Optical micrographs of a representative composition-graded WSSe monolayer, showing a progressive color gradient from the center to the edge. b and c, Raman and normalized PL spectra measured along the dashed arrow (marked in panel a). d, Spatial dependence of the PL emission intensity (black dots) and energy (red dots), obtained from panel c. Based on this evolution pattern, the flake can be divided into three distinct compositional regions: pure WS (black shaded area), Se-WS (Se doping level below 15%), and the alloyed WSSe (Se doping level above 15%). The Se-WS region exhibits a significant PL enhancement compared to both the pure WS and the alloyed WSSe regions. e, Representative PL spectra acquired from three distinct
With increasing Se doping concentration, not only does the PL intensity exhibit a non-monotonic variation, but the full width at half maximum (FWHM) of the PL peak also follows a non-monotonic trend. As illustrated in Fig. S8a, a comparative statistical analysis further reveals the spatial variations in both PL intensity and FWHM. It can be observed that although the FWHM similarly displays a non-monotonic dependence on Se concentration, its behavior is not entirely identical to that of the PL intensity. Notably, the FWHM reaches its maximum only in regions with relatively higher doping (approximately 7%–15%). In contrast, at lower doping levels (<7%), the FWHM remains nearly identical to that of pure WS (Figure 1c and Fig. S8b). Figure 2e compares the PL spectra of pure WS, Se-WS (around 7%–15%), and WSSe alloy. Clearly, the Se-WS (around 7%–15%) exhibits a broad FWHM and an asymmetric lineshape. On the low-energy side of this asymmetric spectrum, clearly resolved multi-peak features with regular energy spacing are observed, ruling out contributions from charged excitons or biexcitons. Reasonably, we attribute this spectral feature to phonon replica features associated with indirect exciton radiation involving multiple phonons.
To further elucidate the origin of the multi-peak features and asymmetric lineshape in the PL spectrum of Se-WS (), we performed power-dependent PL measurements. As shown in Figure 3a, at low laser power, the spectrum is dominated by an asymmetric profile. With increasing laser power, the multi-peak features become more pronounced and exhibit equienergy phonon replicas with meV (corresponding to the out-of-plane acoustic phonon (ZA) mode, see Fig. S4 for detail discussion). Furthermore, the intensity of the lower-energy peaks increases more rapidly with higher excitation power. This behavior can be attributed to the increased photoexcited carrier density at higher laser powers, which enhances the electron–phonon interaction strength[39, 40]. At higher power densities, the increased carrier density raises the probability of collisions with scattering centers. As a result, more carriers undergo relaxation via the emission of one or multiple phonons. This relaxation process populates the lower-energy states more efficiently. Consequently, the indirect radiative recombination process involves the emission of multiple phonons per electron–hole pair (Figure 3b). Therefore, at low Se doping concentrations (), the process of indirect radiative recombination in WS is activated. In this regime, disorder provides an additional center-of-mass momentum that enables the emission of momentum-dark excitons, with each electron–hole pair recombining radiatively with the assistance of a single phonon. As the doping level increases (7%–15%), the number of phonons involved in the recombination process rises, leading to multi-phonon participation in the radiative recombination of each electron–hole pair. When the doping concentration exceeds 15%, the system becomes fully alloyed, structural disorder is reduced, and the pathway for indirect radiative recombination is suppressed.

Figure 3. Multi-phonon-assisted indirect band exciton radiation and strong electron-phonon coupling mechanism. a, Laser power-dependent PL spectra measured at the Se-WS₂ (Se doping concentration ~11%). b, Sketch of the multi-phonon-assisted indirect exciton radiative decay channels, illustrating the underlying scattering processes in the excitonic center-of-mass dispersion (right) and the corresponding PL spectra (left). c and d, The computed electronic density of states near the FS at the VBM for both WS₂ and the Se-WS₂ monolayers (Se doping concentration 2.08%) under 1% biaxial strain, as obtained from first-principles calculations. e and f, The computed phonon spectra for both WS₂ and the Se-WS₂ monolayers (Se doping concentration 2.08%) under 1% biaxial strain.
To investigate the physical mechanism by which Se doping modulates the electron–phonon coupling in WS, we performed first-principles calculations to compute the electronic density of states (DOS) at the Fermi surface (FS) and the phonon spectra of pure WS and the Se-WS (2.08%) under 1% biaxial strain (Figure 3c-Figure 3f). The electron-phonon coupling strength can be described by , where and are the DOS at the FS and the phonon energy, and are the sum among different phonon modes and the square sum of electron-phonon coupling matrix elements on FS, respectively[41, 42]. A comparative analysis of the DOS at the FS near the valence band maximum (VBM) reveals a suppression in the Se-WS relative to pure WS under 1% biaxial strain (Figure 3c and Figure 3d), suggestive of enhanced electron-phonon coupling. This interpretation is corroborated by the phonon spectra (See Fig. S9 for more results), which reveal reduced phonon group velocity in Se-WS compared to pure WS and WSSe alloy (). These results further support the demonstration that slightly Se doping significantly enhances disorder and strengthens electron-phonon coupling.
More remarkably, we discovered that van der Waals contact between - and pure can likewise introduce disorder at the interface, enhancing electron–phonon coupling and yielding highly efficient PL. As simulated in Figure 4a, using a similar growth method—only reversing the introduction sequence of the Se and S sources (S first followed by Se)—we successfully fabricated the /Se-doped vertical heterostructures. Figure 4b presents a typical optical micrograph of the vertically stacked heterostructure, featuring a regular triangular shape with multilayer AA stacking. As expected, the additional Raman peaks induced by Se doping were only observed in the centrally located multilayer stacked region of the sample, whereas the outer monolayer area exhibited the characteristic Raman spectra of pure (Figure 4c). Similarly, the PL signal from the monolayer is notably weak (black curve), comparable in intensity to that of the bilayer region (blue curve), suggesting a direct to indirect bandgap transition under strain. In contrast, at the interface between the monolayer and bilayer regions (on the monolayer side), the PL intensity exhibits a significant enhancement—more than 50 times greater than that in other areas of the monolayer (Figure 4d and Figure 4e).
Figure 4. Optical characterization of WS₂/Se-WS₂ vertical heterostructure. a, Schematic diagram of a bilayer WS₂/Se-WS₂ vertical heterostructure (top and side views). The yellow and purple dashed boxes outline the bottom-layer WS₂ and the top-layer Se-WS₂, respectively. b, The optical image of a trilayer WS₂ vertical heterostructure sample. The yellow and purple dashed boxes outline the bottom-layer WS₂ and the middle-layer Se-WS₂, respectively. c and d, Raman and PL spectra obtained from bottom-layer WS₂ (black curve corresponds to the black star in panel b), monolayer–bilayer interfacial boundary (red curve corresponds to the red star in panel b), and middle-layer Se-WS₂ (blue curve corresponds to the blue star in panel b) regions, respectively. Inset in panel c: Zoom-in of the Raman spectra marked by the black dashed box. e, Fixed-energy PL spatial distribution map at 1.97 eV.
To rule out the possibility that the highly efficient PL originates from direct Se doping in the central monolayer region—which would form a lateral heterostructure similar to those shown in Figs. S2 and S3—we fabricated bilayer heterostructures using the S-source-first followed by Se-source growth sequence, as presented in Figs. S10 and S11. In both the AB-stacked bilayer heterostructure (Fig. S10) and the AA-stacked bilayer with an irregularly shaped top layer (Fig. S11), the PL enhancement is exclusively localized at the interface between the monolayer and bilayer regions. These results provide compelling evidence that the emission enhancement in monolayer is precisely dictated by the morphology of the overlying Se- layer and occurs solely at the interfacial contact area. Therefore, we can conclusively exclude direct Se doping of the monolayer as the origin of the PL enhancement. Furthermore, we synthesized a specially designed vertically stacked heterostructure (Fig. S12), in which the bottom layer consists of pure and the top layer is a lateral heterostructure of pristine and Se-. Significant PL enhancement in the monolayer region was observed only at the three corners contacting the Se- top layer, while no enhancement occurred at interfaces with the pristine part of the top layer. This further confirms that the luminescence enhancement stems from the van der Waals contact between Se- and monolayer , where proximity-induced interfacial disorder and enhanced electron–phonon coupling play critical roles. Moreover, we found that the proximity-induced interfacial PL enhancement via van der Waals contact is not limited to the case where the upper layer is slightly Se-doped . As shown in Fig. S12, the PL peak of the top Se- layer is located at 1.84 eV, corresponding to an estimated doping level of approximately 30%. Remarkably, even such an alloyed layer can significantly enhance the PL of the underlying monolayer through proximity coupling, thereby overcoming the limitations associated with direct doping.
Our results demonstrate that slight Se doping effectively enhances the PL in monolayers by strengthening the coupling between electrons and ZA phonons via entropy-mediated disorder engineering. Compared to both pristine and fully alloyed , the slightly Se-doped exhibits significantly enhanced disorder, which directly reduces the DOS near the FS and induces pronounced phonon flattening alongside an increased phonon DOS. These changes collectively lead to a marked enhancement in electron–phonon coupling, facilitating phonon-assisted radiative recombination of indirect excitons. The tunability of disorder via Se concentration underscores the role of entropy engineering in low-dimensional systems: unlike high-entropy multicomponent alloys[43, 44, 45], even minor single-element doping can effectively introduce configurational disorder and modify the vibrational and electronic properties. This approach provides a new pathway for tailoring light–matter interactions in atomically thin semiconductors through entropy-regulated electron–phonon coupling.
Data availability
All data supporting the findings of this study are available from the corresponding author upon request.
Acknowledgments
This work was supported by the National Natural Science Foundation of China (Grant Nos. 12404204, 12364007, 62575100), Natural Science Foundation of Hunan Province (Grant Nos. 2024JJ6116), Guangdong Basic and Applied Basic Research Foundation (Grant Nos. 2025A1515010434), Natural Science Foundation of Changsha City (Grant Nos. kq2402049, kq2402151).
Author contributions statement
Q.Z. and W.Z designed the experiment. Q.Z., C.Z. and M.Z. performed the sample synthesis, characterization and optical measurements. Q.S. carried out the theoretical calculations. J.D. conceived and provided advice on the theoretical calculations. Q.Z., J.D. and C.Z. analyzed the data and wrote the paper. All authors participated in the data discussion.
Competing interests statement
The authors declare no competing interests.
compositional regions, showing significantly different FWHM: pure ( meV), Se- ( meV), and alloyed ( meV).
References
- [1]Manzeli, S., Ovchinnikov, D., Pasquier, D., Yazyev, O. V. & Kis, A. 2D transition metal dichalcogenides. Nat. Rev. Mater. 2, 17033 (2017).DOI
- [2]Mak, K. F. & Shan, J. Photonics and optoelectronics of 2D semiconductor transition metal dichalcogenides. Nat. Photonics 10, 216–226 (2016).DOI
- [3]Wang, J., Verzhbitskyi, I. & Eda, G. Electroluminescent Devices Based on 2D Semiconducting Transition Metal Dichalcogenides. Adv. Mater. 30, 1802687 (2018).DOI
- [4]Paur, M. et al. Electroluminescence from multi-particle exciton complexes in transition metal dichalcogenide semiconductors. Nat. Commun. 10, 1709 (2019).
- [5]Li, J., Yang, R., Li, R. & Grigoropoulos, C. P. Exciton Dynamics in 2D Transition Metal Dichalcogenides. Adv. Opt. Mater. 13, 2403137 (2025).DOI
- [6]Babu, R. S. & Georgiadou, D. G. 2D transition metal dichalcogenides for energy-efficient two-terminal optoelectronic synaptic devices. Device 100805 (2025) doi:10.1016/j.device.2025.100805.DOI
- [7]Xue, G. et al. Large-Area Epitaxial Growth of Transition Metal Dichalcogenides. Chem. Rev. 124, 9785–9865 (2024).DOI
- [8]Li, T. et al. Epitaxial growth of wafer-scale molybdenum disulfide semiconductor single crystals on sapphire. Nat. Nanotechnol. 16, 1201–1207 (2021).DOI
- [9]Moon, D. et al. Hypotaxy of wafer-scale single-crystal transition metal dichalcogenides. Nature 638, 957–964 (2025).DOI
- [10]Wang, J. et al. Dual-coupling-guided epitaxial growth of wafer-scale single-crystal WS2 monolayer on vicinal a-plane sapphire. Nat. Nanotechnol. 17, 33–38 (2022).DOI
- [11]Lei, L. et al. Size-dependent strain-engineered nanostructures in MoS2 monolayer investigated by atomic force microscopy. Nanotechnology 32, 465703 (2021).DOI
- [12]Blundo, E. et al. Evidence of the direct-to-indirect band gap transition in strained two-dimensional WS 2 , MoS 2 , and WSe 2. Phys. Rev. Res. 2, 012024 (2020).DOI
- [13]Wang, Y. et al. Strain-induced direct–indirect bandgap transition and phonon modulation in monolayer WS2. Nano Res. 8, 2562–2572 (2015).
- [14]Zhou, Y. et al. Probing dark excitons in atomically thin semiconductors via near-field coupling to surface plasmon polaritons. Nat. Nanotechnol. 12, 856–860 (2017).DOI
- [15]Zhang, X.-X., You, Y., Zhao, S. Y. F. & Heinz, T. F. Experimental Evidence for Dark Excitons in Monolayer WSe 2. Phys. Rev. Lett. 115, 257403 (2015).DOI
- [16]Malic, E. et al. Dark excitons in transition metal dichalcogenides. Phys. Rev. Mater. 2, 014002 (2018).DOI
- [17]Feierabend, M. et al. Molecule signatures in photoluminescence spectra of transition metal dichalcogenides. Phys. Rev. Mater. 2, 014004 (2018).DOI
- [18]Lindlau, J. et al. The role of momentum-dark excitons in the elementary optical response of bilayer WSe2. Nat. Commun. 9, 2586 (2018).
- [19]Deilmann, T. & Thygesen, K. S. Finite-momentum exciton landscape in mono- and bilayer transition metal dichalcogenides. 2D Mater. 6, 035003 (2019).DOI
- [20]Selig, M. et al. Dark and bright exciton formation, thermalization, and photoluminescence in monolayer transition metal dichalcogenides. 2D Mater. 5, 035017 (2018).arxiv.org/abs/1703.03317
- [21]Duan, X. et al. Synthesis of WS 2 x Se 2−x Alloy Nanosheets with Composition-Tunable Electronic Properties. Nano Lett. 16, 264–269 (2016).
- [22]Zheng, B. et al. Band Alignment Engineering in Two-Dimensional Lateral Heterostructures. J. Am. Chem. Soc. 140, 11193–11197 (2018).DOI
- [23]Dong, J., Zhao, Y. & Ouyang, G. The effect of alloying on the band engineering of two-dimensional transition metal dichalcogenides. Phys. E Low-Dimens. Syst. Nanostructures 105, 90– 96 (2019).DOI
- [24]Zhao, Y., Zhang, Z. & Ouyang, G. Band shift of 2D transition-metal dichalcogenide alloys: size and composition effects. Appl. Phys. A 124, 292 (2018).DOI
- [25]Catanzaro, A. et al. Resonant Band Hybridization in Alloyed Transition Metal Dichalcogenide Heterobilayers. Adv. Mater. 36, 2309644 (2024).
- [26]Su, S.-H. et al. Controllable Synthesis of Band-Gap-Tunable and Monolayer Transition-Metal Dichalcogenide Alloys. Front. Energy Res. 2, (2014).DOI
- [27]Michail, A. et al. Tuning the Photoluminescence and Raman Response of Single-Layer WS₂ Crystals Using Biaxial Strain. J. Phys. Chem. C 127, 3506–3515 (2023).DOI
- [28]Mlack, J. T. et al. Transfer of monolayer TMD WS2 and Raman study of substrate effects. Sci. Rep. 7, 43037 (2017).DOI
- [29]Wang, F. et al. Strain engineering in monolayer WS₂ and WS₂ nanocomposites. 2D Mater. 7, 045022 (2020).arxiv.org/abs/2010.16184
- [30]Roy, S., Yang, X. & Gao, J. Biaxial strain tuned upconversion photoluminescence of monolayer WS2. Sci. Rep. 14, 3860 (2024).DOI
- [31]Zeng, H. et al. Optical signature of symmetry variations and spin-valley coupling in atomically thin tungsten dichalcogenides. Sci. Rep. 3, 1608 (2013).DOI
- [32]Kang, H. S. et al. Bowing-alleviated continuous bandgap engineering of wafer-scale WS2xSe2(1-x) monolayer alloys and their assembly into hetero-multilayers. NPG Asia Mater. 14, 90 (2022).DOI
- [33]Yao, Y. et al. Stoichiometry-Modulated Resonant Raman Spectroscopy of WS2(1−x) Se2x - Alloyed Monolayer Nanosheets. J. Phys. Chem. C 124, 20547–20554 (2020).DOI
- [34]Zhao, W. et al. Evolution of Electronic Structure in Atomically Thin Sheets of WS₂ and WSe₂. ACS Nano 7, 791–797 (2013).DOI
- [35]Li, X. et al. Rhombohedral-stacked bilayer transition metal dichalcogenides for high-performance atomically thin CMOS devices. Sci. Adv. 9, eade5706 (2023).DOI
- [36]Zeng, Z. et al. Controlled Vapor Growth and Nonlinear Optical Applications of Large-Area 3R Phase WS₂ and WSe₂ Atomic Layers. Adv. Funct. Mater. 29, 1806874 (2019).
- [37]Zhang, X. et al. Transition metal dichalcogenides bilayer single crystals by reverse-flow chemical vapor epitaxy. Nat. Commun. 10, 598 (2019).DOI
- [38]McCreary, K. M. et al. Stacking-dependent optical properties in bilayer WSe₂. Nanoscale 14, 147–156 (2022).
- [39]Zheng, Q. et al. Surface polarons and optical micro-cavity modulated broad range multi-mode emission of Te-doped CdS nanowires. Nanotechnology 29, 465709 (2018).DOI
- [40]Peng, Y. et al. Wide spectrum multi-sub-band modulation of excitons and defect state emission simultaneously in surface oxidized CdS micro/nano-wires. AIP Adv. 10, 125213 (2020).DOI
- [41]Li, R. et al. Underlying Topological Dirac Nodal Line Mechanism of the Anomalously Large Electron-Phonon Coupling Strength on a Be (0001) Surface. Phys. Rev. Lett. 123, 136802 (2019).DOI
- [42]Hu, S.-Q. et al. Nonadiabatic electron-phonon coupling and its effects on superconductivity. Phys. Rev. B 105, 224311 (2022).DOI
- [43]Redka, D. et al. Interplay between disorder and electronic correlations in compositionally complex alloys. Nat. Commun. 15, 7983 (2024).DOI
- [44]Alam, A., Chouhan, R. K. & Mookerjee, A. Phonon modes and vibrational entropy of disordered alloys with short-range order: A first-principles calculation. Phys. Rev. B 83, 054201 (2011).DOI
- [45]Körmann, F., Ikeda, Y., Grabowski, B. & Sluiter, M. H. F. Phonon broadening in high entropy alloys. npj Comput. Mater. 3, 36 (2017).DOI