betaFeedback

WorksPhysics and Astronomy

Excitonic effects in graphene-like C3_3N

Abstract

Monolayer C3_3N is an emerging two-dimensional indirect band gap semiconductor with interesting mechanical, thermal, and electronic properties. In this work we present a description of C3_3N electronic and dielectric properties, focusing on the so-called momentum-resolved exciton band structure. Excitation energies and oscillator strengths are computed in order to characterize bright and dark states, and discussed also with respect to the crystal symmetry. Activation of excitonic states is observed for finite transferred momenta: Indeed, we find an active indirect exciton at ∼\sim 0.9 eV, significantly lower than the direct optical gap of 1.96 eV, with excitonic binding energies in the range 0.6-0.9 eV for the lowest states. As for other 2D materials, we find a quasi-linear excitonic dispersion close to ΓΓ, which however shows a downward convexity related to the indirect band gap of C3_3N as well as to the dark nature of the involved excitons.

Introduction

Since the rise of graphene,[1, 2] two-dimensional (2D) materials attract ever increasing attention in materials science. The reduced dimensionality and high surface-volume ratio affect all the properties of these systems leading to unique features. For example, graphene is well known for its superior mechanical stability[3] and electron mobility,[4] relevant for applications in optoelectronics, sensing, mechanical and energy storage technologies.[5, 6, 7] However, graphene is a zero band-gap semimetal, which limits its real application in digital electronic devices that usually require a semiconducting character. Hence the great effort, from both theoretical and experimental communities, to find post-graphene layered materials with a finite band gap appropriate for the selected applications. The list of candidates is very large[8] and includes, among others, transition metal dichalcogenides,[9] phosphorene,[10] and hexagonal boron nitride.[11]

Carbon-nitrides CxNy\mathrm{C}_x\mathrm{N}_y (e.g. CN, C2N\mathrm{C}_2\mathrm{N}, C3N\mathrm{C}_3\mathrm{N}, or C3N4\mathrm{C}_3\mathrm{N}_4) are gaining significant attention in recent years.[12] These are metal-free carbon-based layered materials with comparable (or even superior) structural, chemical, and electronic properties with respect to graphene. While preserving structural affinities with graphene, they generally display a semiconducting behavior. One of the most studied materials in this class is graphitic-C3N4\mathrm{C}_3\mathrm{N}_4,[13] as its strong optical absorption in the visible makes it suitable for solar energy conversion and photocatalysis applications.[14] Recently, a new carbon nitride, C3N\mathrm{C}_3\mathrm{N} (structurally analogous to graphene and also known as 2D-polyaniline; see Figure 1), an indirect gap semiconductor, has been experimentally synthesized using different methods.[15, 16] Since then, several studies were undertaken to characterize it. Theoretical investigations have shown that monolayer C3N\mathrm{C}_3\mathrm{N} displays interesting features: remarkable mechanical properties, similar to graphene,[17, 18] high stability at room temperature and high thermal conductivity.[19, 20] Moreover, it seems a promising material for acting as an anode for Li-, Na-, and K-ion batteries.[21, 22, 23, 24] It was also studied in heterostructures with graphene,[18] C3B\mathrm{C}_3\mathrm{B},[25] and g-C3N4\mathrm{C}_3\mathrm{N}_4,[26] showing interesting properties for optoelectronic and electrochemical energy storage devices.

Lattice structure of C3N and Brillouin zone inset

Figure 1. Lattice structure of C3N\mathrm{C}_3\mathrm{N}, with the corresponding unit cell. Brown and grey spheres represent the C and N atoms respectively. Inset: Brillouin zone with the kk-path considered in this work.

Despite these interesting features, an extended characterization of excitations, including excitonic effects, in monolayer C3N\mathrm{C}_3\mathrm{N} is still lacking. This knowledge would be relevant when considering C3N\mathrm{C}_3\mathrm{N} for optoelectronic applications like photocatalysis, photodetection, solar cells, or light emitting diodes. Since the system is a 2D monolayer, the electronic screening is strongly reduced, implying that the enhanced electron-hole interaction typically leads to large excitonic binding energies (EBE) for all the relevant excitons. In a complementary direction, as discussed by Qiu et al. 27 and Cudazzo et al. 28, the study of the excitonic dispersion with respect to the transferred momentum q\mathbf{q} can give more information on the excitonic features, in particular for low-dimensional systems. Moreover, it may have implications in plasmon/phonon - exciton coupling phenomena and can help in the determination of the exciton propagation along the crystal, relevant for excitation energy transport in the material.[29] In this work we employ many-body perturbation theory methods in the GW approximation[30, 31] and the Bethe Salpeter equation (BSE)[32] to study C3_3N. In addition to a full characterization of the electronic and optical properties of this system, the excitonic band structure is computed in order to understand the exciton dispersion beyond the long wavelength limit. Specifically, momentum-dependent excitonic wavefunctions are also computed and discussed.

Methods

Ground state electronic structure properties were calculated in the framework of density functional theory (DFT), using a plane wave basis set and pseudopotential approach as implemented in the Quantum ESPRESSO package.[33, 34] We used optimized norm-conserving Vanderbilt (ONCV) pseudopotentials[35] to compute the relaxed structure and the corresponding Kohn-Sham (KS) single-particle energies and electronic density. The KS-DFT exchange-correlation functional was approximated using GGA-PBE.[36] The KS electronic structure was converged using a plane wave kinetic energy cutoff energy of 60 Ry to represent the wavefunctions, and a Monkhorst-Pack k-point grid of 8×8×18 \times8 \times1. We verified that a supercell with a vacuum of 15 Å along the vertical direction was enough to treat the system as 2D, avoiding spurious interactions between layers.

The KS energies are then corrected using many-body perturbation theory methods. In particular, we adopted the GW approximation[31] in the single shot G0W0G_0W_0 approach, and then computed the excitonic properties by solving the BSE.[32] GW and BSE calculations were performed using the Yambo code.[37, 38] In the GW approximation, the expectation values of the self-energy are written as:

Σnk(ω)=−i2π∫dω′ eiω′0+⟨nk∣G(ω+ω′)W(ω′)∣nk⟩(1)\Sigma_{n\mathbf{k}}(\omega)=-\frac{i}{2\pi}\int d\omega'\,e^{i\omega'0^{+}}\langle n\mathbf{k}|G(\omega+\omega')W(\omega')|n\mathbf{k}\rangle \tag*{(1)}

where GG is taken here as the Green’s function built on single particle KS orbitals (and their corresponding eigenvalues ϵnk\epsilon_{n\mathbf{k}}) and WW is the screened Coulomb interaction calculated in the random phase approximation (RPA) with the frequency dependence treated via the Godby-Needs plasmon-pole model.[39] Quasiparticle energies were then obtained by solving the linearized equation

Enkqp=ϵnk+Znk[Σnk(ϵnk)−vnkxc],(2)E^{\mathrm{qp}}_{n\mathbf{k}}=\epsilon_{n\mathbf{k}}+Z_{n\mathbf{k}}\left[\Sigma_{n\mathbf{k}}(\epsilon_{n\mathbf{k}})-v^{\mathrm{xc}}_{n\mathbf{k}}\right], \tag*{(2)}

where vnkxcv^{\mathrm{xc}}_{n\mathbf{k}} is the expectation value of the exchange-correlation potential over the nkn\mathbf{k} KS eigenvectors, and ZnkZ_{n\mathbf{k}} is the renormalization factor

Znk=[1−∂Σnk(ω)∂ω∣ω=ϵnk]−1.(3)Z_{n\mathbf{k}}=\left[1-\left.\frac{\partial\Sigma_{n\mathbf{k}}(\omega)}{\partial\omega}\right|_{\omega=\epsilon_{n\mathbf{k}}}\right]^{-1}. \tag*{(3)}

In all the calculations we used a truncated Coulomb potential[40] in order to avoid spurious interaction between repeated cells.

Converged quasiparticle energies were obtained using a kinetic energy cutoff of 10 Ry to represent the screening matrix, including 300 empty states in the sums over transitions and adopting a k-point grid of 30×30×130 \times30 \times1. Convergence on screening matrix cutoff and empty states is reached by means of automated workflows as implemented in the current version of the AiiDA-Yambo plugin[38] of the AiiDA software,[41] imposing a convergence threshold of 15 meV. More details on the convergence workflow are provided in the Supplemental Material.[42]

The quasiparticle energies were then inserted in the BSE. The excitonic Hamiltonian Hexc\mathrm{H}^{\mathrm{exc}} was built[31, 43] considering a transferred momentum q=kc−kv\mathbf{q}=\mathbf{k}_c-\mathbf{k}_v between valence and conduction states, and reads (in the resonant block):

⟨vck,q∣Hexc∣v′c′k′,q⟩=(Ec′k′qp−Ev′k′−qqp)δvv′δcc′δkk′+⟨vck,q∣v−W∣v′c′k′,q⟩(4)\langle v c \mathbf{k},\mathbf{q}|\mathrm{H}^{\mathrm{exc}}|v'c'\mathbf{k}',\mathbf{q}\rangle=\left(E^{\mathrm{qp}}_{c'\mathbf{k}'}-E^{\mathrm{qp}}_{v'\mathbf{k}'-\mathbf{q}}\right)\delta_{vv'}\delta_{cc'}\delta_{\mathbf{k}\mathbf{k}'}+\langle v c\mathbf{k},\mathbf{q}|v-W|v'c'\mathbf{k}',\mathbf{q}\rangle \tag*{(4)}

where ∣vck,q⟩≡∣c,k⟩⊗∣v,k−q⟩|vc\mathbf{k},\mathbf{q}\rangle\equiv|c,\mathbf{k}\rangle\otimes|v,\mathbf{k}-\mathbf{q}\rangle, ∣v,k−q⟩|v,\mathbf{k}-\mathbf{q}\rangle and ∣c,k⟩|c,\mathbf{k}\rangle being valence and conduction wave-functions, respectively. Concerning the kernel, WW and vv are the (screened) direct and (bare) exchange e–h interactions. The BSE can then be recast in the form of a two-particle eigenproblem for the excitonic eigenvalues ES(q)E^S(\mathbf{q}) and eigenstates ∣S,q⟩|S,\mathbf{q}\rangle:

Hexc(q)∣S,q⟩=ES(q)∣S,q⟩(5)\mathrm{H}^{\mathrm{exc}}(\mathbf{q})|S,\mathbf{q}\rangle=E^S(\mathbf{q})|S,\mathbf{q}\rangle \tag*{(5)}
∣S,q⟩=∑vc,kAvckS(q)∣vck,q⟩.(6)|S,\mathbf{q}\rangle=\sum_{vc,\mathbf{k}} A^S_{vc\mathbf{k}}(\mathbf{q})|vc\mathbf{k},\mathbf{q}\rangle. \tag*{(6)}

It is worth noticing that the q\mathbf{q} index makes the BSE block-diagonal: for different values of the transferred momentum we have different excitonic Hamiltonians Hexc(q)\mathrm{H}^{\mathrm{exc}}(\mathbf{q}). Then, the excitonic band structure is calculated by solving the eigenvalue problem in Eq. (5) for each q\mathbf{q} along a path. In this work the BSE was solved for several values of q\mathbf{q} along the Γ\Gamma-MM and Γ\Gamma-KK directions.

It is also possible to define the inverse macroscopic dielectric function (considering only resonant and anti-resonant parts of the Hexc\mathrm{H}^{\mathrm{exc}}) as:

ϵM−1(ω,q)=1+2VNqv(q)∑SΩS(q)[1ES(q)−(ω+iη)+1ES(q)+(ω+iη)].(7)\epsilon_M^{-1}(\omega,\mathbf{q})=1+\frac{2}{V N_{\mathbf{q}}}v(\mathbf{q})\sum_S\Omega^S(\mathbf{q})\left[\frac{1}{E^S(\mathbf{q})-(\omega+i\eta)}+\frac{1}{E^S(\mathbf{q})+(\omega+i\eta)}\right]. \tag*{(7)}

where VV is the volume of the unit cell and NqN_q is the number of points in the Brillouin zone (BZ) sampling. In the above equation, ΩS(q)\Omega^{S}(\mathbf{q}) are the generalized oscillator strengths, defined as:

ΩS(q)=∣∑vc,kAvc,kS(q)⟨v,k−q∣e−iq⋅r∣c,k⟩∣2.(8)\Omega^{S}(\mathbf{q}) = \left| \sum_{vc,\mathbf{k}} A^{S}_{vc,\mathbf{k}}(\mathbf{q}) \langle v,\mathbf{k}-\mathbf{q} | e^{-i\mathbf{q}\cdot\mathbf{r}} | c,\mathbf{k} \rangle\right|^{2}. \tag*{(8)}

Oscillator strengths are used to distinguish between active and inactive excitons (in the q=0\mathbf{q}=0 limit, in particular, to identify those that are dipole active/forbidden). Experimentally, excitonic effects are observed via photoabsorption spectroscopy in the optical limit of vanishing q\mathbf{q}, while non-vanishing momentum excitations are observed e.g. in electron energy loss spectroscopy (EELS) or non-resonant inelastic X-ray scattering (NRIXS) experiments, by measuring the loss function L(ω,q)L(\omega,\mathbf{q}).[31] The optical absorption and the loss function are related to the inverse of the macroscopic dielectric matrix ϵM−1(ω,q)\epsilon_{M}^{-1}(\omega,\mathbf{q}) by the relations:

Abs⁡(ω,q→0)=Im⁡[1ϵM(ω,q→0)],(9)\operatorname{Abs}(\omega,\mathbf{q}\to0)=\operatorname{Im}\left[\frac{1}{\epsilon_{M}(\omega,\mathbf{q}\to0)}\right], \tag*{(9)}
L(ω,q)=−Im⁡[ϵM−1(ω,q)].(10)L(\omega,\mathbf{q})=-\operatorname{Im}\left[\epsilon_{M}^{-1}(\omega,\mathbf{q})\right]. \tag*{(10)}

In EELS and NRIXS experiments, the measured quantity is the intensity of the scattered particles resolved with respect to the scattering angle and to the energy of the outgoing particles (either electrons or photons). This quantity, that is the differential cross-section d2σdΩdE\frac{d^{2}\sigma}{d\Omega dE} of the process, can be related to the loss function by the relation:[44, 45]

d2σdΩdE∼{q−2L(ω,q)EELS,q2L(ω,q)NRIXS.(11)\frac{d^{2}\sigma}{d\Omega dE}\sim \begin{cases} q^{-2}L(\omega,\mathbf{q}) & \text{EELS},\\ q^{2}L(\omega,\mathbf{q}) & \text{NRIXS}. \end{cases} \tag*{(11)}

Computationally, in order to converge BSE calculations for C3_3N, we used a k-point mesh of 64×64×164\times64\times1. To numerically represent and solve the eigenproblem of Eq. (4) we verified that three valence and three conduction bands are enough to obtain converged excitation energies for the first excitons within 10 meV.

Results and Discussion

Electronic properties. C3_3N has a honeycomb lattice, with a unit cell composed of 6 carbon and 2 nitrogen atoms, as shown in Figure 1. Like graphene, it assumes a planar and continuously bonded geometry, due to the character of the sp2sp^{2} hybridized orbitals. For monolayer C3_3N we find a relaxed lattice constant of 4.857 Å (using GGA-PBE). This result agrees well with previous DFT calculations (4.862 Å)[46] and is slightly larger than the experimental value (4.75 Å).[15] The KS band structure (Figure 2a) shows a Dirac cone at the KK point. Now, since

Orbital projected PBE and G₀W₀ band structures

Figure 2. a) Orbital projected PBE band structure. π\pi and π∗\pi^* bands are indicated in blue, σ∗\sigma^* as orange dots. b) G0_0W0_0 band structure (red); the corresponding PBE bands are reported again as dashed curves for reference. In both panels the zero of the energy scale is set at the top of the valence band for both PBE and G0_0W0_0 results.

C3_3N has two more electrons per unit cell than graphene, the level-filling goes up and the Dirac cone is no longer at the valence-band top. The calculated band gap is indirect (M→ΓM\to\Gamma) and amounts to 0.42 eV (at the GGA-PBE level). The direct gaps at Γ\Gamma and MM are 1.86 eV and 1.61 eV, respectively. Figure 2a highlights also the σ\sigma and π\pi character of the bands in the gap region, and we can observe that the top valence bands show π\pi symmetry as well as the two lowest conduction bands, whereas σ\sigma-like character is seen in the third and the fourth conduction bands (which start above ∼2\sim2 eV with respect to the top valence band).

The inclusion of GW corrections provides a gap opening of ∼1\sim1 eV, resulting in an indirect quasiparticle band gap of 1.42 eV (Figure 2b). The direct gaps at Γ\Gamma and MM are also increased to 2.96 and 2.67 eV, respectively, as summarized in Table I. The minimum direct gap is located in the middle of the Γ\Gamma-MM region of the BZ and has a value of 2.62 eV. The GW band gap is consistent with the one obtained in a recent work by Wu et al.,[47] calculated at the GW level using the Hybertsen-Louie generalized plasmon pole model,[48] and as expected is larger than that obtained directly with the HSE06 hybrid functional,[49] by ∼0.38\sim0.38 eV.[46] The C3_3N gap is narrower with respect to the two well-known carbon nitrides C3N4\mathrm{C}_{3}\mathrm{N}_{4} (∼4.24\sim4.24 eV for the triazine structure)[50] and C2_2N (∼3.75\sim3.75 eV)[51] single layers. This is consistent with the fact that C3_3N is continuously bonded, while the two other carbon nitrides have saturated porous structure resulting in electronic confinement.

gapsPBE (eV)G0_0W0_0 (eV)
M → Γ0.421.42
Γ → Γ1.862.96
M → M1.612.67

Table I. Indirect and direct energy gaps at high symmetry points obtained at PBE and G0_0W0_0 level.

Along the same BZ path, the C3_3N band structure calculated at GW level is qualitatively similar to the one calculated using PBE, as shown in Figure 2b. In fact, the GW gap is still indirect with the valence band maximum located at MM and the conduction band minimum at Γ\Gamma. We observe, anyhow, that the GW correction is not uniform across the bands, as different corrections apply due to wave functions with different character. Orbital-dependent GW corrections are a a well-known feature of GW already discussed in the literature.[52, 53] In particular, the corrections in the low conduction region are distinguished according to the different localization of the KS wavefunctions, as can be observed from Figure 3, where the GW energies are plotted against the respective KS eigenvalues.

Quasiparticle G₀W₀ energies versus Kohn–Sham PBE eigenvalues

Figure 3. Quasiparticle G0_0W0_0 energies vs. Kohn-Sham PBE eigenvalues. The top of the valence band is chosen as a common zero of the energy. The colours and the corresponding insets indicate the predominant π\pi, π∗\pi^* (blue) and σ∗\sigma^* (orange) character. In the conduction region, two branches result from the different localization of the π∗\pi^*- and σ∗\sigma^*-character states leading to different quasiparticle corrections.

A larger correction is observed for the bands with π∗\pi^{*} (blue dots) character with respect to bands having σ∗\sigma^{*} character (orange dots). Since the valence bands considered here only present a π\pi character (σ\sigma-states are deeper in energy), their GW correction shows a more common scissor/stretching behavior. We note that this picture allows us to include the GW correction (for instance in the BSE calculations) as a generalized scissor and stretching operator, taking into account different corrections according to the specific localization character of the KS-states.

Optical properties

The optical absorption, obtained from the q→0\mathbf{q} \to0 limit of the macroscopic dielectric response, according to Eq. (9), is shown in Figure 4. Excitonic effects were included by solving the BSE equation. All the excitation energies are plotted, together with the independent-particle onset, at EIP−GW=2.62E_{\mathrm{IP-GW}}=2.62 eV, indicated by the vertical red line. The absorption spectrum is dominated by a main peak at 1.96 eV, originated by the doubly-degenerate exciton E04,5E_0^{4,5}. At lower energies, three dark excitons are present, the lowest ones (1.82 eV, E01,2E_0^{1,2}) being also doubly-degenerate.

Calculated imaginary part of the macroscopic dielectric function in the optical limit

Figure 4. Calculated Im⁡(εM)\operatorname{Im}(\varepsilon_M) in the optical limit (q→0q \to0), in arbitrary units (arb. units). A Lorentzian broadening of 0.02 eV has been included. The dots indicate the amplitude of each excitonic state in the BSE solution. The vertical dashed red line represents the onset of the single quasiparticle continuum (minimum direct gap in the GW solution, 2.62 eV).

Both bright and dark excitons are strongly bound, displaying EBE of 0.93 eV and 0.66 eV, for E01,2E_0^{1,2} and E04,5E_0^{4,5}, respectively. The EBE are computed considering the difference between the excitation energy of the exciton and the average energy of the involved electron-hole transitions, as shown in the lower panel of Figure 5. Interestingly, the EBE of the lowest bright exciton E04,5E_0^{4,5} satisfies the scaling law EBE ∼14EIP−GW\sim\frac{1}{4}E_{\mathrm{IP-GW}}, found valid for 2D single-layered systems.[54, 55]

Excitonic probability distributions and electron-hole transition distributions

Figure 5. Upper panels: excitonic probability distribution for the dark E01,2E_0^{1,2} and the bright (1.96 eV, E04,5E_0^{4,5}) excitons at vanishing qq. The blue contours represent the probability of finding the electron (hole) when the hole (electron) is fixed on a N atom (yellow circle). Lower panels: distribution of the electron-hole transitions in the BZ for the corresponding excitons of the upper panels.

In order to analyze the spatial extension of the main excitons, we plot their excitonic wavefunction, by showing the electron spatial distribution for a fixed hole position. The upper panel of Figure 5 displays the excitonic wavefunction for the lowest (E01,2E_0^{1,2}) and the brightest (E04,5E_0^{4,5}) direct excitons, with the hole placed on a N site. Both excitons show a 3-fold rotational plus a reflection symmetry with respect to the axis in the armchair direction. Interestingly, these excitons are localized on benzene rings, avoiding the N atoms. We observe that the dark excitons (lower energy) are strongly localized around the hole, while the active ones (higher energy) are more delocalized. We can explain the different spatial localization in terms of the single particle transitions that contribute to the excitations, as represented in the lower panels of Figure 5. The first excitons E01,2E_0^{1,2} are built from electron-hole transitions belonging to a larger region of the Brillouin zone with respect to E04,5E_0^{4,5}, resulting in a larger confinement in real space. Similarly to the fundamental gap, the optical gap of C3_3N is also smaller than the ones calculated for g-C3_3N4_4 and C2_2N (by about ∼\sim2 eV and ∼\sim1 eV,[51] respectively, by considering the first bright excitons), which is consistent with a picture where the presence of saturated pores in each layer of the structure induces wavefunction localization and quantum confinement.

Indirect excitons. Besides the optical absorption limit, our understanding of electron-hole excitations in C3_3N is further enhanced by inspecting the excitonic spectrum over a wider range of transferred momenta q=kelec−khole\mathbf{q}=\mathbf{k}_{\mathrm{elec}}-\mathbf{k}_{\mathrm{hole}}, providing us with the exciton dispersion in momentum space. Indeed, the excitonic dispersion was recently proposed[28] as a powerful tool to distinguish excitons of different character in low-dimensional systems, going beyond the mere evaluation of the EBE.

The solution of the BSE for finite qq then allows us to fully characterize the C3N excitations accessible by means of momentum-resolved electron energy loss spectroscopy or non-resonant inelastic X-ray scattering. Figure 6 shows the loss function calculated for different transferred momenta qq along the Γ−M\Gamma- M path. To compare spectra at

Loss function for different values of the transferred momentum

Figure 6. Loss function for different values of the transferred momentum along the direction Γ\Gamma-MM, starting from the lowest q=M/32q = M/32 (light blue), to the highest q=Mq = M (dark blue). Following Cudazzo et al.[28], we multiplied all spectra by the corresponding q2q^2. This is needed in order to enhance higher momentum spectra and physically motivated by the form of the NRIXS cross section (as discussed in Sec. II).

different momentum, we multiplied the loss function by a q2q^2 factor. While making the plot more readable, this factor is also experimentally motivated by the form of the NRIXS cross section, as discussed in the theory section.

We observe that the low-energy peak goes down in energy for qq moving away from Γ\Gamma, as expected for an indirect gap system. This indicates the presence of a dispersive excitonic band reaching a minimum of ∼0.8\sim0.8 eV at q=Mq = M in correspondence of the indirect gap.

To complement the information provided by the loss spectra, in Figure 7a we present the calculated qq-resolved exciton band structure. A color map is added to indicate the (generalized) amplitude/strength of each excitonic state, actually offering richer information complementary to the loss spectrum. The lowest degenerate exciton E01,2E_0^{1,2} at Γ\Gamma splits into two excitonic bands that we call Eq1E_q^1 and Eq2E_q^2. For both Γ−M\Gamma- M and Γ−K\Gamma- K directions, we observe that the lowest excitons present quadratic and almost linear dispersions in the neighborhood of the Γ\Gamma point, as also found for other 2D systems.[27, 28, 56] Nevertheless, at variance with what reported in the work of Qiu et al.[27] for the direct gap MoS2_2 monolayer, here we find a lower band with quasi-linear dependence on ∣q∣|q| and an upper band with a clear parabolic dispersion, both with a negative slope and concavity. Such a behavior is due to the indirect nature of the gap, and we note that – at difference with other 2D materials such as MoS2_2 and phosphorene[29]– in the case of C3N we do not observe a non-analytical dispersion for the lowest bands. This is related to the fact that the E01,2E_0^{1,2} excitons are dark, making the exchange contribution to the dispersion negligible. Moreover, the observed down-ward quasi-linear behavior can be seen to be connected to the independent-particle contribution to the excitonic Hamiltonian, as shown in Figure S2 in the Supplemental Material.[42]

Momentum-resolved exciton band structure and exciton probability distributions

Figure 7. (a) Momentum-resolved exciton band structure for the lowest seven excitons. Excitonic amplitudes are normalized with respect to the brightest exciton among all the bands for each momenta from dark violet to yellow (active exciton). Inset: focus on the region near the q=0q=0 for the two lowest excitonic bands. (b) Exciton probability distribution for Eq1E^{1}_{q} (top) and Eq2E^{2}_{q} (bottom), at q=Mq=M. The vertical solid line denotes the symmetry plane perpendicular to the figure and the hole position is indicated in yellow near the center of the figures.

Comparison between independent particle and proper excitonic transition energies

Figure S2. Comparison between independent particle (IP) transition energies (red) and proper excitonic energies (black) for the two lowest excitonic bands. The IP energies are shifted in order to match the excitonic energies at the Γ\Gamma point. We can observe that the negative concavity and the linearity of the lowest excitonic bands are effects already included in the IP dispersion. ⟨IP⟩\langle\mathrm{IP}\rangle and BSE points are aligned at q=0q = 0 by including a shift ΔBSE0=−0.93\Delta\mathrm{BSE}_0=-0.93 eV.

Moreover, the Γ−M\Gamma-M direction is of special interest, since it corresponds to q-vector involved in the indirect band gap: the most relevant excitonic transitions occur in that zone, and the decrease of excitation energies going from Γ\Gamma to MM reflects the indirect gap of C3_3N. From Figure 7a we observe that the lowest exciton (Eq1E^{1}_{q}) is inactive, with an energy minimum of 0.8 eV at q=Mq=M. For this momentum, the immediately higher-energy exciton (0.9 eV, Eq2E^{2}_{q}) is active. Concerning the Γ\Gamma-KK path, we observe a minimum near K/2K/2 that corresponds to an inactive state of energy ∼1.3\sim1.3 eV. We find that EBE range from 0.6 eV to 0.93 eV for the lowest excitonic band in the Γ\Gamma-MM direction (Eq1,2E^{1,2}_{q}). As we move out of the long-wavelength regime and choose given directions of the center-of-mass momentum qq, we expect some symmetries in the excitonic wavefunctions, like the 3-fold rotational invariance observed in the plots of Figure 5, to break. Figure 7b shows the square modulus of exciton wavefunctions (Eq1E^{1}_{q} and Eq2E^{2}_{q}) at q=Mq=M, corresponding to minima in the band structure of Figure 7a. As before, the hole is placed on a nitrogen atom. The 3-fold rotational

symmetry is no longer present, and only the reflection invariance with respect to the armchair direction is maintained. Both Eq1E^{1}_{q} and Eq2E^{2}_{q} excitons are delocalized along the zig-zag direction. For the inactive excitons the symmetry axis lies on a nodal plane, where the probability amplitude of finding electrons vanishes. The spatial delocalization increases with qq and is higher for the indirect active exciton Eq2E^{2}_{q}, as happens for the bright excitons in the optical limit case. The behaviour of the excitonic wavefunction of C3_3N is very similar to that observed in hBN by Sponza et al.⁵⁶. This is because, along the armchair direction, both systems present the same reflection symmetry that characterizes the localization of excitons.

Conclusions

In this work we have studied the electronic and optical properties of single-layer C3_3N by using ab initio methods based on DFT and many-body schemes. In particular, we have computed the 2D band structure of C3_3N within the GW approximation, revealing an indirect quasi-particle band-gap of 1.42 eV (top of the valence band located at MM, bottom of the conduction band at Γ\Gamma), with direct gaps at Γ\Gamma and MM of 2.96 and 2.67 eV, respectively. The GW corrections to quasi-particle energies were also discussed in view of the orbital symmetry and localization. Neutral excitations, as those sampled by optical absorption (q=0q = 0) and electron energy loss spectroscopy (finite qq), are computed using the Bethe Salpeter equation. One of the main results of the work comes from the calculation of the full excitonic dispersion of C3N\mathrm{C}_{3}\mathrm{N} in qq-space, giving access to indirect excitons energies and intensities. These excitons play an important role in phonon-assisted photoluminescence,[57, 58] and they can be efficiently exploited for chemical sensing.[59] Interestingly, while the excitonic dispersion shows a parabolic behavior at MM, corresponding to the indirect band gap, at Γ\Gamma we observe a degenerate doublet which splits into a parabolic and a quasi-linear dispersing bands, as for other 2D materials. A peculiarity of C3N\mathrm{C}_{3}\mathrm{N}, connected with its indirect gap as well as with the dark nature of the excitons involved, is that the quasi-linear band has downward convexity, at variance with MoS2\mathrm{MoS}_{2} or hBN and the quasi-linear dispersion of the lower excitonic band comes from its independent-particle contribution. Finally, this work represents a solid starting point to consider the role of excitonic effects of C3N\mathrm{C}_{3}\mathrm{N} in more specific cases, e.g. in describing exciton-phonon scattering or the spectroscopy of in-plane adsorbates/defects.

Acknowledgement

This work was partially funded by the EU through the MaX Centre of Excellence for HPC applications (Project No. 824143), and by Regione Emilia Romagna through a FSE PhD fellowship on Big data analysis & high performance simulations for materials. We also thank SUPER (Supercomputing Unified Platform – Emilia-Romagna) from Emilia-Romagna POR-FESR 2014-2020 regional funds. MJC acknowledges CNPq, FAPESP and CAPES via the INCT-INEO grant. We acknowledge PRACE for awarding us access to the Marconi100 system based in Italy at CINECA.

Supplementary Information: Excitonic effects in graphene-like C3_3N

Miki Bonacci; Matteo Zanfrognini; Elisa Molinari; Alice Ruini; Marilia J. Caldas; Andrea Ferretti; Daniele Varsano

Automatic GW convergences

The convergence of the numerical parameters for the GW calculations, with the exception of the k\mathbf{k}-point grid, was achieved using the automatic workflow implemented in the aiida-yambo plugin.[2] In particular, the automatic workflow was used to converge the kinetic energy cutoff to represent the screening matrix and the number of empty states needed to converge the polarizability and the GW self-energy. These two parameters are strongly interdependent, and cannot be treated separately.[2]

The workflow used here, as shown in Figure S1, performs several convergence tests on each parameter, increasing one value while keeping fixed the other(s). The increment applied in each iteration is provided as input by the user. The convergence threshold is chosen to be ±15\pm15 meV with respect to the last simulation performed by the workflow, meaning that the final error bar is of 30 meV.

Convergence of C3N gap at Gamma

Figure S1. Convergence of the direct gap of C3C_3N at Γ\Gamma, with respect to empty states and cutoff on the screening matrix. As shown in the plot, 30 GW runs are sufficient to achieve a convergence of about 30 meV. Further convergence on kk-points mesh has been done without the workflow.

All the calculations are performed taking advantage of other sub-workflows of the plugin, mainly concerning automatic error handling.

Independent particle effects in the excitonic band structure

As shown in the main text, close to Γ\Gamma the first two bands in the excitonic band structure have negative slope and concavity. Moreover, the lowest one has a quasi-linear dependence on ∣q∣|\mathbf{q}|. The comparison between the full BSE solution at finite q\mathbf{q} close to Γ\Gamma with the average of the independent particle (IP) transition energies, as done in Figure S2, shows that these two peculiar features of the excitonic band structure are inherited from the IP contribution to the Hamiltonian.

Formally, we consider the BSE excitonic Hamiltonian, together with its eigenvectors represented on the transition basis, and separate out its finite-q\mathbf{q} contributions, as follows:

Hexc(q)∣S,q⟩=ΩS(q)∣S,q⟩,(12)H^{\mathrm{exc}}(\mathbf{q})|S,\mathbf{q}\rangle= \Omega^{S}(\mathbf{q})|S,\mathbf{q}\rangle, \tag*{(12)}
∣S,q⟩=∑vckAvckS(q)∣vck,q⟩,(13)|S,\mathbf{q}\rangle= \sum_{vck} A^{S}_{vck}(\mathbf{q})|vck,\mathbf{q}\rangle, \tag*{(13)}

where

Hexc(q)=HIP(q)+Kx(q)+Kd(q)=Hexc(0)+ΔHIP(q)+ΔKx(q)+ΔKd(q).(14)\begin{aligned} H^{\mathrm{exc}}(\mathbf{q}) = H^{\mathrm{IP}}(\mathbf{q}) + K_{x}(\mathbf{q}) + K_{d}(\mathbf{q}) \\ &= H^{\mathrm{exc}}(0) + \Delta H^{\mathrm{IP}}(\mathbf{q}) + \Delta K_{x}(\mathbf{q}) + \Delta K_{d}(\mathbf{q}). \tag*{(14)} \end{aligned}

Then, the average independent particle contribution, ⟨IP⟩\langle\mathrm{IP}\rangle, plotted in Figure S2 is computed as the expectation value of the diagonal IP term of the BSE excitonic Hamiltonian on the eigenvectors obtained diagonalizing the whole Hamiltonian at each q\mathbf{q}, namely ⟨IP⟩S=⟨S,q∣HIP(q)∣S,q⟩\langle\mathrm{IP}\rangle_{S} = \langle S,\mathbf{q}|H^{\mathrm{IP}}(\mathbf{q})|S,\mathbf{q}\rangle. In practice, these IP energies are evaluated as the weighted energies of all the transitions concurring in the formation of the given exciton as:

⟨IP⟩S=∑vck∣AvckS(q)∣2(Ec,kqp−Ev,k−qqp).(15)\langle\mathrm{IP}\rangle_{S} = \sum_{vck} |A^{S}_{vck}(\mathbf{q})|^{2}\left(E^{\mathrm{qp}}_{c,\mathbf{k}} - E^{\mathrm{qp}}_{v,\mathbf{k}-\mathbf{q}}\right). \tag*{(15)}

Moreover, the ⟨IP⟩S\langle\mathrm{IP}\rangle_{S} and BSE points in the plot are also aligned at q=0\mathbf{q}=0 by a shift ΔBSE0\Delta\mathrm{BSE}_{0} (equal to -0.93 eV, i.e. the EBE of the lowest exciton at Γ\Gamma). This amounts to consider the whole BSE Hamiltonian at q=0\mathbf{q}=0, while neglecting the q\mathbf{q}-dependence of ΔKx,d\Delta K_{x,d} at finite q\mathbf{q}, i.e.

⟨IP⟩S+ΔBSE0=⟨S,q∣Hexc(0)+ΔHIP(q)∣S,q⟩.(16)\langle\mathrm{IP}\rangle_{S} + \Delta\mathrm{BSE}_{0} = \langle S,\mathbf{q}|H^{\mathrm{exc}}(0) + \Delta H^{\mathrm{IP}}(\mathbf{q})|S,\mathbf{q}\rangle. \tag*{(16)}

References

  1. [1]K. S. Novoselov, A. K. Geim, S. V. Morozov, D. Jiang, Y. Zhang, S. V. Dubonos, I. V. Grigorieva, and A. A. Firsov, Science 306, 666 (2004), ISSN 0036-8075.
  2. [2]K. S. Novoselov, A. K. Geim, S. V. Morozov, D. Jiang, M. I. Katsnelson, I. V. Grigorieva, S. V. Dubonos, and A. A. Firsov, Nature 438, 197 (2005), ISSN 0028-0836, 1476-4687.
  3. [3]A. E. Galashev and O. R. Rakhmanova, Physics-Uspekhi 57, 970 (2014), ISSN 1063-7869, 1468-4780, URL http://stacks.iop.org/1063-7869/57/i=10/a=970?key=crossref.1ac0bb9edb2500e8aecad6689cad86e.
  4. [4]Y.-C. Lin, C. Jin, J.-C. J. Jen, S.-F. Jen, K. Suenaga, and P.-W. Chiu, ACS Nano 5, 2362 (2011).
  5. [5]S. Das, J. A. Robinson, M. Dubey, H. Terrones, and M. Terrones, Ann. Rev. Mater. Res. 45, 1 (2015).
  6. [6]S. J. Kim, K. Choi, B. Lee, Y. Kim, and B. H. Hong, Ann. Rev. Mater. Res. 45, 63 (2015).
  7. [7]R. Zhang and R. Cheung, in Two-dimensional Materials, edited by P. K. Nayak (IntechOpen, Rijeka, 2016), chap. 10, URL https://doi.org/10.5772/64017.
  8. [8]N. Mounet, M. Gibertini, P. Schwaller, D. Campi, A. Merkys, A. Marrazzo, T. Sohier, I. E. Castelli, A. Cepellotti, and G. Pizzi, Nature Nanotech. 13, 246–252 (2018), ISSN 1748-3395, URL http://dx.doi.org/10.1038/s41565-017-0055-5.
  9. [9]Q. H. Wang, K. Kalantar-Zadeh, A. Kis, J. N. Coleman, and M. S. Strano, Nature Nanotech. 7, 699 (2012).
  10. [10]H. Liu, A. T. Neal, Z. Zhu, Z. Luo, X. Xu, D. Tománek, and P. D. Ye, ACS Nano 8, 4033 (2014).
  11. [11]C. R. Dean, A. F. Young, I. Meric, C. Lee, L. Wang, S. Sorgenfrei, K. Watanabe, T. Taniguchi, P. Kim, K. L. Shepard, et al., Nature Nanotech. 5, 722–726 (2010), ISSN 1748-3387, 1748-3395.
  12. [12]D. Adekoya, S. Qian, X. Gu, W. Wen, D. Li, J. Ma, and S. Zhang, Nano-Micro Letters 13, 13 (2020).
  13. [13]Y. Xu and S.-P. Gao, Int. J. Hydrogen Energy 37, 11072 (2012), ISSN 03603199, URL https://linkinghub.elsevier.com/retrieve/pii/S0360319912010713.
  14. [14]A. Naseri, M. Samadi, A. Pourjavadi, A. Z. Moshfegh, and S. Ramakrishna, J. Mater. Chem. A 5, 23406 (2017), ISSN 2050-7488, 2050-7496, URL http://xlink.rsc.org/?DOI=C7TA05131J.
  15. [15]J. Mahmood, E. K. Lee, M. Jung, D. Shin, H.-J. Choi, J.-M. Seo, S.-M. Jung, D. Kim, F. Li, M. S. Lah, et al., Proc. Natl. Ac. Sci. 113, 7414 (2016), ISSN 0027-8424.
  16. [16]S. Yang, W. Li, C. Ye, G. Wang, H. Tian, C. Zhu, P. He, G. Ding, X. Xie, Y. Liu, et al., Adv. Mater. 29, 1605625 (2017).
  17. [17]L.-B. Shi, Y.-Y. Zhang, X. Xiu, and H.-K. Dong, Carbon 134, 103 (2018).
  18. [18]D. Wang, Y. Bao, T. Wu, S. Gan, D. Han, and L. Niu, Carbon 134, 22 (2018), ISSN 0008-6223, URL http://www.sciencedirect.com/science/article/pii/S0008622318303208.
  19. [19]B. Mortazavi, Carbon 118, 25 (2017), ISSN 0008-6223, URL http://www.sciencedirect.com/science/article/pii/S0008622317302701.
  20. [20]Y. Gao, H. Wang, M. Sun, Y. Ding, L. Zhang, and Q. Li, Phys. E: Low-Dimens. Syst. Nanostructures 99, 194 (2018).
  21. [21]J. Xu, J. Mahmood, Y. Dou, S. Dou, F. Li, L. Dai, and J.-B. Baek, Adv. Mater. 29, 1702007 (2017).
  22. [22]G.-C. Guo, R.-Z. Wang, B.-M. Ming, C. Wang, S.-W. Luo, M. Zhang, and H. Yan, J. Mater. Chem. A 7, 2106 (2019), ISSN 2050-7488, 2050-7496, URL http://xlink.rsc.org/?DOI=C8TA10972A.
  23. [23]Q. Liu, B. Xiao, J.-b. Cheng, Y.-c. Li, Q.-z. Li, W.-z. Li, X.-f. Xu, and X.-f. Yu, ACS Appl. Materials & Interfaces 10, 37135 (2018), ISSN 1944-8244, 1944-8252, URL https://pubs.acs.org/doi/10.1021/acsami.8b14183.DOI
  24. [24]P. Bhauriyal, A. Mahata, and B. Pathak, J. Phys. Chem. C 122, 2481 (2018), ISSN 1932-7447, 1932-7455, URL https://pubs.acs.org/doi/10.1021/acs.jpcc.7b09433.DOI
  25. [25]C. Zhang, Y. Jiao, T. He, S. Bottle, T. Frauenheim, and A. Du, J. Phys. Chem. Lett. 9, 858 (2018).
  26. [26]J. Wang, X. Li, Y. You, X. Yang, Y. Wang, and Q. Li, Nanotechnology 29, 365401 (2018), URL https://doi.org/10.1088/2631-6583/aace20.
  27. [27]D. Y. Qiu, T. Cao, and S. G. Louie, Phys. Rev. Lett. 115, 176801 (2015), ISSN 0031-9007, 1079-7114, URL https://link.aps.org/doi/10.1103/PhysRevLett.115.176801.DOI
  28. [28]P. Cudazzo, L. Sponza, C. Giorgetti, L. Reining, F. Sottile, and M. Gatti, Phys. Rev. Lett. 116, 066803 (2016), URL https://link.aps.org/doi/10.1103/PhysRevLett.116.066803.DOI
  29. [29]D. Y. Qiu, G. Cohen, D. Novichkova, and S. Refaely-Abramson, Nano Lett. 21, 7644 (2021).
  30. [30]L. Hedin, Phys. Rev. 139, 796 (1965).
  31. [31]G. Onida, L. Reining, and A. Rubio, Rev. Mod. Phys. 74, 601 (2002), ISSN 0034-6861, 1539-0756, URL https://link.aps.org/doi/10.1103/RevModPhys.74.601.DOI
  32. [32]G. Strinati, La Rivista del Nuovo Cimento (1978-1999) 11, 1 (1988).
  33. [33]P. Giannozzi, S. Baroni, N. Bonini, M. Calandra, R. Car, C. Cavazzoni, D. Cer esoli, G. L. Chiarotti, M. Cococcioni, I. Dabo, et al., J. Phys.: Condens. Matter 21, 395502 (2009).
  34. [34]P. Giannozzi, O. Andreussi, T. Brumme, O. Bunau, M. Buongiorno Nardelli, M. Calandra, R. Car, C. Cavazzoni, D. Ceresoli, M. Cococcioni, et al., J. Phys.: Condens. Matter 29, 465901 (2017).
  35. [35]D. R. Hamann, Phys. Rev. B 88, 085117 (2013), URL https://link.aps.org/doi/10.1103/PhysRevB.88.085117.DOI
  36. [36]J. P. Perdew, K. Burke, and M. Ernzerhof, Phys. Rev. Lett. 77, 3865 (1996).
  37. [37]A. Marini, C. Hogan, M. Grüning, and D. Varsano, Comput. Phys. Commun. 180, 1392 (2009).
  38. [38]D. Sangalli, A. Ferretti, H. Miranda, C. Attaccalite, I. Marri, E. Cannuccia, P. Melo, M. Marsili, F. Paleari, A. Marrazzo, et al., J. Phys.: Condens. Matter 31, 325902 (2019).
  39. [39]R. W. Godby and R. J. Needs, Phys. Rev. Lett. 62, 1169 (1989), ISSN 0031-9007, URL https://link.aps.org/doi/10.1103/PhysRevLett.62.1169.DOI
  40. [40]C. A. Rozzi, D. Varsano, A. Marini, E. K. U. Gross, and A. Rubio, Phys. Rev. B 73, 205119 (2006), ISSN 1098-0121, 1550-235X, URL https://link.aps.org/doi/10.1103/PhysRevB.73.205119.DOI
  41. [41]S. P. Huber, S. Zoupanos, M. Uhrin, L. Talirz, L. Kahle, R. Häuselmann, D. Gresch, T. Müller, A. V. Yakutovich, C. W. Andersen, et al., Sci. Data 7, 300 (2020), ISSN 2052-4463, URL http://www.nature.com/articles/s41597-020-00638-4.
  42. [42]See Supplemental Material for details on convergence studies for the GW results and for the analysis of the independent particle contribution in the BSE solution of the excitonic dispersion.
  43. [43]M. Gatti and F. Sottile, Phys. Rev. B 88, 155113 (2013), ISSN 1098-0121, 1550-235X, URL https://link.aps.org/doi/10.1103/PhysRevB.88.155113.DOI
  44. [44]K. Sturm, Zeitschrift für Naturforschung A 48, 233 (1993), URL https://doi.org/10.1515/zna-1993-1-244.
  45. [45]F. Fossard, L. Sponza, L. Schué, C. Attaccalite, F. Ducastelle, J. Barjon, and A. Loiseau, Phys. Rev. B 96, 115304 (2017), ISSN 2469-9950, 2469-9969, URL https://link.aps.org/doi/10.1103/PhysRevB.96.115304.DOI
  46. [46]X. Zhou, W. Feng, S. Guan, B. Fu, W. Su, and Y. Yao, J. Mater. Res. 32, 2993–3001 (2017).
  47. [47]Y. Wu, W. Xia, W. Gao, F. Jia, P. Zhang, and W. Ren, 2D Materials 6, 015018 (2018), ISSN 2053-5831.
  48. [48]M. S. Hybertsen and S. G. Louie, Phys. Rev. B 34, 5390 (1986), ISSN 0163-1829, URL https://link.aps.org/doi/10.1103/PhysRevB.34.5390.DOI
  49. [49]A. V. Krukau, O. A. Vydrov, A. F. Izmaylov, and G. E. Scuseria, J. Chem. Phys. 125, 224106 (2006).
  50. [50]W. Wei and T. Jacob, Phys. Rev. B 87, 085202 (2013), ISSN 1098-0121, 1550-235X.
  51. [51]J. Sun, R. Zhang, X. Li, and J. Yang, Appl. Phys. Lett. 109, 133108 (2016), ISSN 0003-6951, 1077-3118, URL http://aip.scitation.org/doi/10.1063/1.4963654.DOI
  52. [52]L. Yang, M. L. Cohen, and S. G. Louie, Nano Letters 7, 3112 (2007), ISSN 1530-6984, 1530-6992, URL https://pubs.acs.org/doi/10.1021/nl0716404.DOI
  53. [53]D. Prezzi, D. Varsano, A. Ruini, A. Marini, and E. Molinari, Phys. Rev. B 77, 041404 (2008), URL https://link.aps.org/doi/10.1103/PhysRevB.77.041404.DOI
  54. [54]J.-H. Choi, P. Cui, H. Lan, and Z. Zhang, Phys. Rev. Lett. 115, 066403 (2015), URL https://link.aps.org/doi/10.1103/PhysRevLett.115.066403.DOI
  55. [55]Z. Jiang, Z. Liu, Y. Li, and W. Duan, Phys. Rev. Lett. 118, 266401 (2017), URL https://link.aps.org/doi/10.1103/PhysRevLett.118.266401.DOI
  56. [56]L. Sponza, H. Amara, C. Attaccalite, S. Latil, T. Galvani, F. Paleari, L. Wirtz, and F. m. c. Ducastelle, Phys. Rev. B 98, 125206 (2018), URL https://link.aps.org/doi/10.1103/PhysRevB.98.125206.DOI
  57. [57]L. Schué, L. Sponza, A. Plaud, H. Bensalah, K. Watanabe, T. Taniguchi, F. Ducastelle, A. Loiseau, and J. Barjon, Phys. Rev. Lett. 122, 067401 (2019), ISSN 0031-9007, 1079-7114, URL https://link.aps.org/doi/10.1103/PhysRevLett.122.067401.DOI
  58. [58]S. Brem, A. Ekman, D. Christiansen, F. Katsch, M. Selig, C. Robert, X. Marie, B. Urbaszek, A. Knorr, and E. Malic, Nano Lett. 20, 2849–2856 (2020), ISSN 1530-6984, 1530-6992.
  59. [59]M. Feierabend, G. Berghäuser, A. Knorr, and E. Malic, Nature Commun. 8, 14776 (2017), ISSN 2041-1723.

Paper details

vlnc:W_5uycn38w
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents