Quantitative measurements of transverse thermoelectric generation and cooling performances in SmCo5_5/Bi0.2_{0.2}Sb1.8_{1.8}Te3_3-based artificially tilted multilayer module

Abstract

The transverse thermoelectric generation and cooling performances in a thermopile module composed of recently developed SmCo5_5/Bi0.2_{0.2}Sb1.8_{1.8}Te3_3 artificially tilted multilayers are evaluated quantitatively. When a large temperature difference of 405 ∘^\circC is applied to the SmCo5_5/Bi0.2_{0.2}Sb1.8_{1.8}Te3_3-based module, the open-circuit voltage and output power reach 0.51 V and 0.80 W, respectively. The corresponding maximum power density is 0.16 W/cm2^2, even if the power is normalized by the device area including areas that do not contribute to the power generation, such as epoxy resin, electrodes, and insulating layers. The maximum energy conversion efficiency for our module in this condition is experimentally determined to be 0.92%. Under the cooling operation, the same module exhibits the maximum temperature difference of 9.0 ∘^\circC and heat flow at the cold side of 1.6 W. Although these values are lower than the ideal thermoelectric performance expected from the material parameters due to the imperfections associated with modularization, the systematic investigations reported here clarify a potential of the SmCo5_5/Bi0.2_{0.2}Sb1.8_{1.8}Te3_3 artificially tilted multilayers as thermoelectric generators and cooling devices.

Contact

Masayuki Murata, [email protected], Research Institute for Energy Conservation, National Institute of Advanced Industrial Science and Technology, 1-1-1 Umezono, Tsukuba, Ibaraki, Japan

Ken-ichi Uchida, [email protected], Research Center for Magnetic and Spintronic Materials, National Institute for Materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan

Introduction

Thermoelectric conversion is a promising technology that enables direct conversion between heat and electricity, offering applications in waste heat recovery, power generation, and solid-state cooling [1, 2]. Most of the current thermoelectric devices rely on the longitudinal thermoelectric effects, i.e., the Seebeck and Peltier effects, where heat and charge currents are interconverted in the same direction. In contrast, transverse thermoelectric conversion exploits alternative mechanisms in which heat and charge currents are interconverted in the orthogonal directions, offering unique advantages in device design and applications [3, 4, 5, 6]. The transverse thermoelectric conversion has been observed in conductors under magnetic fields, magnetic materials with spontaneous magnetization, and conductors exhibiting anisotropic transport properties. The transverse thermoelectric conversion due to the anisotropic carrier conduction is driven by the off-diagonal Seebeck effect, which occurs in single crystals showing unipolar/ambipolar anisotropy [7, 8, 9, 10, 11, 12, 13, 14] and in artificially tilted multilayers (ATMLs) comprising two different materials alternately and obliquely stacked [15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25].

Recently, as a promising transverse thermoelectric material, a multifunctional composite magnet (MCM) has been proposed [25]. Ando et al. have demonstrated that MCM comprising SmCo5/Bi0.2Sb1.8Te3\mathrm{SmCo}_{5}/\mathrm{Bi}_{0.2}\mathrm{Sb}_{1.8}\mathrm{Te}_{3} (BST) ATML exhibits excellent transverse thermoelectric power generation, free from performance degradation due to interfacial electrical and thermal resistances, and permanent magnet features simultaneously. The figure of merit for the off-diagonal Seebeck effect in SmCo5\mathrm{SmCo}_{5}/BST-based MCM was estimated to be zxyT=0.20z_{xy}T = 0.20 at room temperature. Using the MCM-based thermopile module, the thermoelectric power generation of 204 mW at a temperature difference of 152 K has been demonstrated; the corresponding power density normalized by a heat transfer area and temperature gradient is record-high among transverse thermoelectric modules, while the energy conversion efficiency is not experimentally determined. Furthermore, the permanent magnet features of MCM enables easy implementation of the module on a heat source/bath made of magnetic materials through the magnetic attractive force and efficient thermal energy harvesting through reduced contact thermal resistances between the module and heat source/bath. Based on these results and the Onsager reciprocal relation, SmCo5\mathrm{SmCo}_{5}/BST-based MCM is expected to exhibit an excellent transverse thermoelectric cooling performance through the off-diagonal Peltier effect, but its cooling performance is yet to be evaluated. The reduced contact thermal resistance through the magnetic attractive force from MCM should be useful in the cooling operation in the same manner as the power generation operation.

In this study, we have comprehensively investigated the transverse thermoelectric conversion performances for the MCM-based thermopile module consisting of SmCo5\mathrm{SmCo}_{5}/BST ATMLs. First, using an MCM-based module with a larger size than that used in Ref. [25], we experimentally estimated the open-circuit voltage, output power, and energy conversion efficiency under large temperature differences. We also measured the maximum temperature difference and coefficient of performance (COP) for cooling operation using the same module and discussed the relationship between the maximum temperature difference and zxyTz_{xy}T in transverse thermoelectric cooling based on the phenomenological formulation. This work further confirms the significant potential of MCM for thermal energy harvesting and thermal management applications.

Experimental details

Sample preparation

The MCM-based module was constructed in the similar manner to the procedures in Ref. [25]. The alternately stacked SmCo5_5/BST multilayer slab was prepared by a spark plasma sintering method under a pressure of 30 MPa at 450 °C for 30 min, where the thickness of each layer is 0.5 mm. The microstructure analysis for the SmCo5_5/BST junction was also reported in Ref. [25]. The SmCo5_5/BST ATMLs, MCM elements, with a length of 15.0 mm, width of 1.5–1.8 mm, thickness of 7.2–7.3 mm, and tilt angle θ\theta of 25° was cut from the multilayer slab, where Cerasolzer #297 (Kuroda Techno Co., Ltd.) electrodes with a melting point of 297 °C were attached to the 1.5–1.8 × 7.2–7.3 mm surfaces of the elements using an ultrasonic soldering method. The present MCM-based module consists of the 16 MCM elements alternately stacked in the width direction with opposite θ\theta and intermediated by thin insulating papers and glue with a heat resistance of 1100 °C (HJ-112, Cemedine Co., Ltd.), while the module used in Ref. [25] has 14 elements. The MCM elements were electrically connected in series to form a zigzag thermopile circuit and enameled Cu wires were attached to the ends of the circuit by melting Cerasolzer #297. The total length, width, and thickness of the MCM-based module except for the Cu wires are around 17.5, 27.8, and 7.4 mm, respectively, where the module size is slightly larger than the ideal one expected from the element size due to small stacking misalignment. Here, the temperature gradient is applied along the thickness direction. To increase the mechanical strength of the module, the area around the electrodes and the base of the Cu wires were hardened with epoxy resin having a heat resistance of 340 °C (Duralco 4703, Cotronics Corp.). Finally, to flatten the heat transfer surfaces, the 17.5 × 27.8 mm surfaces of the module were also covered with a thin layer of the same resin. As described above, the components with the lowest heat resistance in our MCM-based module are the electrodes. However, during the measurements of thermoelectric power generation, only the top surface is exposed to the highest temperature, and the MCM-based module can operate stably even at a hot side temperature of TH∼400T_{\mathrm{H}} \sim400 °C, as long as a cold side temperature is kept at TC<0T_{\mathrm{C}} < 0 °C. In fact, before performing the power generation measurements shown below, the same module was subjected to two heating/cooling cycles with THT_{\mathrm{H}} ranging from room temperature to 400 °C, and no signs of degradation, e.g., the change in the internal resistance of the module, were observed throughout these repeated cycles. In longitudinal thermoelectric modules, junctions between the elements and electrodes are exposed to high temperatures, which causes degradation, whereas MCM-based modules have the advantage of high durability as described above.

Evaluation of power generation characteristics

The thermoelectric power generation properties, such as the output power and conversion efficiency, of the constructed MCM-based module were evaluated using an in-house developed thermoelectric module characterization system [26]. The configuration for evaluating the power generation characteristics of the module is shown in Figure 1(a). A temperature difference ΔT\Delta T was applied to the module by inputting heat QHQ_{\mathrm{H}} to the hot side of the module using a heater and dissipating heat QCQ_{\mathrm{C}} from the cold side of the module to a cooling stage whose temperature was controlled by Peltier elements and a chiller. THT_{\mathrm{H}} and TCT_{\mathrm{C}} were measured by thermocouples inserted into holes in heat baths of AlN ceramic substrates with an area of 28×28 mm228 \times28\ \mathrm{mm}^{2} and thickness of 2 mm2\ \mathrm{mm} attached via metal-oxide-filled silicone compound (Thermal joint type C, Kataoka Senzai) to the hot and cold side surfaces of the module. In the previous study, the actual temperature gradient inside the module was measured using an infrared camera [25], whereas in this study, THT_{\mathrm{H}} and TCT_{\mathrm{C}} were measured in two heat baths with proper thermal contact to outer surfaces of the module, which is commonly adopted in thermoelectric module evaluations [27, 28]. The evaluation was performed in a vacuum of <10−1 Pa< 10^{-1}\ \mathrm{Pa}. The module and AlN ceramic plates were pressurized at 0.4 MPa0.4\ \mathrm{MPa} to ensure proper thermal contact between these components with suitable thermal interfaces of a graphite sheet with a thickness of 0.127 mm0.127\ \mathrm{mm} (Grafoil, NeoGraf Solutions) and silicone grease (KS-613, Shin-Etsu Silicone). By controlling QHQ_{\mathrm{H}} and QCQ_{\mathrm{C}}, ΔT\Delta T (=TH−TCT_{\mathrm{H}}-T_{\mathrm{C}}) of 115115, 215215, 310310, 405 ∘C405\ ^\circ\mathrm{C} were applied with TCT_{\mathrm{C}} ranging from −15 ∘C-15\ ^\circ\mathrm{C} to −5 ∘C-5\ ^\circ\mathrm{C}. The module output power POP_{\mathrm{O}} at a certain ΔT\Delta T was calculated by the product of the load current ILI_{\mathrm{L}} regulated by an electronic load (PLZ164WA, Kikusui Electronics) and the output voltage VOV_{\mathrm{O}} measured by a digital multimeter (Keithley 6500, Tektronix). The thermoelectric conversion efficiency η\eta is defined as PO/QHP_{\mathrm{O}}/Q_{\mathrm{H}}. Here, QHQ_{\mathrm{H}} was estimated by the sum of QCQ_{\mathrm{C}} and POP_{\mathrm{O}} taking into account the energy balance, since the accurate measurement of QHQ_{\mathrm{H}} is difficult due to heat leakage caused by radiation at high temperatures. The QCQ_{\mathrm{C}} values were determined by a heat flow meter located on an oxygen-free Cu block with known thermal conductivity attached to the cold side of the module. As shown in Figure 1(a), six tiny Pt resistance thermometers were embedded in the Cu block, and QCQ_{\mathrm{C}} was determined from the measured temperature drop along the heat flow direction and the dimensions of the Cu block, considering the one-dimensional Fourier’s law. The AC resistance of the module RACR_{\mathrm{AC}} was measured by an inductance-capacitance-resistance meter (BT3562, HIOKI) at each ΔT\Delta T.

Schematics of evaluation system for MCM-based module

Figure 1. Schematics of evaluation system for MCM-based module. (a) Configuration for evaluating power generation characteristics. (b) Configuration for evaluating cooling characteristics.

Evaluation of electronic cooling characteristics

The thermoelectric cooling properties, such as the maximum temperature difference and COP, of the MCM-based module were evaluated using the same equipment as for power generation. The configuration for evaluating the cooling characteristics of the module is shown in Figure 1(b). While most of the components were common between the power generation and cooling evaluations, the major difference was that the heat flow meter was inserted between the heater and module. In addition, THT_{\mathrm{H}} and TCT_{\mathrm{C}} are defined on the cooling stage and heater sides of the module, respectively, which is the opposite of the case for power generation. The heat baths were fixed to the module surfaces with epoxy resin to stabilize the thermal contact, since the risk of module breakdown due to the application of high temperatures is low in the evaluation of the cooling characteristics. Figure 2 shows photographs of the setup for evaluating the cooling characteristics. COP is defined as the ratio of the amount of heat removed by the cold side of the module QCQ_{\mathrm{C}} to the power input to the module PIP_{\mathrm{I}}, and is expressed as COP=QC/PI\mathrm{COP}=Q_{\mathrm{C}}/P_{\mathrm{I}}. Here, QCQ_{\mathrm{C}} is determined by the heat flow meter and PIP_{\mathrm{I}} is calculated by the product of the input current III_{\mathrm{I}} and voltage VIV_{\mathrm{I}} applied to the module. At each input current II=1I_{\mathrm{I}}=1, 4, 5, 6, 7, 8, and 10 A, THT_{\mathrm{H}} was maintained at 50 °C and VIV_{\mathrm{I}} was measured at several TCT_{\mathrm{C}} controlled by the heater. The degree of vacuum, the pressure applied to the components, and the thermal interfaces were the same as those during the power generation evaluation.

Photographs of the setup for evaluating cooling characteristics of MCM-based module

Figure 2. Photographs of the setup for evaluating cooling characteristics of MCM-based module. (a) Bird's-eye view. (b) Side view.

Results and discussion

Power generation

Figure 3 shows the evaluation results of the thermoelectric power generation characteristics for the MCM-based module. Figure 3(a) shows the ILI_{\mathrm{L}} dependence of VOV_{\mathrm{O}} and POP_{\mathrm{O}} on the left and right axes, respectively. The open-circuit voltage VOCV_{\mathrm{OC}} at ΔT=115\Delta T=115 °C observed here is comparable to but slightly smaller than that at a temperature difference of 106 °C reported in Ref. [25]. This difference can be caused by various factors, such as the small difference in the position where the temperature difference is measured, electrode quality, and average temperature of the module. The VOCV_{\mathrm{OC}} value and maximum output power PO,maxP_{\mathrm{O,max}} increased with ΔT\Delta T and showed maximum values of 0.51 V and 0.80 W at ΔT=405\Delta T=405 °C, respectively. This maximum power was about four times higher than 204 mW in the previous report [25]. In this condition, the maximum power density and that normalized by the temperature gradient were 0.16 W/cm2^2 and 0.055 mW/cm2⋅^2\cdot(mm/K)2^2, respectively, which were comparable to those of commercial longitudinal thermoelectric modules [29, 30, 31]. Here, we note that the device area used for the normalization includes the areas of the epoxy resin, electrodes, and insulating layers that do not contribute to the power generation; if the power is normalized by the total area of the ATML elements, the maximum power density becomes approximately 20% larger. Figure 3(b) shows QCQ_{\mathrm{C}} and η\eta on the left and right axes, respectively. η\eta also increased with ΔT\Delta T, and the maximum efficiency ηmax⁡\eta_{\max} reached 0.92% when ΔT\Delta T and ILI_{\mathrm{L}} were 405 °C and 3.1 A, respectively. Although this ηmax⁡\eta_{\max} value is still smaller than that for longitudinal modules [32, 33, 34, 35, 36, 37, 38, 39, 40, 41], it is a promising value among transverse modules. The device figure of merit was estimated to be 0.063 for the MCM-based module using the measured ηmax⁡\eta_{\max} and the relationship between ηmax⁡\eta_{\max} and zxyTz_{xy}T in transverse thermoelectric conversion [42]. The discrepancy between this device figure of merit and the material zxyTz_{xy}T reported in Ref. [25] is discussed in the next subsection. Figure 3(c) shows the ΔT\Delta T dependence of PO,maxP_{\mathrm{O,max}} and ηmax⁡\eta_{\max} on the left and right axes, respectively. Figure 3(d) shows the ΔT\Delta T dependence of TCT_{\mathrm{C}} and RACR_{\mathrm{AC}} on the left and right axes, respectively. At ΔT=115\Delta T = 115 °C and 215 °C, TCT_{\mathrm{C}} could be maintained at −15 °C; however, due to insufficient cooling capacity, TCT_{\mathrm{C}} increased with ΔT\Delta T and reached TC=−5T_{\mathrm{C}} = -5 °C at ΔT=405\Delta T = 405 °C.

Evaluation results of thermoelectric power generation characteristics for MCM-based module

Figure 3. Evaluation results of thermoelectric power generation characteristics for MCM-based module. (a) ILI_L dependence of VOV_O and POP_O. (b) ILI_L dependence of QCQ_C and η\eta. (c) ΔT\Delta T dependence of PO,max⁡P_{O,\max} and ηmax⁡\eta_{\max}. (d) ΔT\Delta T dependence of TCT_C and RACR_{AC}.

Electronic cooling

Figure 4 shows the evaluation results of the cooling characteristics for the same MCM-based module. Figure 4(a) and 4(b) show the ΔT\Delta T dependence of QCQ_{\mathrm{C}} and PIP_{\mathrm{I}} at each III_{\mathrm{I}}, respectively. By linear fitting the QCQ_{\mathrm{C}} data in Figure 4(a), the III_{\mathrm{I}} dependence of the maximum temperature difference ΔTmax⁡\Delta T_{\max} (ΔT\Delta T at QC=0Q_{\mathrm{C}} = 0 W) and the maximum heat flow at the cold side QC,maxQ_{\mathrm{C,max}} (QCQ_{\mathrm{C}} at ΔT=0\Delta T = 0 °C) were determined as shown on the left and right axes of Figure 4(c), respectively. The values of ΔTmax⁡\Delta T_{\max} and QC,maxQ_{\mathrm{C,max}} were estimated to be 9.0 °C and 1.6 W at II=6.8I_{\mathrm{I}} = 6.8 A and 7.1 A, respectively. Kyarad et al. demonstrated ΔTmax⁡>20\Delta T_{\max} > 20 °C at an extremely large current of 40 A in a single element of Pb/Bi2Te3\mathrm{Pb}/\mathrm{Bi}_{2}\mathrm{Te}_{3} ATML [43]. The applied current can be reduced by constructing the thermopile module with multiple elements as described in this study. However, in exchange, the performance can be degraded due to experimental imperfections including small but finite contact resistances at the electrodes and misalignment of the elements (note that such imperfections are unavoidable in laboratory-level verification, but can be minimized once mass-production processes are established). In addition, ΔTmax⁡\Delta T_{\max} can be increased by introducing an infinite-stage structure as often demonstrated for Ettingshausen coolers [44, 45, 46], while it is difficult to introduce such structures in the thermopile module. Figure 4(d) shows the III_{\mathrm{I}} dependence of COP determined from QCQ_{\mathrm{C}} and PIP_{\mathrm{I}} at the certain ΔT\Delta T by linear fitting the PIP_{\mathrm{I}} data in Figure 4(b).

Evaluation results of cooling characteristics for MCM-based module

Figure 4. Evaluation results of cooling characteristics for MCM-based module. (a) ΔT\Delta T dependence of QCQ_C in each III_I. (b) ΔT\Delta T dependence of PIP_I in each III_I. (c) III_I dependence of ΔTmax⁡\Delta T_{\max} and QC,max⁡Q_{C,\max}. (d) III_I dependence of COP at each ΔT\Delta T.

Here, we analyze ΔTmax⁡\Delta T_{\max} for the present MCM-based module. Following the method of Ref. [47], the maximum attainable temperature difference is calculated as

ΔTmax⁡=12zxyTC2,(1)\Delta T_{\max} = \frac{1}{2} z_{xy} T_{\mathrm{C}}^{2}, \tag*{(1)}

where zxy=Sxy2/ρxxκyyz_{xy} = S_{xy}^{2}/\rho_{xx}\kappa_{yy}, SxyS_{xy} is the off-diagonal Seebeck coefficient, ρxx\rho_{xx} is the electrical resistivity along the applied charge current direction (xx direction), κyy\kappa_{yy} is the thermal conductivity along the generated temperature gradient (yy direction), and we assume the isothermal boundary condition along the xx direction as the device geometry adopted in this study is more like Figure 1(d) of Ref. [11] than Figure 1(c). This equation shows that the simple relationship between the maximum temperature difference and figure of merit is applicable not only to the longitudinal thermoelectric conversion but also to the transverse thermoelectric conversion. On the other hand, for the transverse thermoelectric conversion operating with the Ettingshausen effect in which time-reversal symmetry is broken, the relationship between ΔTmax⁡\Delta T_{\max} and the figure of merit is Equation (1) with TCT_{\mathrm{C}} replaced by THT_{\mathrm{H}} [47, 48]. When the experimentally obtained ΔTmax⁡\Delta T_{\max} value is substituted into Equation (1), zxyTCz_{xy}T_{\mathrm{C}} is estimated to be 0.057.

The device figure of merit calculated from ηmax⁡\eta_{\max} of the power generation and the zxyTCz_{xy}T_{\mathrm{C}} value calculated from ΔTmax⁡\Delta T_{\max} under the cooling operation were close, although the definitions of temperature were different.

These values are significantly reduced from zxyT=0.20z_{xy}T = 0.20 for SmCo5_5/BST ATML reported in Ref. [25] due to the following three reasons. Firstly, the device figure of merit determined from the module performance generally decreases from zxyTz_{xy}T estimated from Sxy2/ρxxκyyS_{xy}^{2}/\rho_{xx}\kappa_{yy} due to the electrical and thermal shunting effects at the boundaries to the electrodes and heat source/bath [16, 18] as well as the bonding condition between the ATML element and electrodes. Thus, there remains room to further improve the power generation and cooling performances by optimizing the electrical and thermal boundaries for MCM-based modules. Secondly, when a large temperature difference is applied, a part of the material in the module is at a temperature outside the optimal operating temperature, and the device figure of merit effectively decreases. Thirdly, the power generation and cooling performances could be underestimated because THT_{\mathrm{H}} and TCT_{\mathrm{C}} were measured outside of the module in this study, while ∇T\nabla T inside the module was measured in the previous study.

Numerical simulation

Finite element method simulations were conducted using COMSOL Multiphysics 6.3 to reproduce the measured results of power generation characteristics. The temperature dependence of the Seebeck coefficient, electrical resistivity, and thermal conductivity of BST and SmCo5_5 reported in Ref. [25] were used for the simulations. To investigate the factors contributing to the reduced power generation performance of the MCM-based module, the simulations at ΔT=405\Delta T = 405 K were systematically carried out in a configuration close to the experimental setup with adjusting three parameters. First, the electrode thickness of the ATML elements was adjusted to align the simulated heat flow with the experimental results. Second, the thermal conductivity of the insulating layer between the AlN ceramic plates and ATML elements was modified to account for potential thermal contact resistance. Third, the influence of the electrical contact resistance was taken into consideration by modifying the conductivity of the lead wires connecting the electrodes of each ATML element. Figure 5(a) and Figure 5(b) present the 3D simulation results of the temperature and electric potential distributions, respectively. Figure 5(c) shows the experimental and simulated results of VOV_{\mathrm{O}} and POP_{\mathrm{O}} as functions of ILI_{\mathrm{L}} at ΔT=405\Delta T = 405 °C. The simulated temperature difference across the ATML elements at IL=0I_{\mathrm{L}} = 0 A was 323 °C, corresponding to approximately 80% of the temperature difference between the AlN ceramic plates due to large thermal contact resistance of the insulating layer. In contrast, the slope of the II-VV characteristics was consistent with the experimental result when an additional contact resistance of 26 mΩ was assumed for the lead wires. The experimentally obtained RACR_{\mathrm{AC}} at ΔT=405\Delta T = 405 °C was 78 mΩ, suggesting that the contact resistance could constitute approximately 33% of the total resistance. Figure 5(d) shows the experimental and simulated results of QCQ_{\mathrm{C}} and η\eta as functions of ILI_{\mathrm{L}}. The simulated heat flow bypassing the electrodes of the ATML elements at IL=0I_L = 0 A was 18 W, corresponding to approximately 21% of the experimentally measured QCQ_C of 84 W. These factors may have caused the zxyTz_{xy}T value estimated from the power generation efficiency to be significantly lower than that obtained from the evaluation of an individual element. On the other hand, our efficiency evaluation is based on heat flow measurements on the cold side and therefore does not take into account radiation losses from the side surfaces of the module. Assuming an emissivity of 1 on the module side surfaces as a worst-case condition, the simulated radiative loss reached up to 3.2 W, possibly leading to an overestimation of the conversion efficiency by up to 4%. Although the MCM-based module was evaluated under a vacuum of <10−1<10^{-1} Pa, our previous findings indicate that convective heat loss at this pressure level is negligible compared to the total heat flow through the module. Achieving proper thermal contact was difficult in transverse modules because they do not allow the use of conductive materials such as graphite sheets commonly used to attach longitudinal modules to heat baths. For longitudinal modules, suitable thermal contact can be achieved by eliminating the hot-side ceramic substrate and directly attaching a graphite sheet to the hot-side electrode [26]. In contrast, for transverse modules based on ATML, where the thermoelectric voltage is generated in the in-plane direction, conductive graphite sheets cannot be directly used at the hot-side contact because they may shunt each ATML element electrically. Instead, an insulating material, such as epoxy resin, must be used, which may potentially degrade the thermal contact. Therefore, further improvements can be expected by obtaining better thermal contact with heat baths, such as using insulating coatings with high thermal conductivity. Nevertheless, the transverse thermoelectric conversion performance estimated here is far superior to that obtained by the anomalous Nernst and Ettingshausen effects in magnetic materials, confirming the usefulness of SmCo₅/BST-based MCM.

Image not extracted

Figure 5. Finite element method simulations of thermoelectric power generation characteristics of MCM-based module. (a) 3D simulation results of the temperature distribution. (b) 3D simulation results of the electric potential distribution. (c) Experimental and simulated results of the ILI_{\mathrm{L}} dependence of VOV_{\mathrm{O}} and POP_{\mathrm{O}} at ΔT=405 ∘C\Delta T = 405\,^{\circ}\mathrm{C}. (d) Experimental and simulated results of the ILI_{\mathrm{L}} dependence of QCQ_{\mathrm{C}} and η\eta at ΔT=405 ∘C\Delta T = 405\,^{\circ}\mathrm{C}.

Trial for construction of larger-area modules

The construction of larger-area modules is important to obtain larger maximum output power and cooling performance. To demonstrate this, we fabricated a larger MCM-based module through the same procedures and performed the same evaluation of the power generation performance. The new module is composed of 40 SmCo₅/BST ATML elements and has an area of ~33 ×\times 31 mm. Therefore, under the same temperature gradient, we expected an output power about twice as great as that of the smaller module used in the above experiments. However, the maximum output power normalized by the square of the temperature gradient for the larger module was only ~1.2 times larger than that for the smaller one. This suggests that the performance degradation due to modularization imperfections becomes more pronounced in larger modules with the larger number of junctions, highlighting the importance of junction-less modules.

Conclusions

In this study, we evaluated the transverse thermoelectric power generation and cooling performances of a MCM-based thermopile module composed of SmCo5\mathrm{SmCo}_{5}/BST ATML having the experimentally determined figure of merit of 0.20 at room temperature. Although the performances were observed to be lower than expected from the material properties due to the modularization, our module showed excellent features as a transverse thermoelectric convertor in both power generation and cooling operations. To construct a large-area module with a higher output that fully utilizes the potential of MCM, it is essential to optimize electrodes and improve cutting and stacking accuracies of MCM elements. If these modularization techniques are established, MCM will bring innovation to the development of next-generation thermal management technologies.

Acknowledgements

The authors thank K. Suzuki, M. Isomura, H. Ohshima, and K. Aoyama for technical support.

Disclosure statement

The authors declare that they have no known competing financial interests or personal relationships that could have appeared to influence the work reported in this paper.

Funding

This work was supported by ERATO “Magnetic Thermal Management Materials” (No. JPMJER2201) from Japan Science and Technology (JST), Grants-in-Aid for Scientific Research (KAKENHI) (No. 24K17610) from Japan Society for the Promotion of Science (JSPS), and NEC Corporation.

Data availability statement

The data that support the findings of this study are available from the corresponding authors upon reasonable request.

References

  1. [1]Zebarjadi M, Esfarjani K, Dresselhaus MS, et al. Perspectives on thermoelectrics: from fundamentals to device applications. Energy Environ Sci. 2012;5:5147-5162.
  2. [2]Petsagkourakis I, Tybrandt K, Crispin X, et al. Thermoelectric materials and applications for energy harvesting power generation. Sci Technol Adv Mater. 2018;19:836-862.DOI
  3. [3]Mizuguchi M, Nakatsuji S. Energy-harvesting materials based on the anomalous Nernst effect. Sci Technol Adv Mater. 2019;20:262-275.DOI
  4. [4]Uchida K, Zhou W, Sakuraba Y. Transverse thermoelectric generation using magnetic materials. Appl Phys Lett. 2021;118:140504.DOI
  5. [5]Boona SR, Jin H, Watzman S. Transverse thermal energy conversion using spin and topological structures. J Appl Phys. 2021;130;171101.DOI
  6. [6]Uchida K, Heremans JP. Thermoelectrics: from longitudinal to transverse. Joule 2022;6;2240-2245.DOI
  7. [7]Zhou C, Birner S, Tang Y, et al. Driving perpendicular heat flow: (p × n)-type transverse thermoelectrics for microscale and cryogenic Peltier cooling. Phys Rev Lett. 2013;110;227701.pubmed.ncbi.nlm.nih.gov/23767747
  8. [8]Tang Y, Cui B, Zhou C, et al. p × n-type transverse thermoelectrics: a novel type of thermal management material. J Electron Mater. 2015;44;2095-2104.
  9. [9]He B, Wang Y, Arguilla MQ, et al. The Fermi surface geometrical origin of axis-dependent conduction polarity in layered materials. Nat Mater. 2019;18;568-572.DOI
  10. [10]Scudder MR, He B, Wang Y, et al. Highly efficient transverse thermoelectric devices with Re₄Si₇ crystals. Energy Environ Sci. 2021;14;4009-4017.
  11. [11]Scudder MR, Koster KG, Heremans JP, et al. Adiabatic and isothermal configurations for Re₄Si₇ transverse thermoelectric power generators. Appl Phys Rev. 2022;9;021420.DOI
  12. [12]McAfee K, Sunderland PB, Rabin O. A heat flux sensor leveraging the transverse Seebeck effect in elemental antimony. Sens Actuators A: Phys. 2023;363;114729.DOI
  13. [13]Goto Y, Usui H, Murata M, et al., Band anisotropy generates axis-dependent conduction polarity of Mg₃Sb₂ and Mg₃Bi₂. Chem Mater. 2024;36;2018-2026.
  14. [14]Manako H, Ohsumi S, Sato YJ, et al., Large transverse thermoelectric effect induced by the mixed-dimensionality of Fermi surfaces. Nat Commun. 2024;15;3907.DOI
  15. [15]Zahner Th, Förg R, Lengfellner H. Transverse thermoelectric response of a tilted metallic multilayer structure. Appl Phys Lett. 1998;73;1364-1366.DOI
  16. [16]Kanno T, Yotsuhashi S, Sakai A, et al. Enhancement of transverse thermoelectric power factor in tilted Bi/Cu multilayer. Appl Phys Lett. 2009;94;061917.DOI
  17. [17]Goldsmid HJ. Application of the transverse thermoelectric effects. J Electron Mater. 2011;40;1254-1259.DOI
  18. [18]Kanno T, Sakai A, Takahashi K, et al. Tailoring effective thermoelectric tensors and high-density power generation in a tubular Bi₀.₅Sb₁.₅Te₃/Ni composite with cylindrical anisotropy. Appl Phys Lett. 2012;101;011906.DOI
  19. [19]Mu X, Zhou H, Zhao W, et al. High-performance YbAl₃/Bi₀.₅Sb₁.₅Te₃ artificially tilted multilayer thermoelectric devices via material genome engineering method. J Power Sources. 2019;430;193-200.DOI
  20. [20]Zhou H, Liu H, Qian G, et al. Geometrical optimization and transverse thermoelectric performances of Fe/Bi₂Te₂.₇Se₀.₃ artificially tilted multilayer thermoelectric devices. Micromachines. 2022;13;233.DOI
  21. [21]Yue K, Zhu W, He Q, et al. High transverse thermoelectric performance and interfacial stability of Co/Bi₀.5Sb₁.5Te₃ artificially tilted multilayer thermoelectric devices. ACS Appl Mater Interfaces, 2022;14;39053-39061.
  22. [22]Zhu W, Zhou H, Wei P, et al. High-throughput optimization and fabrication of Bi₂Te₂.₇Se₀.₃-based artificially tilted multilayer thermoelectric devices. J Eur Ceram Soc. 2022;42:3913-3919.DOI
  23. [23]Uchida K, Hirai T, Ando F, et al. Hybrid transverse magneto-thermoelectric cooling in artificially tilted multilayers. Adv Energy Mater. 2024;14:2302375.DOI
  24. [24]Hirai T, Ando F, Sepehri-Amin H, et al. Hybridizing anomalous Nernst effect in artificially tilted multilayer based on magnetic topological material. Nat Commun. 2024;15:9643.DOI
  25. [25]Ando F, Hirai T, Alasli A, et al. Multifunctional composite magnet realizing record-high transverse thermoelectric generation. Energy Environ Sci. 2025;18:4068-4079.DOI
  26. [26]Ohta M, Jood P, Murata M, et al. An integrated approach to thermoelectrics: combining phonon dynamics, nanoengineering, novel materials development, module fabrication, and metrology. Adv Energy Mater. 2018;9:1801304.DOI
  27. [27]Wang H, Mccarty R, Salvador J R, et al. Determination of thermoelectric module efficiency: A survey. J Electron Mater. 2014;43:2274-2286.DOI
  28. [28]Ziolkowski P, Chetty R, Blaschkewitz P, et al. Interlaboratory testing for high-temperature power generation characteristics of a Ni-based alloy thermoelectric module. Energy Technology, 2020;8:2000557.DOI
  29. [29]KELK Ltd., Products information on thermo generation module, https://www.kelk.co.jp/english/generation/index.html.
  30. [30]Coherent Corp., Thermoelectric Generator (TEG) Modules, https://ii-vi.com/product/thermoelectric-generator-tegmodules/.
  31. [31]Ferrotec Materials Technologies Corp., Power Generation Thermo-electric Modules, https://ftmt.co.jp/en/product/electronic_device/thermo/power_generation/.
  32. [32]Skomedal G, Holmgren L, Middleton H, et al. Design, assembly and characterization of silicide-based thermoelectric modules. Energy Convers. Manag. 2016;110:13-21.DOI
  33. [33]Hao F, Qiu P, Tang Y, et al. High efficiency Bi₂Te₃-based materials and devices for thermoelectric power generation between 100 and 300 °C. Energy Environ. Sci. 2016;9:3120-3127.
  34. [34]Zong P, Hanus R, Dylla M, et al. Skutterudite with graphene-modified grain-boundary complexion enhances zT enabling high-efficiency thermoelectric device. Energy Environ. Sci. 2017;10:183-191.DOI
  35. [35]Deng R, Su X, Hao S, et al. High thermoelectric performance in Bi₀.₄₆Sb₁.₅₄Te₃ nanostructured with ZnTe. Energy Environ. Sci. 2018;11:1520-1535.
  36. [36]Yu J, Xing Y, Hu C, et al. Half-Heusler thermoelectric module with high conversion efficiency and high power density. Adv. Energy Mater. 2020;10:2000888.DOI
  37. [37]Xing Y, Liu R, Liao J, et al. A device-to-material strategy guiding the “double-high” thermoelectric module. Joule 2020;4:2475-2483.
  38. [38]Liu Z, Sato N, Gao W, et al. Demonstration of ultrahigh thermoelectric efficiency of ~7.3% in Mg₃Sb₂/MgAgSb module for low-temperature energy harvesting. Joule 2021;5;1196-1208.DOI
  39. [39]Jia B, Huang Y, Wang Y, et al. Realizing high thermoelectric performance in non-nanostructured n-type PbTe. Energy Environ. Sci., 2022;15;1920-1929.DOI
  40. [40]Jiang B, Wang W, Liu S, et al. High figure-of-merit and power generation in high-entropy GeTe-based thermoelectrics. Science 2022;377:208-213.DOI
  41. [41]Ando F, Tamaki H, Matsumura Y, et al. Dual-boost thermoelectric power generation in a GeTe/Mg₃Sb₂-based module. Mater. Today Phys. 2023;36;101156.DOI
  42. [42]Ando F, Hirai T, Adachi H, et al. Adiabatic transverse thermoelectric conversion enhanced by heat current manipulation in artificially tilted multilayers. Phys. Rev. Appl. (accepted). doi: 10.1103/gqvy-p5p1
  43. [43]Kyarad A, Lengfellner H. Transverse Peltier effect in tilted Pb-Bi₂Te₃ multilayer structures. 2006;89;192103.DOI
  44. [44]O'Brien BJ, Wallace CS. Ettingshausen effect and thermomagnetic cooling. J Appl Phys. 1958;29;1010-1012.
  45. [45]Harman TC. Theory of the infinite stage Nernst-Ettingshausen refrigerator. Adv Energy Conversion. 1963;3;667-676.DOI
  46. [46]Polash MMH, Vashaee D. Infinite-stage Nernst-Ettingshausen cryocooler for practical applications. 2021;15;014011.DOI
  47. [47]Harman TC, Honig JM. Thermoelectric and thermomagnetic effects and applications (McGraw-Hill, New York, 1967).
  48. [48]Kooi CF, Horst RB, Cuff KF, et al. Theory of the longitudinally isothermal Ettingshausen cooler. J Appl Phys. 1963;34:1735-1742.DOI

Paper details

vlnc:W_47qat7e6
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents