betaFeedback

WorksPhysics and Astronomy

On-chip all-electrical determination of the magnetoelastic coupling constant of magnetic heterostructures

Abstract

We have developed an approach to determine the magnetoelastic coupling constant of magnetic layers in thin film heterostructures. The film is formed on a piezoelectric substrate between two interdigital transducers (IDT), a platform often used to construct a surface acoustic wave device. With the substrate piezoelectricity, strain is induced into the film by applying a dc voltage to the IDTs. The strain causes changes in the magnetization direction of the magnetic layer, which is probed by measuring changes, if any, in the transverse resistance of the heterostructure. We find the extracted magnetoelastic coupling constant of the magnetic layer (CoFeB) depends on the film stacking. Such change can be accounted for provided that the elastic properties of the layers that constitute the heterostructures are taken into account. The on-chip all-electrical approach described here provides a versatile means to quantitatively assess the magnetoelastic coupling constant of thin film heterostructures.

Magnonics[1, 2, 3, 4] is a research field that focuses on the transport and manipulation of spin waves or their quanta known as magnons. Magnons are known to form composite quasi-particles when they interact with other degrees of freedom. Of particular interest is the coupled mode of magnons and phonons[5, 6, 7] facilitated by the magnetoelastic coupling. The magnon-phonon coupling can add functionalities to the magnon/phonon system that are otherwise absent in the uncoupled state. For example, the coupling can increase the coherence length[8, 9] of magnons thanks to the phonons’ long coherence length while the phonons can be controlled by magnetic field and acquire nonreciprocity owing to the magnons’ time reversal symmetry breaking characteristics[10, 11, 12].

Surface acoustic waves (SAWs), a form of coherent phonons, are widely used to study the magnon-phonon coupling owing to their low damping loss and high energy density. SAW devices[13], consisting of a pair of interdigital transducers (IDTs) and a ferromagnetic (FM) thin film element formed between the two IDTs and on a piezoelectric substrate, are commonly employed for such study. Effects that originate from the magnon-phonon coupling in such systems have been reported recently that include, for example, the acoustic spin pumping[14, 15], nonreciprocal propagation of SAWs[16, 17, 18, 19, 20, 21, 22, 23], and coherent coupling of magnon-phonon in an acoustic cavity[24].

As the magnon-phonon coupling is primarily determined by the magnetoelastic coupling constant of the magnetic material, it is of great importance to quantitatively characterize its strength. In general, evaluation of the magnetoelastic coupling constant requires mechanical tools, such as bending and/or tension applying systems[25, 26, 27, 28, 29, 30], which require special apparatus and careful calibration of the strain. Here we propose a simple but accurate approach to determining the magnetoelastic coupling constant of a ferromagnetic layer in a thin film heterostructure formed on SAW devices. A constant voltage across a pair of IDTs is applied to induce strain in the film. Due to the magnetoelastic coupling, the strain causes a slight tilting in the magnetization direction, which we quantify using the planar Hall resistance of the ferromagnetic layer. We apply this on-chip all-electrical approach to determine the magnetoelastic coupling constant of a ferromagnetic layer embedded in different heterostructures.

Figure 1 shows a schematic representation of the experimental setup, along with the coordinate system used in this study. The devices employed here consist of a thin film heterostructure element, a pair of IDTs, and electrodes for electrical contact. The films are deposited on piezoelectric Y+128°-cut LiNbO3_3 substrates using radio frequency (rf) magnetron sputtering. The film structure is sub./X/MgO (2)/Ta (1), where X is one of the following: W (2.4)/CoFeB (1), Pt (2.4)/CoFeB (1), and MgO (2)/CoFeB (1)/W (2.4) (thicknesses in unit of nanometers), denoted as W/CoFeB, Pt/CoFeB, and CoFeB/W, respectively, hereafter. MgO (2)/Ta (1) serves as a capping layer to prevent oxidation of the films. Note that the crystallinity of the W layer is different for W/CoFeB and CoFeB/W: the former is predominantly composed of the β\beta-phase whereas the latter is a mixture of α\alpha- and β\beta-phases[31]. The degree of mixture can be roughly inferred from the film resistance[32, 33]. For all films, the magnetic easy axis of the CoFeB layer points along the film plane. Optical lithography and Ar ion etching are used to pattern the films into rectangular elements. The size of the rectangle is approximately 400 μ\mum wide and 450 μ\mum long. Electrodes and the IDTs, composed of Ta (5)/Cu (100)/Pt (5), are patterned using optical lithography and a lift-off process. Two IDTs are placed on the sides of the rectangular element: we denote them as IDT1 and IDT2 (see Figure 1(a)). Each IDT consists of 20 pairs of fingers, with a width and gap of approximately 5 μ\mum, and the length is 450 μ\mum.

Figure 1. (a) Illustration of the device and its dimensions. (b) Schematic diagram of the experimental setup and definition of the coordinate system. The orange arrow (εxx\varepsilon_{xx}) represents the longitudinal strain induced by the voltage (VpV_{\mathrm{p}}) applied to the IDT.

To quantitatively assess the magnetoelastic coupling constants of the FM (here CoFeB), we study the change in the magnetization direction induced by the strain applied. We make use of the piezoelectricity of the substrate to apply strain to the film. A direct current (dc) voltage VpV_{\mathrm{p}} is applied to IDT1 while IDT2 is grounded, which in turn induces a strain between the two IDTs. The strain induced in the film is proportional to VpV_{\mathrm{p}} (see supplementary material for the details). The direction of the FM magnetization is determined by the planar Hall resistance that originates from the anisotropic magnetoresistance[34] and the spin Hall magnetoresistance[35]. A constant electric current (IxI_x) of 10 mA is supplied to the films along the xx-axis. The transverse voltage VyxV_{yx} across the films is measured using a voltmeter. The transverse resistance RyxR_{yx} is obtained from VyxV_{yx} and IxI_x: Ryx=Vyx/IxR_{yx}=V_{yx}/I_x. An in-plane magnetic field of magnitude HH is applied during the transport measurements. The angle between the magnetic field and the xx-axis is defined as φH\varphi_H. To ensure stable measurement conditions, all measurements are performed at least one hour after the electric current begins to flow through the films.

First, we describe the change in RyxR_{yx} induced by the strain. We denote the angle between the equilibrium magnetization direction without the strain and the xx-axis as φ\varphi. (The magnetization lies within the film (xyxy) plane). The strain-induced change in the magnetization direction δφ\delta\varphi can be expressed as follows[31, 36]:

δφ=δφ0sin⁡2φH,(1)\delta\varphi=\delta\varphi_0\sin2\varphi_H, \tag*{(1)}

where the amplitude δφ0\delta\varphi_0 is represented by

δφ0=HMEH.(2)\delta\varphi_0=\frac{H_{\mathrm{ME}}}{H}. \tag*{(2)}

HMEH_{\mathrm{ME}} represents the effective magnetic field induced by strain and is given as

HME=−bεxx(Vp)MS.(3)H_{\mathrm{ME}}=-\frac{b\varepsilon_{xx}(V_{\mathrm{p}})}{M_{\mathrm{S}}}. \tag*{(3)}

εxx(Vp)\varepsilon_{xx}(V_{\mathrm{p}}) is the strain along the xx-axis, MSM_{\mathrm{S}} and bb are the saturation magnetization and the magnetoelastic coupling constant of the FM layer, respectively. Upon application of VpV_{\mathrm{p}} to IDT1, RyxR_{yx} under strain is expressed as

Ryx(Vp)=Ryx2φ⋅12sin⁡2(φH+δφ)≈Ryx2φ⋅12sin⁡2φH+Ryx4φ⋅12sin⁡4φH,(4)\begin{aligned} R_{yx}(V_{\mathrm{p}})&=R_{yx}^{2\varphi}\cdot\frac{1}{2}\sin2(\varphi_H+\delta\varphi)\\ &\approx R_{yx}^{2\varphi}\cdot\frac{1}{2}\sin2\varphi_H+R_{yx}^{4\varphi}\cdot\frac{1}{2}\sin4\varphi_H, \tag*{(4)} \end{aligned}

where in the second line, we defined

Ryx4φ≡Ryx2φδφ0=−Ryx2φbHMSεxx(Vp),(5)R_{yx}^{4\varphi}\equiv R_{yx}^{2\varphi}\delta\varphi_0=-R_{yx}^{2\varphi}\frac{b}{HM_{\mathrm{S}}}\varepsilon_{xx}(V_{\mathrm{p}}), \tag*{(5)}

using Eqs. (2) and (3). It is evident that Ryx4φR_{yx}^{4\varphi} contains information on the magnetoelastic coupling while Ryx2φR_{yx}^{2\varphi} represents the magnitude of the planar Hall resistance at Vp=0V_{\mathrm{p}}=0 V. Note that Eq. (4) holds under the condition δφ0≪1\delta\varphi_0\ll1, which is satisfied in the present study.

The measurement results of Ryx(Vp)R_{yx}(V_{\mathrm{p}}) for W/CoFeB with Vp=±210V_{\mathrm{p}}=\pm210 V are plotted against φH\varphi_H in Figure 2(a). Since the change in RyxR_{yx} caused by the strain [Ryx4φR_{yx}^{4\varphi} in Eq. (4)] is significantly smaller than Ryx2φR_{yx}^{2\varphi}, it is difficult to resolve its effect from such plot. We therefore process data obtained from Ryx(+Vp)R_{yx}(+V_{\mathrm{p}}) and Ryx(−Vp)R_{yx}(-V_{\mathrm{p}}). Noting that εxx(−Vp)=−εxx(+Vp)\varepsilon_{xx}(-V_{\mathrm{p}})=-\varepsilon_{xx}(+V_{\mathrm{p}}), we define the following quantities:

Magnetic field angle and Hall resistance measurements for W/CoFeB, CoFeB/W, and Pt/CoFeB

Figure 2. (a) Magnetic field angle (φH\varphi_H) dependence of RyxR_{yx} for W/CoFeB (a). The orange squares (purple dots) represent the results when a dc voltage VpV_p of +210 V (−210 V) is applied to IDT1. (b-d) δRyx\delta R_{yx} plotted against φH\varphi_H for W/CoFeB (b), CoFeB/W (c), and Pt/CoFeB (d). The magnetic field magnitude HH is fixed to ∼7 mT and ∣Vp∣|V_p| = 210 V. The error bars are standard deviation of the repeated measurements. The black lines in (b-d) show fit to the data with Eq. (6).

R‾yx≡Ryx(+Vp)+Ryx(−Vp)2∼Ryx2φ⋅12sin⁡2φH,δRyx(Vp)≡Ryx(+Vp)−Ryx(−Vp)2∼Ryx4φ⋅12sin⁡4φH.(6)\begin{aligned} \overline{R}_{yx}&\equiv\frac{R_{yx}(+V_{\mathrm{p}})+R_{yx}(-V_{\mathrm{p}})}{2}\sim R_{yx}^{2\varphi}\cdot\frac{1}{2}\sin2\varphi_H,\\ \delta R_{yx}(V_{\mathrm{p}})&\equiv\frac{R_{yx}(+V_{\mathrm{p}})-R_{yx}(-V_{\mathrm{p}})}{2}\sim R_{yx}^{4\varphi}\cdot\frac{1}{2}\sin4\varphi_H. \tag*{(6)} \end{aligned}

Thus Ryx2φR_{yx}^{2\varphi} and Ryx4φR_{yx}^{4\varphi} can be obtained from R‾yx\overline{R}_{yx} and δRyx(Vp)\delta R_{yx}(V_{\mathrm{p}}), respectively. Figures 2(b-d) show the φH\varphi_H dependence of δRyx\delta R_{yx} for W/CoFeB, CoFeB/W, and Pt/CoFeB with H∼7H\sim7 mT and ∣Vp∣=210|V_{\mathrm{p}}|=210 V. As evident, δRyx\delta R_{yx} sinusoidally changes with φH\varphi_H in a period of 90∘90^\circ for all the films. We fit the data using Eq. (6) to extract Ryx4φR_{yx}^{4\varphi}. Deviation from the sin⁡4φH\sin4\varphi_H dependence are found for Pt/CoFeB and to a lesser extent, in CoFeB/W. We believe this is due to the magnetic anisotropy of the FM layer. Note that the signal strength (Ryx4φR_{yx}^{4\varphi}) depends on the planar Hall resistance Ryx2φR_{yx}^{2\varphi} of the samples: see Eq. (5). The planar Hall resistance ratio, Ryx2φR_{yx}^{2\varphi} divided by the longitudinal resistance, is 0.5% ∼ 1% for the samples studied here. For a single layer CoFeB films, the planar Hall resistance ratio is less than 0.1%, which may require longer measurement time to obtain processable data.

FilmHMEH_{\mathrm{ME}} (µT)MSM_S (MA/m)tdt_d (nm)bεxxb\varepsilon_{xx} (µJ/cm3^3)
W/CoFeB10.4 ± 0.31.31 ± 0.060.3 ± 0.114 ± 1
CoFeB/W16.1 ± 0.31.15 ± 0.050.4 ± 0.119 ± 1
Pt/CoFeB9.0 ± 0.41.12 ± 0.06−0.5 ± 0.210 ± 1

Table 1. Summary of the parameters obtained from the experiments for W/CoFeB, CoFeB/W, and Pt/CoFeB. Magnetoelastic effective field: HMEH_{\mathrm{ME}}, saturation magnetization: MSM_S, thickness of the magnetic dead layer: tdt_d, magnetoelastic energy with a piezoelectric strain of ∣Vp∣|V_p| = 210 V: bεxxb\varepsilon_{xx}. Errors represent the fitting errors.

According to Eq. (5), Ryx4φR_{yx}^{4\varphi} must scale with the inverse of HH. We therefore study the magnetic field magnitude (HH) dependence of δRyx\delta R_{yx} (and thereby the HH dependence of Ryx4φR_{yx}^{4\varphi}). Figure 3(a) shows the φH\varphi_H dependence of δRyx\delta R_{yx} for W/CoFeB measured with various HH. Here ∣Vp∣|V_p| is fixed to 210 V. The results show that the amplitude of the sin⁡4φH\sin4\varphi_H variation indeed decreases with increasing HH. We thus fit the φH\varphi_H dependence of RyxR_{yx} (not shown here) and δRyx\delta R_{yx} with Eq. (6) to obtain Ryx2φR_{yx}^{2\varphi} and Ryx4φR_{yx}^{4\varphi}, respectively. Subsequently, we normalize Ryx4φR_{yx}^{4\varphi} by dividing it with Ryx2φR_{yx}^{2\varphi} to estimate δφ0\delta\varphi_0: see Eq. (5). The HH dependence of δφ0\delta\varphi_0 for W/CoFeB, CoFeB/W, and Pt/CoFeB are plotted in Figure 3(b-Figure 3d). We fit the data in Figure 3(b-Figure 3d) with Eq. (2) to determine the magnetoelastic effective field HMEH_{\mathrm{ME}}. The fitting results are shown by the solid lines in Figure 3(b-Figure 3d), which show good agreement with the experimental results.

Field-angle and field-magnitude dependence of Hall resistance

Figure 3. (a) The field angle (φH\varphi_H) dependence of δRyx\delta R_{yx} for W/CoFeB measured under various field magnitudes (HH). Purple, green and orange points are for HH ∼ 7 mT, 14 mT, and 56 mT, respectively. ∣Vp∣|V_p| = 210 V is applied. The offset resistance is subtracted from the plotted data. The error bars indicate standard deviation of the repeated measurements. (b-d) The field magnitude (HH) dependence of δφ0\delta\varphi_0 for W/CoFeB (b), CoFeB/W (c), and Pt/CoFeB (d) with ∣Vp∣|V_p| = 210 V. The error bars represent fitting errors. The black lines show fit to the data with Eq. (2).

The parameters obtained from the fitting are listed in Table I. We find HMEH_{\mathrm{ME}} of the order of 10 µT for all samples. To extract the magnetoelastic coupling constant bb from HMEH_{\mathrm{ME}}, the saturation magnetization MSM_S of CoFeB must be known for each film structure. Magnetic moment of the samples are measured using a vibrating sample magnetometer. The thickness of the CoFeB layer is varied to extract MSM_S. Specifically, films composed of sub./X/MgO (2)/Ta (1) with X=W (2.4)/CoFeB (d), Pt (2.4)/CoFeB (d), and MgO (2)/CoFeB (d)/W (2.4) (thickness in unit of nanometers) are grown on Si substrates coated with 100-nm-thick silicon oxide (SiOx_x) under the same sputtering condition as W/CoFeB, Pt/CoFeB, and CoFeB/W. The CoFeB thickness dd ranges from 1 nm to 2.5 nm.

Figures 4(a-c) show the dd dependence of the magnetic moment (MM) divided by the film area (AA) for W/CoFeB, CoFeB/W, and Pt/CoFeB (on the SiOx_x substrates). M/AM/A linearly scales with dd for all structures. The data is fitted with a linear function: the intercept to the xx-axis and the slope give the magnetic dead layer thickness tdt_d and the saturation magnetization MSM_S, respectively. The obtained values are summarized for each structure in Table I. tdt_d is consistent with previous studies[37, 38]. The negative tdt_d of Pt/CoFeB may originate from the proximity-induced moment of Pt [39, 40, 41]. The obtained MSM_S is close to that reported in Ref. [29]. MSM_S for W/CoFeB is slightly larger than the others, which may originate from a stronger boron absorbing effect of W during deposition of CoFeB.

Using Eq. (3), we extract the product of the magnetoelastic coupling constant bb and the applied strain ϵxx\epsilon_{xx} using the parameters shown in Table I. As evident, bϵxxb\epsilon_{xx} varies among the three structures studied. Assuming that the strain ϵxx\epsilon_{xx} applied to the samples is the same, these results suggest that bb is dependent on the layer adjacent to the FM layer. We infer that this is due to the difference in the elastic properties of the bilayers. Using the magnetostriction constant λs\lambda_s and the shear modulus GG, bb is expressed as −3λsG-3\lambda_sG[28]. While λs\lambda_s is the same for a given material (CoFeB), GG is set by all layers that form the heterostructure. Previous studies reported that GG for bulk Pt (fcc) is 2.4 times smaller than that for bulk W (bcc)[42]. Studies have shown that GG for amorphous metals is about two-thirds of that for crystalline counterparts[43]. Such reported values of GG for the non-magnetic metals suggest that GG is the largest for CoFeB/W and the smallest for Pt/CoFeB. This trend is consistent with the results shown in Table I.

In summary, we have developed an approach that allows determination of the magnetoelastic coupling constant of magnetic thin film heterostructures patterned on a SAW device. Owing to the piezoelectricity of the substrate, a dc voltage applied to a pair of IDT-shaped electrodes induces strain in the film formed between the IDTs. The strain causes the direction of the magnetization to tilt due to the magnetoelastic coupling. The change in the magnetization direction is probed using the planar Hall resistance of the film. From the transport measurements, we determine the magnetoelastic coupling constant of the CoFeB layer in various thin film heterostructures. We find the magnetoelastic coupling constant is dependent on the film stacking, which is primarily attributed to the difference in the elastic properties (shear modulus) of the other layers in the heterostructure. These results thus show the importance of the film stacking on the magnetoelastic coupling constant of a magnetic layer in thin film heterostructures. The method presented in this paper provides a versatile approach to determine the magneto-elastic coupling constant, a key parameter for spin mechantronics[44] and magnomechanics[4, 8].

See supplementary material for the VpV_p dependence of δRyx\delta R_{yx} and δφ0\delta\varphi_0.

CoFeB thickness dependence of magnetic moment per film area for W/CoFeB, CoFeB/W, and Pt/CoFeB

Figure 4. (a-c) CoFeB thickness (dd) dependence of the magnetic moment MM per film area AA for W/CoFeB (a), CoFeB/W (b), and Pt/CoFeB (c). The black straight lines show linear fit to the data.

Acknowledgements

This work was partly supported by JSPS KAKENHI (Grant Numbers 20J21915, 23KJ1419, and 23H05463), MEXT Initiative to Establish Next-generation Novel Integrated Circuits Centers (X-NICS).

References

  1. [1]Y. V. Gulyaev and A. A. Nikitov, Magnonic crystals and spin waves in periodic structures, Doklady Physics 46, 687 (2001).DOI
  2. [2]H. Puszkarski and M. Krawczyk, Magnonic crystals – the magnetic counterpart of photonic crystals, in Interfacial Effects and Novel Properties of Nanomaterials, Solid State Phenomena, Vol. 94 (Trans Tech Publications Ltd, 2003) pp. 125–134.DOI
  3. [3]V. V. Kruglyak, S. O. Demokritov, and D. Grundler, Magnonics, Journal of Physics D: Applied Physics 43, 264001 (2010).
  4. [4]A. Barman, G. Gubbiotti, S. Ladak, A. O. Adeyeye, M. Krawczyk, J. Grafe, C. Adelmann, S. Cotofana, A. Naeemi, V. I. Vasyuchka, B. Hillebrands, S. A. Nikitov, H. Yu, D. Grundler, A. V. Sadovnikov, A. A. Kharchenko, S. E. Sheshukova, J.-Y. Duquesne, M. Marangolo, G. Csaba, W. Porod, V. E. Demidov, S. Urazhdin, S. O. Demokritov, E. Albisetti, D. Petti, R. Bertacco, H. Schultheiss, V. V. Kruglyak, V. D. Poimanov, S. Sahoo, J. Sinha, H. Yang, M. Munzenberg, T. Moriyama, S. Mizukami, P. Landeros, R. A. Gallardo, G. Carlotti, J.-V. Kim, R. L. Stamps, R. E. Camley, B. Rana, Y. Otani, W. Yu, T. Yu, G. E. W. Bauer, C. Back, G. S. Uhrig, O. V. Dobrovolskiy, B. Budinska, H. Qin, S. van Dijken, A. V. Chumak, A. Khitun, D. E. Nikonov, I. A. Young, B. W. Zingsem, and M. Winklhofer, The 2021 magnonics roadmap, Journal of Physics: Condensed Matter 33, 413001 (2021).DOI
  5. [5]M. Weiler, L. Dreher, C. Heeg, H. Huebl, R. Gross, M. S. Brandt, and S. T. B. Goennenwein, Elastically driven ferromagnetic resonance in nickel thin films, Physical Review Letters 106, 117601 (2011).
  6. [6]L. Thevenard, C. Gourdoin, J. Y. Prieur, H. J. von Bardeleben, S. Vincent, L. D. Becerra, L. Largeau, and J.-Y. Duquesne, Surface-acoustic-wave-driven ferromagnetic resonance in (Ga,Mn)(As,P) epilayers, Phys. Rev. B 90, 094401 (2014).DOI
  7. [7]P. G. Gowtham, T. Moriyama, D. C. Ralph, and R. A. Buhrman, Traveling surface spin-wave resonance spectroscopy using surface acoustic waves, Journal of Applied Physics 118, 233910 (2015).DOI
  8. [8]P. Delsing, A. N. Cleland, M. J. A. Schuetz, J. Knorzer, G. Giedke, J. I. Cirac, K. Srinivasan, M. Wu, K. C. Balram, C. Bauerle, T. Meunier, C. J. B. Ford, P. V. San- tos, E. Cerda-Mendez, H. Wang, H. J. Krenner, E. D. S. Nysten, M. Weibel, G. R. Nash, L. Thevenard, C. Gourdon, P. Rouvillain, M. Marangolo, J.-Y. Duquesne, G. Fischerauer, W. Ruile, A. Reiner, B. Paschke, D. Denysenko, D. Volkmer, A. Wixforth, H. Bruus, M. Wiklund, J. Reboud, J. M. Cooper, Y. Fu, M. S. Brugger, F. Rehfeldt, and C. Westerhausen, The 2019 surface acoustic waves roadmap, Journal of Physics D: Applied Physics 52, 353001 (2019).
  9. [9]É. Dumur, K. J. Satzinger, G. A. Peairs, M.-H. Chou, A. Bienfait, H.-S. Chang, C. R. Conner, J. Grebel, R. G. Povey, Y. P. Zhong, and A. N. Cleland, Quantum communication with itinerant surface acoustic wave phonons, npj Quantum Information 7, 173 (2021).DOI
  10. [10]R. Damon and J. Eschbach, Magnetostatic modes of a ferromagnet slab, Journal of Physics and Chemistry of Solids 19, 308 (1961).DOI
  11. [11]M. Jamali, J. H. Kwon, S.-M. Seo, K.-J. Lee, and H. Yang, Spin wave nonreciprocity for logic device applications, Scientific Reports 3, 3160 (2013).DOI
  12. [12]M. Ishibashi, Y. Shiotа, T. Li, S. Funada, T. Moriyama, and T. Ono, Switchable giant nonreciprocal frequency shift of propagating spin waves in synthetic antiferromagnets, Science Advances 6, eaaz6931 (2020).
  13. [13]R. M. White and F. W. Voltmer, Direct piezoelectric coupling to surface elastic waves, Applied Physics Letters 7, 314 (1965).
  14. [14]M. Weiler, H. Huebl, F. S. Goerg, F. D. Czeschka, R. Gross, and S. T. B. Goennenwein, Spin pumping with coherent elastic waves, Phys. Rev. Lett. 108, 176601 (2012).pubmed.ncbi.nlm.nih.gov/22680888
  15. [15]M. Xu, J. Puebla, F. Auvray, B. Rana, K. Kondou, and Y. Otani, Inverse Edelstein effect induced by magnon-phonon coupling, Phys. Rev. B 97, 180301 (2018).
  16. [16]R. Sasaki, Y. Nii, Y. Iguchi, and Y. Onose, Nonreciprocal propagation of surface acoustic wave in Ni/LiNbO₃, Phys. Rev. B 95, 020407 (2017).
  17. [17]M. Kuss, M. Heigl, L. Flacke, A. Horner, M. Weiler, M. Albrecht, and A. Wixforth, Nonreciprocal dzyaloshinskii-moriya magnetoacoustic waves, Phys. Rev. Lett. 125, 217203 (2020).DOI
  18. [18]M. Xu, K. Yamamoto, J. Puebla, K. Baumgaertl, B. Rana, K. Miura, H. Takahashi, D. Grundler, S. Maekawa, and Y. Otani, Nonreciprocal surface acoustic wave propagation via magneto-rotation coupling, Science Advances 6, eabb1724 (2020).
  19. [19]A. Hernández-Mínguez, F. Macià, J. M. Hernández, J. Herfort, and P. V. Santos, Large nonreciprocal propagation of surface acoustic waves in epitaxial ferromagnetic/semiconductor hybrid structures, Phys. Rev. Appl. 13, 044018 (2020).
  20. [20]P. J. Shah, D. A. Bas, I. Lisenkov, A. Matyushov, N. X. Sun, and M. R. Page, Giant nonreciprocity of surface acoustic waves enabled by the magnetoelastic interaction, Science Advances 6, eabc5648 (2020).
  21. [21]S. Tateno and Y. Nozaki, Highly nonreciprocal spin waves excited by magnetoelastic coupling in a Ni/Si bilayer, Phys. Rev. Appl. 13, 034074 (2020).
  22. [22]H. Matsumoto, T. Kawada, M. Ishibashi, M. Kawaguchi, and M. Hayashi, Large surface acoustic wave nonreciprocity in synthetic antiferromagnets, Applied Physics Express 15, 063003 (2022).
  23. [23]M. Kuss, M. Heigl, L. Flacke, A. Horner, M. Weiler, A. Wixforth, and M. Albrecht, Nonreciprocal magnetoacoustic waves in dipolar-coupled ferromagnetic bilayers, Physical Review Applied 15, 034060 (2021).DOI
  24. [24]D. Hatanaka, M. Asano, H. Okamoto, Y. Kunihashi, H. Sanada, and H. Yamaguchi, On-chip coherent transduction between magnons and acoustic phonons in cavity magnomechanics, Phys. Rev. Appl. 17, 034024 (2022).
  25. [25]A. B. Smith and R. V. Jones, Magnetostriction constants from ferromagnetic resonance, Journal of Applied Physics 34, 1283 (1963).
  26. [26]E. Klokholm, The measurement of magnetostriction in ferromagnetic thin films, IEEE Transactions on Magnetics 12, 819 (1976).
  27. [27]C. H. Lee, H. He, F. J. Lamelas, W. Vavra, C. Uher, and R. Clarke, Magnetic anisotropy in epitaxial Co superlattices, Phys. Rev. B 42, 1066 (1990).
  28. [28]J. Betz, E. du Tremolet de Lacheisserie, and L. T. Baczewski, Magnetoelastic properties of nickel thin films, Applied Physics Letters 68, 132 (1996).
  29. [29]P. G. Gowtham, G. M. Stiehl, D. C. Ralph, and R. A. Buhrman, Thickness-dependent magnetoelasticity and its effects on perpendicular magnetic anisotropy in Ta/CoFeB/MgO thin films, Physical Review B 93, 024404 (2016).
  30. [30]D. Schwienbacher, M. Pernepinter, L. Liensberger, E. R. J. Edwards, H. T. Nembach, J. M. Shaw, M. Weiler, R. Gross, and H. Huebl, Magnetoelasticity of Co₂₅Fe₇₅ thin films, Journal of Applied Physics 126, 103902 (2019).pubmed.ncbi.nlm.nih.gov/33149369
  31. [31]T. Kawada, M. Kawaguchi, T. Funato, H. Kohno, and M. Hayashi, Acoustic spin Hall effect in strong spin-orbit metals, Science Advances 7, eabd9697 (2021).DOI
  32. [32]C. F. Pai, L. Q. Liu, Y. Li, H. W. Tseng, D. C. Ralph, and R. A. Buhrman, Spin transfer torque devices utilizing the giant spin hall effect of tungsten, Appl. Phys. Lett. 101, 122404 (2012).
  33. [33]J. Liu, T. Ohkubo, S. Mitani, K. Hono, and M. Hayashi, Correlation between the spin hall angle and the structural phases of early 5d transition metals, Appl. Phys. Lett. 107, 232408 (2015).
  34. [34]T. McGuire and R. Potter, Anisotropic magnetoresistance in ferromagnetic 3d alloys, IEEE Transactions on Magnetics 11, 1018 (1975).
  35. [35]H. Nakayama, M. Althammer, Y.-T. Chen, K. Uchida, Y. Kajiwara, D. Kikuchi, T. Ohtani, S. Geprägs, M. Opel, S. Takahashi, R. Gross, G. E. W. Bauer, S. T. B. Goennenwein, and E. Saitoh, Spin Hall magnetoresistance induced by a nonequilibrium proximity effect, Phys. Rev. Lett. 110, 206601 (2013).
  36. [36]L. Dreher, M. Weiler, M. Pernepinter, H. Huebl, R. Gross, M. S. Brandt, and S. T. B. Goennenwein, Surface acoustic wave driven ferromagnetic resonance in nickel thin films: Theory and experiment, Phys. Rev. B 86, 134415 (2012).
  37. [37]S. Y. Jang, S. H. Lim, and S. R. Lee, Magnetic dead layer in amorphous CoFeB layers with various top and bottom structures, Journal of Applied Physics 107, 09C707 (2010).
  38. [38]J. Sinha, M. Hayashi, A. J. Kellock, S. Fukami, M. Yamanouchi, H. Sato, S. Ikeda, S. Mitani, S.-h. Yang, S. S. P. Parkin, and H. Ohno, Enhanced interface perpendicular magnetic anisotropy in Ta/CoFeB/MgO using nitrogen doped Ta underlayers, Applied Physics Letters 102, 242405 (2013).
  39. [39]S. Y. Huang, X. Fan, D. Qu, Y. P. Chen, W. G. Wang, J. Wu, T. Y. Chen, J. Q. Xiao, and C. L. Chien, Transport magnetic proximity effects in platinum, Phys. Rev. Lett. 109, 107204 (2012).pubmed.ncbi.nlm.nih.gov/23005323
  40. [40]X. Fan, H. Celik, J. Wu, C. Ni, K.-J. Lee, V. O. Lorenz, and J. Q. Xiao, Quantifying interface and bulk contributions to spin–orbit torque in magnetic bilayers, Nature Communications 5, 3042 (2014).DOI
  41. [41]T. Ueno, J. Sinha, N. Inami, Y. Takeichi, S. Mitani, K. Ono, and M. Hayashi, Enhanced orbital magnetic moments in magnetic heterostructures with interface perpendicular magnetic anisotropy, Scientific Reports 5, 14858 (2015).arxiv.org/abs/1510.04756
  42. [42]A. Darling, The elastic and plastic properties of the platinum metals, Platinum Metal Rev 10, 14 (1966).DOI
  43. [43]G. Knuyt, L. D. Schepper, and L. M. Stals, Calculation of elastic constants for an amorphous metal and the influence of relaxation, Journal of Physics F: Metal Physics 16, 1989 (1986).
  44. [44]M. Matsuo, E. Saitoh, and S. Maekawa, Spin-mechatronics, Journal of the Physical Society of Japan 86, 011011 (2017).DOI

Paper details

vlnc:W_fv779hed
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents