Topological Hall effect enhanced at magnetic transition fields in a frustrated magnet EuCd2_2

Abstract

Emergent magnetic fields exerted by topological spin textures of magnets lead to an additional Hall response of itinerant carriers called the topological Hall effect (THE). While THE as a bulk effect has been widely studied, THE driven by magnetic domain boundaries (DBs) has been elusive. Here, we report rich Hall responses characterized by multiple peak structures and a hysteresis loop in films of EuCd2_2, where Eu layers form a geometrically frustrated lattice of Heisenberg spins. We uncover a THE component sharply enhanced at magnetic transition fields, indicating a giant contribution from non-trivial spin textures possibly formed at the DBs.

Hall effects which are neither proportional to the magnetic field nor to the magnetization have been one of the most vital research topics surrounding quantum transport phenomena in condensed-matter physics. Such non-monotonic Hall responses have been associated mostly with a non-monotonic modulation of the Berry phase rooted in either momentum space or real space. The momentum-space case originates from drastic changes of the band structure accompanied by the formation or shift of singular band features such as Weyl points during the magnetization process, and can be understood in the same framework as the intrinsic anomalous Hall effect (AHE) [1, 2]. On the other hand, real-space-based Berry phase is induced when itinerant carriers couple with non-coplanar magnetic orderings [3, 4]. As exemplified by skyrmion phases realized in chiral and geometrically-frustrated magnets [5, 6, 7, 8, 9], a non-coplanar arrangement of spins is characterized by the scalar spin chirality defined by the solid angle spanned by three spins (S1⋅S2×S3S_1 \cdot S_2 \times S_3). The scalar spin chirality acts as an emergent magnetic field on charged carriers, leading to additional contributions to the Hall effect usually termed as topological Hall effect (THE). In addition to the abovementioned Berry-phase origins, recent studies have also revealed that the extrinsic skew scattering can lead to an additional giant Hall response when combined with local scalar spin chirality of fluctuating spins, overcoming the upper limit of the Hall conductivity set by the intrinsic band structure [10, 11, 12]. Thus, the observation of the non-monotonic AHE or THE provides experimental evidence of unique electronic and magnetic structures as well as novel scattering mechanisms.

While the non-monotonic AHE and THE as bulk effects within a single magnetic domain have been widely reported in various systems, the observation of Hall contributions from a domain boundary (DB) has been rare. DBs in magnets generally serve as an additional scattering source or conduction path depending on the details of the magnetic orderings [13, 14, 15], and are expected to give finite contributions to the Hall responses when coupled with a non-zero Berry phase. In ferromagnets, for example, conventional DBs between the ferromagnetic domains exhibit topologically trivial spin textures leading to no THE, whereas chiral domain walls (skyrmion bubbles) induced by interfacial Dzyaloshinskii-Moriya (DM) interaction in films and heterointerfaces, or topological defects such as vertical Bloch lines are predicted to contribute to finite THE [16, 17]. When the system possesses Weyl points near the Fermi level, enhanced skew-scattering of Weyl fermions at the DB is proposed to lead to a giant AHE even comparable to the bulk contribution [18]. The recent observation of a non-monotonic AHE accompanied by a unique hysteresis loop in the ferromagnetic Weyl semimetal CeAlSi and related compounds have been attributed to the scattering at DBs [19, 20, 21]. However, DB contributions in magnets with more complex spin orderings such as non-colinear or non-coplanar configurations have been elusive, except for one known example of pyrochlore-type antiferromagnets where the all-in-all-out ordering forms conductive DBs responsible for unconventional AHE [22]. The DBs in systems with complex magnetic orderings can lead to unique spin configurations formed locally, and thus serve as a fertile playground for exploring novel Hall responses.

In this Letter, we demonstrate a giant THE triggered by magnetic transitions in films of frustrated magnet EuCd2\mathrm{EuCd}_{2}. EuCd2\mathrm{EuCd}_{2} takes the CeCu2\mathrm{CeCu}_{2}-type hexagonal structure, which can be viewed as a lower-symmetry derivative of the AlB2\mathrm{AlB}_{2}-type structure with an alternate stacking of triangular and honeycomb lattices [23]. In the CeCu2\mathrm{CeCu}_{2}-type structure of EuCd2\mathrm{EuCd}_{2}, the Eu triangular lattice is anisotropically distorted in the acac-plane and the Cd honeycomb lattice is buckled along the bb-axis as shown in Figure 1. Several AlB2\mathrm{AlB}_{2}- and CeCu2\mathrm{CeCu}_{2}-type compounds with Heisenberg-type spins located at the triangular sites have been known to host non-colinear/non-coplanar orderings such as the skyrmion phase in Gd2PdSi3\mathrm{Gd}_{2}\mathrm{PdSi}_{3} [8], the spiral spin texture in EuZnGe\mathrm{EuZnGe} [24], or the non-colinear antiferromagnetic ordering in GdCu2\mathrm{GdCu}_{2} [25]. For EuCd2\mathrm{EuCd}_{2}, on the other hand, only magnetization measurements on polycrystalline samples have been reported so far, suggesting a possible antiferromagnetic ordering [26]. Here, we reveal that EuCd2\mathrm{EuCd}_{2} exhibits rich non-monotonic Hall responses, including THE characterized by multiple peak structures and a hysteresis loop. In particular, one of the THE components is sharply enhanced at the magnetic transition, indicating a Hall contribution derived from possible non-trivial spin configurations formed at the magnetic DBs.

Image not extracted

Figure 1. Structural, magnetization, and transport characterization of the EuCd2_2 films. (a) Crystal structure and orientation of CeCu2_2-type EuCd2_2 grown on the Al2_2O3_3(0001) substrate. The Eu distorted triangular lattices and the Cd buckled honeycomb lattices are alternately stacked along the bb-axis. (b) In-plane epitaxial relation between EuCd2_2 and Al2_2O3_3. Eu atoms are displaced oppositely with respect to the center of the Cd hexagon between adjacent Eu layers, preserving the inversion symmetry. (c) Cross-sectional image of the EuCd2_2 film (left), and atomic arrangement of Eu and Cd atoms in the CeCu2_2-type structure viewed along the aa-axis (right). The scale bar corresponds to 1 nm. (d) Temperature dependence of the magnetization (MM) measured in a magnetic field of 0.1 T applied in the out-of-plane (BoutB_{\mathrm{out}}) and in-plane (BinB_{\mathrm{in}}) directions. (e) BoutB_{\mathrm{out}} and BinB_{\mathrm{in}} dependence of the magnetization normalized by the saturation value MsM_s. The insets show magnified views of the hysteresis loop around zero field and the metamagnetic transition at Bout=1.3B_{\mathrm{out}} = 1.3 T. (f) Temperature dependence of the longitudinal resistivity ρxx\rho_{xx}. BoutB_{\mathrm{out}} dependence of (g) ρxx\rho_{xx} and (h) Hall resistivity ρyx\rho_{yx}. (i) Topological Hall signal (ρyxT\rho_{yx}^{\mathrm{T}}) extracted by subtracting the ordinary Hall term (ρyxO\rho_{yx}^{\mathrm{O}}) and the MM-proportional anomalous Hall term (ρyxA=rsρxx2M\rho_{yx}^{\mathrm{A}} = r_s\rho_{xx}^{2}M) from the raw data in (h).

Thin films of EuCd2\mathrm{EuCd}_{2} were epitaxially grown on Al2O3(0001)\mathrm{Al}_{2}\mathrm{O}_{3}(0001) substrates by molecular beam epitaxy. The growth temperature was 350∘C350^\circ\mathrm{C}. Eu and Cd were supplied by an effusion cell with a Cd-rich flux ratio (Cd/Eu = 15-44) due to the highly volatile nature of Cd as compared to Eu. The film thickness is designed to be 60 nm. As summarized in the Supplemental Material [27], structural characterization by x-ray diffraction (XRD) reveals that the bb-axis of EuCd2\mathrm{EuCd}_{2} is oriented along the surface normal, while the acac-plane Cd honeycomb lattice is aligned to that of the Al2O3\mathrm{Al}_{2}\mathrm{O}_{3} cc-plane. Depending on the orientation of the distorted Eu hexagons with respect to the Al2O3\mathrm{Al}_{2}\mathrm{O}_{3} substrate, there are three types of in-plane domains as confirmed by reciprocal space map measurements [27]. Figure 1(c) shows a cross sectional image of the EuCd2\mathrm{EuCd}_{2} film taken along the aa-axis by high-angle annular dark-field scanning transmission electron microscopy. The periodic arrangement of Eu and Cd atoms characteristic to the CeCu2\mathrm{CeCu}_{2}-type structure is clearly resolved.

Figures 1(d)-1(i) summarize magnetization and transport properties of the EuCd2\mathrm{EuCd}_{2} films. The temperature dependence of the magnetization measured with the magnetic field applied out-of-plane (BoutB_{\mathrm{out}}) and in-plane (BinB_{\mathrm{in}}, parallel to Al2O3[112ˉ0]\mathrm{Al}_{2}\mathrm{O}_{3}[11\bar{2}0]) exhibits an onset of antiferromagnetic order at TN=37T_{\mathrm{N}} = 37 K which is consistent with the previous report on polycrystalline bulk samples [26]. Below TNT_{\mathrm{N}}, the magnetization MM keeps increasing, indicating that the magnetic structure is not a simple colinear antiferromagnetic ordering. Magnetization curves measured as functions of BoutB_{\mathrm{out}} and BinB_{\mathrm{in}} at 2 K are presented in Figure 1(f). EuCd2\mathrm{EuCd}_{2} develops ferromagnetic moments at lower temperature as indicated by a small hysteresis loop around zero field as seen in the inset. This ferromagnetism is suppressed above 20 K (see Supplemental Material [27]). While the magnetization monotonically increases when the field is applied in-plane, a metamagnetic transition is observed around 1.3 T when the field is applied along the out-of-plane hard axis. The metamagnetic transition is observed up to TNT_{\mathrm{N}} irrespective of the low-temperature out-of-plane ferromagnetism, implying the occurrence of a spin reorientation or a spin-flop transition from the antiferromagnetic ground state.

The temperature dependence of the resistivity presented in Figure 1(e) exhibits a kink structure at TNT_{\mathrm{N}} reflecting that the metallic conduction is strongly coupled with the localized spins of Eu2+\mathrm{Eu}^{2+}. Figures 1(g) and 1(h) show longitudinal resistivity ρxx\rho_{xx} and Hall resistivity ρyx\rho_{yx} data measured at 2 K in out-of-plane fields. ρxx\rho_{xx} exhibits a peak at the field where the metamagnetic transition occurs, and further increasing BoutB_{\mathrm{out}} leads to a negative magnetoresistance until the spins are fully polarized at around 3.8 T. During such a magnetization process, ρyx\rho_{yx} exhibits rich peak features with a hysteresis loop in stark contrast to a rather monotonic change of MM against BoutB_{\mathrm{out}} in Figure 1(f). Figure 1(i) displays the non-monotonic Hall signal after subtracting the sum of the ordinary Hall term ρyxO\rho_{yx}^{\mathrm{O}} and the MM-proportional anomalous Hall term ρyxA\rho_{yx}^{\mathrm{A}}. We note that the longitudinal conductivity σxx\sigma_{xx} of EuCd2\mathrm{EuCd}_{2} lies in the so-called intrinsic region of the conventional AHE scaling plot [2], and ρyxA\rho_{yx}^{\mathrm{A}} here is calculated via rsρxx2Mr_{\mathrm{s}}\rho_{xx}^{2}M with rsr_{\mathrm{s}} being determined as a fitting parameter. As discussed below, the non-monotonic Hall signal in EuCd2\mathrm{EuCd}_{2} films consists mainly of THE originating from the real-space spin configuration, and hereafter we denote it as ρyxT\rho_{yx}^{\mathrm{T}}.

Figure 2(a) presents a color map of ρyxT\rho_{yx}^{\mathrm{T}} as a function of temperature and out-of-plane field (for the Hall resistivity data at different temperatures, see also the Supplemental Material [27]). For clarity, we label the phases below (above) the metamagnetic transition around 1.3 T as Phase I (II) and the forced-ferromagnetic phase above the saturation field around 3.8 T as FM, and the magnetic phase boundaries separating different phases are indicated by dotted lines which are drawn based on the results of the magnetization (marked by solid triangles)and magnetoresistance measurements. Importantly, the Hall response of the EuCd2\mathrm{EuCd}_{2} films is characterized by two unique features. Firstly, there are multiple positive and negative peaks appearing on both sides across zero field as indicated by circles with labels P1, P2, and P3 in Figure 2(b) and Figure 2(c). These peak structures of ρyxT\rho_{yx}^{\mathrm{T}} start to develop clearly below TNT_{\mathrm{N}}, reflecting their magnetic origin. Moreover, among the ρyxT\rho_{yx}^{\mathrm{T}} peaks, the P1 peak appears sharply at the metamagnetic transition field (marked with a solid triangle), and this tendency is observed in the entire temperature range below TNT_{\mathrm{N}}.

Topological Hall effect enhanced at the metamagnetic transitions

Figure 2. Topological Hall effect enhanced at the metamagnetic transitions. (a) Color map of the topological Hall resistivity ρyxT\rho_{yx}^{\mathrm{T}} as a function of temperature TT and out-of-plane magnetic field BoutB_{\mathrm{out}}. Only data of the field-decreasing sweep from 9 T to −9-9 T are shown. Open and solid triangles denote the field position of the magnetic transition, and dotted lines show the magnetic phase boundaries between I, II and FM. Normalized magnetization and ρyxT\rho_{yx}^{\mathrm{T}} measured upon sweeping the field at (b) 2 K and (c) 25 K, as indicated by the arrows in (a). The ρyxT\rho_{yx}^{\mathrm{T}} peak induced by the metamagnetic transitions is labeled P1 with a green solid circle, while the bulk THE peaks are labeled P2 (yellow circle) and P3 (purple circle). Schematic illustrations of the decomposed Hall contributions from different origins at (d) 2 K and (e) 25 K. The amplitude of the hysteresis loop in the DB-driven THE and the additional AHE below 20 K is denoted by ΔρyxT\Delta\rho_{yx}^{\mathrm{T}} and ΔρyxA\Delta\rho_{yx}^{\mathrm{A}}, respectively.

A Hall resistivity with multiple peaks has been identified as non-monotonic AHE for various Eu-based magnetic semimetals and semiconductors [30, 31, 32, 33, 34]. In those systems, the continuous change of the momentum-space Berry curvature is induced mainly by the formation of Weyl points or their shifting with respect to the Fermi energy during the magnetization process. However, this is not the case for EuCd2\mathrm{EuCd}_{2}. As shown in the Supplemental Material [27], EuCd2\mathrm{EuCd}_{2} exhibits a sign change of AHE with developing the out-of-plane ferromagnetism below 20 K. This observation itself is interesting because it originates from a drastic modulation of the momentum-space band structure taking place in the presence of ferromagnetism in EuCd2\mathrm{EuCd}_{2}, which may imply the appearance of topologically non-trivial band features near the Fermi level. We note that a similar temperature-dependent sign change of AHE has been reported for the ferromagnetic Weyl metal SrRuO3\mathrm{SrRuO}_{3} [35]. Focusing on the non-monotonic Hall term, on the other hand, the overall peak structures of P1, P2, and P3 remain unchanged even across 20 K [27]. The absence of sign changes for those peaks indicates that they do not share the same origin as the intrinsic AHE. Therefore, we can reasonably conclude that the non-monotonic Hall effect is originating in the real-space spin Berry phase rather than in momentum space, and hence, it can be ascribed to THE (see also Supplemental Material [27] for additional discussions).

Having clarified the origin of the unique Hall responses as topological spin structures, we now focus on the second feature of ρyxT\rho_{yx}^{\mathrm{T}} in EuCd2\mathrm{EuCd}_{2}, i.e., the pronounced hysteresis loop.

Generally, the spin chirality of field-induced spin textures changes its sign upon field reversal [5, 6, 7, 8, 9], leading to a field-antisymmetric THE (ρyxT(B)=−ρyxT(−B)\rho_{yx}^{T}(B)=-\rho_{yx}^{T}(-B)). A hysteretic THE has been reported only in special cases such as hysteretic formation of skyrmions in FeGe thin films [36], transitions between skyrmion and anti-skyrmion phases in Mn2_2RhSn [37], and ferromagnet-based systems with interfacial Dzyaloshinskii-Moriya interaction [38, 39, 40, 41]. In EuCd2_2, on the other hand, ferromagnetism develops below 20 K, and the hysteretic behaviour of ρyxT\rho_{yx}^{T} can be straightforwardly associated with the polarized out-of-plane moments.

However, we should emphasize that the hysteresis cannot be explained solely by the additional AHE induced by the out-of-plane ferromagnetic moments. As seen in Figure 2(b), the hysteresis loop is particularly enlarged around the P1 THE peak due to its asymmetric appearance depending on the field scan directions; in the field-decreasing (increasing) sweep at 2 K, the P1 peak is suppressed on the positive (negative) field side, and it is sharply enhanced on the negative (positive) field side, respectively. This highlights the sensitive coupling between the P1 THE peak and the remanent ferromagnetic moment.

Interestingly, such coupling between THE and ferromagnetism is not observed for the other THE peaks (P2 and P3), which appear on both sides of the field regardless of the scan direction and the metamagnetic transition. These two different THE components can be also distinguished by measuring their field-angle dependence [27]. We observe that the amplitude of the P1 peak is quickly diminished as the metamagnetic transition is suppressed with tilting the field toward the in-plane direction, while the P2 peak survives up to high tilting angles (see the Supplemental Material [27] for details). From these findings, the complex Hall responses of EuCd2_2 can be separated into three components as illustrated in Figure 2(d) and Figure 2(e); (i) the THE component appearing without hysteresis before the full polarization of the moments along the out-of-plane direction has been reached (P2 and P3), (ii) the THE component which is sharply enhanced at the metamagnetic transition with coupling to the ferromagnetism (P1), and (iii) the ferromagnetism-induced additional AHE component appearing below 20 K. As discussed in the following, we propose that the former THE component represents the bulk contribution and the latter component the DB contribution.

To clarify the DB-derived nature of the P1 THE peak, we have performed minor loop measurements. Figure 3 presents the Hall term ρyx−ρyxO\rho_{yx}-\rho_{yx}^{O} measured by scanning the field from −5-5 T to a certain maximum value Bmax⁡B_{\max} and then back to −5-5 T. Bmax⁡B_{\max} is varied from −2.2-2.2 T to 2.22.2 T so that the minor loops cover the peak and hysteretic features of ρyx\rho_{yx}. To evaluate the hysteretic behavior, we have also extracted the loop term Δρyx\Delta\rho_{yx} defined as the difference between the field-increasing sweep and the field decreasing sweep as shown in Figure 3(d)-Figure 3(f). Δρyx\Delta\rho_{yx} corresponds to the summation of the hysteresis contribution from the P1 THE term and the additional AHE term as illustrated in Figure 2(d). A striking observation is that there is a region of negative Δρyx\Delta\rho_{yx} in the minor loops of Bmax⁡=0.9B_{\max}=0.9, 1.31.3, 1.51.5, and 1.61.6 T as shown in the inset in Figure 3(e) and Figure 3(f). The negative Δρyx\Delta\rho_{yx} indicates an increase of THE during the field-decreasing sweep as compared to the field-increasing sweep. In particular, the amplitude of negative Δρyx\Delta\rho_{yx} is the largest for Bmax⁡=1.3B_{\max}=1.3 T where the magnetic field is reversed during the metamagnetic transition. These observations reveal that the promoted formation of DBs by the minor loop scans leads to a larger amplitude of THE, highlighting the THE contribution of the DBs. We also note that the constant discrepancy (indicated by a two-headed arrow) in the peak amplitude between the full loop and the minor loops with Bmax⁡=0B_{\max}=0, 0.50.5, 0.90.9, and 1.31.3 T corresponds to the ΔρyxA\Delta\rho_{yx}^{\mathrm{A}} term. ΔρyxA\Delta\rho_{yx}^{\mathrm{A}} is suppressed in the minor loops for Bmax⁡>1.3B_{\max}>1.3 T as shown in Figure 3(c), which means that the metamagnetic transition also promotes the reversal of the out-of-plane moments.

Minor loop measurements of the Hall resistivities after poling at −5 T

Figure 3. Minor loop measurements of the Hall resistivities after poling at −5 T. The Hall term ρyx−ρyxO\rho_{yx}-\rho^{\mathrm{O}}_{yx} measured for the minor loops with Bmax⁡=−2.2,−1.7,−1.3,−0.9B_{\max}=-2.2,-1.7,-1.3,-0.9 T, (b) Bmax⁡=0,0.5,0.9,1.3B_{\max}=0,0.5,0.9,1.3 T, and (c) Bmax⁡=1.5,1.6,1.7,1.9,2.2B_{\max}=1.5,1.6,1.7,1.9,2.2 T. The full hysteresis loop is shown in gray for comparison. The arrows on top of the panels (a)-(c) show the field scan direction. The color code corresponds to the color of the respective data. (d)-(f) The loop term Δρyx\Delta\rho_{yx} extracted from the respective ρyx−ρyxO\rho_{yx}-\rho^{\mathrm{O}}_{yx} curves in (a)-(c). ΔρAHE\Delta\rho_{\mathrm{AHE}} is the width of the zero field hysteresis reflecting the additional anomalous Hall contribution from the out-of-plane ferromagnetic moments. Insets in (e) and (f) show the field region with a negative Δρyx\Delta\rho_{yx} observed for the loops with Bmax⁡B_{\max} around 1.3 T, which indicates that the enhanced formation of DBs yields a larger P1 THE peak.

To further demonstrate the DB-driven nature of the P1 THE peak, we have also examined its dependence on different field cooling processes, which can effectively modulate the DB density. Figure 4 presents ρyx−ρyxo\rho_{yx}-\rho_{yx}^{\mathrm{o}} measured after experiencing two different field cooling paths from above TNT_{\mathrm{N}} to 22 K; in Path 1 the out-of-plane field was gradually increased from 00 T at TNT_{\mathrm{N}} to BFCB_{\mathrm{FC}} at 22 K, while in Path 2 the constant field BFCB_{\mathrm{FC}} was applied from above TNT_{\mathrm{N}} to 22 K as shown in the top panels. After reaching BFCB_{\mathrm{FC}} at 22 K, field scans towards +5+5 T and −5-5 T were performed. ρyx−ρyxo\rho_{yx}-\rho_{yx}^{\mathrm{o}} of the BFC=0B_{\mathrm{FC}}=0 T case presented in Figure 4 (a) reflects the initial magnetization curve after zero field cooling, and exhibits the P1 peak on both positive and negative field sides, in contrast to the full loop shown in gray for comparison. This can be interpreted to reflect the absence of the ferromagnetic component suppressing the DB-driven THE under zero field cooling.

Modulation of THE by different field cooling processes

Figure 4. Modulation of THE by different field cooling processes. Top panels show the two different field cooling paths (Path 1 and Path 2) from above TNT_N to 2K and to the field BFCB_{\mathrm{FC}} = (a) 0 T, (b) 0.7 T, (c) 1.3 T, and (d) 1.8 T. BFCB_{\mathrm{FC}} = 0 T corresponds to the zero field cooling, and Path 1 with BFCB_{\mathrm{FC}} = 1.3 T follows closely the magnetic phase boundary between I and II. Hall term ρyx−ρyxo\rho_{yx}-\rho_{yx}^{\mathrm{o}} measured at 2 K after the respective field cooling path is shown in the middle panels. The solid curve presents the result for Path 1 and dashed line for Path 2 for each BFCB_{\mathrm{FC}}. The field scans were performed in both the directions towards −5-5 T and +5+5 T starting from BFCB_{\mathrm{FC}} as marked by an open circle. For comparison, the Hall resistivity curve of the full loop scan is also shown in gray. The lower panels show modulation of THE evaluated by subtracting ρyx\rho_{yx} of the BFCB_{\mathrm{FC}} = 0 T case from that of respective BFCB_{\mathrm{FC}} case. The peak amplitude of ΔB\Delta_B THE is particularly enhanced when the field cooling path follows the inside region of the phase boundary between I and II.

For evaluating the modulation of DB-driven THE for each BFCB_{\mathrm{FC}} we have specifically taken the change of the Hall resistivity from that of the BFC=0B_{\mathrm{FC}}=0 T case (ρyx−ρyx,BFC=0T)(\rho_{yx}-\rho_{yx,B_{\mathrm{FC}}=0\mathrm{T}}) as presented in the lower panels. When BFCB_{\mathrm{FC}} is much lower than the metamagnetic transition field around 1.31.3 T such as in the case of BFC=0.7B_{\mathrm{FC}}=0.7 T in Figure 4(b), both of the field cooling along Path 1 and Path 2 result in enhanced amplitude of the P1 peak. When BFCB_{\mathrm{FC}} is 1.31.3 T, on the other hand, Path 1 and Path 2 exhibit a contrasting behaviour. As shown in Figure 4(c), Path 1 for BFC=1.3B_{\mathrm{FC}} = 1.3 T following closely along the magnetic phase boundary between I and II leads to significant enhancement of the P1 peak, which even exceeds that of the full loop. In contrast, Path 2 following the outside of the phase boundary results in suppression of the P1 peak. These observations in the BFC=1.3B_{\mathrm{FC}} = 1.3 T case clearly indicates the strong relevance of THE to the DB density formed during different field cooling paths in the EuCd2_2 films. Further increase of BFCB_{\mathrm{FC}} strengthens the development of the out-of-plane moments, suppressing DB-driven THE for both Path 1 and Path 2 as shown in Figure 4(d) (see also the Supplemental Material [27] for the results of other BFCB_{\mathrm{FC}} cases, and also the field cooling dependence of the magnetization curve).

Finally, we would like to discuss the possible origin of the THE signals in EuCd2_2. THE appears as a bulk effect when non-coplanar spin textures with finite scalar spin chirality are stabilized by the external field. If we simply assume a non-colinear ordering such as 120∘120^\circ-spin ordering for the Eu triangular lattice of EuCd2_2, however, the field-induced spin canting generates scalar spin chirality only locally and cancels it out globally due to the contribution of opposite signs from the adjacent triangles. To realize a non-vanishing scalar spin chirality as bulk effect in a triangular lattice system, either strong coupling to the spin-orbit interaction or an incommensurate non-coplanar ordering is required to break the balance of this cancellation [42]. As proposed in the theory [42] and experimentally verified by the realization of a skyrmion phase in AlB2_2-type Gd2_2PdSi3_3[8], the presence of further neighbor interactions on a triangular network of Heisenberg-type spins can lead to incommensurate spiral textures with multiple-QQ vectors. It is worth noting that the nearest-neighbor Eu sites in CeCu2_2-type EuCd2_2 are the interlayer Eu-Eu sites rather than the intralayer triangular sites. The ferromagnetism below 20 K also indicates the presence of ferromagnetic interaction between some Eu-Eu sites. Altogether, it is highly likely that not just a simple two-dimensional antiferromagnetic ordering within the triangular lattice plane but a more complex three-dimensional non-coplanar ordering is realized in EuCd2_2, accounting for the observations of the P2 and P3 THE peaks.

Opposed to the bulk THE, the particularly sharp THE at the metamagnetic transition is attributed to the contribution from the magnetic DBs. In contrast to the bulk scalar spin chirality on the triangular lattice, that of the local DBs is expected to survive owing to the broken symmetry. The fact that the peak amplitude of P1 is suppressed when the out-of-plane moments remain polarized under higher fields, and that it is enhanced when the moments are weakened at the switching field, proves that the spin configuration realized at the DBs is crucial for the appearance of the THE. Such a dependence of THE on ferromagnetism actually resembles the THE observed in ferromagnet-based heterostructures with interfacial DM interaction [38, 39, 40, 41]. There, a THE peak structure appears only at the coercive field of the ferromagnetic layer, where the DM interaction comes in to realize chiral DBs or skyrmions. Since interfacial or bulk DM interaction is not expected for the present case, we speculate that instead the presence of frustration-induced non-coplanar spin textures in EuCd2\mathrm{EuCd}_{2} plays a vital role in realizing non-trivial DBs hosting finite scalar spin chirality.

In summary, we have succeeded in the film growth of the CeCu2\mathrm{CeCu}_{2}-type frustrated magnet EuCd2\mathrm{EuCd}_{2} and have revealed its rich Hall responses, including a temperature-dependent sign change of AHE and multiple THE peaks accompanied by a pronounced hysteresis loop. One of the THE peaks is sharply enhanced at the metamagnetic transition field, indicating the formation of magnetic DBs hosting finite scalar spin chirality. Importantly, compared to the bulk AHE and THE, the DB contribution appears as the leading term. For the formation of non-trivial DBs which give such a dominant Hall response, it is expected that the presence of possible non-coplanar spin textures within the frustrated Eu network is essential. The determination of the actual magnetic structure realized in EuCd2\mathrm{EuCd}_{2} is highly desired to further clarify its unique Hall responses.

We thank M. Kawasaki for fruitful discussions and also the help in parts of the low-temperature magnetotransport measurements. We also thank N. Kanazawa, H. Ishizuka, H. Oike, H. Sakai, T. Nakajima, Y. Yamasaki, K. Matsuura, and F. Kagawa for fruitful discussions. This work was supported by JST FOREST Program grant no. JP-MJFR202N, Japan; and by Grant-in-Aids for Scientific Research JP21H01804, JP22H04471, JP22H04501, JP22K18967, JP22K20353, and JP23K13666 from MEXT, Japan.

References

Figures

Nine-panel figure showing the crystal structure and transport measurements of EuCd2As2

Figure 5.

References

  1. [3]K. Ohgushi, S. Murakami, and N. Nagaosa, Phys. Rev. B 62, R6065(R) (2000).
  2. [4]Y. Taguchi, Y. Oohara, H. Yoshizawa, N. Nagaosa, and Y. Tokura, Science 291, 2573-2576 (2001).
  3. [5]S. Mühlbauer, B. Binz, F. Jonietz, C. Pfleiderer, A. Rosch, A. Neubauer, R. Georgii, and P. Böni, Science 323, 915-919 (2009).
  4. [6]N. Kanazawa, Y. Nii, X.-X. Zhang, A. S. Mishchenko, G. De Filippis, F. Kagawa, Y. Iwasa, N. Nagaosa, and Y. Tokura, Nat. Commun. 7, 11622 (2016).
  5. [7]X. Z. Yu, N. Kanazawa, Y. Onose, K. Kimoto, W. Z. Zhang, S. Ishiwata, Y. Matsui, and Y. Tokura, Nat. Mater. 10, 106-109 (2011).
  6. [8]T. Kurumaji, T. Nakajima, M. Hirschberger, A. Kikkawa, Y. Yamasaki, H. Sagayama, H. Nakao, Y. Taguchi, T. Arima, and Y. Tokura, Science 365, 914-918 (2019).
  7. [9]R. Takagi, N. Matsuyama, V. Ukleev, L. Yu, J. S. White, S. Francoual, J. R. L. Mardegan, S. Hayami, H. Saito, K. Kaneko, K. Ohishi, Y. Ōnuki, T. Arima, Y. Tokura, T. Nakajima, and S. Seki, Nat. Commun. 13, 1472 (2022).
  8. [10]H. Ishizuka and N. Nagaosa, Sci. Adv. 4, eaap9962 (2018).
  9. [11]Y. Fujishiro, N. Kanazawa, R. Kurihara, H. Ishizuka, T. Hori, F. S. Yasin, X. Yu, A. Tsukazaki, M. Ichikawa, M. Kawasaki, N. Nagaosa, M. Tokunaga, and Y. Tokura, Nat. Commun. 12, 317 (2021).
  10. [12]M. Uchida, S. Sato, H. Ishizuka, R. Kurihara, T. Nakajima, Y. Nakazawa, M. Ohno, M. Kriener, A. Miyake, K. Ohishi, T. Morikawa, M. S. Bahramy, T. Arima, M. Tokunaga, N. Nagaosa, and M. Kawasaki, Sci. Adv. 7, eabl5381 (2021).
  11. [13]P. M. Levy, and S. Zhang, Phys. Rev. Lett. 79, 5110 (1997).
  12. [14]E. Y. Ma, Y.-T. Cui, K. Ueda, S. Tang, K. Chen, N. Tamura, P. M. Wu, J. Fujioka, Y. Tokura, and Z.-X. Shen, Science 350, 538-541 (2015).
  13. [15]T. C. Fujita, M. Uchida, Y. Kozuka, W. Sano, A. Tsukazaki, T. Arima, and M. Kawasaki, Phys. Rev. B 93, 064419 (2016).
  14. [16]C. Moutafis, S. Komineas, and J. A. C. Bland, Phys. Rev. B 79, 224429 (2009)
  15. [17]K.-J. Kim, M. Mochizuki, and T. Ono, Appl. Phys. Express 12, 053006 (2019).
  16. [18]S. Sorn and A. Paramekanti, Phys. Rev. B 103, 104413 (2021).
  17. [19]H.-Y. Yang, B. Singh, J. Gaudet, B. Lu, C.-Y. Huang, W.-C. Chiu, S.-M. Huang, B. Wang, F. Bahrami, B. Xu, J. Franklin, I. Sochnikov, D. E. Graf, G. Xu, Y. Zhao, C. M. Hoffman, H. Lin, D. H. Torchinsky, C. L. Broholm, A. Bansil, and F. Tafti, Phys. Rev. B 103, 115143 (2021).
  18. [20]M. M. Piva, J. C. Souza, V. Brousseau-Couture, S. Sorn, K. R. Pakuszewski, J. K. John, C. Adriano, M. Côté, P. G. Pagliuso, A. Paramekanti, and M. Nicklas, Phys. Rev. Res. 5, 013068 (2023).
  19. [21]X. He, Y. Li, H. Zeng, Z. Zhu, S. Tan, Y. Zhang, C. Cao, and Y. Luo, Sci. China-Phys. Mech. Astron. 66, 237011 (2023).
  20. [22]W. J. Kim, J. H. Gruenewald, T. Oh, S. Cheon, B. Kim, O. B. Korneta, H. Cho, D. Lee, Y. Kim, M. Kim, J.-G. Park, B.-J. Yang, A. Seo, and T. W. Noh, Phys. Rev. B 98, 125103 (2018).
  21. [23]R.-D. Hoffman and R. Pöttgen, Z. Kristallogr. 216, 127-145 (2001).
  22. [24]T. Kurumaji, M. Gen, S. Kitou, H. Sagayama, A. Ikeda, and T. Arima, Phys. Rev. Mater. 6, 094410 (2022).
  23. [25]M. Rotter, A. Lindbaum, E. Gratz, G. Hilscher, H. Sassik, H. E. Fischer, M. T. Fernandez-Diaz, R. Arons, and E. Seidl, J. Mag. Mag. Mater. 214, 281-290 (2000).
  24. [26]K. H. J. Buschow, and F. J. van Steenwijk, Physica B 85, 122-126 (1977).
  25. [27]See Supplemental Material at SM-URL for details about the reciprocal space mapping measurements, temperature dependent measurements of the magnetization and the Hall resistivities, field-angle dependent measurements,field cooling dependence measurements, and additional discussion on the origin of the Hall response of the EuCd₂ films. The Supplemental Material also includes Refs. [28, 29].
  26. [30]K. S. Takahashi, H. Ishizuka, T. Murata, Q. Y. Wang, Y. Tokura, N. Nagaosa, and M. Kawasaki, Sci. Adv. 4, eaap7880 (2018).
  27. [31]A. H. Mayo, H. Takahashi, M. S. Bahramy, A. Nomoto, H. Sakai, and S. Ishiwata, Phys. Rev. X 12, 011033 (2022).
  28. [32]X. Cao, J.-X. Yu, P. Leng, C. Yi, X. Chen, Y. Yang, S. Liu, L. Kong, Z. Li, X. Dong, Y. Shi, M. Bibes, R. Peng, J. Zang, and F. Xiu, Phys. Rev. Res. 4, 023100 (2022).
  29. [33]M. Ohno, S. Minami, Y. Nakazawa, S. Sato, M. Kriener, R. Arita, M. Kawasaki, and M. Uchida, Phys. Rev. B 105, L201101 (2022).
  30. [34]M. Kondo, M. Ochi, R. Kurihara, A. Miyake, Y. Yamasaki, M. Tokunaga, H. Nakao, K. Kuroki, T. Kida, M. Hagiwara, H. Murakawa, N. Hanasaki, and H. Sakai, Phys. Rev. B 107, L121112 (2023).
  31. [35]Z. Fang, N. Nagaosa, K. S. Takahashi, A. Asamitsu, R. Mathieu, T. Ogasawara, H. Yamada, M. Kawasaki, Y. Tokura, and K. Terakura, Science 302, 92-95 (2003).
  32. [36]N. Kanazawa, M. Kubota, A. Tsukazaki, Y. Kozuka, K. S. Takahashi, M. Kawasaki, M. Ichikawa, F. Kagawa, and Y. Tokura, Phys. Rev. B 91, 041122(R) (2015).
  33. [37]P. K. Sivakumar, B. Göbel, E. Lesne, A. Markou, J. Gidugu, J. M. Taylor, H. Deniz, J. Jena, C. Felser, I. Mertig, and S. S. P. Parkin, ACS Nano 14, 13463-13469 (2020).
  34. [38]J. Matsuno, N. Ogawa, K. Yasuda, F. Kagawa, W. Koshibae, N. Nagaosa, Y. Tokura, and M. Kawasaki, Sci. Adv. 2, e1600304 (2016).
  35. [39]K. Yasuda, R. Wakatsuki, T. Morimoto, R. Yoshimi, A. Tsukazaki, K. S. Takahashi, M. Ezawa, M. Kawasaki, N. Nagaosa, and Y. Tokura, Nat. Phys. 12, 555-559 (2016).
  36. [40]J. Jiang, D. Xiao, F. Wang, J.-H. Shin, D. Andreoli, J. Zhang, R. Xiao, Y.-F. Zhao, M. Kayyalha, L. Zhang, K. Wang, J. Zang, C. Liu, N. Samarth, M. H. W. Chan, and C.-Z. Chang, Nat. Mater. 19, 732-737 (2020).
  37. [41]W. Wang, Y.-F. Zhao, F. Wang, M. W. Daniels, C.-Z. Chang, J. Zang, D. Xiao, and W. Wu, Nano Lett. 21, 1108-1114 (2021).
  38. [42]T. Okubo, S. Chung, and H. Kawamura, Phys. Rev. Lett. 108, 017206 (2012).

Paper details

vlnc:W_b2c2najp
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents