Resonant inter-mode second harmonic generation by backward spin waves in YIG nano-waveguides

Abstract

We experimentally study nonlinear generation of the second harmonic by backward volume spin waves propagating in microscopic magnonic waveguides fabricated from a low-loss magnetic insulator with a thickness of several tens of nanometers. We show that highly efficient resonant second harmonic generation is possible in the inter-mode regime at microwave powers of the order of 10^-4 W. In contrast to previously observed second harmonic generation processes, the generation by backward waves is characterized by the nonlinearly generated waves propagating opposite to the initial waves, and can be realized at zero bias magnetic field.

‡: authors that contributed equally to the work

One of the most important and practical advantages of large-amplitude spin-wave dynamics, which is not available in the small-amplitude linear propagation regime, is the possibility to nonlinearly generate spin waves with frequencies and wavelengths different from those of the initially excited wave[1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16]. This possibility can be used, for example, to excite waves that are difficult to generate directly using a linear excitation mechanism due to their short wavelengths[9, 14, 16], to perform frequency up- and down-conversion of signals[2, 3, 4, 5, 6, 7, 8, 13], as well as for amplitude- and phase-shaping of spin-wave pulses[1, 10]. In addition to these traditional signal-processing applications, nonlinear coupling of spin-wave modes at different frequencies has also been shown to enable the implementation of systems capable of neuromorphic-like computing[12].

Processes leading to nonlinear generation of additional spectral components can be described in terms of three- and four-magnon interactions[17]. For these interactions to be efficient, the conservation of energy and momentum for interacting magnons must be satisfied simultaneously. Due to this strict constraint, the peculiar characteristics of magnon dispersion are essential to achieve efficient resonant nonlinear generation. One of the important examples is the generation of the second harmonic by propagating spin waves[2, 3, 4, 5, 6, 7, 8]. Because of the nonlinear dependence of the frequency of spin waves on their wavenumber, it is generally difficult to achieve resonant conditions for magnons with frequencies that differ by a factor of two. Recently it was shown that this can be accomplished using an inter-mode interaction process in microscopic waveguides with an engineered dispersion spectrum[14].

In this Letter, we experimentally study the inter-mode resonant second harmonic generation for spin waves propagating in yttrium-iron-garnet (YIG) nano-waveguides, where the static magnetization is oriented parallel to the waveguide axis. This configuration is particularly promising for technical applications because it establishes a way for magnonic circuits to operate under small[18] or even zero[19, 20] bias magnetic field. We show that, in YIG waveguides with a thickness of several tens of nanometers, efficient resonant second-harmonic generation can be achieved for the above geometry, corresponding to backward-volume spin waves. Due to the backward dispersion of these waves, the second-harmonic wave propagates in the direction opposite to the direction of the initial wave. This results in a maximization of the intensity of the second-harmonic wave near the spatial position where the initial wave is excited, in stark contrast with waves with forward dispersion that exhibit a gradual increase in the intensity of the second harmonic along the propagation distance. This feature can be used to control the propagation direction of the second-harmonic wave by simply changing the direction of the bias magnetic field. We also show that by varying the thickness of the waveguide, one can achieve resonant second-harmonic generation conditions at zero bias magnetic field, which paves the way for implementation of nonlinear magnonic devices and circuits that do not require a bias magnetic field for their operation.

In Figure 1, we show the schematics of the experiment. We study the generation of the second harmonic by spin waves propagating in a 500 nm wide waveguide fabricated by electron-beam lithography and lift-off technique from an 80 nm thick YIG film deposited using pulsed-laser deposition[21]. The spin waves are excited using an inductive Au antenna that is 500 nm wide and 200 nm thick. The waveguide is magnetized by a static magnetic field HH applied parallel to its axis. Therefore, the excited spin waves propagate along the direction of the static magnetization. This corresponds to the case of the so-called backward-volume spin waves (BVSW)[17] known for their peculiar dispersion relation, which will be discussed below.

Schematics of the experiment

Figure 1. Schematics of the experiment.

We study the propagation of the excited spin waves and the generation of the second harmonic using micro-focus Brillouin light scattering (BLS) spectroscopy[22]. We focus the probing laser light with a wavelength of 473 nm into a diffraction-limited spot on the surface of the YIG film (see Figure 1) and analyze the modulation of this light due to its inelastic scattering from spin waves. The BLS intensity is proportional to the intensity of the spin wave at the position of the laser spot, which enables one to analyze the propagation of spin waves with sub-micrometer spatial resolution. Thanks to the frequency resolution of the technique, the initial spin wave and the nonlinearly generated second harmonic can be observed independently. Additionally, by using the interference of scattered light with light modulated at the frequency of spin waves, we can also resolve the phase of spin waves. This allows us to directly measure the dispersion relations of the waves under study[22].

Figure 2 shows the dispersion relations obtained from the experiment (diamonds) and from micromagnetic simulations (solid curves) at H=300H = 300 Oe. The calculations are performed using the simulation package mumax3[23] and the method described in detail in Ref. 24. In the calculations, we use the standard for YIG saturation magnetization, 4πMs=17504\pi M_s = 1750 G and the nominal YIG thickness of 80 nm. The width of the waveguide ww is used as an adjustable parameter. The best agreement with the experimental data is achieved for w=480w = 480 nm, which is very close to the nominal value of 500 nm. The dispersion relation f0(k)f_0(k) corresponds to the fundamental mode of the waveguide characterized by a uniform distribution of the dynamic magnetization through the thickness of the film and the relation f1(k)f_1(k) corresponds to the first-order thickness mode characterized by a non-uniform thickness distribution (see the insets in Figure 2).

Dispersion spectrum of spin waves in the studied waveguides

Figure 2. Dispersion spectrum of spin waves in the studied waveguides. Diamonds show the experimental data. Curves labeled f0(k)f_0(k) and f1(k)f_1(k) show dispersion relations for the fundamental and the first-order thickness mode, respectively, obtained from the micromagnetic simulations. Insets schematically show the distributions of the dynamic magnetization for the two modes. Circles mark the spin-wave states, for which resonant conditions for the second harmonic generation are satisfied. The data are obtained at H=300H = 300 Oe.

As seen from Figure 2, the dispersion curve of the fundamental mode exhibits behaviors typical for BVSW – the frequency of the wave decreases with increasing wavenumber kk (often referred to as backward dispersion). This dispersion leads to opposite signs of the phase velocity vp=2πfkv_p = 2\pi\frac{f}{k} and the group velocity vg=2πdfdkv_g = 2\pi\frac{df}{dk}. In practice, this means that a wave propagating away from the antenna in the positive direction of the zz-axis has a wavevector oriented in the negative direction, i.e., towards the antenna. In most cases, this feature of BVSW does not play a decisive role. However, as will be shown below, it has a crucial impact on the relevant process of resonant second harmonic generation.

In terms of magnon interactions, the process of second-harmonic generation can be considered as the confluence of two magnons of the initially excited spin wave into a magnon of doubled energy (frequency), as required by the energy conservation law. Simultaneously, to conserve the linear momentum, the wavevector of the new magnon must be twice as large as the wavevector of the initial magnons. Accordingly, efficient generation of the second harmonic can be achieved only if the magnon states with the combination of wavenumber and frequency (k,f)(k,f) and (2k,2f)(2k,2f) belong to the resonant spectrum of spin waves.

To find out whether this condition can be satisfied for BVSW, we plot in Figure 2 function 2f0(2k)2f_0(2k) (dashed curve) and find its intersections with the dispersion curves of spin-wave modes. As seen from Figure 2, the curve 2f0(2k)2f_0(2k) does not intersect the dispersion curve of the fundamental mode f0(k)f_0(k) anywhere. However, it intersects the dispersion curve of the first-order thickness mode f1(k)f_1(k) at the point marked by a solid circle. This indicates that the resonant phase-matched generation of the second harmonic by BVSW is possible in the inter-mode regime (dashed arrow in Figure 2): a fundamental-mode spin wave with frequency frf_\mathrm{r} and wavenumber krk_\mathrm{r} (open circle in Figure 2) can resonantly generate a second-harmonic spin wave with frequency 2fr2f_\mathrm{r} and wavenumber 2kr2k_\mathrm{r}, which belongs to the first-order thickness mode.

We emphasize that in the case of BVSW, the resonant second harmonic generation has rather unusual features. As seen from Figure 2, in contrast to the dispersion curve of the fundamental mode f0(k)f_0(k), the dispersion curve f1(k)f_1(k) exhibits a positive slope. Due to the positive slope, for this mode, the direction of the group velocity coincides with the direction of the phase velocity, i.e., the direction of the energy flow coincides with the direction of the wavevector. Since, as discussed above, the initial BVSW transferring energy in the positive zz-direction possesses a negative wavenumber kr<0k_\mathrm{r}<0, the second harmonic possesses a negative wavenumber 2kr<02k_\mathrm{r}<0, as well. For this wave, this corresponds to an energy transfer in the negative direction of the zz axis, i.e., towards the antenna, as schematically shown in Figure 1.

Figures 3(a) and 3(b) present experimental evidence for the resonant second harmonic generation described above. In these experiments, we place the probing laser spot on the axis of the waveguide at a distance z=1 μmz=1\,\mu\mathrm{m} from the center of the antenna and measure the BLS spectra as a function of the excitation frequency fef_\mathrm{e}. The power of the excitation signal is fixed at Pe=0.05P_e = 0.05 mW. As seen from Figure 3a, we detect linear excitation of spin waves (f=fef = f_e) in the frequency range of 2.4–2.8 GHz, which corresponds to the frequency band of BVSW (Figure 2). In addition to the signal at frequency f=fef = f_e, we also observe an intense spectral peak at f=2fef = 2f_e, when the excitation frequency is close to 2.57 GHz (horizontal dashed line in Figure 3a). This frequency corresponds to the spectral state (kr,frk_r, f_r) in Figure 2, for which the conservation conditions are satisfied. Note that at all other frequencies, the BLS intensity at f=2fef = 2f_e remains negligible. This indicates that the generation of the second harmonic has a well-pronounced resonant character and becomes highly efficient only when the conservation conditions are met.

Figure 3(b) shows the BLS spectrum recorded at fe=2.57f_e = 2.57 GHz (section of Figure 3a along the horizontal dashed line). As seen from these data, the detected BLS intensity from the second harmonic significantly exceeds the BLS intensity from the initial wave, which reflects the high efficiency of the resonant process.

Figure 3(c) shows the BLS intensities from the second harmonic and the initial wave as a function of the excitation power PeP_e recorded at fe=2.57f_e = 2.57 GHz. These data show that the ratio of the two intensities increases with increasing power, reaching more than a factor of five at Pe=0.2P_e = 0.2 mW. In other words, an increase in PeP_e leads to an increase in the efficiency of the second harmonic generation process. As seen from Figure 3c, the intensity of the second harmonic starts to saturate at Pe>0.15P_e > 0.15 mW. This is likely due to an onset of parasitic nonlinear damping associated with four-magnon scattering of the initial wave into short-wavelength spin-wave states that cannot be detected by BLS[25, 26, 27]. This assumption is consistent with the observed power dependence of the intensity of the initial wave recorded near the antenna (squares in Figure 3c). The dependence is linear at small powers and starts to saturate at Pe>0.15P_e > 0.15 mW. This indicates that at Pe>0.15P_e > 0.15 mW, the efficiency of the excitation by the antenna starts to decrease, which is a clear signature of the onset of nonlinear damping. Note that, in contrast to four-magnon scattering processes, which become active when the intensity of the spin wave exceeds a certain threshold, the second harmonic generation is a threshold-less phenomenon, which is present at any intensity. Therefore, by setting the excitation power slightly below the threshold of the nonlinear scattering, one can achieve optimal energy efficiency of the process.

We now turn to the analysis of the spatial dependences of the intensities of the initial wave and the second harmonic. Figure 4 shows these dependences recorded at fe=2.57f_e = 2.57 GHz and Pe=0.05P_e = 0.05 mW. As seen from these data, the initial wave shows a well-defined exponential decrease with the distance from the antenna ∼exp⁡(−2z/ξ)\sim\exp(-2z/\xi), where ξ\xi is the propagation length (note the logarithmic scale of the vertical axis). This exponential decay is observed over the entire range Pe=0.01−0.2P_e = 0.01 - 0.2 mW, although the propagation length strongly decreases with the increase in PeP_e (Figure 4(b)). Note that this decrease is pronounced even at Pe<0.15P_e < 0.15 mW, i.e., it is not dominated by the nonlinear damping due to four-magnon scattering. We attribute these behaviors to an increase in the efficiency of the second-harmonic generation (Figure 3c), which results in faster energy transfer from the initial wave to the second harmonic and leads to faster spatial decay of the former.

Spatial dependences of the intensities of the initial wave and the second harmonic, and power dependence of the propagation length of the initial wave

Figure 4. (a) Spatial dependences of the intensities of the initial wave and the second harmonic. Line shows an exponential fit of the data for the initial wave (note the logarithmic scale of the vertical axis). (b) Power dependence of the propagation length of the initial wave. Symbols show the experimental data. Curve is a guide for the eye. The data are obtained at HH = 300 Oe.

Similar to the initial wave, the intensity of the second harmonic also exhibits a decrease with distance from the antenna (albeit it is clearly non-exponential). We emphasize that this is a non-trivial observation. For optical waves[28] as well as for spin waves possessing forward dispersion[14], the intensity of the second harmonic typically increases with the propagation distance, which is a natural result of the continuous resonant energy transfer between the initial wave and the co-propagating second harmonic. However, as discussed above, in the case of BVSW, the direction of the energy flow for the second harmonic is opposite to that of the initial wave. As a result of this opposite flow of energy, the intensity of the second harmonic maximizes close to the input antenna. This interpretation is also supported by the intensity oscillations observed near the antenna (z=1z = 1-5 μ\mum). We associate these oscillations with the interference of two counterpropagating second-harmonic waves generated to the left and right of the antenna.

Finally, we analyze the controllability of the second harmonic generation by the static magnetic field. We perform measurement similar to those characterized in Figure 3a at HH varying from 200 to 400 Oe and determine the resonant frequency frf_r for each field value. Additionally, from phase-resolved measurements at frf_r, we find the wavelength of BVSW corresponding to the resonant conditions. As seen from Figure 5(a), the resonant frequency increases with the increase in HH. This is expected, since the entire dispersion spectrum (Figure 2) shifts towards higher frequencies. Simultaneously, an increase in HH leads to a decrease in the resonant wavelength, which is caused by a relative shift of the 2f0(2k)2f_0(2k) curve with respect to the f1(k)f_1(k) curve. Due to this shift, the intersection point (filled circle in Figure 2) moves towards larger kk (smaller wavelengths), as the field increases. Note, that the resonant condition can be satisfied at any field H>Hmin⁡H > H_{\min}, where Hmin⁡H_{\min} is determined by the condition 2f0(0)=f1(0)2f_0(0) = f_1(0) (intersection at k=0k = 0). Figure 5(b) shows the field dependences of 2f0(0)2f_0(0) and f1(0)f_1(0) obtained from micromagnetic simulations. These data show Hmin⁡=150H_{\min} = 150 Oe for the parameters used in our experiment. Because the frequencies of the first-order thickness mode strongly depend on the waveguide thickness, Hmin⁡H_{\min} can be further reduced by increasing the thickness, as shown in Figure 5(c). Note that for thicknesses >89> 89 nm, resonant generation of the second harmonic can also be realized for BVSW propagating at zero bias magnetic field[20].

Image not extracted

Figure 5. (a) Dependences of the resonant frequency and the resonant wavelength on the static magnetic field. Symbols show the experimental data. Curves are guides for the eye. (b) Field dependences of the frequencies 2f0(k=0)2f_0(k=0) and f1(k=0)f_1(k=0) obtained from micromagnetic simulations. Vertical dashed line marks the minimum static magnetic field Hmin⁡H_{\min}, at which the resonant conditions can be satisfied. (c) Dependence of the minimum field on the thickness of the waveguide obtained from micromagnetic simulations. Horizontal dashed line marks Hmin⁡=0H_{\min}=0. Curves in (b) and (c) are guides for the eye.

In conclusion, we have experimentally demonstrated highly efficient resonant generation of second harmonic by backward volume spin waves propagating in YIG nano-waveguides magnetized parallel to the axis. We have shown that the peculiar dispersion properties of these waves result in unusual features, such as the opposite propagation of the initial wave and the second harmonic wave. Together with the possibility to achieve resonant processes at zero bias magnetic field, this feature paves the way for the realization of highly flexible nonlinear spin-wave devices and circuits for advanced signal processing.

This work was supported by the Deutsche Forschungsgemeinschaft (DFG, German Research Foundation) – project number 529812702.

Image not extracted

(a)

Image not extracted

(b)

Image not extracted

(c)

Figure 3. (a) Color-coded map of the BLS intensity as a function of detection and excitation frequencies. Note the resonant excitation of the second harmonic close to fe=2.57f_{\mathrm{e}} = 2.57 GHz. (b) BLS spectrum recorded at the excitation frequency fe=2.57f_{\mathrm{e}} = 2.57 GHz (horizontal dashed line in (a)). The data are obtained at the power of the excitation signal Pe=0.05P_{\mathrm{e}} = 0.05 mW. (c) Intensities of the second harmonic and the initial wave as a function of the excitation power. The data are obtained at the excitation frequency fe=2.57f_{\mathrm{e}} = 2.57 GHz. Line is the linear fit of the experimental data for the initial wave at Pe<0.15P_{\mathrm{e}} < 0.15 mW. The data are obtained at H=500H = 500 Oe.

References

  1. [1]M. Wu and B. A. Kalinikos, “Coupled Modulational Instability of Copropagating Spin Waves in Magnetic Thin Films,” Phys. Rev. Lett. 101, 027206 (2008).pubmed.ncbi.nlm.nih.gov/18764225
  2. [2]V. E. Demidov, M. P. Kostylev, K. Rott, P. Krzysteczko, G. Reiss, and S. O. Demokritov, “Generation of the second harmonic by spin waves propagating in microscopic stripes,” Phys. Rev. B 83, 054408 (2011).DOI
  3. [3]J. Marsh, V. Zagorodnii, Z. Celinski, and R. E. Camley, “Nonlinearly generated harmonic signals in ultra-small waveguides with magnetic films: Tunable enhancements of 2nd and 4th harmonics,” Appl. Phys. Lett. 100, 102404 (2012).DOI
  4. [4]O. Rousseau, M. Yamada, K. Miura, S. Ogawa, and Y. Otani, “Propagation of nonlinearly generated harmonic spin waves in microscopic stripes,” J. Appl. Phys. 115, 053914 (2014).DOI
  5. [5]S. Wang, J. Ding, X. Guan, M. B. Jungfleisch, Z. Zhang, X. Wang, W. Gu, Y. Zhu, J. E. Pearson, X. Cheng, A. Hoffmann, and X. Miao, “Linear and nonlinear spin-wave dynamics in ultralow-damping microstructured Co2FeAl Heusler waveguide,” Appl. Phys. Lett. 113, 232404 (2018).DOI
  6. [6]H. J. J. Liu, G. A. Riley, C. L. Ordóñez-Romero, B. A. Kalinikos, and K. S. Buchanan, “Time-resolved study of nonlinear three-magnon processes in yttrium iron garnet films,” Phys. Rev. B 99, 024429 (2019).DOI
  7. [7]D. R. Rodrigues, J. Nothhelfer, M. Mohseni, R. Knapman, P. Pirro, and K. Everschor-Sitte, “Nonlinear Dynamics of Topological Ferromagnetic Textures for Frequency Multiplication,” Phys. Rev. Applied 16, 014020 (2021).DOI
  8. [8]F. Groß, M. Weigand, A. Gangwar, M. Werner, G. Schütz, E. J. Goering, C. H. Back, and J. Gräfe, “Imaging magnonic frequency multiplication in nanostructured antidot lattices,” Phys. Rev. B 106, 014426 (2022).
  9. [9]R. Dreyer, A. F. Schäffer, H. G. Bauer, N. Liebling, J. Berakdar, and G. Woltersdorf, “Imaging and phase-locking of non-linear spin waves,” Nat. Commun. 13, 4939 (2022).
  10. [10]H. Merbouche, B. Divinskiy, K. O. Nikolaev, C. Kaspar, W. H. P. Pernice, D. Gouéré, R. Lebrun, V. Cros, J. Ben Youssef, P. Bortolotti, A. Anane, S. O. Demokritov, and V. E. Demidov, “Giant nonlinear self-phase modulation of large-amplitude spin waves in microscopic YIG waveguides,” Sci. Rep. 12, 7246 (2022).DOI
  11. [11]T. Hache, L. Körber, T. Hula, K. Lenz, A. Kákay, O. Hellwig, J. Lindner, J. Fassbender, and H. Schultheiss, “Control of four-magnon scattering by pure spin current in a magnonic waveguide,” Phys. Rev. Applied 20, 014062 (2023).DOI
  12. [12]L. Körber, C. Heins, T. Hula, J.-V. Kim, S. Thlang, H. Schultheiss, J. Fassbender, and K. Schultheiss, “Pattern recognition in reciprocal space with a magnon-scattering reservoir,” Nat. Commun. 14, 3954 (2023).DOI
  13. [13]M. G. Copus, T. Hula, C. Heins, L. Flacke, M. Weiler, K. Schultheiss, H. Schultheiss, and R. E. Camley, “Generation of localized, half-frequency spin waves in micron sized ferromagnetic stripes: Experiments and simulations,” Appl. Phys. Lett. 124, 192401 (2024).DOI
  14. [14]K. O. Nikolaev, S. R. Lake, G. Schmidt, S. O. Demokritov, and V. E. Demidov, “Resonant generation of propagating second-harmonic spin waves in nano-waveguides,” Nat. Commun. 15, 1827 (2024).DOI
  15. [15]K. An, M. Xu, A. Mucchietto, C. Kim, K.-W. Moon, C. Hwang, and D. Grundler, “Emergent coherent modes in nonlinear magnonic waveguides detected at ultrahigh frequency resolution,” Nat. Comm. 15, 7302 (2024).DOI
  16. [16]K. O. Nikolaev, B. Das Mohapatra, G. Schmidt, S. O. Demokritov, and V. E. Demidov, “Spatially extended nonlinear generation of short-wavelength spin waves in yttrium iron garnet nanowaveguides,” Phys. Rev. Applied 22, 044083 (2024).DOI
  17. [17]A. G. Gurevich and G. A. Melkov, Magnetization Oscillations and Waves (CRC, New York, 1996).
  18. [18]Q. Wang, M. Kewenig, M. Schneider, R. Verba, F. Kohl, B. Heinz, M. Geilen, M. Mohseni, B. Lägel, F. Ciubotaru, C. Adelmann, C. Dubs, S. D. Cotofana, O. V. Dobrovolskiy, T. Brächer, P. Pirro, and A. V. Chumak, “A magnonic directional coupler for integrated magnonic half-adders,” Nat. Electr. 3, 765–774 (2020).DOI
  19. [19]Q. Wang, P. Pirro, R. Verba, A. Slavin, B. Hillebrands, A.V. Chumak, “Reconfigurable nanoscale spin-wave directional coupler,” Sci. Adv. 4, e1701517 (2018).DOI
  20. [20]K. O. Nikolaev, S. R. Lake, G. Schmidt, S. O. Demokritov, and V. E. Demidov, “Zero-Field Spin Waves in YIG Nanowaveguides,” Nano Lett. 23, 8719–8724 (2023).DOI
  21. [21]C. Hauser, T. Richter, N. Homonnay, C. Eisenschmidt, M. Qaid, H. Deniz, D. Hesse, M. Sawicki, S. G. Ebbinghaus, and G. Schmidt, “Yttrium iron garnet thin films with very low damping obtained by recrystallization of amorphous material,” Sci. Rep. 6, 20827 (2016).DOI
  22. [22]V. E. Demidov and S. O. Demokritov, “Magnonic waveguides studied by micro-focus Brillouin light scattering,” IEEE Trans. Mag. 51, 0800215 (2015).
  23. [23]A. Vansteenkiste, J. Leliaert, M. Dvornik, M. Helsen, F. Garcia-Sanchez, and B. Van Waeyenberge, “The design and verification of MuMax3,” AIP Adv. 4, 107133 (2014).DOI
  24. [25]M. M. Scott, C. E. Patton, M. P. Kostylev, and B. A. Kalinikos, “Nonlinear damping of high-power magnetostatic waves in yttrium–iron–garnet films,” J. Appl. Phys. 95, 6294 (2004).DOI
  25. [26]T. Hula, K. Schultheiss, A. Buzdakov, L. Körber, M. Bejarano, L. Flacke, L. Liensberger, M. Weiler, J. M. Shaw, H. T. Nembach, J. Fassbender, and H. Schultheiss, “Nonlinear losses in magnon transport due to four-magnon scattering,” Appl. Phys. Lett. 117, 042404 (2020).DOI
  26. [27]S. R. Lake, B. Divinskiy, G. Schmidt, S. O. Demokritov, and V. E. Demidov, “Interplay Between Nonlinear Spectral Shift and Nonlinear Damping of Spin Waves in Ultrathin Yttrium Iron Garnet Waveguides,” Phys. Rev. Appl. 17, 034010 (2022).DOI
  27. [28]R. W. Boyd, Nonlinear Optics. 4 Edition (Academic Press, London, 2020).

Paper details

vlnc:W_4gwyjff6
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents