Fabrication of high electron mobility and high photoluminescence quantum yield nanoscrolled monolayer MoS2

Abstract

We fabricated the 1D nanoscrolled monolayer MoS2 (1L-MoS2) with superior characteristics from 1L-MoS2 film in a facile route, using a suitable organic solvent with optimum surface tension, evaporation rate and dielectric constant, which facilitates the controlled scroll formation. These nanoscrolls behave as multilayers in morphology and monolayer electronically. The nanoscrolls exhibited a direct optical gap with enhanced photoluminescence quantum yield stemming from the weak interlayer coupling among constituent layers and were corroborated by low-frequency Raman measurements and Kelvin probe force microscopy measurements. Furthermore, enhanced photoluminescence emission after annealing uncovers the thermal stability of nanoscrolls. In addition, conducting atomic force microscopy results exhibit a significantly higher photocurrent in the nanoscrolled 1L-MoS2 compared to the 1L-MoS2. We also realized significantly improved field effect transistor device parameters in nanoscrolled 1L-MoS2 devices. In nanoscrolled devices, we report the highest mobility value of 2400 cm2V-1s-1 reported in any form of 1L-MoS2.

*Corresponding authors e-mail id: [email protected], [email protected], [email protected]

keywords: Monolayer; Raman; TMDs; mobility; Surface potential; Shear mode; Breathing mode

Introduction

Ultra-thin monolayer MoS2\mathrm{MoS}_2 (1L1\mathrm{L}-MoS2\mathrm{MoS}_2) attracted a great deal of attention among the research community because of its interesting electronic and optical properties, with the observation of direct band gap and enhanced photoluminescence (PL) quantum yield (QY). [1] The PL QY of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 can be enhanced by doping, [2] surface treatment, [3] and increasing the heat dissipation area. [4] Recently, it has been reported that PL QY of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 can be enhanced with an increase in the flake area owing to the availability of a large heat-dissipating area. [4] In particular, large-area 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 provides one-order higher PL QY than mechanically exfoliated 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 and two-order higher than small-sized as-grown chemical vapour deposition (CVD) grown flakes. [4] At the same time, devices fabricated with large channel dimensions may not meet the required demand to fabricate miniaturized and compact next-generation electronic devices. In other words, there is a trade-off between the availability of large heat-dissipating areas and the compactness of the devices. Therefore, it is imperative to eliminate the bottleneck by designing a compact structure that retains the characteristics of large-area 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. It is worth mentioning that the optical absorption coefficient in the visible wavelength of the electromagnetic spectrum of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 is significantly high compared to that for conventional semiconductors. [4] However, the overall light absorption is limited by the atomic scale thickness of monolayer MoS2\mathrm{MoS}_2. Thus, the structure containing multiple layers possessing the monolayer behaviour will be necessary for a significant amount of absorbed light in the visible range.

Recently, the one-dimensional (1D1\mathrm{D}) nanostructures designed from 2D2\mathrm{D} monolayers have opened new avenues for tuning their structural, electronic, and optical properties. [5, 6]

According to the theoretical calculations, the nanoscrolls have a unique topology, which makes them useful in flexible electronics, energy storage, and optical resonator applications.[7]

The scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} gained substantial attention because it exhibited higher light-matter interactions, which resulted in higher photo-responsivity than the planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}[8]. In scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}, the transportation of the carriers occurs in their constituent layers, which is quite different from their respective multilayers.[9] For the first time, amorphous MoS2\mathrm{MoS}_{2} nanoscrolls were prepared by the Ar plasma-assisted method.[10] The PL properties of nanoscrolled MoS2\mathrm{MoS}_{2} vary significantly depending on the fabrication process.[8, 9, 11, 12, 13] Table S1 summarizes the optical properties of reported nanoscrolled MoS2\mathrm{MoS}_{2} samples. So far, the nanoscrolls were mostly fabricated by the self-rolling method. The self-rolling was initiated by the evaporation of volatile organic solvent over the monolayer. Usually, isopropyl alcohol (IPA)[12] and acetone[11] were used as organic solvents because of their low surface tension and high evaporation rates. However, the PL emission studies were absent in nanoscrolls fabricated using IPA.[8, 12] In contrast, the self-rolled nanoscrolls fabricated with the aid of acetone showed four times higher PL intensity.[11] Unfortunately, PL emission in these samples was quenched after annealing (100 °C for 1h). In addition, capillary force-driven self-rolls of vertical van der Waals heterostructures (SnS2/WSe2\mathrm{SnS}_{2}/\mathrm{WSe}_{2}) were also prepared using a mixture of ethanol, water, and ammonia.[5] However, a reduction in PL emission was observed in heterostructured scrolls compared to planar structures, and it was attributed to their intimate interlayer interactions. Alternatively, the mechanical force-induced scroll fabrication has also been investigated using a mixture of ethanol and pure water.[8, 9] The strain-induced MoS2\mathrm{MoS}_{2} nanoscrolls fabricated using ethanol solution (volume ratio of ethanol: water = 2:1) showed properties of multilayered MoS2\mathrm{MoS}_{2} with reduced PL QY.[9, 13] Scrolls fabricated by wtheater-drag method lack PL measurements.[8] In addition, the mechanical force-induced rolls are mostly prone to structural deformity due to stacking disorder and non-uniform rolling. So far, PL emission was either not observed or quenched after annealing in earlier reported nanoscrolled MoS2\mathrm{MoS}_2[8]. Thus, fabrication of nanoscroll MoS2\mathrm{MoS}_2 retaining the monolayer properties and maintaining thermal stability also is necessary for device applications.

In this report, we developed and demonstrated the effective and facile route to fabricate the thermally stable nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. The self-rolled nanoscrolls were fabricated by using absolute ethanol. The scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 exhibits a high quantum yield of 2.95% and up to five times more PL intensity than remnant 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. The enhancement in the PL emission was attributed to negligible interlayer coupling among constituent layers. Low-frequency Raman and Kelvin probe force measurements confirm negligible interlayer coupling. From the PL analysis, it was found that interlayer coupling in nanoscrolls further weakened after annealing. The annealed nanoscrolls have shown nearly six times higher PL intensity compared to its counter planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 structures. The nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 showed significantly improved electronic and optoelectronic properties compared to their planar counterparts.

Self-rolled nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 fabrication

The nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 was fabricated from CVD-grown 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 film. The as-grown large-area 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 on SiO2/Si\mathrm{SiO}_2/\mathrm{Si} substrate was taken as the starting material. A little (15–20 µl) amount of absolute ethanol (Sigma Aldrich, purity 99.9 %) was dropped on the sample surface containing 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. The optical microscope captured the step-by-step image of an exemplary nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 at the formation stage (Figure 1). In addition, nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 fabrication steps were provided schematically in supplementary (Figure S1). Figure 1a-Figure 1c illustrates the optical micrographs at each stage of the nanoscroll formation. Figure 1a depicts the ethanol drop on the planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 surface. Subsequently, the size of the ethanol drop shrinks due to evaporation at room temperature (RT) (Figure 1b). The complete evaporation of ethanol generates the rolled structures in a few areas (Figure 1c). The high magnification image of one of the fabricated nanoscrolls was provided in Figure 1d. Moreover, the optical contrast between 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 and rolled structure exhibits the successful formation of scrolled MoS2\mathrm{MoS}_2 (Figure 1d). Immediately after the formation of the scroll, sample was placed under an IR lamp for 1 h to remove any ethanol residues from MoS2\mathrm{MoS}_2 surface. Interestingly, scroll formation was only observed in certain regions of the sample. In particular, scroll formation was initiated at the grain boundaries region of large area MoS2\mathrm{MoS}_2 film and edges of triangular flakes. Thus, one can speculate that the scroll formation might have happened because of the penetration of ethanol between the flake and substrate at the grain boundaries and edge region and subsequent evaporation. Ethanol delaminated the 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 during the evaporation at RT. During the evaporation of ethanol, the heat might be extracted from the planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 structure, which resulted in reduction of surface energy.[9] The decrease in surface energy is compensated by the change of planar MoS2\mathrm{MoS}_2 structure to its scrolled form.

Image not extracted

Figure 1. Step-by-step monitoring the fabrication of nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}. (a) The surface of 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} under the drop of absolute ethanol. (b) Shrinkage of ethanol drops during its evaporation (boundary marked with red dotted curve and arrow marks indicate the direction of shrinkage). (c) Multiple scrolls formed after ethanol evaporation (pointed by arrow marks). The given scroll selected for further studies was highlighted with a dotted box. Scale bar: 20 μ\mum (d) High magnification image of one of the nanoscrolls. Scale bar: 10 μ\mum.

In general, the scroll formation process is governed by solid-liquid interfacial energy and the solvent surface tension and evaporation rate.[5] The interfacial energy is solely responsible for the intercalation of solvent molecules to delaminate the 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 from the SiO2\mathrm{SiO}_2 substrate. The surface tension and evaporation rate of the solvent are two important parameters as they decide the capillary force (flow direction of the solvent during evaporation) at the scroll formation stage.[5] In earlier reports, the mixture of ethanol and water, IPA, and acetone solvents were used for the scroll fabrication. Unfortunately, PL emission was either suppressed or reduced after annealing in these scrolls compared to the planar MoS2\mathrm{MoS}_2.[11] Here, we fabricated the scrolls using absolute ethanol because of its optimum physical properties, such as surface tension and evaporation rate. Generally, the mixture of ethanol and water has a higher surface tension (∼72.8 mN⋅m−1\sim72.8\ \mathrm{mN}\cdot\mathrm{m}^{-1} of water-air @ 20 ∘C20\,^\circ\mathrm{C}) than that of pure organic solvents like ethanol (∼22.1 mN⋅m−1\sim22.1\ \mathrm{mN}\cdot\mathrm{m}^{-1} of ethanol-air @ 20 °C), IPA (∼23 mN⋅m−1\sim23\ \mathrm{mN}\cdot\mathrm{m}^{-1} of IPA-air @ 20 °C) and acetone (∼25.2 mN⋅m−1\sim25.2\ \mathrm{mN}\cdot\mathrm{m}^{-1} of acetone-air @ 20 °C). [14] The high surface tension of the solvent is prone to bead-up and deteriorates the uniformity of the scroll.[5] Moreover, ethanol has optimum evaporation rate of 119 mg⋅m−2⋅s−1119\ \mathrm{mg}\cdot\mathrm{m}^{-2}\cdot\mathrm{s}^{-1} and vapour pressure ∼7.86 kPa\sim7.86\ \mathrm{kPa}@25 °C compared to those of acetone (evaporation rate 504 mg⋅m−2⋅s−1504\ \mathrm{mg}\cdot\mathrm{m}^{-2}\cdot\mathrm{s}^{-1} and vapour pressure ∼30.8 kPa\sim30.8\ \mathrm{kPa}@25 °C) and IPA (evaporation rate 75.6 mg⋅m−2⋅s−175.6\ \mathrm{mg}\cdot\mathrm{m}^{-2}\cdot\mathrm{s}^{-1} and vapour pressure ∼5.69 kPa\sim5.69\ \mathrm{kPa}@25 °C).[14] The optimum evaporation rate of ethanol is reasonably advantageous as it allows sufficient time for a uniform scroll formation process.

In addition, it was also reported that the formation of scrolls and their stability is governed by the thermodynamical parameters. The formation of scrolls is allowed if the enthalpy (HH) decreases upon scrolling. The change in enthalpy, ΔH=ΔU+ΔW\Delta H = \Delta U + \Delta W, where ΔU\Delta U stands for change in internal energy and ΔW\Delta W stands for work done due to rolling. Most importantly, the ΔW\Delta W is dependent on the dielectric constant of the solvents involved in the scroll formation. [6] At room temperature, the dielectric constant of ethanol, IPA and acetone are 24.55, 18.3, and 20.7, respectively. The dielectric constant value of ethanol is comparatively higher than IPA and acetone. Thus, the self-rolling process in an ethanol medium is relatively slower than in IPA and acetone.[15] Therefore, absolute ethanol is advantageous over other organic solvents for controlled and uniform scroll formation.

Results and Discussions

The cross-sectional view of the scrolled 1L-MoS2_2 is represented as a schematic in Figure 2a. In the present study, we compared the optical properties of the scroll with remnant 1L-MoS2_2 for the fair assessment. The multiple scrolls were formed using a single drop of ethanol (Figure S2). Among them, we carried out a detailed optical analysis on a particular scroll (Figure 2b). FESEM images of other scrolled 1L-MoS2_2 structures are shown in Fig S3.

Image not extracted

Figure 2. a) Schematic representing a cross-sectional view of 1L-MoS2_2 nanoscroll. The optical image (b) and its respective FESEM image (c) of the particular scroll. Scale bar: 5 μ\mum. d) The topographic image of the same nanoscroll. Inset shows the height profile across the scroll. The line profile was taken along the green line shown (d).

Figure 2c shows the typical FESEM image of the same scroll shown in Figure 2b, and its high magnification image is provided in Figure S4a. It reveals that the monolayer is uniformly rolled to form the tubular structure. In addition, it is apparent that the fabricated scrolls are clean and wrinkle-free. The length of the given nanoscroll is measured to be ~13.5 μm. The lateral size of the scroll across length was in the range of 220-250 nm. We have carried out an AFM study to estimate the thickness of the 1L-MoS2_2 and the height of the nanoscroll. The thickness of 1L-MoS2_2 is 0.85 nm (Figure S4b,c). The AFM image of the typical nanoscrolled 1L-MoS2_2 was provided in Figure 2d. The surface topography of the nanoscroll is uniform. From the height profile, the thickness of the nanoscroll was calculated to be 160±\pm10 nm (insets of Figure 2d). We calculated the number of layers present in the scroll by assuming it as tubular form, and detailed calculation steps are provided in the supplementary material. In the given scroll, approximately 28 number of 1L-MoS2_2 layers are estimated to be present.

Raman measurements were carried out to assess the phase and number of layers present in the planar and nanoscrolled MoS2_2. In the back-scattering configuration, the 1L-MoS2_2 has two prominent Raman peaks corresponding to E2g1E^{1}_{2g} and A1gA_{1g} modes.[16, 17] Raman spectra of a typical planar and nanoscrolled MoS2_2 are provided in Figure 3a. In planar MoS2_2, the E2g1E^{1}_{2g} and A1gA_{1g} Raman modes are observed with ca. 383.9 cm−1^{-1} and 403.6 cm−1^{-1}, respectively. At the same time, E2g1E^{1}_{2g} and A1gA_{1g} Raman modes are observed at 383.5 cm−1^{-1} and 402.6 cm−1^{-1}, respectively, for nanoscrolled 1L-MoS2_2. A small red-shift in E2g1E^{1}_{2g} mode is attributed to the development of tensile strain due to the curved morphology in the scroll.[18] The red-shift of A1gA_{1g} (1 cm−1^{-1}) can be understood in terms of restoring force. It is well known that out-of-plane A1gA_{1g} phonon mode frequency is strongly dictated by the restoring force, whereas in-plane E2g1E^{1}_{2g} mode is dictated by dielectric screening.[17, 19, 20] In the form of a scroll, the bonding between flake and SiO2\mathrm{SiO}_{2} happened to be broken, leading to the disappearance of restoring force originated from the bonding between SiO2\mathrm{SiO}_{2} and MoS2\mathrm{MoS}_{2}. Thus, A1g\mathrm{A}_{1\mathrm{g}} phonon mode red-shifted in nanoscrolled MoS2\mathrm{MoS}_{2} as compared to planar MoS2\mathrm{MoS}_{2}. Raman analysis was carried out on multiple nanoscrolls and the results were summarized in Table S2. In addition, we compare the frequency difference (Δ\Delta) between two prominent Raman modes (E2g1\mathrm{E}^{1}_{2\mathrm{g}} and A1g\mathrm{A}_{1\mathrm{g}}), as it reveals the number of layers present in a MoS2\mathrm{MoS}_{2} flake.[16] In planar MoS2\mathrm{MoS}_{2}, Δ\Delta is 19.7 cm−1^{-1}, which confirms that planar flake is indeed monolayer.[4, 16] Interestingly, the Δ\Delta value in scrolled MoS2\mathrm{MoS}_{2} was 19.1 cm−1^{-1}. The Δ\Delta value of nanoscrolls was similar to that for monolayer flakes, which confirmed the monolayer characteristics of the scroll.[16] As mentioned before, the scroll contains approximately 28 layers. Thus, the Δ\Delta was expected to be of the bulk MoS2\mathrm{MoS}_{2} (>25>25 cm−1^{-1}).[16] It is worth mentioning that scrolls fabricated by many other groups by using different organic solvents have shown multilayer characteristics.[8, 9, 11, 12, 13] In their work, Δ\Delta value was in the range of 21-24 cm−1^{-1}, which confirms that the scrolls were indeed multilayer in nature (Table S1). The increased Δ\Delta values were attributed to the stacking-induced structural changes in scrolled MoS2\mathrm{MoS}_{2}.[9] As a result, the potential application of the monolayers cannot be fulfilled through scrolls with interacting constituent layers. In the present study, monolayer characteristics (Δ<20\Delta< 20 cm−1^{-1}) were observed in nanoscrolled MoS2\mathrm{MoS}_{2}. In other words, in contrast to the reported works, the fabricated nanoscrolls act as a monolayer even though they contain multiple layers. The monolayer behaviour of nanoscrolled 1L-MoS2\mathrm{MoS}_{2} may be attributed to the non-interacting nature of constituent layers.

Image not extracted

Figure 3. Figure 3. Comparative optical characterization of planar and nanoscrolled 1L-MoS2_2. (a) Raman and (b) PL spectra of planer and scrolled MoS2_2. The Δ\Delta value in both planar and nanoscrolled MoS2_2 confirms the monolayer nature of MoS2_2. Dotted lines are guide to the eye. Insets of (b) show the intensity map at a peak energy of A-exciton (1.84 eV). Scale bar (inset figure): 2 μ\mum.

A 1L-MoS2\mathrm{MoS}_{2}, being a direct band gap semiconductor, shows intense PL emission, which makes it suitable for many optoelectronic applications.[1, 2] The RT PL spectra of 1L-MoS2\mathrm{MoS}_{2} and nanoscrolled 1L-MoS2\mathrm{MoS}_{2} are shown in Figure 3b. The spectra fitted with Gaussian curves were provided in the supplementary material (Figure S5 and analysis in Table S3a). In 1L-MoS2\mathrm{MoS}_{2}, PL spectrum was majorly contributed by A-excitons (1.84 eV) over B-excitons (1.96 eV) and trions (1.80 eV) emission. Similarly, PL spectra of nanoscrolled 1L-MoS2\mathrm{MoS}_{2} were contributed by A-exciton (1.83 eV), B-exciton (1.94 eV) and trions (1.79 eV) emission. Interestingly, the nanoscrolled 1L-MoS2\mathrm{MoS}_{2} exhibits the direct band gap features, which is a primary signature of 1L-MoS2\mathrm{MoS}_{2}. Compared to 1L-MoS2\mathrm{MoS}_{2}, the PL spectra of nanoscrolled 1L-MoS2\mathrm{MoS}_{2} were red-shifted by 10 meV. The observed negligible red-shift may be attributed to the reduction in the dielectric screening upon rolling, as it becomes free-standing after being detached from the SiO2\mathrm{SiO}_{2}substrate.[21] Moreover, it was also reported that the red-shift in exciton peak energy was also attributed to the introduction of bending strain.[22] Previously, blue-shift in exciton peak positions in nanoscrolled MoS2\mathrm{MoS}_{2} were reported, and it was attributed to the existence of solvent molecules among the interlayer gaps.[11] In the present work, the negligible shift in exciton peak positions reveals the non-existence of ethanol molecules at interlayer gaps. PL analyses on various spots of a given scroll and other scrolls were provided in the supplementary material (Figure S6 and analysis in Table S3b). Furthermore, a low emission peak at 1.64 eV was observed in the PL spectrum of scrolled 1L-MoS2\mathrm{MoS}_{2} (Figure 3b). The low energy peak might be attributed to interlayer coupling (II) peak, and it is usually observed in multilayer MoS2\mathrm{MoS}_{2} with weak inter-layer coupling and twisting of layers. [23, 24] However, II–peak in PL spectra of monolayer MoS2\mathrm{MoS}_{2} was also reported earlier under the application of external strain.[18, 20] Moreover, a small curvature or bending in the monolayer MoS2\mathrm{MoS}_{2} film can modulate the band gap by enhancing the interlayer coupling.[18] Therefore, the origin of II–peak in scrolled 1L-MoS2\mathrm{MoS}_{2} may be traced from the developed local bending strain. Compared to 1L-MoS2\mathrm{MoS}_{2}, the mean and maximum enhancement in PL integrated intensity of nanoscrolled 1L-MoS2\mathrm{MoS}_{2}is ~ 4 and ~5.2 times, respectively (Figure 3b and Table S4). The inset of Figure 3b shows the PL imaging of scrolled region. The PL imaging was carried out using A-exciton intensity. The PL intensity was high over the scroll region compared to remnant MoS2\mathrm{MoS}_{2}. Here, the overall enhanced PL intensity in nanoscrolls is attributed to the noninteracting nature of constituent monolayers. The constituent layers of the scrolled MoS2\mathrm{MoS}_2 are quite different from the bulk MoS2\mathrm{MoS}_2. In general, the bilayer MoS2\mathrm{MoS}_2 (2L-MoS2\mathrm{MoS}_2) shows a two-order less PL intensity compared to 1L-MoS2\mathrm{MoS}_2, and the emission intensity further reduces as the number of layers increases.

PL quantum yield (QY) was measured using optical absorbance and PL, as described in our earlier report.[4] Absorbance for the nanoscrolled 1L-MoS2\mathrm{MoS}_2 and 1L-MoS2\mathrm{MoS}_2 films were measured to be 0.62±0.080.62 \pm0.08 and 0.3±0.050.3 \pm0.05, respectively, and detailed in the supplementary information (Figure S7). The improved absorbance was attributed to the enhanced light-matter interaction originating from the existence of multiple layers in the scroll. The PL QY of 1L-MoS2\mathrm{MoS}_2 and nanoscrolled 1L-MoS2\mathrm{MoS}_2 were calculated to be 1.3% and 2.95%, respectively. The higher QY was attributed to the enhancement of PL emission in nanoscrolled 1L-MoS2\mathrm{MoS}_2 compared to the planar form.

The interlayer coupling can be analyzed using shear (SS) and layer breathing (LB) modes of MoS2\mathrm{MoS}_2.[25] Usually, shear and breathing modes are not shown in Raman spectra because of the constraints of the Rayleigh rejection filter. Low-frequency (LF) Raman measurements were carried out on fabricated nanoscrolls to investigate the interlayer coupling. The LF Raman spectra of multilayered MoS2\mathrm{MoS}_2 are dominated by interlayer shear (SS or E2g2E^2_{2g}) and layer-breathing (LB or B2g2B^2_{2g}) mode. The SS mode represents out-of-phase in-plane vibrations of constituent MoS2\mathrm{MoS}_2 layers, whereas the LB mode represents out-of-phase out-of-plane vibrations of the MoS2\mathrm{MoS}_2 layers.[26] Thus, SS and LB modes are always absent in 1L-MoS2\mathrm{MoS}_2 due to the non-existence of an additional layer for interactions. Figure 4 shows the typical LF Raman spectra of mono-, bi-, and nanoscrolled MoS2\mathrm{MoS}_2. The bilayer spectrum was provided for the comparison. The SS and LB modes were absent in 1L-MoS2\mathrm{MoS}_2, whereas SS (20.6 cm−1^{-1}) and LB (36.5 cm−1^{-1}) modes were observed in bilayer (2L) MoS2\mathrm{MoS}_2. Interestingly, in nanoscrolled 1LMoS2_2, the existence of insignificantly minute SS-mode and the absence of LB mode reveals the existence of weak interlayer coupling.[25] Thus, the LF Raman results reinforced the PL results that interlayer coupling is negligible in nanoscrolled 1L-MoS2_2.

Image not extracted

Figure 4. Low-frequency Raman spectra of 1L-MoS₂, 2L-MoS₂ and nanoscrolled 1L-MoS₂.

The surface potential (SP) of a MoS2_2 film is quite sensitive to the number of layers because of the interlayer screening effect.[27] We carried out Kelvin probe force microscopy (KPFM) measurements on as-grown MoS2_2 flake, which contains the mono-, bi- and multilayer to corroborate our assumption (Figure 5a). The presence of mono-, bi and multilayer was confirmed by the Raman and PL analysis (not shown in the figure). From the contact potential difference map, it is apparent that SP varied depending on the thickness of the flake (Figure 5b). The SP of the bilayer increased by 100 mV compared to the monolayer MoS2_2. Thus, SP would change if there is a strongly interacting layer. Subsequently, KPFM measurements were carried out on nanoscrolled MoS2_2 and the remnant MoS2_2. Figure 5c shows the SP map of the scrolled and monolayer region. It was found that the SP of SiO2_2 was higher than 1L-MoS2_2 and nanoscrolled MoS2_2. The SP values of SiO2_2 and 1L-MoS2_2 were 520 and 280 mV, respectively (Figure 5d). Interestingly, negligible change in SP was observed for the monolayer and scrolled region except for the edges of scrolls. The unchanged surface potential infers a negligible change in electronic properties. Importantly, the unchanged SP value among the monolayer and scrolls concludes the negligible inter-layer coupling among the constituent layers of nanoscrolled 1L-MoS2_2.

Image not extracted

Figure 5. Surface potential analysis of 1L-, 2L- and nanoscrolled 1L-MoS2_2 using KPFM. a) KPFM image showing the spatial variation of SP in a flake containing, mono-, bi- and multi-layered MoS2_2. b) Line profile across flake. The line profile was taken along the green line (a). c) SP map of nanoscrolled 1L-MoS2_2 region. d) Line profile of SP provided was taken along the green line in (c).

To investigate the thermal stability of the as-fabricated scroll, we have carried out vacuum annealing at 200 °C for 2h. We restricted the annealing temperature to 200 °C to avoid the defect introduction to the 1L-MoS2_2 system.[4, 28] The PL spectra of the annealed sample are shown in Figure 6a. The integrated PL intensity was increased by ~6.4 times compared to remnant 1L-MoS2_2. Moreover, annealed scrolled 1L-MoS2_2 shows ~ 5 times. higher integrated PL intensity compared to as-fabricated scroll (Figure 3b). The enhancement of PL intensity further ascertains the weakening of interlayer coupling among constituent layers. To date, all the studies have failed to fabricate thermally stable nanoscrolls of 1L-MoS2\mathrm{MoS}_{2}.[8, 9, 11, 12, 13] Here, we achieve the formation of thermally stable scrolls because of the selection of absolute ethanol over other solvents. In this context, as discussed earlier, the vacuum annealing of MoS2\mathrm{MoS}_{2} nanoscrolls at 100 °C for 1h with Ar atmosphere was previously reported.[11] The PL integrated intensity was quenched ~ 4 times with significant red-shift. In contrast, we found a negligible blue shift of 10 meV in the A-exciton peak position after annealing. Thus, our PL results of annealed 1L-MoS2\mathrm{MoS}_{2} nanoscrolls signify that scrolls are devoid of ethanol residues because of negligible shifts in peak positions and enhanced intensity. We also observed that the interlayer peak in the nanoscrolled 1L-MoS2\mathrm{MoS}_{2} disappeared after annealing. It demonstrates further weakening of the interlayer coupling among their constituent layers. The reduction in interlayer coupling after annealing may also contribute to enhanced PL intensity.

Image not extracted

Figure 6. Raman and PL analysis of vacuum annealed nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}. Photoluminescence (a), Raman (b) and LF Raman (c) spectra of vacuum annealed nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}. LF Raman measurements were carried out at three arbitrary positions (P1, P2, and P3) on nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}.

We have carried out Raman analysis on annealed MoS2\mathrm{MoS}_{2} scrolls to further investigate the annealing effect. The Raman peak positions of E2g1E^{1}_{2g} Raman mode are 383.7 and 384.0 cm−1\mathrm{cm}^{-1} for monolayer and scrolled 1L-MoS2\mathrm{MoS}_{2}, respectively. The small blue-shift in E2g1E^{1}_{2g} mode in scrolled 1L-MoS2\mathrm{MoS}_{2} may be because of possible molecular rearrangement in the constituent layers with the annealing treatment.[16] Similarly, the A1gA_{1g} Raman mode in 1L-MoS2\mathrm{MoS}_{2} and scrolled 1L-MoS2\mathrm{MoS}_{2} was found at 402.8, and 404.0 cm−1\mathrm{cm}^{-1}, respectively (Figure 6b). After annealing, the Δ\Delta value of scrolled 1L-MoS2\mathrm{MoS}_{2} was 20 cm−1\mathrm{cm}^{-1} which confirmed the retaining of monolayer nature even after annealing. Thus, the fabricated nanoscrolls were thermally stable. The E2g1E^{1}_{2g} and A1gA_{1g} phonon modes were blue-shifted by 0.5 cm−1\mathrm{cm}^{-1} and 1.4 cm−1\mathrm{cm}^{-1}, respectively, compared to the as-fabricated scroll. The observed blue-shift was attributed to the relaxation of local bending strain which was developed during the nanoscroll formation stage.[22] It is also well known that the A1gA_{1g} mode is sensitive to carrier density, and the hardening of A1gA_{1g} was reported with decreased carrier density.[17] The blue-shift of A1gA_{1g} mode indicates the reduced carrier density after annealing. The increased PL intensity after annealing may be attributed to the reduction in carrier density, which decreases the Auger recombination. The effect of annealing on SS and LB modes is probed by LF Raman measurements (Figure 6c). It was found that SS and LB modes were absent in nanoscrolls after annealing. Thus, the minor signal of SS mode observed in the as-fabricated scroll (Figure 4) disappeared after annealing. The absence of SS and LB modes in an annealed sample further confirms the negligible effect of annealing on the non-interacting nature of the constituent layers.

I-V measurements were carried out using conducting atomic force microscopy (C-AFM) under dark and illumination conditions to study the photo-response of the annealed nanoscrolled 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2. The illumination was performed using the feedback laser (wavelength ∼650 nm\sim650\ \mathrm{nm}) source. The detailed measurement steps are provided in the experimental section. The inset of Figure 7a represents the schematic of the C-AFM measurement set-up. I-V characteristics of the 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2 and nanoscrolled 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2 without illumination are provided in Figure 7a. The non-linear behaviour of I-V graphs represents the formation of the Schottky junction between the Pt-tip with MoS2\mathrm{MoS}_2 layers. Pt and Au electrodes form Schottky and Ohmic junctions, respectively, with MoS2\mathrm{MoS}_2 material.[29] Further, I-V curves also indicate the pp-type behavior of both 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2 and nanoscrolled 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2. The origin of pp-type behaviour stemmed from the induced doping by the Pt tip used in C-AFM measurements. In general, the dark I-V characteristics are nearly the same for both 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2 and nanoscrolled 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2. The result is obvious because the constituent layers in the nanoscrolls are not interacting with each other. Under illumination in the forward bias condition, the measured current increases approximately from - 0.5 to - 0.8 nA and - 0.5 to - 2.24 nA at -4.5 V in 1L-MoS21\mathrm{L}\text{-}\mathrm{MoS}_2 and nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2, respectively. Here, the scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 shows approximately six times higher photocurrent as compared to the 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. In addition, under positive bias, the measured photocurrent in scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 is significantly higher as compared to that of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. The higher net photocurrent in nanoscrolled MoS2\mathrm{MoS}_2 may have originated from its higher absorption cross-section due to the availability of multiple monolayers. Each monolayer generated the photo-carriers and contributed to enhancement in the overall current. Along with point I-V measurements, we have also carried out a current map at a constant voltage of −3.5-3.5 V. Figure 7c and Figure 7d represent the current mapping of the nanoscrolls under dark and illumination, respectively. In the dark, the measured current is ∼100\sim100 pA in the region of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 (lower right corner) and a relatively higher current over the scroll region (nA). These current values slightly increase under illumination. To sum up, the photocurrent in the scrolled region is higher as compared to remnant 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. The topography of a typical scroll is provided in the inset of Figure 7b.

Image not extracted

Figure 7. Conductive AFM-based I-V characteristics of 1L-MoS2_2 and scrolled 1L-MoS2_2 without (a) and (b) with spill-over light from feedback laser. Inset of (a) represents the schematic of C-AFM measurement. The Inset of (b) corresponds to the topography of the scroll. The C-AFM image of scrolled 1L-MoS2_2 region under (c) dark and (d) illumination. Scale bar: 1 μ\mum.

FET devices were fabricated on planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 and nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 to evaluate the electrical properties. The detailed fabrication protocols were provided in the experimental section. After fabricating the multiple FETs, we measured both their output and transfer characteristics. In the output characteristics, the gate voltage (VgsV_{\mathrm{gs}}) was varied from 0 V to 20 V with an interval of 5 V (Figure 8a and Figure 8b). In both planar and scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 based FET devices, IdsI_{\mathrm{ds}} were found to raise linearly up to VdsV_{\mathrm{ds}} of ∼4\sim4 V and thereafter saturated. The observed IdsI_{\mathrm{ds}} versus VdsV_{\mathrm{ds}} results in both the devices are typical behaviour of FET devices. At VgsV_{\mathrm{gs}} of 20 V, the saturation drain currents are 3 and 45 μA/μm\mu\mathrm{A}/\mu\mathrm{m} for planar and nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2, respectively. The one-order (15 times) higher drain current is attributed to the availability of multiple paths for transporting the electrons in constituent layers in scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 compared to 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. For similar device configurations, the saturation drain currents reported in literature are 1.35 and 0.14 μA/μm\mu\mathrm{A}/\mu\mathrm{m} for planar 1L1\mathrm{L}MoS2\mathrm{MoS_2},[30, 31] Moreover, we have also plotted the transfer characteristics of both planar and scrolled 1L-MoS2\mathrm{MoS_2} to extract the threshold voltage, electron mobility and on/off current ratio (Figure 8c and Figure 8d). In addition, we fabricated the multiple devices on planar and nanoscrolled 1L-MoS2\mathrm{MoS_2} and the transfer characteristics of these devices were provided in Figure S8 and Figure S9, respectively. Subsequently, the key device parameters are summarized in the Table 1. The threshold voltage (VtV_\mathrm{t}) was calculated using Y-function method.[32] The mean VtV_\mathrm{t} values are 5.7 and 5.2 V for planar and nanoscrolled 1L-MoS2\mathrm{MoS_2}, respectively. Earlier it was reported that VtV_\mathrm{t} was substantially decreased by increasing the number of MoS2\mathrm{MoS_2} layers.[33] However, the minute decrement in VtV_\mathrm{t} for nanoscrolled 1L-MoS2\mathrm{MoS_2} is attributed to weak interlayer coupling that exists among the constituent layers of the scroll. Generally, the on-state performance of the FET is influenced by the carrier mobility. We calculated the field-effect electron mobility (μ\mu) from peak transconductance using equation (Eq. (1))[32]

Channel MaterialIonI_{\mathrm{on}} (max) (μA/μm\mu\mathrm{A}/\mu\mathrm{m})Threshold Voltage (V)Mobility (cm2V−1s−1\mathrm{cm}^{2}\mathrm{V}^{-1}\mathrm{s}^{-1})ON/OFF current ratio
1L-MoS2_2 film35.7 ±\pm 0.210.5 ±\pm 2.510610^{6}
Nanoscrolled 1L-MoS2_2455.2 ±\pm 0.22400 ±\pm 40010710^{7}

Table 1. Summary of key device parameters of back-gated FET fabricated on planar and nanoscrolled 1L-MoS2_2.

Image not extracted

Figure 8. Transfer and output characteristics of FET devices fabricated on planar and nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}. Output characteristics of (a) planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} FET and (b) nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} FET. Transfer characteristics of (c) planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} FET and (d) nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} FET. The insets of (c) and (d) show the FESEM image of typical FET devices fabricated on planar and scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}, respectively. Scale bar: 5 μm5\ \mu\mathrm{m}.

μ=LWCoxVds(ΔIdsΔVgs)(1)\mu= \frac{L}{W C_{\mathrm{ox}} V_{\mathrm{ds}}}\left(\frac{\Delta I_{\mathrm{ds}}}{\Delta V_{\mathrm{gs}}}\right) \tag*{(1)}

where CoxC_{\mathrm{ox}} is the gate insulator capacitance per unit area (11.51 ×10−9\times10^{-9} F⋅\cdotcm−2^{-2} for SiO2_2 of 300 nm), LL and WW are the length and width of the channel, respectively. The dimensions (L×WL \times W) of the planar and scrolled device are 10 μ\mum ×\times 10 μ\mum and 10 μ\mum ×\times 0.5 μ\mum, respectively. The slope ΔIds/ΔVgs\Delta I_{\mathrm{ds}}/\Delta V_{\mathrm{gs}} is calculated from the transfer characteristics curve in a linear regime at VdsV_{\mathrm{ds}} of 1 V. The field-effect electron mobility is calculated to be ∼\sim10.5 and ∼\sim2400(±\pm400) cm2^2V−1^{-1}s−1^{-1} for planar and nanoscrolled 1L-MoS2\mathrm{MoS_2}, respectively. The on/off current ratios were 10610^6 and 10710^7 for planar and scrolled 1L-MoS2\mathrm{MoS_2}, respectively. The above results indicate that nanoscrolled 1L-MoS2\mathrm{MoS_2} exhibits superior electronic properties compared to planar 1L-MoS2\mathrm{MoS_2}. Moreover, a one-order higher current ratio makes the scrolled 1L-MoS2\mathrm{MoS_2} suitable for digital applications. The key device parameters of nanoscrolled 1L-MoS2\mathrm{MoS_2} FETs were compared with the existing literature (Table S5). The two-order higher on/off current ratio and one-order higher electron mobility in our nanoscrolled 1L-MoS2_2 were observed compared to other reported nanoscrolled devices. As a matter of fact, the mobility value is the highest reported so far in any form of 1L-MoS2_2, including that for top gated planar 1L-MoS2_2, showing a mobility value of 1090 cm2V−1s−1\mathrm{cm}^{2}\mathrm{V}^{-1}\mathrm{s}^{-1} (Table S6).[34] Thus, compact optoelectronic devices can be realized using nanoscrolled 1L-MoS2_2, which retains the monolayer characteristics. Our results can be further extended to other 2D transition metal dichalcogenides monolayer structures to fabricate thermally stable scrolls.

As discussed earlier, countless attempts are made to fabricate the scrolled MoS2_2 with multiple layers which retain the monolayer nature.[8, 9, 11, 12, 13] Unfortunately, the fabricated scrolls behaved as multilayer MoS2_2 where PL emission either disappeared or was suppressed. Moreover, the fabricated nanoscrolls have poor thermal stability where PL emission was suppressed after annealing.[11] In the present study, nano-scrolls showed enhancement of PL intensity and negligible shift compared to the planar 1L-MoS2_2. In other words, the result signifies that nano-scrolls behave electronically in a similar manner to monolayers. The enhanced PL intensity is attributed to the non-interacting nature of constituent layers in the scroll. Interestingly, the monolayer behavior was further improved upon thermal annealing, which manifested their thermal stability. The properties of nanoscrolls are dependent on the arrangement of layers inside the scroll at their formation stage. The choice of solvent is most important as physical properties such as surface tension, evaporation rate, and dielectric constant strongly influence the scroll formation. The scrolls fabricated using the solvent with higher surface tension and evaporation rate increase the rolling speed. As a result, the stacking becomes imperfect and closely spaced layers are expected to form. Therefore, the interlayer interaction increases, and the scroll behaves as a multilayer. However, a solvent with optimum surface tension and evaporation rate can provide sufficient time for the formation of a scroll. In addition, the moderate dielectric constant of the solvent can further slowdown the formation of the scroll. In this context, the formation of a scroll using absolute ethanol is advantageous because of its optimum evaporation rate and moderate dielectric constant, which may slowdown the self-rolling process. As a result, one can expect a large separation between the constituent layers. The non-interacting nature of constituent layers might have originated from the large separation. Moreover, the constituent layers also retained the optical properties after a few months of fabrication (not shown here). It suggests that the scrolls have long-term stability in their optical properties. Therefore, our results find that absolute ethanol is a suitable solvent for the fabrication of nanoscrolls.

Conclusions

We strategically developed and demonstrated an effective and facile method to fabricate the thermally stable nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} from CVD-grown 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} film. A suitable solvent with low surface tension and evaporation rate, ethanol, was used to fabricate the nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}. The nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} retained the monolayer behaviour even though multilayer in morphology, which was confirmed by Raman spectroscopy. The nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2} showed enhanced PL QY because of approximately two times increase in the absorbance and five times increase in the PL emission, compared to 1L1\mathrm{L}-MoS2\mathrm{MoS}_{2}. In addition, low-frequency Raman measurements confirm the negligible interlayer coupling among constituent layers in the insignificant presence of S and LB mode. Moreover, the KPFM study revealed insignificant variation in SP between monolayers and scrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2, showing similar electronic properties of them. Furthermore, the enhancement of PL intensity (approximately six times) after annealing confirmed the thermal stability of fabricated nanoscrolls. The PL QY (2.95%) of nanoscroll 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 was significantly higher than the reported the PL QY of untreated 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. In addition, C-AFM measurements delineate that the nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 shows approximately six times higher photocurrent as compared to the 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. FET device fabricated on nanoscroll 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 has shown one order higher on/off ratio and two order higher mobility compared to the device fabricated on planar 1L1\mathrm{L}-MoS2\mathrm{MoS}_2. Therefore, fabricated nanoscrolls can be used for compact and high-performance optoelectronic devices.

Experimental section

The synthesis of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 flakes was carried out by the atmospheric pressure CVD technique. The MoS2\mathrm{MoS}_2 phase was formed by using molybdenum trioxide (MoO3\mathrm{MoO}_3) and S as precursor materials. The details of the synthesis steps can be found elsewhere.[2] The deposition of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 was carried out on SiO2\mathrm{SiO}_2(300 nm)/Si susbstrate. The growth of planar and nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 was confirmed by optical microscopy. All morphological information, including the lateral dimension of the nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 was extracted from field emission scanning electron microscopy (FESEM; Supra 55, Zeiss, Germany) images. The thickness of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 and the height of the nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 were measured by the atomic force microscopy (AFM) technique (MultiView 4000, Nanonics Imaging Ltd, Israel). The AFM measurements were carried out in intermittent mode. Vibrational and emission properties were studied usingRaman and PL spectroscopy, respectively. Raman and PL measurements were performed by using a 532 nm laser line with a power of 0.01 mW.

Raman scattered light and PL emission light were dispersed through 2400 lines/mm and 1800 lines/mm grating, respectively. Subsequently, the dispersed light was collected by using a charged coupled device detector. Low-frequency Raman measurements were carried out by using a WiTec Alpha 300RA micro-Raman spectrometer. Here, the sample was excited with a 532 nm laser source, and scattered light was dispersed through 1800 lines/mm grating. A Bragg grating (Rayshield{sup}TM`) was employed to cut off the Rayleigh line.

Current mapping and II-VV measurements were carried out using the conducting atomic force microscopy (C-AFM; Model No-NTEGRA II, NT-MDT, Russia). The whole metal Pt tip cantilever was used in contact mode. A typical load applied on the cantilever was ∼50\sim50 nN during electrical measurement. Gold wire with pressure contact served as one electrode, and the AFM tip served as the second electrode. The sample was biased, and the AFM tip was grounded during the measurement. The current mapping was performed under the two-pass technique. In first-pass, the current was measured with the illumination of an in-built laser (650 nm) which was used for the feedback mechanism. The spill-over light from the feedback laser generated significant photo-carriers, which increased the net current during mapping. In the second pass, the feedback laser was off, and hence, the current mapping was performed in the dark. Similarly, II-VV characteristics were also measured with and without the illumination of light from the feedback laser.

PL QY measurements

The PL QY of 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 and nanoscrolled 11-MoS2\mathrm{MoS}_2 was estimated using Rhodamine 6G (R6G) dye. The R6G shows 95% PL QY under 532 nm excitation. The steps involved in the estimation of PL QY can be found elsewhere.[4]

Nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2 based FET devices

Both planar and nanoscrolled 1L1\mathrm{L}-MoS2\mathrm{MoS}_2-based back-gated FETs were fabricated with the same channel length of 10 μm10\ \mu\mathrm{m}. The FET fabrication protocols can be found elsewhere.[28]

The electrodes (Au\mathrm{Au} (200 nm)/Ti\mathrm{Ti} (100 nm)) were prepared via the lift-off method by direct laser writer (M/s Microtech, Italy, Model No: LW405B) and wet chemical methods. The electrodes were deposited by dual-target DC magnetron sputtering. The FET characteristics were measured by source measurement unit (Keysight, Model-B2902A).

Acknowledgment

We thank Dr. Suman Paul, attocube Systems AG, Egflinger Weg 2, 85540 Haar, for nano FTIR measurements. We also thank the Director, MSG, and the Director, IGCAR, for their constant encouragement.

Conflict of Interest

The authors declare no conflict of interest.

Figures

References

  1. [1]Mak, K. F.; Lee, C.; Hone, J.; Shan, J.; Heinz, T. F. Atomically thin MoS₂: a new direct-gap semiconductor. Phys. Rev. Lett. 2010, 105, 136805.DOI
  2. [2]Splendiani, A.; Sun, L.; Zhang, Y. ; Li, T.; Kim, J.; Chim, C.Y.; Galli, G.; Wang, F. Emerging photoluminescence in monolayer MoS₂. Nano Lett. 2010, 10, 1271.DOI
  3. [3]Nan, H.; Wang, Z.; Wang, W.; Liang, Z.; Lu, Y.; Chen, Q.; He, D.; Tan, P.; Miao, F.; Wang, X.; Wang, J. Strong photoenhancement of MoS₂ through defect engineering and oxygen bonding. ACS Nano 2014, 8, 5738.DOI
  4. [4]Madapu, K. K.; Bhuyan, C. A.; Srivastava, S. ; Dhara, S. A novel mechanism for understanding the strong enhancement of photoluminescence quantum yield in large-area monolayer MoS₂ grown by CVD. J. Mater. Chem. C 2021, 9, 3578.DOI
  5. [5]Zhao, B.; Wan, Z.; Liu, Y.; Xu, J.; Yang, X.; Shen, D.; Zhang, Z.; Guo, C.; Qian, Q. ; Li, J.; Wu, R. High-order superlattices by rolling up van der Waals heterostructures. Nature 2021, 591, 385.DOI
  6. [6]Trushin, M.; Neto, A. C. Stability of a rolled-up conformation state for two-dimensional materials in aqueous solutions. Phys. Rev. Lett. 2021, 127, 156101.DOI
  7. [7]Aftab, S.; Iqbal, M. Z.; Rim, Y. S. Recent advances in rolling 2D TMDs nanosheets into 1D TMDs nanotubes/nanoscrolls. Small, 2022, 2205418.DOI
  8. [8]Zhao, Y.; You, H.; Li, X.; Pei, C.; Huang, X.; Li, H. Solvent-Free Preparation of Closely Packed MoS₂ Nanoscrolls for Improved Photosensitivity. ACS Appl. Mater. Interfaces 2022, 14 9515.DOI
  9. [9]Cui, X.; Kong, Z.; Gao, E.; Huang, D.; Hao, Y.; Shen, H.; Di, C.A.; Xu, Z.; Zheng, J.; Zhu, D. Rolling up transition metal dichalcogenide nanoscrolls via one drop of ethanol. Nat. Commun. 2018, 9, 1.DOI
  10. [10]Meng, J.; Wang, G.; Li, X.; Lu, X.; Zhang, J.; Yu, H.; Chen, W.; Du, L.; Liao, M.; Zhao, J.; Chen, P. Rolling up a monolayer MoS₂ sheet. Small 2016, 12, 3770.DOI
  11. [11]Lin, C.; Cai, L.; Fu, J.H.; Sattar, S.; Wang, Q.; Wan, Y.; Tseng, C.C.; Yang, C.W.; Aljarb, A.; Jiang, K.; Huang, K.W. Direct Band Gap in Multilayer Transition Metal Dichalcogenide Nanoscrolls with Enhanced Photoluminescence. ACS Mater. Lett. 2022, 4, 1547.DOI
  12. [12]Na, J.; Park, C.; Lee, C.H.; Choi, W.R.; Choi, S.; Lee, J.U.; Yang, W.; Cheong, H.; Campbell, E.E.; Jhang, S.H. Indirect Band Gap in Scrolled MoS₂ Monolayers. Nanomaterials 2022, 12, 3353.DOI
  13. [13]Wang, R.; Guo, S.; Li, Z.; Weller, D.; Quan, S.; Yu, J.; Wu, M.; Jiang, J.; Wang, Y.; Liu, R. Strong anisotropic optical properties by rolling up MoS₂ nanoflake. J. Phys. Chem. Lett. 2022, 13, 8409.DOI
  14. [14]Mackay, D.; Wesenbeeck, van Correlation of chemical evaporation rate with vapor pressure. I. Environ. Sci. Technol. 2014, 48, 10259.DOI
  15. [15]Wyman, J. The dielectric constant of mixtures of ethyl alcohol and water from-5 to 40. J. Am. Chem. Soc. 1931, 53, 3292.DOI
  16. [16]Madapu, K. K.; Dhara, S. Laser-induced anharmonicity vs thermally induced biaxial compressive strain in mono-and bilayer MoS₂ grown via CVD. AIP Adv. 2020, 10, 085003.DOI
  17. [17]Madapu, K. K.; Bhuyan, C. A.; Dhara, S. Origin of bound exciton emission in CVD-grown monolayer MoS₂. Phys. Rev. B 2023, 108, 085429.DOI
  18. [18]Castellanos-Gomez, A.; Roldán, R.; Cappelluti, E.; Buscema, M.; Guinea, F.; Van Der Zant, H.S.; Steele, G.A. Local strain engineering in atomically thin MoS₂. Nano Lett. 2013, 13, 5361.
  19. [19]Lee, C.; Yan, H.; Brus, L.E.; Heinz, T.F.; Hone, J.; Ryu, S. Anomalous lattice vibrations of single-and few-layer MoS₂. ACS Nano 2010, 4, 2695.DOI
  20. [20]Chakraborty, B.; Bera, A.; Muthu, D.V.S.; Bhowmick, S.; Waghmare, U.V.; Sood, A.K. Symmetry-dependent phonon renormalization in monolayer MoS₂ transistor. Phys. Rev. B 2012, 85, 161403.DOI
  21. [21]Lin, Y.; Ling, X.; Yu, L.; Huang, S.; Hsu, A.L.; Lee, Y.H.; Kong, J.; Dresselhaus, M.S.; Palacios, T. Dielectric screening of excitons and trions in single-layer MoS₂. Nano Lett. 2014, 14, 5569.DOI
  22. [22]Shin, B. G.; Han, G.H.; Yun, S.J.; Oh, H.M.; Bae, J.J.; Song, Y.J.; Park, C.Y.; Lee, Y.H. Indirect bandgap puddles in monolayer MoS₂ by substrate-induced local strain. Adv. Mater. 2016, 28, 9378.DOI
  23. [23]Conley, H. J.; Wang, B.; Ziegler, J.I.; Haglund Jr, R.F.; Pantelides, S.T.; Bolotin, K.I. Bandgap engineering of strained monolayer and bilayer MoS₂. Nano Lett. 2013, 13, 3626.DOI
  24. [24]Huang, S.; Ling, X.; Liang, L.; Kong, J.; Terrones, H.; Meunier, V.; Dresselhaus, M.S. Probing the interlayer coupling of twisted bilayer MoS₂ using photoluminescence spectroscopy. Nano Lett. 2014, 14, 5500.DOI
  25. [25]Liang, L.; Zhang, J.; Sumpter, B.G.; Tan, Q.H.; Tan, P.H.; Meunier, V. Low-frequency shear and layer-breathing modes in Raman scattering of two-dimensional materials. ACS Nano 2017, 11, 11777.DOI
  26. [26]Boukhicha, M.; Calandra, M.; Measson, M.-A.; Lancry, O.; Shukla, A. Anharmonic phonons in few-layer MoS₂: Raman spectroscopy of ultralow energy compression and shear modes. Phys. Rev. B 2013, 87, 195316.DOI
  27. [27]Choi, S.; Shaolin, Z.; Yang, W. Layer-number-dependent work function of MoS₂ nanoflakes. Journal of the Korean Physical Society 2014, 64, 1550.DOI
  28. [28]Bhuyan, C. A.; Madapu, K. K.; Prabakar, K.; Das, A.; Polaki, S.R.; Sinha, S.K.; Dhara, S. A Novel Methodology of Using Nonsolvent in Achieving Ultraclean Transferred Monolayer MoS₂. Adv. Mater. Interfaces 2022, 9, 2200030.DOI
  29. [29]Gong, C.; Colombo, L.; Wallace, R. M.; Cho, K. The unusual mechanism of partial Fermi level pinning at metal-MoS₂ interfaces. Nano Lett. 2014, 14, 1714.DOI
  30. [30]Amani, M.; Burke, R. A.; Proie, R. M.; Dubey, M. Flexible integrated circuits and multifunctional electronics based on single atomic layers of MoS₂ and graphene. Nanotechnol. 2015, 26, 115202.DOI
  31. [31]Dumcenco, D.; Ovchinnikov, D.; Marinov, K.; Lazic, P.; Gibertini, M.; Marzari, N.; Sanchez, O.L.; Kung, Y.C.; Krasnozhon, D.; Chen, M.W.; Bertolazzi, S. Large-area epitaxial monolayer MoS₂. ACS Nano 2015, 9, 4611.DOI
  32. [32]Sebastian, A.; Pendurthi, R.; Choudhury, T. H.; Redwing, J. M.; Das, S. Benchmarking monolayer MoS₂ and WS₂ field-effect transistors. Nat. Commun. 2021, 12, 1.DOI
  33. [33]Lin, M.-W.; Lin, M. W.; Kravchenko, I. I.; Fowlkes, J.; Li, X.; Puretzk y, A.A.; Rouleau, C.M.; Geohegan, D.B.; Xiao, K. Thickness-dependent charge transport in few-layer MoS₂ field-effect transistors. Nanotechnol. 2016, 27, 165203.DOI
  34. [34]Lembke, D.; Kis, A. Breakdown of high-performance monolayer MoS₂ transistors. ACS Nano 2012, 6, 10070.DOI

Paper details

vlnc:W_bjk22ma6
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents