Signature of geometry modulation on interface magnetism emerged in isomeric IrO2-CoFe2O4 heterostructures

Abstract

The interface composed of magnets and strong spin-orbit coupling (SOC) materials forms an important platform for spintronic devices and intriguing magnetic phenomena, such as the chiral spin textures and magnetic proximity effect (MPE). The interface exchange interaction and Dzyaloshinskii-Moriya interaction (DMI) have been discussed in a wide range of heterostructures, while the crystal stacking geometry modulation on these interface interactions has rarely been considered. Here, we show a pronounced geometry modulation on the interface magnetism through comparing a rutile and an anatase IrO2 capping on a ferrimagnetic CoFe2O4. The rutile heterostructure with a high-symmetry interface shows a conventional anomalous Hall effect (AHE) profile due to the MPE. In contrast, the anatase one with a low-symmetry interface exhibits a topological-like AHE even at zero-field, suggesting the emergence of non-coplanar magnetic order at the interface. Our results suggest that the influence of DMI at the interface can be more accentuated by forming a low-symmetry interface and raises a new means of designing interface magnetism via the geometry modulation.

When a ferromagnet and a strong SOC paramagnetic-metal (PM) come into contact and form an interface, the combination of the inversion symmetry breaking at the interface and the strong SOC could lead to a finite DMI in the magnetic layer, which furthermore could generate a non-coplanar spin texture, such as skyrmion, as reported in some systems[1, 2, 3, 4, 5, 6]. At the same time, through the exchange interaction and/or charge transfer effect across the interface, the magnetic texture near the interface in the ferromagnetic material can have an impact on the PM material near the interface, potentially leading to a spin-ordered state in the PM layer, a phenomenon known as the magnetic proximity effect (as shown in Supplementary Fig. 1)[7, 8, 9, 10, 11, 12].

In general, the MPE-induced spin-order in the PM material is confined within a thickness of ∼1\sim1 nm, because the impact of the interface exchange interaction decays dramatically into the PM material as being away from the interface[12]. Besides, the induced spin order near the interface has often been assumed to be either parallel or antiparallel to the magnetic layer, depending on the signs of the exchange interactions. The interface exchange coupling energy (∼\simmeV) is generally larger than Zeeman energy (at ∼10\sim10 T),[13] and hence the MPE-induced spin order within the PM layer exhibits a switching concomitantly with the magnetization reversal of the ferromagnetic layer (Supplementary Fig. 1). Thus, the interface magnetism can be expected to be probed by the AHE measurement of the PM layer.

The interface-induced DMI in the FM material works exclusively in the top layer adjacent to the strong SOC ions.[14] It imparts a handedness to the magnetic exchange interaction with a so-called DM vector and could give rise to the formation of chiral spin textures in some heterostructures[1, 2, 3, 4, 5, 6]. Note that the DM vector depends on both the strength of SOC and the bonding geometry. Compared with the interfaces in which the PM and the ferromagnetic layers share a similar crystal symmetry,[3, 4, 5] the interface built with materials belonging to different crystal space groups could form a low-symmetry stacking geometry and strongly modulate the interface DMI in some systems. However, such an effect has not yet been explored clearly.

Here, we grew isomeric binary oxides IrO2\mathrm{IrO}_{2} on a spinel CoFe2O4\mathrm{CoFe}_{2}\mathrm{O}_{4} (CFO) for comparison and studied the interface magnetic states by AHE measurements. The CFO (space group, Fd3m) is a ferrimagnetic insulator due to the antiparallel spin coupling of the octahedral (OhO_h) Fe and tetrahedral (TdT_d) Co sites with a cubic structure (a=8.38a = 8.38 Å).[15] It can be grown on MgO substrate (cubic, a=4.21a = 4.21 Å) with a tiny strain.

Prior first principle calculations predicted that the IrO2_2 can form different crystal structures, while the stable phase that has been reported is the rutile (space group, P42_2/mnm, a=b=4.54a = b = 4.54 Å, c=3.81c = 3.81 Å)[16, 17]. Here, we succeeded in fabricating a metastable phase, anatase (space group, I41_1/amd, a=b=3.92a = b = 3.92 Å, c=9.78c = 9.78 Å),[17] by tuning the growth condition of IrO2_2 films (See Methods).

The structures of the interfaces can be first roughly considered from the lattice-constant point of view. The expected interface structures with rutile and anatase IrO2_2 are illustrated in Figure 1a,Figure 1b and Figure 1c,Figure 1d, respectively. The lattice mismatch and crystal symmetry determine that the rutile IrO2_2 will grow on CFO along the [1 1 0] as the out-of-plane orientation, while the anatase along the [1 0 0] (See methods). As will be discussed later, this expectation is experimentally confirmed by our X-ray diffraction (XRD) results. The combination of the rutile structure and CFO is expected to maintain two mirror planes orthogonal to the interface as a symmetry operation (M\mathcal{M}), as illustrated in Figure 1b. In contrast, for the stacking of the anatase IrO2_2 on CFO, a much larger lattice mismatch between the anatase [0 0 1] and CFO [1 0 0] inhibit the formation of such a high-symmetry interface, thereby leading to a more complex connection between the Ir and Fe/Co ions across the interface (Figure 1c, Figure 1d). As a result, the two mirror planes are lost, and thus, the anatase/CFO has a lower symmetry than the rutile/CFO. Moreover, the distribution of the Ir ions in anatase/CFO interface will potentially exhibit more kinds of crystallographically inequivalent sites than the rutile/CFO, as shown in Supplementary Fig. 2. Inspired by the observations of the enhanced DMI in asymmetrical sandwich structures, such as the Pt/Co/Ta[4] and the LaO/MnO2_2/SrO/IrO2_2,[5] we expect that the reduced symmetry due to the complex connection between the Ir and Fe/Co ions could lead to a larger DMI, thus having more chance to drive the interface magnetism toward a non-coplanar order. If a spin chirality (Ω\Omega)[18, 19] remains finite in such a non-coplanar spin texture (Figure 1e), one could expect a corresponding topological Hall feature in the transport measurements.

Illustration of the atomic stacking and magnetism at two kinds of interfaces

Figure 1. Illustration of the atomic stacking and magnetism at two kinds of interfaces. a, c, Crystal structures of the IrO2_2/CoFe2_2O4_4 (CFO) interfaces with a side-view for rutile (a) and anatase (c) IrO2_2, respectively. b, d, Top-views of the IrO2_2/CFO interfaces with the rutile (c) and anatase (d) capping on CFO, respectively. The crystal orientations of CFO and IrO2_2 are determined by minimizing the lattice mismatch, and are shown by the blue and orange axis, respectively. The mirrors (M\mathcal{M}) of the of the rutile type interface are shown by green lines in (b). The oxygen ions are shown with small gray spheres. e, Illustration of the spin chirality (Ω\Omega) due to the non-coplanar magnetic order.

The IrO2\mathrm{IrO_2}/CFO heterostructures with different IrO2\mathrm{IrO_2} phases were first verified by XRD measurements (See Methods). As shown in Figure 2a, the diffraction peaks at 27.8° and 47.4° are in excellent agreement with the rutile (1 1 0) and anatase (2 0 0), respectively[16, 17]. Besides, both heterostructures show a single phase without other XRD diffraction peaks. Compared to the rutile phase, the anatase one was fabricated for the first time in this work, to the best of our knowledge, which was further confirmed by a cross-sectional scanning transmission electron microscopy (STEM) measurement (See Methods). As shown in Supplementary Fig. 3, both the atomic column image and electron diffraction consistently confirm the successful fabrication of the anatase IrO2\mathrm{IrO_2} on a CFO layer. The energy-dispersive spectrometry (EDS) mappings suggest the ionic diffusion over the interface is negligible, which is attributable to the large difference of ionic radii among Fe, Co and Ir ions, as well as the relatively low growth temperature (~300°C). The CFO surface morphology with a roughness of half unit-cell level further guarantees a high-quality interface on a large scale (Supplementary Fig. 4). In addition, to investigate the valence states at the interfaces, we performed the soft X-ray absorption spectroscopy (XAS) on Fe and Co LL-edges (See Methods). As shown in Figure 2b and Supplementary Fig. 5, the samples capped with two types of IrO2\mathrm{IrO_2} show almost identical spectral features in both Fe LL-edge and Co LL-edge, indicating nearly identical valence in the two phases. The magnetic state of IrO2\mathrm{IrO_2} itself was studied by investigating the films directly grown on bare nonmagnetic MgO substrates. We observed the linear magnetic-field-dependent Hall resistivity and small positive magnetoresistance (MR), as shown in the Supplementary Fig. 6, concluding the paramagnetic metallic states of both rutile and anatase IrO2\mathrm{IrO_2}.

Characteristics of the two kinds of heterostructures

Figure 2. Characteristics of the two kinds of heterostructures. a, XRD 2θ2\theta-ω\omega scans of the two heterostructures built with CFO and rutile or anatase IrO2_2, respectively. b, XAS around Fe LL-edges measured on two heterostructures, with a comparison to that from bare CFO. Capping layers of anatase and rutile IrO2_2 are 2 nm. c, Temperature dependent resistivity (ρ\rho-TT) curves of the rutile and anatase IrO2_2 films grown on CFO. Inset, an illustration of the Hall bar for the transport measurement. d, Raw data of the Hall resistivity at 3 K measured from the two heterostructures. Dash lines indicate the ordinary Hall contributions with a linear fitting at high magnetic field regions. The thickness of IrO2_2 is 5 nm in rutile and 4 nm in anatase.

Figure 2c shows the temperature-dependent resistivity (ρ\rho–TT) curves of the IrO2\mathrm{IrO_2} grown on CFO, demonstrating a metallic state down to the lowest temperature in both phases. The anatase shows higher conductivity than the rutile, and this situation is similar to the case of anatase and rutile TiO2−δ_{2-\delta}, in which a key role of the electron-phonon interaction in the transport properties is discussed.[20, 21] To probe the interface magnetism, we measured the Hall resistivity and studied AHE on both IrO2_2/CFO heterostructures with the Hall bar illustrated in Figure 2c, inset (see methods). As shown in Figure 2d and Supplementary Fig. 7, the rutile and anatase IrO2_2 grown on CFO show p-type and n-type carriers, respectively, consistent with the results on the IrO2_2 directly grown on the nonmagnetic MgO substrate (Supplementary Fig. 6). To obtain the AHE signal, we decompose the Hall resistivity data into two contributions, i.e., ordinary Hall resistivity proportional to the external magnetic field (HH) with a coefficient RoR_{\mathrm{o}}, and anomalous Hall resistivity (ρyxAHE\rho_{yx}^{\mathrm{AHE}})[22]:

ρyx=Ro⋅H+ρyxAHE.(1)\rho_{yx} = R_{\mathrm{o}} \cdot H + \rho_{yx}^{\mathrm{AHE}}. \tag*{(1)}

Accordingly, by subtracting the ordinary Hall contributions (See Methods), the anomalous Hall resistivity of the two heterostructures can be obtained at various temperatures. Figure 3a and Figure 3b display the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH curves obtained in two heterostructures, respectively. The magnetic-field-dependent magnetization (MM-HH) curves of the CFO films are also shown in gray for comparison.

Comparing AHE curves of the two kinds of IrO2/CFO heterostructures

Figure 3. Comparing AHE curves of the two kinds of IrO2/CFO heterostructures. a, b, Magnetic field dependent anomalous Hall resistivity (ρyxAHE\rho_{yx}^{\mathrm{AHE}}-H) curves at a series of representative temperatures of the two heterostructures with rutile (a) and anatase (b) capping on CFO, respectively. Blue and orange curves correspond to the external magnetic field sweeping from 14 T to -14 T and reverse, respectively. Gray curves in (a) and (b) are the MM-HH curve of CFO, with a scale-bar of 200 emu/cm3^{3}. HcH_{\mathrm{c}}, coercive field, defined by the sign reversal from -14 T to +14 T.

We first focus on the rutile IrO2_2 on CFO. Note that in the temperature range of 10–100 K, the MM-HH curves of CFO and the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH curves of rutile IrO2_2 invariably exhibit almost identical profiles and coercive field (HcH_{\mathrm{c}}) (Figure 3a), indicating ρyxAHE∝M\rho_{yx}^{\mathrm{AHE}} \propto M and a concomitant switching of the MPE-induced magnetic order in rutile IrO2_2 and the magnetic moment of CFO. The tiny difference in the MM-HH and ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH profiles is seen at low temperatures, but this is attributable to the fact that the maximum magnetic field for the MM-HH measurements (7 T) is slightly smaller than the saturation field of the CFO.

In contrast, we find that the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH curves in the anatase phase show qualitatively different behaviour from those in the rutile phase (Figure 3b). While the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH curves in the anatase phase show the identical sign and profile with the rutile one at (or above) 50 K, the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH curve with a reversed sign and a reversed direction of hysteresis loop is observed at the lowest temperature; i.e., the coercive magnetic field, HcH_{\mathrm{c}}, is apparently negative (Figure 3b, 3 K). This unconventional hysteretic behaviour unique to the anatase phase can be seen even in the raw ρyx\rho_{yx}-HH curve at 3 K (Figure 2d). Assuming that the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH is saturated at 14 T, both the magnetic moments of anatase IrO2_2 induced by MPE and the CFO should be aligned toward the direction of the external magnetic field. Such a sign reversal of the ρyxAHE\rho_{yx}^{\mathrm{AHE}} with decreasing temperature has been reported for the ferromagnetic SrRuO3_3, and the sign reversal of the momentum-space Berry curvature is thought to underlie the observation.[3, 23] A similar mechanism may account for the temperature dependence of ρyxAHE\rho_{yx}^{\mathrm{AHE}} at the magnetic interface of anatase. The sign reversal ρyxAHE\rho_{yx}^{\mathrm{AHE}} occurs at the intermediate temperature, 20 K, at which ρyxAHE(14 T)\rho_{yx}^{\mathrm{AHE}}(14\ \mathrm{T}) becomes nearly zero (Figure 3b). However, a hump-like feature emerges in the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH profile at low fields, which can not be interpreted by an artifact of the process of subtracting ordinary Hall resistivity (Supplementary Fig. 8), suggesting that an additional term that is not proportional to MM is intrinsic and should be considered in more detail to understand the whole profile[3, 5, 24].

To gain more insight into the ρyxAHE\rho_{yx}^{\mathrm{AHE}}-HH profile that is not proportional to magnetization, we further assumed that the anomalous Hall conductance, GxyAHEG_{xy}^{\mathrm{AHE}} (=ρyxAHE⋅ρxx−2⋅t=\rho_{yx}^{\mathrm{AHE}}\cdot\rho_{xx}^{-2}\cdot t; tt is the thickness of IrO2_2), of the anatase heterostructure consists of two contributions:[24]

GxyAHE(H)=GxyM(H)+GxyT(H)(2)G_{xy}^{\mathrm{AHE}}(H)=G_{xy}^{\mathrm{M}}(H)+G_{xy}^{\mathrm{T}}(H) \tag*{(2)}
=SHM(H)+GxyT(H),(3)= S_{\mathrm{H}}M(H)+G_{xy}^{\mathrm{T}}(H), \tag*{(3)}

where the GxyMG_{xy}^{\mathrm{M}} and GxyTG_{xy}^{\mathrm{T}} denote the anomalous Hall contributions proportional to the uniform magnetization (MM) and the spin chirality (Ω\Omega, as shown in Figure 1e)[19], respectively. The latter contribution may be referred to as the topological Hall effect[3, 5, 19, 24]. Considering that the GxyM(H)G_{xy}^{\mathrm{M}}(H) curve should be an identical profile to the MM-HH curve at each temperature in both the rutile and anatase heterostructures, the GxyM(H)G_{xy}^{\mathrm{M}}(H) curve of the anatase heterostructure is expected to be proportional to the GxyM(H)G_{xy}^{\mathrm{M}}(H) of the rutile one, which is ≈GxyAHE(H)\approx G_{xy}^{\mathrm{AHE}}(H) because of the absence of GxyT(H)G_{xy}^{\mathrm{T}}(H) for the rutile one. The coefficient, SHS_H, for the anatase can be determined by fitting the GxyAHE(H)G_{xy}^{\mathrm{AHE}}(H), where all the magnetic moments are aligned toward the external field (at 14 T, for instance). Thus, the GxyT(H)G_{xy}^{\mathrm{T}}(H) can be obtained by calculating GxyAHE(H)−SHM(H)G_{xy}^{\mathrm{AHE}}(H)-S_HM(H). The resulting decomposition of GxyAHE(H)G_{xy}^{\mathrm{AHE}}(H) for the case of 3 K is shown in Figure 4a. Distinctly, the resulting GxyTG_{xy}^{\mathrm{T}} appears at −9 T (+9 T), becomes maximum at +2 T (−2 T), which is close to the magnetization reversal of CFO, and disappears at +6 T (−6 T) in the field increasing (decreasing) process. Thus, the magnetic field dependence of GxyTG_{xy}^{\mathrm{T}} exhibits a hump feature. The calculated GxyTG_{xy}^{\mathrm{T}} is summarized as a contour map in the HH-TT space (Figure 4b), in which only the data measured during the magnetic field sweeping from −14 T to +14 T are shown for clarity. The contour map clearly shows that GxyTG_{xy}^{\mathrm{T}} signal decreases gradually as the temperature increases and eventually disappears at ~50 K. Note that the hypothetical two channels mechanism based on the coexisting opposite-sign GxyAHE(H)G_{xy}^{\mathrm{AHE}}(H) with non-synchronous switching of the magnetization can also exhibit a hump feature [25, 26]. However, this model does not produce negative HcH_c in the AHE curves and therefore appears irrelevant to the present system. Thus, the emergent GxyTG_{xy}^{\mathrm{T}} signal suggests that a non-coplanar spin texture with a finite spin chirality feature is formed in the anatase/CFO interface, such as the magnetic skyrmions [1, 2, 3, 4, 5, 6], the textures analogous to that of CoTa3_3S6_6 [27] or Pr2_2Ir2_2O7_7 [28], etc [29].

Analyses of the anomalous Hall conductance curves in the anatase-$\mathrm{IrO_2}$/CFO heterostructure

Figure 4. Analyses of the anomalous Hall conductance curves in the anatase-IrO2\mathrm{IrO_2}/CFO heterostructure. a, Two components of the anomalous Hall conductance (GxyAHEG_{xy}^{\mathrm{AHE}}) at 3 K. The measured GxyAHEG_{xy}^{\mathrm{AHE}} (solid line) can be divided into two contributions, i.e., the term GxyMG_{xy}^{\mathrm{M}} derived from the uniform magnetization and that GxyTG_{xy}^{\mathrm{T}} generated by spin chirality (non-coplanar order). b, Contour plot of the GxyTG_{xy}^{\mathrm{T}} in the HH-TT space. The data were measured with magnetic field sweeping from -14 T to 14 T. The coercive fields (HcH_{\mathrm{c}}) of the CFO with different temperatures are shown.

Although the details of the non-coplanar magnetic order in the anatase/CFO heterostructure remain unclear due to the difficulty of direct observation of the interface magnetism, the contrasting behaviour of the AHE in the two isomeric heterostructures indicates that lowering the symmetry of the crystal stacking geometry is an effective way to produce a topological-Hall-like signal in a heterostructure consisting of a paramagnetic metal and an insulating ferromagnet. Note that the isomeric materials are widespread in binary oxides, such as rutile, anatase, λ\lambda-phase, etc [20, 21, 30]. We envision that the concept of isomeric heterostructure can be extended into more systems to design novel electronic and magnetic states.

Methods

Synthesis of IrO2\mathrm{IrO_2}/CFO heterostructures. The heterostructures were fabricated by pulsed laser deposition method equipped with an excimer laser (λ=248\lambda= 248 nm). The CFO films were first grown on MgO (001) substrate with a temperature of 450°C, and oxygen pressure of 15 mTorr, the energy fluence was controlled at 1.5 J/cm2^{2} and the frequency was 5 Hz. The thickness of CFO for transport and magnetization measurements were controlled at ∼\sim 20 nm. After that, the rutile IrO2\mathrm{IrO_2} was fabricated with a relatively high oxygen pressure of 40 mTorr, a temperature of 350-380 °C, a fluence of 1.3 J/cm2^{2}, and a frequency of 2 Hz. The anatase IrO2\mathrm{IrO_2} phase was obtained with a growth oxygen pressure of 8 mTorr, a temperature of 270∼\sim300°C, a fluence of 0.8 J/cm2^{2}, and a frequency of 7 Hz. After the depositions, all films were annealed with a high oxygen pressure of 10 Torr at 200°C for 15 minutes to reduce the oxygen vacancy and then cooled to room temperature at a rate of 10 °C/min. The in-plane [−1 1 0][-1\ 1\ 0] and [0 0 1][0\ 0\ 1] of rutile have a mismatch of ∼\sim7.2% and ∼\sim6.4% to the [1 −1 0][1\ -1\ 0] and [1 1 0][1\ 1\ 0] of CFO, respectively. The in-plane [0 1 0][0\ 1\ 0] of anatase has a lattice mismatch of ∼\sim 6.8% to the [0 1 0][0\ 1\ 0] of CFO, while the [0 0 1][0\ 0\ 1] of anatase has a huge mismatch of ∼\sim16.1% to the [1 0 0][1\ 0\ 0] of CFO.

XRD and XAS measurements. The XRD 2θ2\theta-ω\omega scans were carried out with a high-resolution system (Smartlab, Rigaku) with a Cu-Kα1\alpha_1 (λ=0.15406\lambda= 0.15406 nm). The XAS curves of Fe and Co were measured at room temperature in BL14, Hiroshima Synchrotron Radiation Center (HiSOR), Hiroshima University with a total electron yield mode. The curves were normalized by subtracting a background.

STEM measurements. The sample was prepared by mechanical polishing and Ar-ion milling process. The cross-sectional scanning transmission electron microscopy (STEM) and corresponding element-mapping images were acquired using a TEM (JEM-2800, JEOL) equipped with energy-dispersive X-ray spectrometry (EDS) at an accelerating voltage of 200 kV. These results were analyzed using an X-ray microanalysis system (NORAN SYSTEM 7, Thermo Scientific). The cross-sectional high-resolution transmission electron microscopy (HRTEM) images were acquired using a TEM (JEM-2800, JEOL) at an accelerating voltage of 200 kV.

Anomalous Hall measurements. The Hall bars with a size of 300 μm×60 μm\mu\mathrm{m} \times60\ \mu\mathrm{m} were used for all measurements, which were fabricated by a photo-lithography and an Ar-ions milling system. The transport measurements were conducted with a 14 T PPMS system (Quantum Design) with an in-plane DC current of ∼1.0×105 A/cm2\sim1.0 \times10^{5}\ \mathrm{A}/\mathrm{cm}^{2}. The Hall resistivity ρyx\rho_{yx} was measured by ρyx=Vyx/Ixx⋅t\rho_{yx} = V_{yx}/I_{xx} \cdot t, where VyxV_{yx}, IxxI_{xx}, and tt correspond to the transverse voltage, longitudinal current, and the IrO2_2 film thickness, respectively. The longitudinal magnetoresistance was subtracted by the method in the reference[31]. The anomalous Hall resistivity ρyxAHE\rho_{yx}^{\mathrm{AHE}} was obtained by subtracting the ordinary Hall contribution, which was determined with a linear fitting on the high magnetic field regions. The anomalous Hall conductance GxyAHEG_{xy}^{\mathrm{AHE}} was obtained by

GxyAHE=ρyxAHE/ρxx2⋅t.G_{xy}^{\mathrm{AHE}} = \rho_{yx}^{\mathrm{AHE}} / \rho_{xx}^{2} \cdot t.

Acknowledgments: This study was financially supported by JSPS KAKENHI (Grant Nos. 21H04442, 21K14398) and JST CREST (Grant No. JPMJCR1874). P. Y. acknowledges the supports from the National Key R&D Program of China (grant No. 2021YFE0107900) and the National Natural Science Foundation of China (grant No. 52025024).

Data availability: All the data presented in the article and Supplementary Information are available from the corresponding authors upon reasonable request.

Author contributions: M. W. and F. K. conceived the project. M. W. fabricated the samples with the help of P. Y. M. W. performed the magnetization, XRD, and transport measurements. S. M. and X. Y. performed the STEM measurements. M. W. performed the XAS measurements with the help of M. S. N. K. and P. Y. provided deep discussions. M. W. and F. K. wrote the manuscript. All authors discussed the results and commented on the manuscript.

Competing Interests: The authors declare no competing interests.

Figures

References

  1. [1]Tokura, Y. & Kanazawa, N. Magnetic skyrmion materials. Chem. Rev. 121, 2857-2897 (2021).DOI
  2. [2]Jani, H. et al. Antiferromagnetic half-skyrmions and bimerons at room temperature. Nature 590, 74-79 (2021).
  3. [3]Matsuno, J. et al. Interface-driven topological Hall effect in SrRuO3-SrIrO3 bilayer. Sci. Adv. 2, e1600304 (2016).DOI
  4. [4]Woo, S. et al. Observation of room-temperature magnetic skyrmions and their current-driven dynamics in ultrathin metallic ferromagnets. Nat. Mater. 15, 501-506 (2016).
  5. [5]Skoropata, E. et al. Interfacial tuning of chiral magnetic interactions for large topological Hall effects in LaMnO3/SrIrO3 heterostructures. Sci. Adv. 6, eaaz3902 (2020).
  6. [6]Soumyanarayanan, A., Reyren, N., Fert, A. & Panagopoulos, C. Emergent phenomena induced by spin–orbit coupling at surfaces and interfaces. Nature 539, 509 (2016).
  7. [7]Katmis, F. et al. A high-temperature ferromagnetic topological insulating phase by proximity coupling. Nature 533, 513-516 (2016).DOI
  8. [8]Yoo, M.-W. et al. Large intrinsic anomalous Hall effect in SrIrO₃ induced by magnetic proximity effect. Nat. Commun. 12, 3283 (2021).DOI
  9. [9]Jaiswal, A. K. et al. Direct observation of strong anomalous Hall effect and proximity-induced ferromagnetic state in SrIrO₃. Adv. Mater. 34, 2109163 (2022).
  10. [10]Wihelm, F. et al. Interface magnetism in 3d/5d multilayers probed by X-ray magnetic circular dichroism. Phys. stat. sol. (a) 196, 33-36 (2003).
  11. [11]Mogi, M. et al. Current-induced switching of proximity-induced ferromagnetic surface states in a topological insulator. Nat. Commun. 12, 1404 (2021).DOI
  12. [12]Graulich, D. et al. Quantitative comparison of the magnetic proximity effect in Pt detected by XRMR and XMCD. Appl. Phys. Lett. 118, 012407 (2021).
  13. [13]Haugen, H., Huertas-Hernando, D. & Brataas, A. Spin transport in proximity-induced ferromagnetic graphene. Phys. Rev. B 77, 115406 (2008).DOI
  14. [14]Yang, H., Thiaville, A., Rohart, S., Fert, A. & Chshiev, M. Anatomy of Dzyaloshinskii-Moriya interaction at Co/Pt interfaces. Phys. Rev. Lett. 115, 267210 (2015)DOI
  15. [15]Dorsey, P. C., Lubitz, P., Chrisey, D. B. & Horwitz, J. S. CaFe₂O₄ thin films grown on (100) MgO substrates using pulsed laser deposition. J. Appl. Phys. 79, 6338-6340 (1996).DOI
  16. [16]Stoerzinger, K. A. et al. Orientation-dependent oxygen evolution activities of rutile IrO₂ and RuO₂. J. Phys. Chem. Lett. 5, 1636-1641 (2014).DOI
  17. [17]Sen, F. G., et al. Towards accurate prediction of catalytic activity in IrO₂ nanoclusters via first principles-based variable charge force field. J. Mater. Chem. A, 3, 18970-18982 (2015).DOI
  18. [18]Taguchi, Y. et al. Spin chirality, Berry phase, and anomalous Hall effect in a frustrated ferromagnet. Science 291, 2573-2576 (2001).pubmed.ncbi.nlm.nih.gov/11283363
  19. [19]Wang, W. et al. Spin chirality fluctuation in two-dimensional ferromagnets with perpendicular magnetic anisotropy. Nat. Mater. 18, 1054-1059 (2019).DOI
  20. [20]Yan, B. et al. Anatase TiO₂-A model system for large polaron transport. ACS Appl. Mater. Interfaces 10, 38201-38208 (2018).
  21. [21]Shen, S. et al. Coexistence of both localized electronic states and electron gas at rutile TiO₂ surfaces. Adv. Mater. 35, 2301453 (2023).DOI
  22. [22]Nagaosa, N. et al. Anomalous Hall effect. Rev. Mod. Phys. 82, 1539 (2010).DOI
  23. [23]Fang, Z. et al. The anomalous Hall effect and magnetic monopoles in momentum space. Science 302, 92-95 (2003).
  24. [24]Vistoli, L. et al. Giant topological Hall effect in correlated oxide thin films. Nat. Phys. 15, 67-72 (2019).DOI
  25. [25]Kimbell, G. et al. Two-channel anomalous Hall effect in SrRuO₃. Phys. Rev. Mater. 4, 054414 (2020).
  26. [26]Wang, L. et al. Controllable thickness inhomogeneity and berry curvature engineering of anomalous Hall effect in SrRuO₃ ultrathin films. Nano Lett. 20, 2468 (2020).DOI
  27. [27]Takagi, H. et al. Spontaneous topological Hall effect induced by non-coplanar antiferromagnetic order in intercalated van der Waals materials. Nat. Phys. 19, 961-968 (2023).DOI
  28. [28]Machida, Y., Nakatsuji, S., Onoda, S., Tayama, T. & Sakakibara, T. Time-reversal symmetry breaking and spontaneous Hall effect without magnetic dipole order. Nature 463, 210-213 (2010).
  29. [29]Seddon, S. D. et al. Real-space observation of ferroelectrically induced magnetic spin crystal in SrRuO₃. Nat. Commun. 12, 2007 (2021).DOI
  30. [30]Kuriyama, H. et al. Epitaxially stabilized iridium spinel oxide without cations in the tetrahedral site. Appl. Phys. Lett. 96, 182103 (2010).DOI
  31. [31]Li, Z. et al. Reversible manipulation of the magnetic state in SrRuO₃ through electric-field controlled proton evolution. Nat. Commun. 11, 184 (2020).DOI

Paper details

vlnc:W_dhw2bsyu
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents