Abstract

Magnetic topological semimetals present open questions regarding the interplay of crystal symmetry, magnetism, band topology, and electron correlations. LnSbxTe2−x−δLnSb_{x}Te_{2-x-δ} (Ln= lanthanide) is a family of square-net-derived topological semimetals that allows compositional control of band filling, and access to different topological states via an evolving charge density wave (CDW) distortion. Previously studied Gd and Ce members containing a CDW have shown complex magnetic phase diagrams, which implied that spins localized on Ln interact with the CDW, but to this date, no magnetic structures have been solved within the CDW regime of this family of compounds. Here, we report on the interplay of the CDW with magnetism in NdSbxTe2−x−δNdSb_{x}Te_{2-x-δ}, by comparing the undistorted square net member NdSb0.94Te0.92NdSb_{0.94}Te_{0.92} with the CDW-distorted phase NdSb0.48Te1.37NdSb_{0.48}Te_{1.37}, via single-crystal x-ray diffraction, magnetometry, heat capacity, and neutron powder diffraction. NdSb0.94Te0.92NdSb_{0.94}Te_{0.92} is a collinear antiferromagnet with TNT_N ∼\sim 2.7 K, where spins align antiparallel to each other, but parallel to the square net of the nuclear structure. NdSb0.48Te1.37NdSb_{0.48}Te_{1.37} exhibits a nearly five-fold modulated CDW (qCDW=0.18b∗q_{CDW}=0.18b^*), isostructural to other LnSbxTe2−x−δLnSb_{x}Te_{2-x-δ} at similar x. NdSb0.48Te1.37NdSb_{0.48}Te_{1.37} displays more complex magnetism with TN=2.3KT_N = 2.3 K, additional metamagnetic transitions, and an elliptical cycloid magnetic structure with qmag=−0.41b∗q_{mag}=-0.41b^*.The magnitudes of qCDWq_{CDW} and qmagq_{mag} exhibit a integer relationship, 1+2qmag=qCDW1+2q_{mag}=q_{CDW}, implying a coupling between the CDW and magnetic structure. Given that the CDW is localized within the nonmagnetic distorted square net, we propose that conduction electrons "template" the spin modulation via the Ruderman-Kittel-Kasuya-Yosida interaction.

I Introduction

In the search for new topological matter, materials with a square-net structural motif have been heavily studied as a popular platform to host topological electronic states.[1, 2, 3, 4, 5, 6, 7, 8] The pxp_x and pyp_y orbitals that contribute much of the bonding in the square-net yield band structures with multiple topological band crossings, and thus the materials have been found to host Dirac, Weyl, and nodal line topological semimetals (TSMs), as well as topological insulators[9, 10, 11]. From a chemical standpoint, the bonding within the square net can be described as “hypervalent”, which means that it is delocalized over the square net, as the electrons occupy an exactly half-filled px/pyp_x/p_y band. Deviation from a half-filled electron count will disturb this type of bonding, causing electron localization that is accommodated by distortions of the net.[12] Such a deviation is reflected in the band structure by the appearance of nesting at the Fermi surface, wherein pockets coincide by translation of some wavevector q\mathbf{q}[13] Such an instability can be alleviated by formation of a charge density wave (CDW), in which bond localization, also influenced by electron-phonon coupling, leads to a periodic distortion of the structure with a modulation wavevector reflecting the nesting vector q\mathbf{q}[14]

The canonical nodal line semimetal ZrSiS, as well as several isostructural relatives, contains a nodal line at the Fermi level and a non-symmorphic Dirac node above EFE_F.[11] Members of the family crystallize in the tetragonal P4/nmmP4/nmm space group, in which, if using ZrSiS as an example, the Si square net lies in the abab plane. The square net is sandwiched by layers of Zr and S along the cc axis, in a puckered rock-salt layer between each square net. One isostructural subgroup of the ZrSiS family, LnLnSbTe (LnLn=Lanthanide), affords chemical tuning of EFE_F by substitution of Te into the Sb square net[15], allowing access to the nonsymmorphic Dirac node; such solid solutions are largely overlooked by popular databases used to predict TSMs due to the limits of the computational methods which they are built upon.[16, 17, 18, 19] Magnetic rare earth ions also make the LnLnSbTe family attractive to study the interplay of topological states with magnetism. This allows for opportunities to observe new topological states through the breaking of time-reversal symmetry, leveraging magnetic order as another tunable parameter to control electronic structure and access multiple topologically distinct phases. LnLnSbx_xTe2−x−δ_{2-x-\delta} (δ\delta indicating vacancy concentration in the square net) materials also exhibit charge density waves (CDWs), which are coupled with structural distortions in the square-net that evolve continuously with Sb/Te composition, and are a result of changes in band filling within the square net. [20, 21, 22] We have recently reported that the CDW is responsible for the gapping of topologically trivial states in GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48}, yielding an ideal nonsymmorphic Dirac semimetal band structure free of all other states about EFE_F, separated by hundreds of meV. [15] Depending of the doping level, the CDW can have one or multiple qq-vectors that describe the structure modulation. The single qq-vector region usually lies in the intermediate doping range. Here, the qq-vector is in-plane and agrees with a nesting vector that connects the two sheets of the diamond-shaped Fermi surface that is typical to such square-net materials. [15, 20] GdSbxTe2−x−δ\mathrm{GdSb}_x\mathrm{Te}_{2-x-\delta} also displays highly complex magnetism in which magnetic phase diagrams evolve with the compositionally driven CDW. [23] In-plane magnetic anisotropy has been reported in mechanically detwinned GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48} crystals, indicating that the unidirectional CDW distortion yields especially complex HH-TT magnetic phase diagrams along the direction of the distortion. Notably, magnetoentropic analysis of this composition also suggests the signature of an antiferromagnetic skyrmion phase at low applied field. [23] Across all distorted phases, the CDW does not significantly distort the puckered magnetic LnTeLnTe layers in the parent structure. However, the evolving distortion and composition of the nonmagentic (Sb,Te) square net is suggested to influence couplings through Ruderman–Kittel–Kasuya–Yosida (RKKY) interaction. RKKY interactions are sensitive to the also-evolving density of states, yielding a Sb-concentration dependent magnetic phase diagram.

The highly neutron-absorbing nature of Gd complicates the feasibility of determining the magnetic structures of GdSbxTe2−x−δ\mathrm{GdSb}_x\mathrm{Te}_{2-x-\delta} with neutron diffraction. In an effort to study evolving magnetism and topology with neutron-friendly analogues, we have previously synthesized isostructural CeSbxTe2−x−δ\mathrm{CeSb}_x\mathrm{Te}_{2-x-\delta}. [22] The stoichiometric parent compound, CeSbTe, is capable of switching between Dirac and Weyl semimetal states by changing the strength of an applied magnetic field. [24] Single-crystal x-ray diffraction (SCXRD) has shown that CDWs are continuously tunable in CeSbxTe2−x−δ\mathrm{CeSb}_x\mathrm{Te}_{2-x-\delta} and exhibit modulated structures consistent with GdSbxTe2−x−δ\mathrm{GdSb}_x\mathrm{Te}_{2-x-\delta} at similar Sb compositions. Distortions and calculations on CeSb0.51Te1.40\mathrm{CeSb}_{0.51}\mathrm{Te}_{1.40} suggest that the approach of driving CDWs to discover “clean” TSMs can be extended to several members of the LnSbxTe2−x−δLn\mathrm{Sb}_x\mathrm{Te}_{2-x-\delta} family [22]. In the single-qq CDW region of the phase diagram, the magnetism of CeSbxTe2−x−δ\mathrm{CeSb}_x\mathrm{Te}_{2-x-\delta} does not exhibit the same complexity, but does yield a composition and distortion dependent magnetic phase diagram. Spins align out-ofplane in CeSbxTe2−x−δ\mathrm{CeSb}_{x}\mathrm{Te}_{2-x-\delta}, perpendicular to the square net, which is consistent with neutron diffraction studies of the parent compound, CeSbTe,[24] and divergent from GdSbxTe2−x−δ\mathrm{GdSb}_{x}\mathrm{Te}_{2-x-\delta}, which exhibits an in-plane easy axis. Thus, in the Ce system, the spins do not align with the CDW q\mathbf{q}-vector, at least in the single q\mathbf{q}-vector region, which might be the cause of its less complex magnetism. We now direct our efforts to a different neutron-friendly analog, NdSbxTe2−x−δ\mathrm{NdSb}_{x}\mathrm{Te}_{2-x-\delta}, where spins are oriented in-plane, similarly to GdSbxTe2−x−δ\mathrm{GdSb}_{x}\mathrm{Te}_{2-x-\delta}.

NdSbTe has been reported to exhibit metamagnetic transitions and field-dependent transport, implying an interaction of magnetism with electronic structure [25]. Herein we report the magnetism and magnetic structures of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} and NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37}, two members of NdSbxTe2−x−δ\mathrm{NdSb}_{x}\mathrm{Te}_{2-x-\delta}, which we studied by magnetometry, single crystal x-ray diffraction, and neutron powder diffraction. NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} is found to have a crystal structure consistent with other tetragonal LnSbxTe2−x−δLn\mathrm{Sb}_{x}\mathrm{Te}_{2-x-\delta} phases, and exhibits a collinear magnetic structure in which spins align within the abab plane. NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} is nearly isostructural to GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48} with a single-q\mathbf{q} CDW modulation; and displays a complex elliptical cycloid magnetic structure. The magnitude of the magnetic propagation vector qmag\mathbf{q}_{mag} is found to have an integer relationship with that of qCDW\mathbf{q}_{CDW}, 1+2qmag=qCDW1 + 2\mathbf{q}_{mag} = \mathbf{q}_{CDW}, which implies the interaction of conduction electrons from the distorted square net with the unpaired electrons in Nd that lead to magnetism, which are considered to sit at energy levels far below the Fermi energy. This is the first magnetic structure solved for a CDW LnSbxTe2−x−δLn\mathrm{Sb}_{x}\mathrm{Te}_{2-x-\delta} phase, and may give insight into the interaction between magnetism and topological bands in these “ideal” TSMs.

(LnLn in LnSbxTe2−x−δLn\mathrm{Sb}_{x}\mathrm{Te}_{2-x-\delta})Spin alignmentNeutron absorption cross-section (barn)[26]
Gd→\rightarrow (∥ab\parallel ab)[23]49700
Ce↑\uparrow (⊥ab\perp ab)[22]0.63
Nd→\rightarrow (∥ab\parallel ab) this work50.5

Table 1. Easy-axis and neutron absorptivity in LnSbxTe2−x−δLn\mathrm{Sb}_{x}\mathrm{Te}_{2-x-\delta}

Experimental

Synthesis of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} and NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37}

Single crystals of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} and NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} were prepared using a chemical vapor transport (CVT) method. Prior to CVT growth, precursor powders with nominal compositions of NdSb0.5Te1.5\mathrm{NdSb}_{0.5}\mathrm{Te}_{1.5} and NdSbTe\mathrm{NdSbTe} were prepared from Nd pieces (Sigma Aldrich, 99.9%), Sb shot (Alfa Aesar, 99.999%), and Te pieces which were purified in-house after purchase from a commercial source (Sigma Aldrich, 99.999%). The elements were loaded into a 12 mm fused quartz tube and flame sealed under vacuum with an Ar backfill at approximately 60 mTorr, heated to 1000 ∘C1000\,^{\circ}\mathrm{C} over 12 hr, held for 2d and cooled over 12 hr in a box furnace. The resulting powders were ground and loaded into a 16 mm tube with 120 mg I2\mathrm{I}_2 as a vapor transport agent, sealed under vacuum resulting in tubes of 6-8 cm in length. CVT growth was carried out by placing the tubes in a single zone tube furnace, with the powder sides placed in the middle of the furnace to create a thermal gradient at the sink side. The tubes were heated to 1000 ∘C1000\,^{\circ}\mathrm{C} over 12 hr, held for 7d and cooled over 12 hr, resulting in crystals formed at the sink end. The elemental composition and approximate stoichiometry of the structure were confirmed via scanning electron microscopy (SEM)/Energy-Dispersive Spectroscopy (EDS). In attempted preparation of NdSbTe\mathrm{NdSbTe}, Sb loss was frequently observed during CVT growth, confirmed by composition analysis.

Powder phase samples for neutron diffraction were prepared from the elements using a vapor-assisted technique. Samples were sealed in quartz tubes with I2\mathrm{I}_2 identically to the previously described procedure. The tubes were heated in a box furnace to 950 ∘C950\,^{\circ}\mathrm{C} over 12 hr, held for 7d and cooled over 12 hr, yielding highly crystalline powders. Single crystals of NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37}, of size and quality for magnetic and specific heat measurement were also obtained from this method in the same tube.

Single-crystal X-ray Diffraction and Magnetic Measurements

SCXRD data for NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} and NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} were collected on a Bruker D8 VEN-TURE with a PHOTON 3 CPAD detector and a graphite-monochromatized Mo-KαK_{\alpha} radiation source. Integrated data were corrected with a multiscan absorption correction using SADABS. The structure of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} was solved via SHELXT[27] using intrinsic phases ing and refined with SHELXL[28] using the least squares method, as implemented in the OLEX2 program.[29] Satellite peaks, indicative of a structural modulation were observed in NdSb0.48_{0.48}Te1.37_{1.37}. The satellite peaks were indexed to an incommensurate modulation of q=0.18bq=0.18\mathbf{b}. Refinement was thus carried out using the superspace approach, where the displacive distortion of atomic positions is expressed by a periodic modulation function, yielding a 3+13+1 dimensional superspace group. Refinements with the superspace approach were carried out in JANA2006.[30] This approach included positional, ADP and site occupancy modulations in the refinement. Determination of Sb/Te occupancy and ordering within the square-net was limited by near-identical scattering power due to their closeness in atomic number (Z=51Z=51 and 5252, respectively). At laboratory-accessible X-ray wavelengths, the two species were indistinguishable if present on the same crystallographic site. Thus, for all refinements, atomic occupancies within the Sb/Te square-net were constrained to the stoichiometry derived from EDS.

Magnetic measurements were conducted using the vibrating sample magnetometer (VSM) option of either a Quantum Design DynaCool Physical Property Measurement System (PPMS) or a Magnetic Property Measurement System (MPMS) 3 SQUID magnetometer between 1.8 and 300 K. Single crystals were fixed between quartz paddles in a brass sample holding using GE Varnish, with field applied parallel and perpendicular to the abab plane. Magnetic phase diagrams were generated by collecting temperature-dependent magnetization curves during warming, with varying fields, up to 0.1 T in 0.01 T increments, then up to 5.0 T in 0.1 T increments. Critical temperatures and phase boundaries are derived from peaks in the temperature derivative of the DC magnetic susceptibility, dχ/dT\mathrm{d}\chi/\mathrm{d}T. dχ/dT\mathrm{d}\chi/\mathrm{d}T curves were plotted to build the magnetic phase diagram in the HH-TT space.

Heat Capacity

Heat Capacity (CPC_{\mathrm{P}}) measurements of NdSb0.48_{0.48}Te1.37_{1.37} were carried out using a Quantum Design DynaCool PPMS using the semiadiabatic method. The single-crystal sample was fixed to the stage using Apiezon N grease, and measurements were carried out between 1.8 and 300 K. Variable-field measurements were conducted by applying a magnetic field perpendicular to the abab plane.

Neutron powder diffraction

Neutron powder diffraction data were collected on the WISH instrument at the ISIS Muon and Neutron Source (UK). [31] The samples were contained in sealed Vanadium cans and the neutron diffraction data were collected in the 1.5–5 K temperature range. The diffraction data were collected in five detectors banks each covering 32 degrees of the scattering plane. The Rietveld refinement of the powder data were conducted with the help of the JANA2020 software. [30, 32] Group theoretical calculations and symmetry analysis were performed with the help of the ISOTROPY [33] and ISODISTORT[34] software and of the Bilbao crystallographic server [35, 36, 37].

Results and discussion

Crystal Structure

The crystal structures of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} and NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37}, as determined by SCXRD at 100 K are shown in Figure 1. The structure and lattice parameters of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} are consistent with other reported tetragonal LnSbxTe2−x−δ\mathit{Ln}\mathrm{Sb}_{x}\mathrm{Te}_{2-x-\delta} members, where no CDW ordering is observed. The Sb-Sb bond length within the square net is 3.0574(2) Å. The Sb-Sb bond lengths in the square net are significantly longer than what would be expected in a localized and covalent Sb-Sb single bond, as it appears for example in elemental Sb (approximately 2.9 Å at 78 K)[38]. The elongated, symmetric bonding can be rationalized by “hypervalent” bonding, where a -1 charge on Sb is stabilized by electron delocalization across the entire net, as detailed by Papoian and Hoffmann. [12] The NdTe layer of the structure displays the aforementioned puckered rock salt structure, with Nd-Te bond length nearly parallel to abab (within the unit cell) held constant at 3.1931(2) Å, and bond length parallel to cc (across unit cells) held at 3.2788(6) Å.

Crystal structures of NdSb$_{0.91}$Te$_{0.89}$ and NdSb$_{0.48}$Te$_{1.37}$

Figure 1. Crystal structures of (a,b) NdSb0.91_{0.91}Te0.89_{0.89} and (c, d) NdSb0.48_{0.48}Te1.37_{1.37}, as determined by single-crystal x-ray diffraction with bond distances given. Bonds in the distorted net of NdSb0.48_{0.48}Te1.37_{1.37} are drawn for distances equal to or shorter than the determined Sb-Sb bond length in undistorted NdSb0.91_{0.91}Te0.89_{0.89}, emphasizing the loss of bond delocalization upon CDW. Bond distances in d) are shown as their average lengths ± distance modulation, with errors given in parenthesis.

The structure of NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} displays a CDW distortion, as evidenced by the appearance of low intensity satellite peaks visible in the precession images of the diffraction patterns (Figure S2). The pattern can be indexed as an incommensurately modulated structure, with a modulation wavevector q=0.18b∗\mathbf{q}=0.18\mathbf{b}^{*}. This modulation wavelength corresponds to an approximate five-fold expansion of the unit cell along b∗\mathbf{b}^{*}. Using the superspace approach to structure solution and refinement, NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} is found to crystallize in the Pmmn(0β0)00sPmmn(0\beta0)00s superspace group, and when visualized as a commensurate five-fold approximant, is isostructural to CeSb0.51_{0.51}Te1.40_{1.40} and GdSb0.46_{0.46}Te1.48_{1.48}, where the (Sb,Te) square net is found to distort into a pattern of zigzag chains and more isolated atoms. This is congruent with our previous studies on the evolving CDWs observed in GdSbx_xTe2−x−δ_{2-x-\delta} and CeSbx_xTe2−x−δ_{2-x-\delta}. This same structure was found to give rise to an ideal nonsymmorphic Dirac semimetal band structure.[15]

Using the Sb-Sb bond length in tetragonal NdSb0.91_{0.91}Te0.89_{0.89} as a reference for an undistorted square net with fully delocalized bonding, we discuss the localization and symmetry breaking of the square net in NdSb0.48_{0.48}Te1.37_{1.37}. The square net breaks into a repeating pattern of parallel chains separated by lines of more isolated (Sb,Te) atoms (Figure 1d). Intra-chain Sb-Sb bonding varies from 2.92105(1) to 2.9593(1) Å, and remains constant within each chain. The nearest distance from a chain atom to an isolated atom ranges from 3.1098(1) to 3.1706(1) Å. Inter-chain atom distances are the largest, ranging from 3.2655(1) to 3.2872(1) Å. The significant deviations from the hypervalent bond length found in the undistorted square-net imply a strong localization of bonding along the chain directions, with minimal bonding interactions between the chains. The chain-to-isolated atom distance sits in an intermediate range, larger than the expected value for delocalized bonding, but may carry more bonding interaction than inter-chain interactions.

The heavy distortion of the square net due to the CDW in NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} is contrasted with minimal changes to bond length within the NdTe layer. NdTe bond length nearly parallel to abab held constant at 3.2122(1) Å, and bond length parallel to cc is 3.2699(2) Å. These bond lengths are quite similar to that in undistorted NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89}, with the deviation well explained by differences in the parent cell lattice parameters between the two. Figure S3a shows the modulation amplitude of bond distances in the NdTe structural unit and within the distorted square net. Nd-Te bonds do not vary more than 0.01 Å, whereas the amplitude of bond modulations within the distorted square net vary as much as 0.4 Å. (Figure S3b) This feature is common to all of the modulated LnSbxTe2−x−δ\mathrm{LnSb}_{x}\mathrm{Te}_{2-x-\delta} we have studied [21, 22], and consistent with our understanding of bonding in the square net. The CDW distortion is driven by electronic instability that arises from adding Te (and additional electrons) into the square net, breaking the bond delocalization. We consider the electrons involved in bonding in the NdTe layer to lie well below the Fermi energy, and thus will be unaffected by the CDW. This lack of structural interaction with the CDW will become interesting to consider in our discussion of the magnetic structure and its connection to the CDW.

Magnetic measurements and specific heat

In Figure 2, we present the magnetic phase diagrams of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89} (Figure 2a, Figure 2b) and NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} (Figure 2c, Figure 2d), constructed by plotting the first-order derivative of χ(T)\chi(T) curves measured along the crystallographic abab plane and cc axis. In the case of NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89}, a Neel temperature TN=2.7T_{\mathrm{N}} = 2.7 K is observed. A magnetic field of 3 T eventually suppresses the AFM order when applied along the abab plane (Figure 2a); the system presumably transitions to a fully spin-polarized state at this field. If the field is applied along the cc axis (Figure 2b), no metamagnetic transition is clearly visible from the variable field moment versus temperature measurements used to construct the phase diagram. Field-dependent magnetization curves show a subtle change in slope at 3 T in the derivative curve (Fig. S4b), and a smaller magnetic moment at all fields compared to in-plane measurements (Fig S2a). Thus, the feature at 3 T may be an in-plane contribution due to imperfect alignment of the crystal in the applied field. Significantly different moments at the maximum applied field (M7T,ab≳2M7T,cM_{7\mathrm{T},ab} \gtrsim2M_{7\mathrm{T},c}) along in- and out-of-plane directions, further implies magnetic anisotropy (Fig S4a). These results are similar to previously reported magnetic measurements on tetragonal NdSbx_xTe2−x−δ_{2-x-\delta}, where x=0.8x = 0.8[25].

Magnetic phase diagrams of NdSb$_{0.91}$Te$_{0.89}$ and NdSb$_{0.48}$Te$_{1.37}$

Figure 2. Magnetic phase diagrams (HH vs TT) of NdSb0.91_{0.91}Te0.89_{0.89} and NdSb0.48_{0.48}Te1.37_{1.37}. Plots were generated from the first order derivative of χ\chi over temperature (dχ/dT\mathrm{d}\chi/\mathrm{d}T).

In NdSb0.48_{0.48}Te1.37_{1.37}, the observed TNT_\mathrm{N} is 2.3 K, lower than the tetragonal compound. This contrasts behavior observed in Ce and Gd members of LnSbx_xTe2−x−δ_{2-x-\delta}. CeSbx_xTe2−x−δ_{2-x-\delta} displays an increase in TNT_\mathrm{N} with decreasing xx; GdSbx_xTe2−x−δ_{2-x-\delta} shows nonlinear behavior where TNT_\mathrm{N} increases to a maximum at x=0.48x = 0.48, and decreases at lower Sb compositions. [22, 23]

Measurements with fields applied within the abab plane (Figure 2c) detect a metamagnetic transition at ∼0.6\sim0.6 T, with a region of enhanced χ\chi that persists to 3 T, where another metamagnetic transition occurs, presumably to a fully spin-polarized state. Both phase boundaries are corroborated by magnetization vs field measurements (Figure S4d) collected at 1.8 K. Measurements with fields applied along the cc axis (Figure 2d) indicate a pair of metamagnetic transitions at ∼0.7 and ∼1.2 T, which is also observed in the magnetization curves at 1.8 K as a shoulder in the derivative curve followed by a peak with increasing field. The presence of more metamagnetic transitions at lower critical fields in both directions, implies that spins are more readily polarized along either crystallographic direction in comparison to NdSb0.91Te0.89\mathrm{NdSb}_{0.91}\mathrm{Te}_{0.89}. Field-dependent magnetization also shows a smaller difference between in- and out-of-plane saturating moments in NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} (Fig S4c), altogether indicating that the CDW phase displays less magnetic anisotropy than its undistorted relative. In addition, the CDW phase exhibits more complex magnetism as compared with the tetragonal one, as evidenced by the multiple metamagnetic transitions.

The magnetic phase diagram of NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} can be compared to the isostructural CDW-containing relatives GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48} and CeSb0.51Te1.40\mathrm{CeSb}_{0.51}\mathrm{Te}_{1.40}[22, 23]. GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48} exhibits a significantly more complex phase diagram than its tetragonal family member GdSb0.85Te1.15\mathrm{GdSb}_{0.85}\mathrm{Te}_{1.15}[21], along all measured directions, but particularly under fields applied along the abab plane, a behavior also observed in NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37}. In the latter case the magnetic ordering temperature is much lower and so the various magnetic transitions may be more difficult to resolve, whereas the Gd compound shows multiple temperature-induced phase transitions. The observed multiple in-plane transitions contrast with CeSb0.51Te1.40\mathrm{CeSb}_{0.51}\mathrm{Te}_{1.40}, where no metamagnetic transitions are observed if a field is applied along abab, but multiple are observed for fields along cc. This corresponds with the out-of-plane magnetic structure of its stoichiometric parent, CeSbTe.

To corroborate the observed TNT_{\mathrm{N}} and field dependence of the magnetic transitions in NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37}, we performed heat capacity measurements on a single crystal. At zero applied field, the observed TNT_{\mathrm{N}} is identical to that observed in the χ\chi plots, and is suppressed with applied field in a manner consistent with them. The spin state of NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} can also be determined by integrating the magnetic component of the total heat capacity over temperature (CPT\frac{C_{P}}{T}) to calculate the change in the magnetic entropy (ΔSmag\Delta S_{\mathrm{mag}}). To determine the magnetic heat capacity, CmagC_{\mathrm{mag}}, the phonon contribution to heat capacity was subtracted using a single Debye mode as described in the equation shown below:

Heat capacity measurements

Figure 3. Heat capacity measurements. a) Temperature dependence of the heat capacity CPC_{\mathrm{P}} for NdSb0.48_{0.48}Te1.37_{1.37} at variable applied fields. Inset focuses on low-temperature behavior at applied fields, highlighting the suppression of TNT_{\mathrm{N}} with applied field. b) Debye fit of CP/TC_{\mathrm{P}}/T with fitted phonon contribution shown. c) Magnetic entropy SmS_{\mathrm{m}} calculated from heat capacity data.

CD(θD,T)=9sR(TθD)3∫0θD/T(θ/T)4eθ/T[eθ/T−1]2 dθT(1)C_D(\theta_D,T)=9sR\left(\frac{T}{\theta_D}\right)^3\int_{0}^{\theta_D/T}\frac{(\theta/T)^4e^{\theta/T}}{[e^{\theta/T}-1]^2}\,\mathrm{d}\frac{\theta}{T} \tag*{(1)}

where ss is the oscillator strength, RR is the molar Boltzmann constant, and θD\theta_D is the Debye temperature. The parameters extracted from the least-squares fit between T=25T=25 - 265K265\mathrm{K} is s=3.007(8)s=3.007(8) and θD=182.8(4) K\theta_D=182.8(4)\ \mathrm{K} respectively. The total oscillator strength is in reasonable agreement with the total number of atoms per formula unit in NdSb0.48_{0.48}Te1.37_{1.37}. In the phonon fit, an Einstein mode was not incorporated because there was no Tmax⁡T_{\max} in the CpT3\frac{C_p}{T^3} plot. Thus, a single Debye mode was sufficient for the phonon fit. The ΔSmag\Delta S_{mag} with respect to temperature is found to saturate at ≃4.99 J/mol\simeq4.99\ \mathrm{J/mol}-K, slightly below what would be expected for a S=12S=\frac{1}{2} spin state (Rln⁡2R\ln2). The slight decrease in the ΔSmag\Delta S_{mag} result from additional entropy release below T=2 KT=2\ \mathrm{K} that is not captured by a linear extrapolation of Cp/T→0C_p/T\to0 at T=0 KT=0\ \mathrm{K}. The presence of artifacts and magnetic entropy beyond the phonon subtraction region are viable possibilities; thus the heat capacity analysis had some limitations. Our results notably contrast with entropy observed by Pandey et. al. in NdSbx_xTe2−x−δ_{2-x-\delta}, where x=0.8x=0.8, which more closely indicates a S=32S=\frac{3}{2} state consistent with a free Nd3+^{3+} ion. [25]

Neutron diffraction and magnetic structures

The magnetic ground state in zero applied magnetic field for both compounds has been investigated through powder neutron diffraction in the 5 – 1.5 K temperature range. The paramagnetic data set of NdSb0.94_{0.94}Te0.92_{0.92}, collected at 5 K, is in good agreement with the structural model obtained on single crystal specimens (see Figure S5 and Table S3 and S4 in the supporting information for details). On cooling below TN≈2KT_N\approx2\mathrm{K}, broad magnetic reflections are observed in the diffraction pattern, which indicates a magnetic correlation length significantly shorter than the nuclear one. The peaks can be indexed with the propagation vector k=(0 1/2 1/2)\mathbf{k}=(0\ 1/2\ 1/2). The possible magnetic isotropy subgroups consistent with both, the parent structure symmetry and the observed propagation vector, were obtained with the help of the ISODISTORT software. [34] The best agreement with the experimental data is obtained for the magnetic space group Ab21_{2_1}/c (Pc21_{2_1}/c, basis=(0,1,1),(-1,0,0),(0,-2,0) origin=(1,1,0) in standard settings, see Table S3 in the SI for details). The refined magnetic structure, together with the magnetic Rietveld plot, are shown in Figure 4a and 4b. The spin ordering consists of AFM chains that run along the b axis, where the spins lie parallel to b and antiparallel to each other along the chain. A refined moment of 1.674(8)μB\mu_{B} per Nd was obtained. The two AFM chains within a NdTe layer are shifted by half a unit cell in plane, due to the presence of the n-glide symmetry operation in the parent structure, which leads to one ferromagnetic (J1J_{1}) and one antiferromagnetic (J2J_{2}) Nd-Nd interaction. This geometrical frustration of the intra-chain interactions could be the reason of the very broad magnetic reflections observed in the neutron data. In fact, in VOCl, which is structurally closely related to tetragonal NdSb0.94Te0.92NdSb_{0.94}Te_{0.92}, a lattice distortion, which lifts this frustration, is observed at the magnetic ordering temperature. [39] Since no such distortion is observed NdSb0.94Te0.92NdSb_{0.94}Te_{0.92}, the frustration between the intra-chain interaction remains, resulting in the broad magnetic Bragg peaks. In general, the observed magnetic structure is typical for PbFCl-type compounds, as VOCl adopts a very similar one. [39] Still, it is different than that observed in CeSbTe, where spins point along the c axis and the AFM coupling doubles the unit cell.[24]

Magnetic structures and magnetic Rietveld fits for NdSb$_{0.94}$Te$_{0.92}$ and NdSb$_{0.48}$Te$_{1.37}$

Figure 4. Magnetic structures determined by neutron diffraction. a) Magnetic structure of NdSb0.94_{0.94}Te0.92_{0.92}. b) Magnetic structure of NdSb0.48_{0.48}Te1.37_{1.37}, with exchange coupling terms J1J_1 and J2J_2 shown. In parenthesis, standard crystallographic axes used in Rietveld model are given. c) Magnetic Rietveld fit for NdSb0.94_{0.94}Te0.92_{0.92}, with magnetic scattering at 1.5 K plotted by subtraction of nuclear scattering collected at 5 K. d) Magnetic Rietveld fit for NdSb0.48_{0.48}Te1.37_{1.37}, with magnetic scattering at 1.5 K plotted by subtraction of nuclear scattering collected at 5 K.

The paramagnetic diffraction pattern of modulated NdSb0.48Te1.37NdSb_{0.48}Te_{1.37}, collected at 5 K, is in agreement with the structural model obtained from the single crystal data (see Table S7-8 and Figure S6 in the SI for details). The refinement has been conducted in the Pmnm(00γ)000Pmnm(00\gamma)000 superspace group and due to the small intensity of the modulation satellite peaks, only the first order positional modulation parameters have been refined. The obtained structural parameters are reported in the SI and the refined value of the modulation vector is qCDW=(0,0.183(1),0)q_{CDW}=(0,0.183(1),0) (with respect to the parent P4/nmmP4/nmm structure). On cooling below TN=2.0(1)T_{N}=2.0(1) K, sharp magnetic reflections are observed in the diffraction pattern. These can be indexed with the propagation vector qmag=(0,−0.408(1),0)q_{mag}=(0,-0.408(1),0), the minus sign and the relation with the nuclear modulation vector will be discussed in detail later. The possible magnetic superspace groups consistent with the observed modulation vector and the tetragonal P4/nmmP4/nmm parent structure have been calculated with the help of the ISOTROPY and ISODISTORT software.[33, 34] The best agreement with the experimental data has been achieved with the Pmnm.1′(00γ)s00sPmnm.1^{\prime}(00\gamma)s00s superspace group and the obtained spin structure and the relative magnetic Rietveld plots are shown in Figure 4c,Figure 4d (see table S9 and S10 in the SI for detail). The magnetic structure can be refined as an elliptical cycloid with a sinusoidal in plane amplitude that is ≈3\approx3 times larger than the out of plane cosinusoidal component. The rotation of the moments between adjacent unit cells along the propagation vector is of π−ϕ\pi-\phi (the sign choice of the propagation vector component change the rotation angle from π−ϕ\pi- \phi to π+ϕ\pi+ \phi). Due to the presence of the {n∣0000}\{n|0000\} symmetry element in the superspace group, the two cycloids on the Nd atoms in the NdTe layer are rotating in opposite directions. This suggests that the magnetic interaction between these two positions will average to zero over the period of the magnetic structure. The solution shown in Figure 4 is the only model that is able to fit the observed intensity correctly; attempts to constrain a constant moment structure with a circular cycloid return worse fits of the data, as shown in Figure S7. The same is true for attempts using a positive propagation vector i.e. a cycloid with a rotation angle of π+ϕ\pi+ \phi (Figure S8).

Coupling between the CDW and the elliptical cycloid

It is worth underlining the strong coupling between the observed elliptical magnetic structure and the charge density wave, which occurs above the magnetic transition. By observing the value of the modulation vectors, one can notice that they are related by 1+2ν2=ν11 + 2\nu_2 = \nu_1 where ν1\nu_1 and ν2\nu_2 are the components of the CDW and cycloidal modulation vectors, respectively. Indeed, this relation can be rewritten, in vectorial form, as qCDW+2qmag=(01ˉ0)\mathbf{q}_{CDW} + 2\mathbf{q}_{mag} = (0\bar{1}0) which suggest that the nuclear modulation can be considered the second harmonic of the magnetic distortion, with the caveat that with respect to the parent P4/nmmP4/nmm structure the two propagation vectors have opposite sign (the sign choice being a consequence of symmetry decomposition from the parent structure).

With respect to the parent P4/nmmP4/nmm structure the nuclear modulation transforms as the Δ3\Delta_3 irreducible representation with the order parameter (δ,δ∗;η,η∗)(\delta, \delta^*; \eta, \eta^*), defined in a complex basis, and modulation vector qCDW=(0,ν1,0)\mathbf{q}_{CDW} = (0, \nu_1, 0). On the other hand, the elliptical magnetic structure transform as the time-even irreducible representation mΔ2m\Delta_2 with the order parameter (μ,μ∗;ξ,ξ∗)(\mu, \mu^*; \xi, \xi^*) and propagation vector qCDW=(0,ν2,0)\mathbf{q}_{CDW} = (0, \nu_2, 0). By inspecting the transformation matrices of the generators of the P4/nmm.1P4/nmm.1 space group for these two irreducible representations (reported in table S9), it is possible to write a third degree free energy invariant that couples these two distortions. The coupling term is δ∗μ2+δμ∗2+η∗ξ2+ηξ∗2\delta^*\mu^2 + \delta\mu^{*2} + \eta^*\xi^2 + \eta\xi^{*2} and it is allowed only if the components of the propagation vector of the two distortions verify the condition 1+2ν2=ν11 + 2\nu_2 = \nu_1. This coupling term gives a natural explanation why the system decides to order magnetically with the observed propagation vector and the observed symmetry. In fact, by choosing the mΔ2m\Delta_2 symmetry for the magnetic order parameter and the value of the magnetic propagation vector such that 1+2ν2=ν11 + 2\nu_2 = \nu_1, the system lowers its free energy by coupling to the nuclear modulation already present above the magnetic transition. The coupling term also provides the system a mechanism to relieve the magnetic frustration as can be appreciated from the sharper magnetic peaks in NdSb0.48_{0.48}Te1.37_{1.37} compared to NdSb0.94_{0.94}Te0.92_{0.92}. The coupling term alone does not justify the elliptical character of the cycloidal structure, which is likely the result of the competition between the magnetic anisotropy observed in the magnetization data and the magnetoelastic coupling term with the CDW. The energy gain offered by activating the coupling term could resolve the frustration of the Nd-Nd interactions by stabilizing the elliptical cycloid structure instead of the collinear structure observed in tetragonal NdSb0.94_{0.94}Te0.92_{0.92}.

To further confirm the coupling term, the diffraction data collected at 1.5 K were refined in the Pmnm.1′(00γ)s00sPmnm.1^{\prime}(00\gamma)s00s magnetic superspace group, refining the magnetic modulation as first order harmonics and the nuclear modulation as second order harmonics. The results of the refinement are summarised in table S9 and S10 and the corresponding Rietveld plots are shown in fig:S9. As can be appreciated, the refined nuclear modulation is in good agreement with the refined structure at 5 K, as well as the single crystal data.

Discussion

Both charge- and spin-density waves are phenomena driven by Fermi surface nesting, and are frequently considered as competing phase transitions, as they both result in the opening of an energy gap to relieve the electronic instability of the nesting.[13] The coexistence of both in a system implies the coupling of charge and spin degrees of freedom, which has been observed in metallic Cr [40, 41], FeTe1−y_{1-y}[42], and in layered nickelate La4_4Ni3_3O10_{10}[43], and recently, KMn6_6Bi5_5[44]. In a majority of these cases, CDW and SDW onset coincide at the same transition temperature, frequently attributed to magnetoelastic coupling, and the CDW can be considered as a secondary order parameter induced by the SDW. [45] In NdSb0.48_{0.48}Te1.37_{1.37}, the CDW is observed at room temperature, well above the appearance of the spin modulation. In this case, the spin modulation is caused by the RKKY interaction, where the ordering of localized Nd moments is mediated by the conduction electrons that come from the (Sb,Te) square net, which carry the information of the lattice modulation to the spins. Thus, the CDW plays a role in “templating” the resulting spin wave below TNT_{\mathrm{N}}, as well as relieving the magnetic frustration apparent by comparison to NdSb0.94_{0.94}Te0.92_{0.92}.

A similar “templating” effect has been observed in CaMn7O12CaMn_{7}O_{12}[46] in which the observed orbital density wave [47] influence the exchange interactions stabilizing the intermediate temperature SDW, [46] and in ζ−Mn2O3\zeta-Mn_{2}O_{3} where the commensurate orbital order drives the selection of the magnetic ground state.[48] The “templating” effect of the CDW and the subsequent relief of the exchange frustration explains why the temperature induced antiferromagnetic transitions occur more sharply in NdSb0.48_{0.48}Te1.37_{1.37}. The lower critical field for metamagnetic transitions, both in-plane (abab) and in the out-of-plane direction (cc), agree well with the magnetic structure, since the elliptical cycloid lies in the bcbc plane.

The coupling term constructed for NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} also implies that for a CDW phase involving 2 arms of the star of q\mathbf{q}, the resultant magnetic structures will have the same number of arms involved. Given that multi-q\mathbf{q} magnetic states are known to give rise skyrmion phases and other related spin textures, it is possible that CDW can be used as a tool to access them via RKKY interactions in addition to the more-common Dzyaloshinskii–Moriya interaction which drives their presence in other systems. Indeed, it has been shown that densely packed skyrmion lattices can exist in centrosymmetric crystals, where the skyrmions are believed to originate from frustrated RKKY interactions. [49, 50, 51, 52] Recent powder neutron diffraction on stoichiometric HoSbTe and TbSbTe, tetragonal members of LnSbxTe2−x−δ\mathrm{LnSb}_{x}\mathrm{Te}_{2-x-\delta}, reveal complex, multi-q\mathbf{q} magnetic structures, requiring multiple commensurate propagation vectors in the ground state, which transform to incommensurate upon warming while still below TNT_{\mathrm{N}}. [53] Exploring the synthesis of their CDW-containing derivatives may hold potential to access such skyrmion lattices. In previously mentioned GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48}, a low-field region of the magnetic phase diagram in the out-of-plane direction shows possible signatures of an antiferromagnetic skyrmion phase by magnetoentropic analysis. The multiple low-field transitions present in the out-of-plane magnetization of NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} may bear relation to the magnetic phases observed in GdSb0.46Te1.48\mathrm{GdSb}_{0.46}\mathrm{Te}_{1.48}, also hinting to the role that the CDW may play therein. A recent single-crystal neutron diffraction study on single-q\mathbf{q}, near-6-fold CDW phase GdSb0.71Te1.22\mathrm{GdSb}_{0.71}\mathrm{Te}_{1.22} reports the appearance of two magnetic phases which arise subsequently below TNT_{\mathrm{N}} and below the final transition at 5 K, respectively. [54] The multi-q\mathbf{q} CDW phase CeSb0.10Te1.79\mathrm{CeSb}_{0.10}\mathrm{Te}_{1.79} shows complex out-of-plane metamagnetic transitions in the form of a “devil’s staircase”[22] in the out-of-plane magnetization, where it is also suggested that the CDW couples to a type of spin wave. However, in this system, the CDW wavevectors contain out-of-plane components, which may allow interaction with the expected out-of-plane spin structure.

Conclusion

In conclusion, we have investigated the crystal structure, magnetic properties, and magnetic structure of the undistorted square-net TSM NdSb0.94Te0.92\mathrm{NdSb}_{0.94}\mathrm{Te}_{0.92} and its CDW-distorted relative NdSb0.48Te1.37\mathrm{NdSb}_{0.48}\mathrm{Te}_{1.37} to understand the interactions between the charge density wave and magnetism in LnSbxTe2−x−δ\mathrm{LnSb}_{x}\mathrm{Te}_{2-x-\delta} systems. NdSb0.94Te0.92\mathrm{NdSb}_{0.94}\mathrm{Te}_{0.92} is isostructural to other stoichiometric LnSbTeLnSbTe, where delocalized bonding stabilizes the Sb square net. NdSb0.48_{0.48}Te1.37_{1.37} exhibits a CDW distortion that breaks the square net into zig-zag chains with isolated atoms, isostructural to other LnSbxTe2−x−δLnSb_xTe_{2-x-\delta} with similar xx and nearly commensurate (q=0.18b∗\mathbf{q}=0.18\mathbf{b}^{*}). While NdSb0.94_{0.94}Te0.92_{0.92} behaves as a typical collinear antiferromagnet with a TNT_{\mathrm{N}} of 2.7 K, NdSb0.48_{0.48}Te1.37_{1.37} displays additional complex magnetism, with a lower TNT_{\mathrm{N}} of 2.3 K and additional metamagnetic transitions. NdSb0.48_{0.48}Te1.37_{1.37} has an elliptical cycloid magnetic structure with a propagation vector q=−0.41b∗\mathbf{q}=-0.41\mathbf{b}^{*}. The near-integer multiple of the CDW vector provides a rare example of CDW inducing complex spin order through coupling of propagation vectors, as well as the most direct evidence of CDW coupling with magnetism in LnSbxTe2−x−δLnSb_xTe_{2-x-\delta} to date. This is also the first example of a magnetic structure of a CDW phase within the LnSbxTe2−x−δLnSb_xTe_{2-x-\delta} family. The existence of the CDW above the magnetic transition temperature suggests that it plays a role in “templating” the spin interactions between LnLn atoms via RKKY interaction. Furthermore the complexity of the magnetism and the richness of CDW phases accessible in LnSbxTe2−x−δLnSb_xTe_{2-x-\delta} phases, suggest that it is possible to achieve RKKY interaction-induced skyrmions in these materials.

Acknowledgments

This work is supported by an NSF CAREER grant (DMR-2144295) to LMS. Additional support was provided by the Air Force office of Scientific Research under award number FA9550-20-1-0246. This work was further supported by the Gordon and Betty Moore Foundation (EPiQS Synthesis Award) through grant GBMF9064, the David and Lucile Packard Foundation, the Alfred P. Solan foundation, and the Arnold and Mabel Beckman foundation through a BYI grant awarded to LMS and an AOB postdoctoral fellowship awarded to JFK. TB acknowledges support from NSF-MRSEC through the Princeton Center for Complex Materials NSF-DMR-2011750. THS is grateful to Marceline Martineau for helpful discussions. F.O. and P.M. are grateful to Dr. Dmitry Khalyavin for the very fruitful discussion. For the purpose of open access, the author has applied a creative commons attribution (CC BY) licence to any author accepted manuscript version arising.

References

References

  1. [1]S. Klemenz, S. Lei, and L. M. Schoop, Topological semimetals in square-net materials, Annu. Rev. Mater. Res. 49, 185 (2019).DOI
  2. [2]S. Klemenz, A. K. Hay, S. M. Teicher, A. Topp, J. Cano, and L. M. Schoop, The role of delocalized chemical bonding in square-net-based topological semimetals, J. Am. Chem. Soc. 142, 6350 (2020).DOI
  3. [3]S. Klemenz, L. Schoop, and J. Cano, Systematic study of stacked square nets: From dirac fermions to material realizations, Physical Review B 101, 165121 (2020).DOI
  4. [4]L. M. Schoop, F. Pielnhofer, and B. V. Lotsch, Chemical principles of topological semimetals, Chem. Mater. 30, 3155 (2018).DOI
  5. [5]J. Liu, J. Hu, H. Cao, Y. Zhu, A. Chuang, D. Graf, D. J. Adams, S. M. A. Radmanesh, L. Spinu, I. Chiorescu, and Z. Mao, Nearly massless Diracfermions hosted by Sb square net in BaMnSb2, Scientific Reports 6, 30525 (2016), number: 1 Publisher: Nature Publishing Group.DOI
  6. [6]J. Park, G. Lee, F. Wolff-Fabris, Y. Y. Koh, M. J. Eom, Y. K. Kim, M. A. Farhan, Y. J. Jo, C. Kim, J. H. Shim, and J. S. Kim, Anisotropic Dirac Fermions in a Bi Square Net of ${\mathrm{SrMnBi}}_{2}$, Physical Review Letters 107, 126402 (2011), publisher: American Physical Society.
  7. [7]J. Hu, Z. Tang, J. Liu, X. Liu, Y. Zhu, D. Graf, K. Myhro, S. Tran, C. N. Lau, J. Wei, and Z. Mao, Evidence of Topological Nodal-Line Fermions in ZrSiSe and ZrSiTe, Physical Review Letters 117, 016602 (2016), publisher: American Physical Society.DOI
  8. [8]H. Wu, A. M. Hallas, X. Cai, J. Huang, J. S. Oh, V. Loganathan, A. Weiland, G. T. McCandless, J. Y. Chan, S.-K. Mo, D. Lu, M. Hashimoto, J. Denlinger, R. J. Birgeneau, A. H. Nevidomskyy, G. Li, E. Morosan, and M. Yi, Nonsymmorphic symmetry-protected band crossings in a square-net metal PtPb4, npj Quantum Materials 7, 1 (2022), number: 1 Publisher: Nature Publishing Group.DOI
  9. [9]K. Wang, D. Graf, L. Wang, H. Lei, S. W. Tozer, and C. Petrovic, Two-dimensional dirac fermions and quantum magnetoresistance in camnbi2, Phys. Rev. B 85, 041101 (2012).
  10. [10]S. Borisenko, D. Evtushinsky, Q. Gibson, A. Yaresko, K. Koepernik, T. Kim, M. Ali, J. van den Brink, M. Hoesch, A. Fedorov, E. Haubold, Y. Kushnirenko, I. Soldatov, R. Schäfer, and R. J. Cava, Time-reversal symmetry breaking type-II Weyl state in YbMnBi2, Nature Communications 10, 3424 (2019), number: 1.DOI
  11. [11]L. M. Schoop, M. N. Ali, C. Straßer, A. Topp, A. Varykhalov, D. Marchenko, V. Duppel, S. S. P. Parkin, B. V. Lotsch, and C. R. Ast, Dirac cone protected by non-symmorphic symmetry and three-dimensional dirac line node in zrsis, Nat. Commun. 7, 1 (2016).DOI
  12. [12]G. A. Papoian and R. Hoffmann, Hypervalent bonding in one, two, and three dimensions: Extending the zintl–klemm concept to nonclassical electron-rich networks, Angew. Chem. Int. Ed. 39, 2408 (2000).pubmed.ncbi.nlm.nih.gov/10941096
  13. [13]G. Grüner, Density waves in solids, Frontiers in physics ; v. 89 (Reading, Mass: Addison-Wesley Pub. Co., Advanced Book Program, 1994).
  14. [14]M. D. Johannes and I. I. Mazin, Fermi surface nesting and the origin of charge density waves in metals, Physical Review B 77, 165135 (2008), publisher: American Physical Society.DOI
  15. [15]S. Lei, S. M. Teicher, A. Topp, K. Cai, J. Lin, G. Cheng, T. H. Salters, F. Rodolakis, J. L. McChesney, S. Lapidus, N. Yao, D. Marchenko, A. Varykhalov, C. R. Ast, R. Car, J. Cano, M. G. Vergniory, N. P. Ong, and L. M. Schoop, Band engineering of dirac semimetals using charge density waves, Adv. Mater. , 2101591 (2021).DOI
  16. [16]A. Zunger, Beware of plausible predictions of fantasy materials, Nature (2019).DOI
  17. [17]B. Bradlyn, L. Elcoro, J. Cano, M. G. Vergniory, Z. Wang, C. Felser, M. I. Aroyo, and B. A. Bernevig, Topological quantum chemistry, Nature 547, 298 (2017).
  18. [18]A. Weiland, D. G. Chaparro, M. G. Vergniory, E. Derunova, J. Yoon, I. W. H. Oswald, G. T. McCandless, M. Ali, and J. Y. Chan, Band structure engineering of chemically tunable lnsbte (ln = la, ce, pr), APL Mater. 7, 101113 (2019).DOI
  19. [19]M. G. Vergniory, L. Elcoro, C. Felser, N. Regnault, B. A. Bernevig, and Z. Wang, A complete catalogue of high-quality topological materials, Nature 566, 480 (2019).DOI
  20. [20]E. DiMasi, B. Foran, M. Aronson, and S. Lee, Stability of charge-density waves under continuous variation of band filling in late₂−ₓsbₓ (0 ≤ x ≤ 1), Phys. Rev. B 54, 13587 (1996).pubmed.ncbi.nlm.nih.gov/9985270
  21. [21]S. Lei, V. Duppel, J. M. Lippmann, J. Nuss, B. V. Lotsch, and L. M. Schoop, Charge density waves and magnetism in topological semimetal candidates gdsbxte₂−ₓ−δ, Adv. Quantum Technol. 2, 1900045 (2019).DOI
  22. [22]R. Singha, T. H. Salters, S. M. Teicher, S. Lei, J. F. Khoury, N. P. Ong, and L. M. Schoop, Evolving devil’s staircase magnetization from tunable charge density waves in nonsym-morphic dirac semimetals, Adv. Mater. 33, 2103476 (2021).
  23. [23]S. Lei, A. Saltzman, and L. M. Schoop, Complex magnetic phases enriched by charge density waves in the topological semimetals gdsbₓte₂₋ₓ₋δ, Phys. Rev. B 103, 134418 (2021).DOI
  24. [24]L. M. Schoop, A. Topp, J. Lippmann, F. Orlandi, L. Müchler, M. G. Vergniory, Y. Sun, A. W. Rost, V. Duppel, M. Krivenkov, S. Sheoran, P. Manuel, A. Varykhalov, B. Yan, R. K. Kremer, C. R. Ast, and B. V. Lotsch, Tunable weyl and dirac states in the nonsymmorphic compound cesbte, Sci. Adv. 4, eaar2317 (2018).DOI
  25. [25]K. Pandey, R. Basnet, A. Wegner, G. Acharya, M. R. U. Nabi, J. Liu, J. Wang, Y. K. Takahashi, B. Da, and J. Hu, Electronic and magnetic properties of the topological semimetal candidate NdSbTe, Physical Review B 101, 235161 (2020).DOI
  26. [26]V. F. Sears, Neutron scattering lengths and cross sections, Neutron News 3, 26 (1992), publisher: Taylor & Francis eprint: https://doi.org/10.1080/10448639208218770.
  27. [27]G. M. Sheldrick, Shelxt–integrated space-group and crystal-structure determination, Acta Crystallogr. A 71, 3 (2015).DOI
  28. [28]G. M. Sheldrick, A short history of SHELX, Acta Crystallographica Section A: Foundations of Crystallography 64, 112 (2008), number: 1 Publisher: International Union of Crystallography.pubmed.ncbi.nlm.nih.gov/18156677
  29. [29]O. V. Dolomanov, L. J. Bourhis, R. J. Gildea, J. a. K. Howard, and H. Puschmann, OLEX2: a complete structure solution, refinement and analysis program, Journal of Applied Crystallography 42, 339 (2009), number: 2 Publisher: International Union of Crystallography.DOI
  30. [30]V. Petříček, M. Dušek, and L. Palatinus, Crystallographic computing system JANA2006: General features, Zeitschrift für Kristallographie 229, 345 (2014).DOI
  31. [31]L. C. Chapon, P. Manuel, P. G. Radaelli, C. Benson, L. Perrott, S. Ansell, N. J. Rhodes, D. Raspino, D. Duxbury, E. Spill, and J. Norris, Wish: The new powder and single crystal magnetic diffractometer on the second target station, Neutron News 22, 22 (2011).DOI
  32. [32]V. Petříček, M. Henriques, and M. Dušek, JANA2020 – magnetic option, Acta Crystallographica Section A 77, C175 (2021).DOI
  33. [33]H. T. Stokes, D. E. Tanner, D. Hatch, and B. J. M. Campbell, ISOTROPY Software Suite, .
  34. [34]B. J. Campbell, H. T. Stokes, D. E. Tanner, and D. M. Hatch, ISODISPLACE: A web-based tool for exploring structural distortions, Journal of Applied Crystallography 39, 607 (2006).DOI
  35. [35]M. I. Aroyo, A. Kirov, C. Capillas, J. M. Perez-Mato, and H. Wondratschek, Bilbao Crystallographic Server. II. Representations of crystallographic point groups and space groups, Acta Crystallographica Section A 62, 115 (2006).pubmed.ncbi.nlm.nih.gov/16489249
  36. [36]M. I. Aroyo, J. M. Perez-Mato, C. Capillas, E. Kroumova, S. Ivantchev, G. Madariaga, A. Kirov, and H. Wondratschek, Bilbao crystallographic server: I. databases and crystallographic computing programs, Zeitschrift für Kristallographie - Crystalline Materials 221, 15 (2006).DOI
  37. [37]L. Elcoro, B. Bradlyn, Z. Wang, M. G. Vergniory, J. Cano, C. Felser, B. A. Bernevig, D. Orobengoa, G. de la Flor, and M. I. Aroyo, Double crystallographic groups and their representations on the Bilbao Crystallographic Server, Journal of Applied Crystallography 50, 1457 (2017).DOI
  38. [38]C. S. Barrett, P. Cucka, and K. Haefner, The crystal structure of antimony at 4.2, 78 and 298° K, Acta Crystallographica 16, 451 (1963), number: 6 Publisher: International Union of Crystallography.DOI
  39. [39]A. C. Komarek, T. Taetz, M. T. Fernández-Díaz, D. M. Trots, A. Möller, and M. Braden, Strong magnetoelastic coupling in VOCl: Neutron and synchrotron powder x-ray diffraction study, Physical Review B 79, 104425 (2009).DOI
  40. [40]E. Fawcett, Spin-density-wave antiferromagnetism in chromium, Reviews of Modern Physics 60, 209 (1988), publisher: American Physical Society.DOI
  41. [41]Y. Hu, T. Zhang, D. Zhao, C. Chen, S. Ding, W. Yang, X. Wang, C. Li, H. Wang, D. Feng, and T. Zhang, Real-space observation of incommensurate spin density wave and coexisting charge density wave on Cr (001) surface, Nature Communications 13, 445 (2022), number: 1 Publisher: Nature Publishing Group.DOI
  42. [42]M. Enayat, Z. Sun, U. R. Singh, R. Aluru, S. Schmaus, A. Yaresko, Y. Liu, C. Lin, V. Tsurkan, A. Loidl, J. Deisenhofer, and P. Wahl, Real-space imaging of the atomic-scale magnetic structure of Fe1+yTe, Science 345, 653 (2014), publisher: American Association for the Advancement of Science.
  43. [43]J. Zhang, D. Phelan, A. S. Botana, Y.-S. Chen, H. Zheng, M. Krogstad, S. G. Wang, Y. Qiu, J. A. Rodriguez-Rivera, R. Osborn, S. Rosenkranz, M. R. Norman, and J. F. Mitchell, Intertwined density waves in a metallic nickelate, Nature Communications 11, 6003 (2020), number: 1 Publisher: Nature Publishing Group.DOI
  44. [44]J.-K. Bao, H. Cao, M. J. Krogstad, K. M. Taddei, C. Shi, S. Cao, S. H. Lapidus, S. van Smaalen, D. Y. Chung, M. G. Kanatzidis, S. Rosenkranz, and O. Chmaissen, Spin and charge density waves in the quasi-one-dimensional KMn6Bi5 (2022), arXiv:2208.02456 [cond-mat].DOI
  45. [45]J. C. Tolédano and P. Tolédano, The Landau Theory of Phase Transitions: Application to Structural, Incommensurage, Magnetic, and Liquid Crystal Systems, World Scientific Lecture Notes in Physics, Vol. Volume 3 (WORLD SCIENTIFIC, 1987).
  46. [46]R. D. Johnson, D. D. Khalyavin, P. Manuel, A. Bombardi, C. Martin, L. C. Chapon, and P. G. Radaelli, Modulated spin helicity stabilized by incommensurate orbital density waves in a quadruple perovskite manganite, Phys. Rev. B 93, 180403 (2016).DOI
  47. [47]N. Perks, R. Johnson, C. Martin, A. Bombardi, C. Martin, L. Chapon, and P. G. Radaelli, Magneto-orbital helices as a route to coupling magnetism and ferroelectricity in multiferroic camn7o12, Nature Communications 3, 1277 (2012).DOI
  48. [48]D. D. Khalyavin, R. D. Johnson, P. Manuel, A. A. Tsirlìn, A. M. Abakumov, D. P. Kozlenko, Y. Sun, L. Dubrovinsky, and S. V. Ovsyannikov, Magneto-orbital texture in the perovskite modification of mn2o3, Phys. Rev. B 98, 014426 (2018).DOI
  49. [49]R. Takagi, N. Matsuyama, V. Ukleev, L. Yu, J. S. White, S. Francoual, J. R. L. Mardegan, S. Hayami, H. Saito, K. Kaneko, K. Ohishi, Y. Ōnuki, T.-h. Arima, Y. Tokura, T. Nakajima, and S. Seki, Square and rhombic lattices of magnetic skyrmions in a centrosymmetric binary compound, Nature Communications 13, 1472 (2022), number: 1 Publisher: Nature Publishing Group.DOI
  50. [50]M. Hirschberger, T. Nakajima, S. Gao, L. Peng, A. Kikkawa, T. Kurumaji, M. Kriener, Y. Yamasaki, H. Sagayama, H. Nakao, K. Ohishi, K. Kakurai, Y. Taguchi, X. Yu, T.-h. Arima, and Y. Tokura, Skyrmion phase and competing magnetic orders on a breathing kagomé lattice, Nature Communications 10, 5831 (2019), number: 1 Publisher: Nature Publishing Group.DOI
  51. [51]N. D. Khanh, T. Nakajima, X. Yu, S. Gao, K. Shibata, M. Hirschberger, Y. Yamasaki, H. Sagayama, H. Nakao, L. Peng, K. Nakajima, R. Takagi, T.-h. Arima, Y. Tokura, and S. Seki, Nanometric square skyrmion lattice in a centrosymmetric tetragonal magnet, Nature Nanotechnology 15, 444 (2020), number: 6 Publisher: Nature Publishing Group.DOI
  52. [52]T. Kurumaji, T. Nakajima, M. Hirschberger, A. Kikkawa, Y. Yamasaki, H. Sagayama, H. Nakao, Y. Taguchi, T.-h. Arima, and Y. Tokura, Skyrmion lattice with a giant topological Hall effect in a frustrated triangular-lattice magnet, Science 365, 914 (2019), publisher: American Association for the Advancement of Science.
  53. [53]I. Plokhikh, V. Pomjakushin, D. J. Gawryluk, O. Zaharko, and E. Pomjakushina, Competing Magnetic Phases in LnSbTe (Ln = Ho and Tb), Inorganic Chemistry 61, 11399 (2022), publisher: American Chemical Society.DOI
  54. [54]I. Plokhikh, O. Fabelo, L. Prodan, M. Wörle, E. Pomjakushina, A. Cervellino, V. Tsurkan, I. Kézsmárki, and O. Zaharko, Magnetic and crystal structure of the antiferromagnetic skyrmion candidate GdSb0.71Te1.22, Journal of Alloys and Compounds 936, 168348 (2023).

Paper details

vlnc:W_gnjhx7mv
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 9

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents