betaFeedback

WorksPhysics and Astronomy

HZO-based FerroNEMS MAC for In-Memory Computing

Abstract

This paper demonstrates a hafnium zirconium oxide (HZO)-based ferroelectric NEMS unimorph as the fundamental building block for very low-energy capacitive readout in-memory computing. The reported device consists of a 250 μμm ×\times 30 μμm unimorph cantilever with 20 nm thick ferroelectric HZO on 1 μμm SiO2SiO_2.Partial ferroelectric switching in HZO achieves analog programmable control of the piezoelectric coefficient (d31d_{31}) which serves as the computational weight for multiply-accumulate (MAC) operations. The displacement of the piezoelectric unimorph was recorded by actuating the device with different input voltages VinV_{in}. The resulting displacement was measured as a function of the ferroelectric programming/poling voltage VpV_p. The slopes of central beam displacement (δmaxδ_{max}) vs VinV_{in} were measured to be between 182.9nm/V (for -8 VpV_p) and -90.5nm/V (for 8 VpV_p), demonstrating that VpV_p can be used to change the direction of motion of the beam. The resultant (δmaxδ_{max}) from AC actuation is in the range of -18 to 36 nm and is a scaled product of the input voltage and programmed d31d_{31} (governed by the VpV_p). The multiplication function serves as the fundamental unit for MAC operations with the ferroelectric NEMS unimorph. The displacement from many such beams can be added by summing the capacitance changes, providing a pathway to implement a multi-input and multi-weight neuron. A scaling and fabrication analysis suggests that this device can be CMOS compatible, achieving high in-memory computational throughput.

Neuromorphic computation is of great interest to computing theory and practical implementations due to the potential for low-power, high efficiency, and small form factor information processing with deep neural networks (DNNs) [1, 2, 3]. The building blocks of DNNs are perceptron blocks, which inherently necessitate brain-like synaptic functions achieved through arrays of MAC units. With the ever-increasing number of variables required for neuromorphic computation with high accuracy, there is an urgent need to develop highly energy-efficient device architectures [3, 4, 5]. The energy used per MAC unit is, therefore, a useful metric to compare technologies. Ferroelectric field-effect transistors (Fe-FET) have been used to mimic analog synaptic operation with gate-ferroelectric switching in silicon and germanium channel devices to realize multi-level conductance modulation with potentiation and depression with 50-100 ns switching pulses and 3-5 MV/cm fields[6, 7]. FET-based in-memory computation architectures are susceptible to large read and write energy consumption and high leakage currents in idle mode, particularly with gate dielectric thickness scaling down to < 5 nm [8]. NEMS switches and beams offer an alternate pathway to zero-leakage in-memory compute synaptic functionality, provided that the beam actuation has embedded programmable weights in the form of tunable capacitive or piezoelectric coupling. We have previously reported a graphene-on-HZO ferroelectric device that uses potential gradients across the graphene to achieve fractional switching, with the modulated graphene resistance also used for resistive memory readout [9]. While analog in-memory computing has been demonstrated using different architectures which use transistors or memristors, few prior works have used a NEMS-based approach that takes advantage of a released beam structure to eliminate energy leakage in an idle state [10, 11, 12, 13]. In previous work, the idea of using nanomechanical electrostatic actuators to produce MAC units has been described [13]. In contrast, we present a ferroelectric/piezoelectric beam transducer to enable the multiplication that can be read out capacitively, eliminating any DC currents.

This paper presents a novel technique to store the neural net weights in the form of the programmable piezoelectric coefficient d31d_{31} of HZO-driven unimorph, which changes by applying a polarization switching voltage VpV_p. After polarization programming, different actuation inputs (VinV_{in}), actuate the cantilever such that the unimorph displacement is a scaled product of VpV_p and VinV_{in}. The displacement can in turn be measured as capacitive sense current from a capacitive divider circuit, for massively parallel MAC operations from arrays of such NEMS elements. Figure 1 shows the concept of the partial polarization in a ferroelectric for analog control of beam-bending in a unimorph. In addition to the active ferroelectric film, the unimorph stack also includes metal contact layers and an insulating elastic layer. The polarization versus E-field (PE loop) for an 80 μ\mum diameter metal-ferroelectric-metal (MFM) capacitor on a 20 nm thin HZO film is shown in Figure 1a. Moving counterclockwise along the PE loop starting with all dipoles point downward (point O), the film can be in a state of net-zero polarization (points A and A′) at the positive and negative coercive fields, fully down or up-switched (points C and C′) or partially polarized (along the slopes of A-B and A′-B′). Each point along the PE loop achieves a specific macroscopic value of d31d_{31}, with the maximum and minimum values at the two extrema (at points C and C′) with the appropriate choice of bias voltage Vp=EtHZOV_p = E t_{\mathrm{HZO}}. After programming, if a much smaller actuation voltage VinV_{in} is applied such that it produces no dipole switching, an in-plane stress is generated due to expansion or contraction of the HZO film along its length, resulting in the piezoelectric bending moment MPiezoM_{\mathrm{Piezo}}. The programming would enable weight-storage in DNNs at reduced rates compared to inference events. The beam displacement is a solution of the Euler–Bernoulli equation:

Image not extracted

Figure 1. (a) PUND loop of 20 nm-thick HZO film (b) Polarization-dependent bending moment generated in ferroelectric-on-elastic unimorph at various points along the PE loop (ECE_C is coercive field) (c) Conceptual multiplier unit with ferroelectric actuation and capacitive readout. The output voltage is the product of VinV_{in} and stored weights in the form of d31d_{31} coefficients. (d) Several multipliers with capacitive readout can be placed in parallel to form a MAC unit that can perform accumulation operation by summing up the capacitances from each device.

∂2y∂x2=−MPiezoC(1)\frac{\partial^2 y}{\partial x^2}=-\frac{M_{\mathrm{Piezo}}}{C} \tag*{(1)}

Here, MpiezoM_{piezo} is the piezoelectric moment generated due to applied VinV_{in} and CC is the total flexural rigidity of the multi-layer piezoelectric stack [14]. By using zero displacements and zero slopes boundary conditions on each end of the clamped-clamped beam, the Euler–Bernoulli equation yields the beam displacement profile. The maximum beam displacement occurs at the center i.e. y(L/2)=δmax⁡y(L/2)=\delta_{\max}. For piezoelectric coefficient d31d_{31} and in-plane stress σ1\sigma_1 in HZO, the beam displacement can be expressed as:

δmax⁡∝MPiezo∝σ1∝d31∝P(Polarization)∝Vp(2)\delta_{\max} \propto M_{Piezo} \propto\sigma_1 \propto d_{31} \propto P(Polarization) \propto V_p \tag*{(2)}

For an input voltage VinV_{in}, the NEMS beam displacement is, hence, a scaled product of weights and inputs.

δmax⁡=SF⋅Vp⋅Vin(3)\delta_{\max}=SF\cdot V_p\cdot V_{in} \tag*{(3)}

Here, the scale factor (SF) depends on ferroelectric material properties, beam geometry, Young’s modulus, etc. However, we can design the multiplier to achieve linear behavior in the transfer characteristics curve along the rising and falling slopes of the PE loop to accomplish a multiplicative function for parallel MAC operations. Figure 1c represents the multiplier unit with a capacitive readout to measure the output voltage. The left and right beams are poled with the same magnitude but with opposite polarity. Thus, for the same input voltage VinV_{in}, the left and right beams displace such that the difference between the two represents the product of VinV_{in} and VpV_p. The differential motion causes differential capacitance between left and right capacitive parallel plates. The output voltage is given by:

Vout=2VddCL−CRCL+CR=−2Vddγ(xL−xR)2g=SF⋅Vp⋅Vin(4)V_{out}=2V_{dd}\frac{C_L-C_R}{C_L+C_R}=-2V_{dd}\frac{\gamma(x_L-x_R)}{2g}=SF\cdot V_p\cdot V_{in} \tag*{(4)}

Where γ\gamma is an constant which depends on beam geometry, and xLx_L and xRx_R are left and right parallel plate displacements with initial gap gg. Several multiplier units can then be further connected in parallel with an activation unit to form a perceptron. The output voltage of the MAC unit (Figure 1d) is:

Vout,MAC=2Vdd∑i=1NCL,i−∑i=1NCR,i∑i=1NCL,i+∑i=1NCR,i=SF∑i=1NVp,iVin,i(5)V_{out,MAC}=2V_{dd}\frac{\sum_{i=1}^{N}C_{L,i}-\sum_{i=1}^{N}C_{R,i}}{\sum_{i=1}^{N}C_{L,i}+\sum_{i=1}^{N}C_{R,i}}=SF\sum_{i=1}^{N}V_{p,i}V_{in,i} \tag*{(5)}

Figure 2a and 2b show the top and cross-section views respectively of the clamped-clamped ferroelectric unimorph used to demonstrate piezoelectric coefficient programming. 11 μm thick thermal SiO2\mathrm{SiO_2} forms the elastic layer underneath 2020 nm ferroelectric HZO. The HZO is capped by 33 nm of alumina (Al2O3\mathrm{Al_2O_3}), followed by annealing at 400400°C to crystallize the HZO in its ferroelectric orthorhombic phase. 200200 nm platinum (Pt) and 100100 nm aluminum (Al) were deposited to form the bottom and top metal contacts for the HZO respectively. The beam was released by isotropic etching of the silicon substrate using Xactix XeF2\mathrm{XeF_2} etcher. Details of the fabrication process and challenges encountered are included in the supplementary material. A scanning electron microscope image of the fabricated device is shown in Figure 2c. After release, the beams were observed to be buckled due to residual film-stress generated during microfabrication. A 3D optical profilometer (Zygo{sup}TM system) was used to measure the beam buckling profile (Figure 2d). The maximum displacement for a 250250 μm ×30\times30 μm was 4.984.98 μm.

Image not extracted

Figure 2. (a),(b) Schematic top and cross-section view of the ferroelectric beam (c) SEM image of the beam showing released structure (d) 3D profile of the released beam measured using ZygoTM^{\mathrm{TM}} profilometer showing beam curvature due to residual stresses in the stack. For 250×30μm250 \times30\mu\mathrm{m} beam, the measured maximum displacement at the center was 4.98μm4.98\mu\mathrm{m}.

HZO ferroelectric characterization was performed using a Sawyer-Tower circuit configuration on a custom probe station with continuous wave (CW) positive-up-negative-down (PUND) input waveforms to extract the coercive field (ECE_{\mathrm{C}}) and remnant polarization (PrP_{\mathrm{r}}). In prior work, we have used electrical breakdown under a large top metal pad to contact the bottom electrode with 55-10Ω10\Omega resistance [15]. The PUND input signal has 83μs83\mu\mathrm{s} rise, fall, and wait times (corresponding to 1kHz1\mathrm{kHz} PUND frequency), and a peak-to-peak amplitude of 15V15\mathrm{V}. Figure 3a shows time-domain input voltage and output sense current measured with an 11.8kΩ11.8\mathrm{k}\Omega sense resistor. The P and N pulses show a switching current peak below the peak voltage, indicative of polarization switching, whereas the U and D pulses show capacitive displacement current and low leakage. This confirms ferroelectricity in the released HZO films without any degradation, consistent over 10,000 cycles of switching with CW operation. Figure 3b plots the switching current density (JJ) vs E-field. The PUND measurement was performed on multiple such released NEMS beams with a range of lengths from 100100-400μm400\mu\mathrm{m} and widths spanning 1515-39μm39\mu\mathrm{m}. The overlay from these measurements is shown with multiple dotted lines in Figure 3c. For comparison, the PUND loop for an unreleased 80μm80\mu\mathrm{m} diameter circular electrode is also shown on the same plot (solid black line). This shows that there is little/no degradation of ferroelectric properties of the HZO before and after release. Multiple release devices with different electrode sizes had overlapping loops suggesting high repeatability. PUND measurements yield an extracted Ec≈1.5MV/cmE_{\mathrm{c}} \approx1.5\mathrm{MV}/\mathrm{cm} and Pr≈10μC/cm2P_{\mathrm{r}} \approx10\mu\mathrm{C}/\mathrm{cm}^{2}, consistent with previously reported values[16, 17, 18]. The devices were also tested for DC breakdown as shown in Figure 3d. The device's current density exceeds 10μA/cm210\mu\mathrm{A}/\mathrm{cm}^{2} at 3.15MV/cm3.15\mathrm{MV}/\mathrm{cm}.

Image not extracted

Figure 3. (a) Input voltage and output current vs time plot of the device showing much larger switching currents as compared to leakage currents. Inset- Setup for poling the NEMS beam (b) Switching current density vs electric field plot showing ferroelectric switching peaks. (c) Measured Polarization vs E-field characteristics of released beam devices with different lengths and widths showing repeatability. The Measured PE loop of the standard unreleased circular electrode is shown with a solid black (d) DC I-V of the device showing high current density above 3.15 MV/cm3.15\ \mathrm{MV/cm} indicating leakage.

The central device concept of this work is to use analog weight storage in the bending motion of the NEMS beam for in-memory computation, which relies on the programming of the d31d_{31} coefficient of the device by using different poling voltages. The test methodology used for this experiment is as follows:

Step 1: Device poling with CW single-sided pulses at 3 kHz. The configuration used for poling is depicted in Figure 3a (inset). The test signal is applied to the top electrode, and the ground connection is made to the bottom electrode by breaking down the HZO under a large top metal pad to short it to the bottom electrode.

Step 2: Beam actuation with small VinV_{\mathrm{in}} to measure the displacement amplitude, without additional polarization switching.

Step 3: Increase poling voltage by 0.5V and repeat steps 1-2, while tracing the PE loop counterclockwise from 0V→8V→0V→−8V→0V0\mathrm{V}\to8\mathrm{V}\to0\mathrm{V}\to-8\mathrm{V}\to0\mathrm{V}.

This voltage sweep for VpV_{\mathrm{p}} is similar to the PUND loop with one key difference. In this technique, we stepped the VpV_{\mathrm{p}} by 0.5V and then measured the beam displacement with a fixed VinV_{\mathrm{in}} amplitude, unlike the PUND measurements in CW operation with increasing voltages.

A Polytec MSA-400 laser doppler vibrometer (LDV) was used to measure the beam motion. For a 250 μm×30μm\mu\mathrm{m} \times30 \mu\mathrm{m} beam, a 0.1 V amplitude frequency chirp from 1 kHz to 1 MHz was applied. A resonance at f0=455.23f_0=455.23 kHz was identified with a quality factor of 305. AC voltage Vin=0.1V_{\mathrm{in}}=0.1 V was used to measure peak amplitudes. Figure 4a shows the peak beam displacement δmax⁡\delta_{\max} and resonant frequency f0f_0 vs poling voltage VpV_p plot for the nominal 250 μm×30μm\mu\mathrm{m} \times30 \mu\mathrm{m} ferroelectric clamped-clamped beam. δmax⁡\delta_{\max} (red line) is modulated for different values of VpV_p and traces a hysteresis loop, similar to the PE loop from PUND measurements. The net effect of the number of upward and downward pointing dipoles that control the macroscopic polarization in the beam (induced due to VpV_p) also changes the beam stiffness resulting in resonance frequency modulation (black line), which presents a separate modality of weight storage in the beam. The two dips in f0f_0 correspond to the positive and negative coercive fields of the HZO film, where the net polarization is almost zero. As illustrated in Figure 1b, domain randomization is a potential cause for likely film relaxation at these points causing f0f_0 to drop.

Image not extracted

Figure 4. (a) Central beam displacement δmax⁡\delta_{\max} and resonant frequency f0f_0 vs poling voltage VpV_p plot for the 250 μm×30μm\mu\mathrm{m} \times30 \mu\mathrm{m} ferroelectric clamped-clamped beam. Devices were poled at different VpV_p with 0.5 V increment along the loop (0 V→\rightarrow8 V→\rightarrow0 V→\rightarrow-8 V→\rightarrow0 V) and the beam displacement profile was measured using the Polytec LDV at Vin=0.1V_{\mathrm{in}}=0.1 V in the frequency range of 450–460 kHz. The δmax⁡\delta_{\max} (red line) changes for different values of VpV_p and traces a hysteresis loop similar to PUND measurements. The polarization in the beam, induced due to VpV_p, changes the internal stress resulting in the frequency f0f_0 tuning (black line) which could be exploited for memory storage. (b) The resonance vibration magnitude and phase plots of the same beam at different points on plot (a).

From Figure 4a, the positive linear dependence of δmax⁡\delta_{\max} can be seen in the voltage interval 2.5 V→\rightarrow8 V. Similarly, negative linear dependence in the interval -2.5 V→\rightarrow-8 V. Here, the slope of δmax⁡\delta_{\max} vs. VpV_p is SF×Vin\times V_{\mathrm{in}} as defined in Eq. (3). The effect of VinV_{\mathrm{in}} on δmax⁡\delta_{\max} is explained in the next section. Two points were selected on the positive slope to show the resonance vibration magnitude and phase plots of the vibrating beam (Figure 4b). Points 1 and 2 have almost the same displacement magnitude but exactly opposite phases. This 180° phase difference is a signature of polarization inversion corresponding to a sign change for δmax⁡\delta_{\max}. To show the effect of VinV_{\mathrm{in}} on δmax⁡\delta_{\max}, VinV_{\mathrm{in}} was swept from 0.02 V to 0.20 V for different values of the VpV_p (Figure 5).

Image not extracted

Figure 5. The displacement vs VinV_{\mathrm{in}} for different values of VpV_{\mathrm{p}}. The black and red traces correspond to the positive VpV_{\mathrm{p}} (5.5→\rightarrow8V) red negative VpV_{\mathrm{p}} (-5.5→\rightarrow-8V) poling voltages respectively, showing the multiplication functionality.

Figure 5 plots δmax⁡\delta_{\max} vs VinV_{\mathrm{in}} at different values of VpV_{\mathrm{p}} which emulates the transfer characteristics of the analog multiplier. For a fixed poling voltage, an input voltage sweep yields a linear increase in displacement value. Similarly, for constant inputs, different poling voltages outputs different displacement values. We can calculate the scale factor from previous plots as follows:

SF=δmax⁡VpVin(6)SF = \frac{\delta_{\max}}{V_{\mathrm{p}}V_{\mathrm{in}}} \tag*{(6)}

Eq. 6 demonstrates that δmax⁡\delta_{\max} is the product of inputs (VinV_{\mathrm{in}}) and weights (VpV_{\mathrm{p}}). As shown in Figure 4a and Figure 5, Eq. 6 behaves linearly in the range of VpV_{\mathrm{p}} from ±2.5\pm2.5V to ±8\pm8V and VinV_{\mathrm{in}} from 0 to 0.2V for the device tested here (250 μ\mum×\times30 μ\mum beam). The beam displacement can be measured using a capacitive divider circuit to measure VoutV_{\mathrm{out}}. The slope of the plot in Figure 5 is the experimental SF×Vp\times V_{\mathrm{p}}. For Vp=±8V_{\mathrm{p}}=\pm8V, the measured slopes were 182.9 nm/V and -90.5 nm/V respectively. The asymmetry in the negative and positive VpV_{\mathrm{p}} slopes is likely due to the non-symmetric device stack. Above HZO, there is a very thin top electrode (Al) but below it, we have a thick SiO2_2 and electrode (Pt) stack. Thus, for the same VpV_{\mathrm{p}}, actuation with opposite polarity will have an unequal effect on the partial polarization resulting in different δmax⁡\delta_{\max} values.

In conclusion, we have demonstrated the successful working of an HZO-based NEMS multiplier with weight storage functionality. The device was fabricated and characterized showing the dependence of beam displacement on the poling voltage of the ferroelectric film. Polarization-dependent frequency-tuning was also observed, which can be further explored to achieve an electrically reconfigurable filter. For a 250 μ\mum ×\times 30 μ\mum beam poled at 8V, δmax⁡\delta_{\max} of 18 nm and f0f_0 of 455.23 kHz with Q=305 was measured. The δmax⁡\delta_{\max} vs VinV_{\mathrm{in}} plot at different values of VpV_{\mathrm{p}} demonstrate the successful operation of an analog NEMS multiplier. While in this paper AC drive was used to obtain observable displacements, in the future DC input voltages are anticipated for DNN applications. A capacitive readout of the beam motion can be used instead of a topical readout for much higher resolution.

The dimensional and voltage scaling of the prototype device demonstrated is important for CMOS-integrated adoption while maximizing computational throughput. For CMOS compatibility, <1V operation is necessary. This sets an upper bound for HZO film thickness of < 7 nm for Ec=1.5 MV/cmE_c = 1.5\,\mathrm{MV/cm}. Non-resonant actuation of the devices would require a settling time of ∼2QT0\sim2QT_0. Assuming two operations per device, multiplication and addition, the computation speed (FLOPS per device) and power consumption can be estimated as f0Q\frac{f_0}{Q} and Ef0QE\frac{f_0}{Q} respectively. Where E is the energy consumption per operation for individual device given by 12CHZO⋅Vin2\frac{1}{2}C_{HZO}\cdot V_{in}^{2}. For example, unimorph device of size 5×0.55 \times0.5 µm and thickness 28nm (~4×HZO thickness) with a Q=10, which can be realized by high-pressure gas damping, yields f0f_0 ~20MHz and computation speed of 2MFLOPS/device. Considering driving electrodes of size 1×0.31 \times0.3 µm with 7nm thick HZO between Vin_\mathrm{in} (0.1V) and GND electrodes, the energy consumption per operation can be calculated as ~500 aJ (E=12CHZO⋅Vin2E = \frac{1}{2}C_{HZO}\cdot V_{in}^{2}). Combining both values result in 2 PFLOPS/watt computational performance. This computation speed with ultra-low energy consumption and zero leakage current will pave the path toward brain-level computation efficiency.

Supplementary Material:

See supplementary material for the detailed fabrication process and challenges faced.

Acknowledgment:

This work was performed in part at the Cornell NanoScale Facility, an NNCI member supported by NSF Grant NNCI-2025233. Funding was provided by the DARPA TUFEN program.

References

  1. [1]C. Mead, “Neuromorphic electronic systems,” Proc. IEEE, vol. 78, no. 10, pp. 1629–1636, 1990.DOI
  2. [2]E. R. Kandel and J. H. Schwartz, The Nervous System: Principles of Neural Science, vol. 217, no. 4556. 1982.
  3. [3]A. Keshavarzi, K. Ni, W. Van Den Hoek, S. Datta, and A. Raychowdhury, “FerroElectronics for Edge Intelligence,” IEEE Micro, vol. 40, no. 6, pp. 33–48, Nov. 2020.DOI
  4. [4]W. Haensch, T. Gokmen, and R. Puri, “The Next Generation of Deep Learning Hardware: Analog Computing,” Proc. IEEE, vol. 107, no. 1, pp. 108–122, 2019.
  5. [5]M. Horowitz, “Computing” ’s Energy Problem ( and what we can do about it ),” pp. 10–14, 2014.
  6. [6]M. Si, X. Lyu, and P. D. Ye, “Ferroelectric Polarization Switching of Hafnium Zirconium Oxide in a Ferroelectric/Dielectric Stack,” ACS Appl. Electron. Mater., vol. 1, no. 5, pp. 745–751, May 2019.DOI
  7. [7]M. Jerry et al., “Ferroelectric FET analog synapse for acceleration of deep neural network training,” in 2017 IEEE International Electron Devices Meeting (IEDM), 2017, pp. 6.2.1-6.2.4.DOI
  8. [8]S. S. Cheema et al., “Enhanced ferroelectricity in ultrathin films grown directly on silicon,” Nature, vol. 580, no. 7804, pp. 478–482, Apr. 2020.DOI
  9. [9]V. Gund et al., “Multi-level Analog Programmable Graphene Resistive Memory with Fractional Channel Ferroelectric Switching in Hafnium Zirconium Oxide,” in IEEE Frequency Control Symposium (FCS), 2022.
  10. [10]A. Chen, S. Datta, X. S. Hu, M. T. Niemier, T. Š. Rosing, and J. J. Yang, “A Survey on Architecture Advances Enabled by Emerging Beyond-CMOS Technologies,” IEEE Des. Test, vol. 36, no. 3, pp. 46–68, 2019.
  11. [11]A. Sebastian, M. Le Gallo, R. Khaddam-Aljameh, and E. Eleftheriou, “Memory devices and applications for in-memory computing,” Nat. Nanotechnol., vol. 15, no. 7, pp. 529–544, 2020.DOI
  12. [12]D. E. Nikonov and I. A. Young, “Benchmarking Delay and Energy of Neural Inference Circuits,” IEEE J. Explor. Solid-State Comput. Devices Circuits, vol. 5, no. 2, pp. 75–84, 2019.DOI
  13. [13]A. Lal, J. Hoople, S. Ardanuç, and J. Kuo, “Computation Devices and Artificial Neurons Based on Nanoelectromechanical Systems,” 2019.
  14. [14]R. . Ballas, Piezoelectric Multilayer Beam Bending Actuators. 2007.
  15. [15]V. Gund et al., “Temperature-dependent Lowering of Coercive Field in 300 nm Sputtered Ferroelectric Al10.70Sc0.30N,” in IEEE International Symposium on Applications of Ferroelectric (ISAF), 2021, pp. 1–3.
  16. [16]M. Ghatge, G. Walters, T. Nishida, and R. Tabrizian, “A Nano-Mechanical Resonator with 10nm Hafnium-Zirconium Oxide Ferroelectric Transducer,” Tech. Dig. - Int. Electron Devices Meet. IEDM, vol. 2018-Decem, pp. 4.6.1-4.6.4, 2019.DOI
  17. [17]S. Starschisch, T. Schenk, U. Schroeder, and U. Boettger, “Ferroelectric and piezoelectric properties of Hf 1-x Zr x O 2 and pure ZrO 2 films,” Appl. Phys. Lett., vol. 110, no. 18, p. 182905, May 2017.
  18. [18]S. Riedel, P. Polakowski, and J. Müller, “A thermally robust and thickness independent ferroelectric phase in laminated hafnium zirconium oxide,” AIP Adv., vol. 6, no. 9, p. 095123, Sep. 2016.DOI

Paper details

vlnc:W_c2dgtdu7
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 10

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents