Abstract

Large intrinsic anomalous Hall effect (AHE) originating in the Berry curvature has attracted growing attention for potential applications. Recently proposed magnetic Weyl semimetal EuCd2_2Sb2_{\mathrm{2}} provides an excellent platform for controlling the intrinsic AHE because it only hosts a Weyl-points related band structure near the Fermi energy. Here we report the fabrication of EuCd2_2Sb2_{\mathrm{2}} single-crystalline films and control of their anomalous Hall effect by film technique. As also analyzed by first-principles calculations of energy-dependent intrinsic anomalous Hall conductivity, the obtained anomalous Hall effect shows a sharp peak as a function of carrier density, demonstrating clear energy dependence of the intrinsic AHE.

Topological semimetals, characterized by massless Dirac band dispersion in the low energy excitation, exhibit unique magnetotransport due to their nontrivial band topology in the momentum space [1, 2, 3, 4]. Recently reported magnetic topological semimetals further enrich the understanding of magnetotransport, where entanglement between magnetism and nontrivial topology can lead to exotic magnetotransport such as a large anomalous Hall effect (AHE) [5, 6, 7]. Integration of the Berry curvature for all occupied states gives rise to a large intrinsic contribution to anomalous Hall conductivity. Namely, anomalous Hall conductivity is closely related to the electron occupation determined by the position of Fermi level [7, 8].

Paired Weyl points (WPs) in magnetic Weyl semimetals can be viewed as monopoles with opposite chirality corresponding to the sources (W+) and sinks (W−) of the Berry curvature (Figure 1(a)). Due to the Berry flux of paired WPs, anomalous Hall conductivity σxy,AHE\sigma_{\mathrm{xy,AHE}} is expected to exhibit a large peak at the energy position of WPs (EWE_{\mathrm{W}}) [9, 10] and be strongly dependent on the Fermi level. Specifically, σxy,AHE\sigma_{\mathrm{xy,AHE}} can be maximized if the Fermi level can be adjusted to EWE_{\mathrm{W}} [11, 12]. However, such an energy dependence of σxy,AHE\sigma_{\mathrm{xy,AHE}} has not been demonstrated yet due to high carrier densities (∼1020\sim10^{20}–1022 cm−310^{22}\ \mathrm{cm}^{-3}) and complicated band structures of conventional magnetic Weyl semimetals, while the modulation of σxy,AHE\sigma_{\mathrm{xy,AHE}} has been attempted by chemical doping and pressure application for Co3Sn2S2\mathrm{Co}_{3}\mathrm{Sn}_{2}\mathrm{S}_{2} [13, 14, 15, 16], Mn3Sn\mathrm{Mn}_{3}\mathrm{Sn} [17, 18, 19, 20], and Mn3Ge\mathrm{Mn}_{3}\mathrm{Ge} [21].

Image not extracted

Figure 1. (a) Energy dispersion of paired Weyl points (WPs) and energy-dependent anomalous Hall conductivity σxy,AHE\sigma_{xy,\mathrm{AHE}}. Weyl points W+/W−\mathrm{W}^{+}/\mathrm{W}^{-} are the source/sink of the Berry curvature. (b) Crystal structure of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} [24] drawn using VESTA [46]. (c) Energy dispersion calculated for EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films, showing four pairs of WPs near the Fermi energy. They emerge along the Γ\Gamma−Z direction in the Brillouin zone when magnetic moments are forcedly aligned along the cc axis. Blue/green circles represent WPs (W1\mathrm{W}_{1}−W4\mathrm{W}_{4}) with plus/minus chirality. (d) Cross-sectional schematic illustration and (e) top-view photograph of the electrostatic gate device fabricated from a EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} film, where holes are depleted (accumulated) when VGV_{\mathrm{G}} is positively (negatively) biased.

In this context, EuCd2As2\mathrm{EuCd}_{2}\mathrm{As}_{2} and isostructural EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2}, where one of three Cd atoms is substituted with Eu in the parent Dirac semimetal Cd3As2\mathrm{Cd}_{3}\mathrm{As}_{2}, provide an ideal platform for experimentally demonstrating the peculiar energy dependence of intrinsic anomalous Hall conductivity. This is because they have a simple band structure near the Fermi energy (EFE_{\mathrm{F}}) and much lower carrier densities (∼1018\sim10^{18}–1019 cm−310^{19}\ \mathrm{cm}^{-3}) [22, 23]. On the other hand, difficulties in the growth of thin films have prevented the study of carrier density dependence with taking these advantages.

EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} has a trigonal crystal structure with space group P3ˉm1P\bar{3}m1 [23, 24, 25, 26]. It consists of an alternate stacking of triangular Eu layers and Cd2Sb2\mathrm{Cd}_{2}\mathrm{Sb}_{2} layers (Figure 1(b)). Eu atoms contribute to magnetism in this compound, forming AA-type antiferromagnetic structure below the Néel temperature TN=7.4 KT_{\mathrm{N}} = 7.4\ \mathrm{K} with Eu2+\mathrm{Eu}^{2+} magnetic moments lying in the abab plane [25, 26]. As shown in Figure 1(c), four pairs of WPs (W1\mathrm{W}_{1}–W4\mathrm{W}_{4}) near EFE_{\mathrm{F}} along the kzk_z direction are protected by C3zC_{3z} symmetry when the magnetic Eu moments are ferromagnetically polarized along the cc axis under the out-of-plane magnetic field [23]. There are no other bands near EFE_{\mathrm{F}} and all the hole carriers occupy the WPs-related valence bands. Therefore, it is expected that the Fermi level dependence of intrinsic anomalous Hall conductivity can be demonstrated by modulating hole carrier densities in EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} with film techniques.

Here we report the fabrication of single-crystalline EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films by molecular beam epitaxy and investigation of their anomalous Hall effect using film techniques. By adjusting the Fermi level with controlling Sb flux conditions and also performing electrostatic gating experiments, we find that their anomalous Hall effect is largely enhanced compared to bulks and strongly dependent on the carrier density with a sharp peak, as also demonstrated by first-principles calculations.

EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films were grown in an Epiquest RC1100 chamber [27, 28, 29, 30] on single-crystalline (111)A CdTe substrates. In-plane lattice mismatch between EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} and CdTe is 2.4% as shown in Figure 2(b). CdTe substrates were etched with 0.01% Br2\mathrm{Br}_{2}-methanol before loading it into the chamber and then heated to 750°C with Cd flux supplied to obtain an atomically smooth surface [27]. After annealing the substrate, it was cooled to the growth temperature of 360°C. The beam equivalent pressures were measured by an ionization gauge, and were set to 1.2×10−51.2 \times10^{-5} Pa for Eu, 5.0×10−45.0 \times10^{-4} Pa for Cd, and 8.5×10−68.5 \times10^{-6} Pa for Sb during the co-deposition, which is the same growth condition as EuCdSb2\mathrm{EuCdSb}_{2} films on Al2O3\mathrm{Al}_{2}\mathrm{O}_{3} (0001) substrates [29]. This Cd-rich growth condition offers advantages in reducing carrier densities in EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films, because Cd deficiency is a major origin of the hole carriers. The films were then annealed in-situ at 500°C for 5 minutes under exposure of Cd flux. The film thickness was set at 50 nm, and the growth rate was about 0.07 Å/s.

XRD scan, crystal structures, microscopy image, atomic arrangement, and elemental maps of EuCd$_2$Sb$_2$

Figure 2. (a) XRD θ\theta-2θ2\theta scan of a EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} film grown on a CdTe substrate. Substrate peaks are marked with an asterisk. (b) Crystal structures of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} film and CdTe substrate, viewed along the out-of-plane direction. (c) Cross-sectional image of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} film, taken by high-angle annular dark-field scanning transmission electron microscopy. (d) Atomic arrangement of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} viewed along [110][110] direction. Energy dispersive x-ray spectrometry maps taken for (e) Eu LL, (f) Cd LL, and (g) Sb LL edge in the boxed region in (c).

The films were patterned to Hall bars with a channel width of 10 μ\mum through conventional photolithography, Ar ion milling, and chemical wet etching processes: 10 nm thick Ni and 50 nm thick Au electrodes were deposited for ohmic contact by electron beam evaporation, and then 30 nm thick Al2O3\mathrm{Al}_{2}\mathrm{O}_{3} was deposited as gate dielectric by atomic layer deposition, as shown in Figure 1(d) and Figure 1(e). Low-temperature magnetotransport was measured using a Quantum Design Physical Property Measurement System cryostat equipped with a 9 T superconducting magnet. Hall measurements were performed using a lock-in technique. The excitation current was kept constant at 0.5 mA with a frequency of 13 Hz. For gating experiments, DC bias (VG=−8∼+8V_{\mathrm{G}} = -8 \sim+8 V) voltage was applied to the gate electrode.

First-principles calculations of the band structure with spin-orbit coupling were performed using the VASP package [31, 32, 33] for experimentally determined film lattice parameters. The generalized gradient approximation of Perdew-Burke-Ernzerhof was adopted for the exchange-correlation functional [34]. The correlation effect was considered by a Hubbard UU correction of U=4.5U = 4.5 eV for the Eu-ff orbitals [35], which was determined by comparing the band structures revealed by angle-resolved photoemission spectroscopy and first-principles calculations [23]. 16×16×1016 \times16 \times10 kk-point mesh with Monkhorst-Pack scheme [36] was used for the Brillouin zone sampling of the primitive cell and Gaussian smearing with a width of 0.020.02 eV was applied. From the Bloch states obtained in the DFT calculation, a Wannier basis set is constructed by using the Wannier90 code [37]. The basis consists of ss, ff-character orbitals localized at the Eu site, ss, dd-character orbitals at the Cd, and ss, pp-character orbitals at the Sb. The intrinsic anomalous Hall conductivity is computed using a kk-point mesh of 300×300×300300 \times300 \times300 [38].

Figure 2 shows structural characterization of EuCd2_2Sb2_2 film. As shown in the x-ray diffraction (XRD) θ\theta-2θ2\theta scan in Figure 2(a), reflections from the (001) EuCd2_2Sb2_2 lattice planes are observed without any impurity phases. Its out-of-plane lattice constant along the cc-axis is calculated to be 7.73 Å. Figure 2(c) shows a cross-section image of the EuCd2_2Sb2_2, taken by high-angle annular dark-field scanning transmission electron microscopy. The periodic atomic arrangement corresponding to the EuCd2_2Sb2_2 crystal structure in Figure 2(d) is clearly confirmed. Elemental maps are also taken by energy dispersive x-ray spectrometry, as shown in Figure 2(e)-Figure 2(g). The alternate stacking of Eu layers and Cd2_2Sb2_2 layers is clearly resolved. Further structural characterization was performed for examining the in-plane epitaxial relation (See Supplementary Materials for details [39]).

Figure 3 summarizes fundamental magnetotransport of the EuCd2_2Sb2_2 film. As shown in Figure 3(a), longitudinal resistivity ρxx\rho_{xx} exhibits a metallic behavior in the whole temperature regime. Below 50 K, ρxx\rho_{xx} gradually increases upon cooling until it shows a clear kink at 7.4 K. Then it exhibits a sudden drop upon further cooling. This kink observed at 7.4 K corresponds to Néel temperature TNT_{\mathrm{N}} [23, 25, 26]. The kink disappears at the out-of-plane magnetic field B=9B = 9 T, where the Eu2+^{2+} magnetic moments are completely aligned along the cc-axis [23, 26]. This low temperature behavior can be understood considering the scattering of conduction electrons by the localized Eu2+^{2+} spins. Figure 3(b) presents magnetoresistance (MR) taken by sweeping the out-of-plane magnetic field at various temperatures. At T=2.0T = 2.0 K, a peak ends at the saturation field Bsat=3.4B_{\mathrm{sat}} = 3.4 T, and which shifts to lower fields upon increasing temperature and then disappears above TNT_{\mathrm{N}}. This peak below BsatB_{\mathrm{sat}} is ascribed to an increase of magnetic scattering in the canted spin structure. At high-fields above BsatB_{\mathrm{sat}}, the Eu2+\mathrm{Eu}^{2+} spins are fully polarized along the cc-axis, resulting in reduced magnetic scattering. At higher temperatures above TNT_{\mathrm{N}}, the peak becomes smaller and shifts to higher magnetic fields. Finally, the peak disappears and conventional positive MR appears.

Image not extracted

Figure 3. Magnetotransport measured for a EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} film with a carrier density p=0.8×1019 cm−3p = 0.8 \times10^{19}\,\mathrm{cm}^{-3}. (a) Temperature dependence of longitudinal resistivity ρxx\rho_{xx}, with a clear kink at the Néel temperature TN=7.4T_{\mathrm{N}} = 7.4 K. The inset shows measurement configuration. (b) Magnetoresistance (ρxx(B)−ρxx(0 T))/ρxx(0 T)(\rho_{xx}(B) - \rho_{xx}(0\,\mathrm{T}))/\rho_{xx}(0\,\mathrm{T}) taken with sweeping the out-of-plane magnetic field at various temperatures. The saturation field is estimated Bsat=3.4B_{\mathrm{sat}} = 3.4 T at T=2.0T = 2.0 K. (c) Hall resistivity ρyx\rho_{yx} taken at various temperatures. (d) Anomalous Hall resistivity ρyx,AHE\rho_{yx,\mathrm{AHE}}, obtained by subtracting the ordinary term at various temperatures. Anomalous Hall resistivity ρyx,AHE\rho_{yx,\mathrm{AHE}} of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films with (e) different carrier densities and (f) electrostatic gating at 2.0 K.

Figure 3(c) shows Hall resistivity ρyx\rho_{\mathrm{yx}} measured at various temperatures. At temperatures above 50 K, Hall resistivity depends almost linearly on the magnetic field. In contrast, it deviates from the linear behavior upon cooling below 50 K. Here ρyx\rho_{\mathrm{yx}} is expressed as ρyx=RHB+ρyx,AHE\rho_{\mathrm{yx}} = R_{\mathrm{H}}B + \rho_{\mathrm{yx,AHE}} with the ordinary Hall coefficient RHR_{\mathrm{H}} and the anomalous Hall resistivity ρyx,AHE\rho_{\mathrm{yx,AHE}}. Deviation from the linear behavior disappears above BsatB_{\mathrm{sat}}, showing clear contribution of the anomalous Hall term (See Supplementary Materials [39]). By subtracting the ordinary term with a linear fit, the anomalous term is obtained as shown in Figure 3(d). ρyx,AHE\rho_{\mathrm{yx,AHE}} taken at T=2.0T = 2.0 K exhibits a kink at Bsat=3.4B_{\mathrm{sat}} = 3.4 T. With increasing temperature, BsatB_{\mathrm{sat}} shifts to lower fields below TNT_{\mathrm{N}} and then disappears above TNT_{\mathrm{N}}, as confirmed in MR. Besides, a broad but pronounced peak appears around BsatB_{\mathrm{sat}} below TNT_{\mathrm{N}}, showing deviation from the magnetization behavior. While this peak suggests the existence of the so-called topological Hall term, it is unlikely that this is caused by the real-space spin Berry phase on noncoplanar spin configuration during simple spin polarization process. Rather, this may be understood by intrinsic AHE corresponding to band structure changes during the polarization process, as also reported for other Eu compounds [40, 41, 42, 43].

Here we define the saturation value of ρyx,AHE\rho_{\mathrm{yx,AHE}} at 9 T as ρyx,AHEsat\rho^{\mathrm{sat}}_{\mathrm{yx,AHE}}. It is expected that ρyx,AHE\rho_{\mathrm{yx,AHE}} is dominated by intrinsic AHE in the forced ferromagnetic phase. In addition, σxx\sigma_{\mathrm{xx}} and σxy,AHE\sigma_{\mathrm{xy,AHE}} are calculated by

σxx=ρxx(B=0 T)(ρyx,AHEsat)2+ρxx(B=0 T)2,(1)\sigma_{\mathrm{xx}} = \frac{\rho_{\mathrm{xx}}(B = 0\ \mathrm{T})}{(\rho^{\mathrm{sat}}_{\mathrm{yx,AHE}})^2 + \rho_{\mathrm{xx}}(B = 0\ \mathrm{T})^2}, \tag*{(1)}

and

σxy,AHE=ρyx,AHEsat(ρyx,AHEsat)2+ρxx(B=0 T)2.(2)\sigma_{\mathrm{xy,AHE}} = \frac{\rho^{\mathrm{sat}}_{\mathrm{yx,AHE}}}{(\rho^{\mathrm{sat}}_{\mathrm{yx,AHE}})^2 + \rho_{\mathrm{xx}}(B = 0\ \mathrm{T})^2}. \tag*{(2)}

AHE has been roughly categorized into three regimes based on the range of σxx\sigma_{\mathrm{xx}} [6, 44]. For EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films in this study, σxx\sigma_{\mathrm{xx}} is below 1×104 Ω−1cm−11 \times10^{4}\ \Omega^{-1}\mathrm{cm}^{-1}, and the carrier density is located between 0.3×10190.3 \times10^{19} and 4.8×1019 cm−34.8 \times10^{19}\ \mathrm{cm}^{-3}. This suggests that the anomalous Hall velocity induced by the Berry curvature is suppressed with following the scaling relation σxy,AHE∝σxx1.6\sigma_{xy,\mathrm{AHE}} \propto\sigma_{xx}^{1.6}. With reducing the hole carrier density of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films at 2.0 K, ρyx,AHE\rho_{yx,\mathrm{AHE}} increases at first, decreases, and then increases again as shown in Figure 3(e). As confirmed in Figure 3(f), modulating carriers with electrostatic gating also follows this trend.

In order to discuss the carrier density dependence of AHE in the dirty metal regime [6, 44], we show the carrier density dependence of σxy,AHE/σxx1.6\sigma_{xy,\mathrm{AHE}}/\sigma_{xx}^{1.6} obtained by measuring EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films at 2.0 K, as shown in Figure 4(a). Remarkably, σxy,AHE/σxx1.6\sigma_{xy,\mathrm{AHE}}/\sigma_{xx}^{1.6} exhibits a large peak at about p=1×1019 cm−3p = 1 \times10^{19}\ \mathrm{cm}^{-3} and the same trend is confirmed by continuously modulating the carrier density with electrostatic gating. We also confirm that a similar large peak is observed in the plots of σxy,AHE\sigma_{xy,\mathrm{AHE}} and σxy,AHE/σxx\sigma_{xy,\mathrm{AHE}}/\sigma_{xx} (See Supplementary Materials [39]). σxy,AHE/σxx1.6\sigma_{xy,\mathrm{AHE}}/\sigma_{xx}^{1.6} values previously reported for bulk single crystals [23] also follow the same trend as revealed by the set of film measurements. Therefore, the observed peak is ascribed to successful adjustment of the Fermi level to EWE_{\mathrm{W}}.

Image not extracted

Figure 4. (a) Carrier density dependence of σxy,AHE/σxx1.6\sigma_{xy,\mathrm{AHE}}/\sigma_{xx}^{1.6} in EuCd2_2Sb2_2 films, compared to bulks of EuCd2_2Sb2_2 [23] and EuCd2_2As2_2 [40]. Electrostatic gating data obtained for low carrier samples (p<1×1019 cm−3p < 1 \times10^{19}\ \mathrm{cm}^{-3}) are also plotted with curves, colored by the sign of VGV_{\mathrm{G}}. (b) Magnified energy dispersion. (c) σxy,AHE\sigma_{xy,\mathrm{AHE}} and density of states (DOS) calculated as a function of energy. (d) σxy,AHE\sigma_{xy,\mathrm{AHE}} plotted for carrier density converted from DOS.

In order to understand the enhancement of σxy,AHE/σxx1.6\sigma_{xy,\mathrm{AHE}}/\sigma_{xx}^{1.6} more quantitatively, we perform first-principles calculations of band structure and intrinsic σxy,AHE\sigma_{xy,\mathrm{AHE}}. As shown in Figure 4(c), σxy,AHE\sigma_{xy,\mathrm{AHE}} exhibits a sharp peak at about E−EF=−0.02 eVE - E_{\mathrm{F}} = -0.02\ \mathrm{eV}, which corresponds to the energy position of W2\mathrm{W}_{2} and W3\mathrm{W}_{3} in Figure 4(b). The energy can be converted to carrier density by integrating density of states from E−EF=0 eVE - E_{\mathrm{F}} = 0\ \mathrm{eV}. As confirmed in Figure 4(d), σxy,AHE\sigma_{xy,\mathrm{AHE}} exhibits clear carrier density dependence consistent with the experimental data, demonstrating that the Fermi level of EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films passes through the energy position of W2\mathrm{W}_{2} and W3\mathrm{W}_{3}.

In summary, we have systematically investigated carrier density dependence of the intrinsic anomalous Hall conductivity by adjusting the Fermi level in simple magnetic Weyl semimetal EuCd2Sb2\mathrm{EuCd}_{2}\mathrm{Sb}_{2} films. The peak observed for σxy,AHE/σxx1.6\sigma_{xy,\mathrm{AHE}}/\sigma_{xx}^{1.6} has been also reproduced by first-principles calculations of energy-dependent intrinsic anomalous Hall conductivity. Our findings have provided transport evidence of intrinsic anomalous Hall conductivity originating in WPs. The present work paves the way for further exploring the potential of WPs-based exotic magnetotransport using film techniques.

This work was supported by JST PRESTO Grant No. JPMJPR18L2 and JST CREST Grant No. JPMJCR16F1, Japan and by Grant-in-Aid for Scientific Research (B) No. JP21H01804 from MEXT, Japan, and by TEPCO Memorial Foundation, Japan. The data that support the findings of this study are available from the corresponding author upon reasonable request.

References

Figures

References

  1. [1]A. A. Burkov, M. D. Hook, and L. Balents, Phys. Rev. B **84**, 235126 (2011).
  2. [2]S. Wang, B. C. Lin, A. Q. Wang, D. P. Yu, and Z. M. Liao, Adv. Phys.: X **2**, 518 (2017).
  3. [3]N. P. Armitage, E. J. Mele, and A. Vishwanath, Rev. Mod. Phys. **90**, 015001 (2018).
  4. [4]B. Q. Lv, T. Qian, and H. Ding, Rev. Mod. Phys. **93**, 025002 (2021).
  5. [5]T. Miyasato, N. Abe, T. Fujii, A. Asamitsu, S. Onoda, Y. Onose, N. Nagaosa, and Y. Tokura, Phys. Rev. Lett. **99**, 086602 (2007).
  6. [6]N. Nagaosa, J. Sinova, S. Onoda, A. H. MacDonald, and N. P. Ong, Rev. Mod. Phys. **82**, 1539 (2010).
  7. [7]D. Xiao, M. C. Chang, and Q. Niu, Rev. Mod. Phys. **82**, 1959 (2010).
  8. [8]D. J. Thouless, M. Kohmoto, M. P. Nightingale, and M. den Nijs, Phys. Rev. Lett. **49**, 405 (1982).
  9. [9]A. A. Burkov and L. Balents, Phys. Rev. Lett. **107**, 127205 (2011).
  10. [10]H. Z. Lu, S. B. Zhang, and S. Q. Shen, Phys. Rev. B **92**, 045203 (2015).
  11. [11]J. Noky, J. Gooth, C. Felser, and Y. Sun, Phys. Rev. B **98**, 241106 (R) (2018).
  12. [12]L. Muechler , E. Liu, J. Gayles, Q. Xu, C. Felser, and Y. Sun, Phys. Rev. B **101**, 115106 (2020).
  13. [13]J. Shen, Q. Zeng, S. Zhang, H. Sun, Q. Yao, X. Xi, W. Wang, G. Wu, B. Shen, Q. Liu et al., Adv. Funct. Mater. **30**, 2000830 (2020).
  14. [14]J. Shen, Q. Yao, Q. Zeng, H. Sun, X. Xi, G. Wu, W. Wang, B. Shen, Q. Liu, and E. Liu, Phys. Rev. Lett. **125**, 086602 (2020).
  15. [15]H. Zhou, G. Chang, G. Wang, X. Gui, X. Xu, J. X. Yin, Z. Guguchia, S. S. Zhang, T. R. Chang, H. Lin, W. Xie, M. Z. Hasan, and S. Jia, Phys. Rev. B **101**, 125121 (2020).
  16. [16]G. S. Thakur, P. Vir, S. N. Guin, C. Shekhar, R. Weihrich, Y. Sun, N. Kumar, and C. Felser, Chem. Mater. **32**, 1612 (2020).
  17. [17]K. Kuroda, T. Tomita, M. T. Suzuki, C. Bareille, A. A. Nugroho, P. Goswami, M. Ochi, M. Ikhlas, M. Nakayama, S. Akebi et al., Nat. Mater. **16**, 1090 (2017).
  18. [18]D. Khadka, T. R. Thapaliya, S. H. Parra, X. Han, J. Wen, R. F. Need, P. Khanal, W. Wang, J. Zang, J. M. Kikkawa et al., Sci. Adv. **6**, eabc1977 (2020).
  19. [19]T. Chen, T. Tomita, S. Minami, M. Fu, T. Koretsune, M. Kitatani, I. Muhammad, D. Nishio-Hamane, R. Ishii, F. Ishii et al., Nat. Commun. 12, 572 (2021).
  20. [20]X. Chen, H. Xie, Q. Zhang, Z. Luo, L. Shen, and Y. Wu, arXiv:2107.00959 (2021).arxiv.org/abs/2107.00959
  21. [21]N. Kiyohara, T. Tomita, and S. Nakatsuji, Phys. Rev. Appl. 5, 064009 (2016).
  22. [22]J. R. Soh, F. de Juan, M. G. Vergniory, N. B. M. Schröter, M. C. Rahn, D. Y. Yan, J. Jiang, M. Bristow, P. Reiss, J. N. Blandy et al., Phys. Rev. B 100, 201102(R) (2019).
  23. [23]H. Su, B. Gong, W. Shi, H. Yang, H. Wang, W. Xia, Z. Yu, P. J. Guo, J. Wang, L. Ding et al., APL Mater. 8, 011109 (2020).
  24. [24]A. Artmann, A. Mewis, M. Roepke, and G. Michels, Z. Anorg. Allg. Chem. 622, 679 (1996).
  25. [25]Y. Goryunov, V. Fritsch, H. V. Löhneysen, and A. Nateprov, J. Phys. Conf. Ser. 391, 012015 (2012).
  26. [26]J. R. Soh, C. Donnerer, K. M. Hughes, E. Schierle, E. Weschke, D. Prabhakaran, and A. T. Boothroyd, Phys. Rev. B 98, 064419 (2018).
  27. [27]Y. Nakazawa, M. Uchida, S. Nishihaya, S. Sato, A. Nakao, J. Matsuno, and M. Kawasaki, APL Mater. 7, 071109 (2019).
  28. [28]M. Ohno, M. Uchida, R. Kurihara, S. Minami, Y. Nakazawa, S. Sato, M. Kriener, M. Hirayama, A. Miyake, Y. Taguchi, R. Arita, M. Tokunaga, and M. Kawasaki, Phys. Rev. B 103, 165144 (2021).
  29. [29]M. Ohno, M. Uchida, Y. Nakazawa, S. Sato, M. Kriener, A. Miyake, M. Tokunaga, Y. Taguchi, and M. Kawasaki, APL Mater. 9, 051107 (2021).
  30. [30]M. Uchida, S. Sato, H. Ishizuka, R. Kurihara, T. Nakajima, Y. Nakazawa, M. Ohno, M. Kriener, A. Miyake, K. Ohishi et al., Sci. Adv. 7, eabl5381 (2021).
  31. [31]G. Kresse and J. Furthmüller, Comput. Mater. Sci. 6, 15 (1996).
  32. [32]G. Kresse and J. Furthmüller, Phys. Rev. B 54, 11169 (1996).
  33. [33]G. Kresse and D. Joubert, Phys. Rev. B 59, 1758 (1999).
  34. [34]J. P. Perdew, M. Ernzerhof, and K. Burke, J. Chem. Phys. 105, 9982 (1996).
  35. [35]S. L. Dudarev, G. A. Botton, S. Y. Savrasov, C. J. Humphreys, and A. P. Sutton, Phys. Rev. B 57, 1505 (1998).
  36. [36]H. J. Monkhorst and J. D. Pack, Phys. Rev. B 13, 5188 (1976).
  37. [37]G. Pizzi, V. Vitale, R. Arita, S. Blügel, F. Freimuth, G. Géranton, M. Gibertini, D. Gresch, C. Johnson, T. Koretsune et al., J. Phys.: Condens. Matter 32, 165902 (2020).
  38. [38]Q. S. Wu, S. N. Zhang, H. F. Song, M. Troyer, and A. A. Soluyanov, Comput. Phys. Commun. 224, 405 (2018).
  39. [39]See Supplementary Material [URL] for detailed characterization, which includes Refs. [6, 23, 44].
  40. [40]X. Cao, J.-X. Yu, P. Leng, C. Yi, Y. Yang, S. Liu, L. Kong, Z. Li, X. Dong, Y. Shi et al., arXiv:2103.09395 (2021).arXiv
  41. [41]K. S. Takahashi, H. Ishizuka, T. Murata, Q. Y. Wang, Y. Tokura, N. Nagaosa, and M. Kawasaki, Sci. Adv. 4, eaar7880 (2018).
  42. [42]A. H. Mayo, H. Takahashi, M. S. Bahramy, A. Nomoto, H. Sakai, and S. Ishiwata, Phys. Rev. X 12, 011033 (2022).
  43. [43]J. Shen, J. Gao, C. Yi, Q. Zeng, S. Zhang, J. Yang, X. Zhang, B. Wang, J. Cong, Y. Shi et al., arXiv:2106.02904 (2021).
  44. [44]S. Onoda, N. Sugimoto, and N. Nagaosa, Phys. Rev. Lett. 97, 126602 (2006).
  45. [46]K. Momma and F. Izumi, J. Appl. Crystallogr., 44, 1272 (2011).

Paper details

vlnc:W_cynv6jyr
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents