betaFeedback

WorksPhysics and Astronomy

Spin current generation from an epitaxial tungsten dioxide WO2_{2}

Abstract

We report on efficient spin current generation at room temperature in rutile type WO2_{2} grown on Al2_{2}O3_{3}(0001) substrate. The optimal WO2_{2} film has (010)-oriented monoclinically distorted rutile structure with metallic conductivity due to 5d\it{d}2^2 electrons, as characterized by x-ray diffraction, electronic transport, and x-ray photoelectron spectroscopy. By conducting harmonic Hall measurement in Ni81_{81}Fe19_{19}/WO2_{2} bilayer, we estimate two symmetries of the spin-orbit torque (SOT), i.e., dampinglike (DL) and fieldlike ones to find that the former is larger than the latter. By comparison with the Ni81_{81}Fe19_{19}/W control sample, the observed DL SOT efficiency ξξDL_{DL} of WO2_{2} (+0.174) is about two thirds of that of W (-0.281) in magnitude, with a striking difference in their signs. The magnitude of the ξξDL_{DL} of WO2_{2} exhibits comparable value to those of widely reported Pt and Ta, and Ir oxide IrO2_{2}. The positive sign of the ξξDL_{DL} of WO2_{2} can be explained by the preceding theoretical study based on the 4d\it{d} oxides. These results highlight that the epitaxial WO2_{2} offers a great opportunity of rutile oxides with spintronic functionalities, leading to future spin-orbit torque-controlled devices.

Recently, strong spin-orbit coupling (SOC) of 5d5d electrons has attracted interest for emerging spin related functionality. One of the promising functionalities is a generation of the spin current that can be converted by charge current via the bulk spin-Hall effect (SHE)[1] of nonmagnet with strong SOC, enabling the development of the magnetic device application[2]. An efficient spin current generation via the SHE has been widely investigated for 5d5d transition metals (TMs) such as Pt[3, 4, 5, 6, 7, 8, 9, 10], Ta[11, 12, 13], and W[14, 15, 16]. More recently, an efficient spin current generation is also found in 5d5d Ir oxides[17, 18, 19, 20, 21, 22, 23] possibly due to its unique electronic structure dominated only by 5d5d electrons; the 5d5d transition metal oxides (TMOs) contrast well with the 5d5d TMs of which the electronic structure is dominated by both 6s6s and 5d5d electrons. Much effort has been so far made in epitaxial SrIrO3_3[17, 18, 19, 20], epitaxial IrO2_2[21], and amorphous IrO2_2[22, 23], highlighting 5d5d TMOs as a class of spintronic materials.

Despite the importance of 5d5d TMOs in terms of spintronics, only the Ir oxides with Ir4+^{4+} valence state (5d55d^5) have been a subject of the spintronic study because of their high conductivity among TMOs and their high chemical stability[24, 25, 26]. The situation motivates us to explore conductive 5d5d oxides with different 5d5d electron numbers as efficient spin current generator; we then expect that we can find a better material in a variety of 5d5d TMOs as well as we can obtain deeper insight into the spin-current physics related to 5d5d electrons. Of particular interest is a binary tungsten dioxide WO2_2 with W4+^{4+} valence state (5d25d^2)[27, 28, 29, 30, 31] since the WO2_2 has been known as a good conductor which provides a great opportunity to examine the spin current generation. In contrast to the WO2_2, highest-oxidation phase WO3_3 with W6+^{6+} valence state[32, 33, 34] is 5d05d^0 band insulator which is significantly more thermodynamically stable. It is thus essential to control the phase stability of the WO2_2 film by fine-tuning oxidizing conditions[30, 31]. Within this context, previous reports have demonstrated the epitaxially grown WO2_2 with metallic character[30, 31], allowing us to attack an open question whether or not 5d5d TMOs other than Ir oxides can be an efficient spin current generator.

In this article, we report on room-temperature spin current generation from the epitaxial WO2_2 grown on Al2_2O3_3(0001). We first characterize the optimal WO2_2 film by investigating the crystal structure, resistivity, and electronic structure. Second, the spin-orbit torque (SOT) with dampinglike (DL) and fieldlike (FL) symmetries is quantified by harmonic Hall measurement. The measurement reveals that sizable DL- and FL-SOTs in Ni81_{81}Fe19_{19}/WO2_2 bilayer and control sample Ni81_{81}Fe19_{19}/W bilayer, while the DL SOT is much larger than the FL SOT in both bilayers. The observed DL SOT with positive sign in WO2_2 is smaller than that with negative sign in W. The magnitude of the DL SOT is comparable to reported values found in Pt and IrO2_2, suggesting an efficient spin current arising from the epitaxial WO2_2. These findings highlight that the unique electronic structure of WO2_2 dominated by strong SOC plays an important role in spin current physics.

Figure 1(a) displays a crystal structure of the stoichiometric WO2\mathrm{WO}_2, which has a monoclinically distorted-rutile structure[27]. The lattice vector represents a monoclinic (MM) and a pseudorutile (RR) unit cell[27, 30]: aM∼2cRa_{\mathrm{M}} \sim2c_{\mathrm{R}}, bM∼aRb_{\mathrm{M}} \sim a_{\mathrm{R}}, and cM∼(bR2+cR2)1/2c_{\mathrm{M}} \sim(b_{\mathrm{R}}^2 + c_{\mathrm{R}}^2)^{1/2}, where aM=0.556a_{\mathrm{M}} = 0.556 nm, bM=0.490b_{\mathrm{M}} = 0.490 nm, cM=0.556c_{\mathrm{M}} = 0.556 nm, and β=120.47∘\beta= 120.47^\circ. This monoclinic unit cell has pseudo-trigonal symmetry, namely, combination of aM∼cMa_{\mathrm{M}} \sim c_{\mathrm{M}} and β∼120∘\beta\sim120^\circ, which is inherent to the rutile structure. This is shown in the simplified sketch for surface oxygen-oxygen distance, which helps to understand the crystallographic relationship between the WO2\mathrm{WO}_2 and the Al2O3\mathrm{Al}_2\mathrm{O}_3 as discussed later. The Al2O3\mathrm{Al}_2\mathrm{O}_3 is known to have the corundum structure, which has the hexagonal bravais lattice with the lattice constant of 0.476 nm[35, 36]. While the gray area represents the bb-axis-orientated WO2\mathrm{WO}_2 plane, its rotation of 30 degree corresponds to the red area on the (0001)-oriented Al2O3\mathrm{Al}_2\mathrm{O}_3 plane.

Illustration of monoclinic and pseudrutile WO$_2$ structures, X-ray diffraction scans, and azimuthal scans

Figure 1. (a) (left) Illustration of structure for monoclinic (MM) WO2_2 (space group #14 P21/cP2_1/c) and pseudrutile (RR) WO2_2. (right) The crystallographic relationship between the monoclinic WO2_2(010) and the Al2_2O3_3(0001). (b) X-ray diffraction (XRD) 2θ2\theta-θ\theta scan of a WO2_2 film grown on the Al2_2O3_3(0001) substrate at sputtering condition with partial oxygen of 15% and the power of 150 W. The asterisk indicates the forbidden (0003) reflections of Al2_2O3_3. (c) Magnified view of the scan around WO2_2(020) reflection in (b) and the XRD pattern around pseudocubic WO3_3(111) reflection at the condition with partial oxygen of 30%. (d) The azimuthal ϕ\phi scan of (101ˉ410\bar{1}4) diffraction for Al2_2O3_3 substrate (bottom) and of (011) diffraction for WO2_2 film (top).

We fabricate the WOx\mathrm{WO}_x films grown on Al2O3\mathrm{Al}_2\mathrm{O}_3 (0001) substrates by a reactive magnetron sputtering of a W target at the working pressure of 0.4 Pa with Ar and oxygen. The sputtering parameters are sputtering power (PP) and partial oxygen pressure; the former and the latter is 125 and 150 W, and 10–30%, respectively. Substrate temperature was fixed at 550°C. While the crystalline quality of the WOx\mathrm{WO}_x films was confirmed by x-ray diffraction (XRD) measurement, the thickness was confirmed by x-ray reflectivity (XRR) measurements; all of the examined films have thickness of 20–30 nm. Figure 1(b) shows the out-of-plane XRD pattern of an epitaxial WO2\mathrm{WO}_2 film grown at optimized growth conditions, 150 W and 15 %. We observe two peaks, (020) and (040), of the monoclinic WO2\mathrm{WO}_2 without any secondary phases. Figure 1(c) [bottom] is a magnified view around the WO2\mathrm{WO}_2 (020) and the Al2O3\mathrm{Al}_2\mathrm{O}_3(0006) peaks. The WO2\mathrm{WO}_2 (020) peak gives the out-of-plane lattice constant of 0.488 nm, which is close to ~0.490 nm for the bulk form[29, 30, 31]. The Laue fringes around the (020) diffraction evidence a good crystallinity of the film, which is also supported by narrow full width at half maximum (FWHM) of the rocking curve around the WO2\mathrm{WO}_2(020) (~0.018 deg.). Since the crystallinity is degraded to 0.028 deg. at lower oxygen ratio of 10%, we consider that the film grown at 15% has a better quality. In Figure 1(c) [top], the film grown at 150 W and 30% has a relatively small diffraction peak close to the Al2O3\mathrm{Al}_2\mathrm{O}_3 (0006) peak. The diffraction matches with bulk WO3\mathrm{WO}_3(111) in pseudocubic notation[33, 34]; the WO3\mathrm{WO}_3 typically forms a perovskite structure without A site cation[32, 33, 34]. The WO3\mathrm{WO}_3 (111) film is relaxed, judging from the wide FWHM of the rocking curve around WO3\mathrm{WO}_3 (111) (~1.1 deg.). Calculated lattice constant of 0.380 nm is slightly longer than the bulk lattice constant 0.376 nm[32, 33, 34], resulting from the oxygen vacancy; we roughly estimate xx to be 2.97 based on the relation between the bulk lattice constant and amount of the oxygen vacancy[32].

In order to understand the in-plane crystalline orientation of the WO2\mathrm{WO}_2 film, we measured azimuthal ϕ\phi scan at the WO2\mathrm{WO}_2 (011) [top] and Al2O3\mathrm{Al}_2\mathrm{O}_3 (101‾4)(10\overline{1}4) [bottom] diffractions as shown in Figure 1(d). The diffraction of Al2O3\mathrm{Al}_2\mathrm{O}_3 (101‾4)(10\overline{1}4) presents three-fold rotational symmetry with 120° step, consistent with the three-fold axis of the corundum structure[36]. The diffraction of the WO2\mathrm{WO}_2 (011) exhibits six peaks with 60° step and shifts in 30° with respect to the Al2O3\mathrm{Al_2O_3} (101ˉ410\bar{1}4) in accordance with the epitaxial relationship in Figure 1(a); the hatched area of the WO2\mathrm{WO_2} (011) is rotated in 30° relative to that of Al2O3\mathrm{Al_2O_3} (101ˉ410\bar{1}4). We ascribe the observed six peaks of the WO2\mathrm{WO_2} (011) to the formation of three-type WO2\mathrm{WO_2} domains stemming from the trigonal symmetry of the Al2O3\mathrm{Al_2O_3} substrate; each domain gives rise to two peaks corresponding to two-fold symmetry of the monoclinic unit cell.

Electronic transport in our WOx\mathrm{WO_x} films also provides an important information. In order to examine how the resistivity varies with sputtering conditions, we measured room-temperature resistivity by carrying out the van der Pauw technique on all of the films. Figure 2(a) shows the resistivity as a function of the oxygen ratio in cases of sputtering power P=125P = 125 and 150 W. The resistivity is ∼0.82\sim0.82 mΩ\Omegacm for WO2\mathrm{WO_2} and ∼7300\sim7300 mΩ\Omegacm for WO3\mathrm{WO_3}, corresponding to the lowest and highest values at P=150P = 150 W. Since the resistivity of the WO2\mathrm{WO_2} records less than 1 mΩ\Omegacm, we consider our WO2\mathrm{WO_2} film as a conductor. Irrespective of PP, the resistivity shows a moderate increase at lower oxygen ratio and a drastic increase at higher oxygen ratio. While the low oxygen ratio promotes WO2−δ\mathrm{WO_{2-\delta}}, the high oxygen ratio does WO3−δ\mathrm{WO_{3-\delta}} or WO3\mathrm{WO_3}; the δ\delta represents the degree of oxygen vacancy. The oxygen ratio associated with the lowest resistivity decreases with the PP, naturally explained by the fact that lower PP corresponds to higher oxygen ratio. We also note that the higher PP gives rise to lower resistivity at around the oxygen ration of 15% while there is no discernible difference of the crystallinity as a function of PP; the optimal PP is concluded to be 150 W in terms of resistivity. Thus, the relation between PP and oxygen ratio is crucial for controlling the WOx\mathrm{WO_x} phase, as demonstrated in the previous study[31].

Image not extracted

Figure 2. (a) Electrical resistivity as a function of the partial oxygen ratio with respect to working pressure of 0.4 Pa at sputtering power of 125 W and 150 W. (b) Valence band spectra measured by x-ray photoelectron spectroscopy for the WO2_2 and WO3_3 films, respectively. Insets are photographs of the films.

We conducted x-ray photoelectron spectroscopy (XPS) measurement to illustrate the effect of electron filling for WO2\mathrm{WO_2} and WO3\mathrm{WO_3}. The XPS measurements were performed with an Al KαK_{\alpha} radiation; the binding energy was calibrated with respect to the C 1s peak at 284.8 eV. Figure 2(b) shows the valence band spectra for the WO2\mathrm{WO_2} [bottom] and for the WO3\mathrm{WO_3} [top]. The electronic structure of the 5d25d^2 WO2\mathrm{WO_2} is dominated by two electrons in t2gt_{2g} bands near the Fermi energy (EFE_{\mathrm{F}}). When the rutile type WO2\mathrm{WO_2} is formed, the degeneracy of the t2gt_{2g} orbitals are lifted due to the metal-metal bonding in the edge-sharing WO6\mathrm{WO_6} octahedra[29]; the one electron is accommodated to the most stable σ\sigma-bonding band whereas the other electron is accommodated to the π\pi-bonding band and higher-energy bands. We actually observe the double peaks at around 2 and 0.8 eV near EFE_{\mathrm{F}}, corresponding to the σ\sigma-bonding and the π\pi-bonding bands, respectively[35, 36, 37]. This manifests that our WO2\mathrm{WO_2} film is a 5d25d^2 conductor with the rutile structure while the conducting nature is supported as well by black color of the film shown in the inset. On the other hand, the electronic structure of the 5d05d^0 WO3\mathrm{WO_3} has no electron in t2gt_{2g} bands near the EFE_{\mathrm{F}}. The inset shows that the film is almost transparent and hence is close to insulator. The valence band spectrum indicates a tiny spectral weight of the W 5d electron near EFE_{\mathrm{F}} stemming from the oxygen vacancy, which is consistent with the XRD and the resistivity results. To summarize the film characterization, we fabricated epitaxial rutile-type WO2_2 film with 5d25d^2 electrons dominating its conducting nature; the film is suitable for measuring the spin current generation.

We focus on observation of the SOT arising from the WO2_2, which is manifestation of the spin current generation[37]. We prepared bilayer consisting of epitaxial WO2_2 and ferromagnetic Fe19_{19}Ni81_{81} alloy (permalloy, Py). The whole film structures are represented by TiOx_x(2)/Py(3)/WO2_2(20), where the number in parenthesis indicates the thickness in nanometer Figure 3(a). After the WO2_2 growth with the sputtering parameters as stated above, Ti and Py were deposited in situ by a radio-frequency magnetron sputtering at Ar deposition pressure of 0.4 Pa. The TiOx_x layer is obtained from the as-deposited Ti metal by natural oxidation in the air. The purpose of the TiOx_x layer is to prevent the Py layer from being oxidized; we can neglect current shunting by the TiOx_x layer due to its high resistance. We also prepared a Py(3)/W(4) bilayer as a control sample. The Py, W, and TiOx_x thickness were estimated from growth rate of each layer determined by XRR measurement beforehand. The resistivity of W and Py is 180 and 100 μΩ\mu\Omegacm, respectively, obtained from the relation between the inverse sheet resistance and the Py thickness (not shown); a good linear relation is found when the Py thickness ranges from 3 to 6 nm, indicating that an increase of the resistivity stemming from interface effects is negligibly small. While the W thickness of 4 nm is chosen by reference to the previous studies[1, 2, 14], we set the WO2_2 thickness to 20 nm so that the resistance of the WO2_2 layer matches with that of the W layer; the current and the SOT data quality is expected to be roughly comparable between the W and WO2_2 layers. The Py/WO2_2 (Py/W) bilayer was fabricated into a Hall bar with two arms by photolithography and Ar ion milling. Ti(5)/Pt(60) contact pads were attached at the end of devices for electrical measurement. The Hall bar has channel dimensions of 50 μ\mum length and 10 μ\mum width, as shown in Figure 3(a). The ϕ\phi represents the azimuthal angles of the external magnetic field (BextB_{\mathrm{ext}}). We apply an ac current Iac=2Irmssin⁡(2πft)I_{\mathrm{ac}} = \sqrt{2}I_{\mathrm{rms}}\sin(2\pi ft) with root mean square of current IrmsI_{\mathrm{rms}} in the xx axis direction and frequency f=13f = 13 Hz. We define the current flow direction (xx axis) as the (101ˉ0)(10\bar{1}0)-orientation of the Al2_2O3_3 (0001) substrate; note that this choice has no significance because we cannot expect anisotropy in any transport measurements considering that the WO2_2 film consists of the multidomains discussed in Figure 1(d). We set IrmsI_{\mathrm{rms}} to be 0.2 mA for longitudinal resistance (RR) measurement in xx-axis direction, and 0.2 mA for Hall resistance (RHR_{\mathrm{H}}) measurement and 2.0 mA for harmonic Hall measurement in the yy-axis directions.

Image not extracted

Figure 3. (a) Schematic illustration of the device and cross section of the samples. The ϕ\phi represents the azimuthal angles of the external magnetic field (BextB_{\mathrm{ext}}). AC current is applied along the xx axis direction to detect Hall resistance (RHR_{\mathrm{H}}) in the yy-axis direction, and detect longitudinal resistance (RR) in the xx-axis direction. (b) First-harmonic Hall resistance (RH1ωR_{\mathrm{H}}^{1\omega}) of Py(3)/WO2_{2}(20) measured at 0.5 T. The solid curve is fit to the data using Eq. (1). (c) The corresponding second-harmonic Hall resistance (RH2ωR_{\mathrm{H}}^{2\omega}) with curve fit using Eq. (2) (top). The data is separated to cos⁡ϕ\cos\phi and (2cos⁡3ϕ−cos⁡ϕ)(2\cos^{3}\phi-\cos\phi) components (bottom) from the fitting result, which indicate DL contribution and FL contribution, respectively.

We evaluate the SOT by conducting harmonic Hall measurement[4, 5, 12]. By applying the IacI_{\mathrm{ac}} to the Hall bar, the SOT is induced at FM/NM interface, which has two components with different symmetries, namely, DL and FL SOTs[4, 12, 37]. These SOTs correspond to DL effective field BDL∥(σ×m)B_{\mathrm{DL}} \parallel(\boldsymbol{\sigma} \times\boldsymbol{m}) and FL effective field BFL∥σB_{\mathrm{FL}} \parallel\boldsymbol{\sigma}, where m\boldsymbol{m} and σ\boldsymbol{\sigma} is the direction of the magnetization and accumulated spin polarization; the latter is along the yy-axis direction. Of these two SOTs, the DL SOT is most relevant to the magnetization switching[4, 37]. In order to distinguish the BDLB_{\mathrm{DL}} and BFLB_{\mathrm{FL}}, the harmonic Hall measurements were performed by measuring an angle dependence of first and second harmonic resistance (RH1ωR_{\mathrm{H}}^{1\omega}, RH2ωR_{\mathrm{H}}^{2\omega}) at fixed BextB_{\mathrm{ext}} in xyxy plane; the applied BextB_{\mathrm{ext}} varies 0.1 to 1.2 T. The RH1ωR_{\mathrm{H}}^{1\omega} corresponds to the conventional dc Hall measurement, while the RH2ωR_{\mathrm{H}}^{2\omega} reflects the influence of SOT; the former and the latter obey following Eq. (1) and Eq. (2)[5].

RH1ω=RPHEsin⁡2ϕsin⁡2θ(1)R_{\mathrm{H}}^{1\omega}=R_{\mathrm{PHE}}\sin2\phi\sin^{2}\theta \tag*{(1)}
RH2ω=−(RAHEBDLBext+Bk+R∇T)cos⁡ϕ+2RPHEBFL+BOeBext(2cos⁡3ϕ−cos⁡ϕ)(2)R_{\mathrm{H}}^{2\omega}=-\left(R_{\mathrm{AHE}}\frac{B_{\mathrm{DL}}}{B_{\mathrm{ext}}+B_{\mathrm{k}}}+R_{\nabla T}\right)\cos\phi+2R_{\mathrm{PHE}}\frac{B_{\mathrm{FL}}+B_{\mathrm{Oe}}}{B_{\mathrm{ext}}}\left(2\cos^{3}\phi-\cos\phi\right) \tag*{(2)}
≡−RDL+∇Tcos⁡ϕ+RFL+Oe(2cos⁡3ϕ−cos⁡ϕ)(3)\equiv-R_{\mathrm{DL}+\nabla T}\cos\phi+R_{\mathrm{FL}+\mathrm{Oe}}\left(2\cos^{3}\phi-\cos\phi\right) \tag*{(3)}

Here, RPHER_{\mathrm{PHE}}, RAHER_{\mathrm{AHE}}, BkB_{\mathrm{k}}, R∇TR_{\nabla T}, and BOeB_{\mathrm{Oe}} correspond to planar Hall resistance, anomalous Hall resistance, out-of-plane anisotropy field, thermal induced second-harmonic resistance driven by a temperature gradient, e.g. the anomalous Nernst effect[38] and spin Seebeck effect[39], and current induced Oersted field, respectively. RAHER_{\mathrm{AHE}} and BkB_{\mathrm{k}} were estimated by Hall resistance depending on the out-of-plane BextB_{\mathrm{ext}}. The ϕ\phi dependence of RH2ωR_{\mathrm{H}}^{2\omega} is induced by the small modulation of the magnetization from its equilibrium position due to the current-driven SOTs. We can define the BDLB_{\mathrm{DL}} contribution (RDL+∇TR_{\mathrm{DL}+\nabla T}) and the BFLB_{\mathrm{FL}} contribution (RFL+OeR_{\mathrm{FL}+\mathrm{Oe}}) as the coefficients of the cos⁡ϕ\cos\phi and (2cos⁡3ϕ−cos⁡ϕ)(2\cos^{3}\phi-\cos\phi) in Eq. (3). Figure 3(b) shows RH1ωR_{\mathrm{H}}^{1\omega} as a function of ϕ\phi with Bext=0.5B_{\mathrm{ext}}=0.5 T; RPHE=0.42 ΩR_{\mathrm{PHE}}=0.42\ \Omega was obtained as the fitting results in accordance with Eq. (1). The top panel of Figure 3(c) shows the corresponding RH2ωR_{\mathrm{H}}^{2\omega} measured at 0.5 T, which is well fitted by Eq. (2). We estimated the RDL+∇TR_{\mathrm{DL}+\nabla T} and RFL+OeR_{\mathrm{FL}+\mathrm{Oe}} from the RH2ωR_{\mathrm{H}}^{2\omega} fitting, which is shown in the bottom panel in Figure 3(c), respectively; the result indicates the large RDL+∇TR_{\mathrm{DL}+\nabla T} contribution and the small RFL+OeR_{\mathrm{FL}+\mathrm{Oe}} contribution to the RH2ωR_{\mathrm{H}}^{2\omega} in Py/WO2_2 bilayer.

Then we extract two SOT effective fields BDLB_{\mathrm{DL}} and BFLB_{\mathrm{FL}} through the coefficients RDL+∇TR_{\mathrm{DL}+\nabla T} and RFL+OeR_{\mathrm{FL}+\mathrm{Oe}}. Figure 4(a) shows the RDL+∇TR_{\mathrm{DL}+\nabla T} for the Py/WO2_2 bilayer and Py(3)/W(4) as control sample. The data indicates linear dependence on 1/(Bext+Bk)1/(B_{\mathrm{ext}}+B_{\mathrm{k}}) in accordance with Eq. (2). The data point in the low-field region for Py/W bilayer is deviated from the linear fitting, possibly due to unsaturated in-plane magnetization[23]. The slopes and intercepts of the RDL+∇TR_{\mathrm{DL}+\nabla T} correspond to the BDLB_{\mathrm{DL}} and the R∇TR_{\nabla T}, respectively. We estimated the DL effective field per current density BDL/JB_{\mathrm{DL}}/J, where JJ is the applied charge current density flowing in the WO2_2 (W) layer. The estimated BDL/JB_{\mathrm{DL}}/J is +3.03 mT/(1011^{11} A m−2^{-2}) for Py/WO2_2 and −4.58 mT/(1011^{11} A m−2^{-2}) for Py/W, suggesting the sizable DL SOT generation in Py/WO2_2 as well as in Py/W. The R∇TR_{\nabla T} of Py/WO2_2 is much larger than Py/W.

Image not extracted

Figure 4. (a) RDL+∇TR_{\mathrm{DL}+\nabla T} as a function of 1/(Bext+Bk)1/(B_{\mathrm{ext}}+B_{\mathrm{k}}) in Py(3)/WO2_{2}(20) and Py(3)/W(4) samples. (b) RFL+OeR_{\mathrm{FL}+\mathrm{Oe}} as a function of 1/Bext1/B_{\mathrm{ext}} in Py(3)/WO2_{2}(20) and Py(3)/W(4) samples. The solid lines are linear fits to the experimental data. (c) Dampinglike and fieldlike SOT efficiencies for WO2_{2} and W. The error bars are smaller than the symbol size.

The temperature gradient in Py/WO2\mathrm{Py}/\mathrm{WO}_{2} is larger compared with Py/W\mathrm{Py}/\mathrm{W} due to the higher resistivity of WO2\mathrm{WO}_{2} than that of W\mathrm{W}, resulting in the large R∇TR_{\nabla T}. The RFL+OeR_{\mathrm{FL+Oe}} for Py/WO2\mathrm{Py}/\mathrm{WO}_{2} and Py/W\mathrm{Py}/\mathrm{W} bilayers are plotted as a function of 1/Bext1/B_{\mathrm{ext}} as shown in Figure 4(b), which is well explained by Eq. (2). The BFLB_{\mathrm{FL}} were obtained by subtracting the BOeB_{\mathrm{Oe}} contribution estimated by Ampere’s law as BOe=μ0Jd/2B_{\mathrm{Oe}}=\mu_{0}Jd/2, where μ0\mu_{0} is the magnetic permeability in a vacuum, and dd is the thickness of WO2\mathrm{WO}_{2} (W\mathrm{W}). The BFL/JB_{\mathrm{FL}}/J for Py/WO2\mathrm{Py}/\mathrm{WO}_{2} and Py/W\mathrm{Py}/\mathrm{W} are +0.75×10−1+0.75 \times10^{-1} and −0.30 mT/(1011 A m−2)-0.30\ \mathrm{mT}/(10^{11}\ \mathrm{A}\,\mathrm{m}^{-2}), respectively.

In order to further discuss the SOT, we evaluate the efficiency ξDL(FL)\xi_{\mathrm{DL(FL)}} from the BDL(FL)/JB_{\mathrm{DL(FL)}}/J using following equation[40]:

ξDL(FL)=2eμ0MstPyℏBDL(FL)J(4)\xi_{\mathrm{DL(FL)}}=\frac{2e\mu_{0}M_{\mathrm{s}}t_{\mathrm{Py}}}{\hbar}\frac{B_{\mathrm{DL(FL)}}}{J} \tag*{(4)}

where ee, MsM_{\mathrm{s}}, and ℏ\hbar are the elementary charge, the saturation magnetization, and the Dirac constant, respectively. The MsM_{\mathrm{s}} for Py/WO2\mathrm{Py}/\mathrm{WO}_{2} and Py/W\mathrm{Py}/\mathrm{W} are 6.2×1056.2 \times10^{5} and 6.7×105 A/m6.7 \times10^{5}\ \mathrm{A/m}, respectively, measured by the superconducting quantum interference device magnetometer, in agreement with those for typical Py thin film[6, 8, 10, 16, 17, 22]. The ξDL\xi_{\mathrm{DL}} and ξFL\xi_{\mathrm{FL}} for WO2\mathrm{WO}_{2} and W\mathrm{W} are summarized in Figure 4(c). We obtain ξDL=+0.174±0.021\xi_{\mathrm{DL}}=+0.174\pm0.021 for WO2\mathrm{WO}_{2} and −0.281±0.006-0.281\pm0.006 for W\mathrm{W}. The ξDL\xi_{\mathrm{DL}} for W is quantitatively consistent with the previous reports including its negative sign[14, 15, 16], demonstrating validity of our experimental setup. Note that while recent reports point out the importance of the DL-SOT generation from single FM layers[41, 42, 43], we experimentally confirmed that the DL-SOT efficiency of single 3-nm-thick Py layer is as small as 0.001. In our bilayers, the contributions from the Py layer is thus negligible compared to the above-mentioned DL-SOT efficiencies of WO2\mathrm{WO}_{2} and W. We also consider that the ξDL\xi_{\mathrm{DL}} for WO2\mathrm{WO}_{2} is saturated since the WO2\mathrm{WO}_{2} layer thickness of 20 nm is sufficiently above the spin-diffusion length. The prior studies have shown that the typical spin-diffusion length is ∼2\sim2 nm for non-magnets with efficient spin current generation such as Pt, W, and Ir oxide[4, 5, 6, 7, 8, 9, 10, 16, 22], suggesting that the spin diffusion length of WO2\mathrm{WO}_{2} is also around 2 nm; this rough estimate would not affect the above-mentioned ξDL\xi_{\mathrm{DL}} as far as the WO2\mathrm{WO}_{2} thickness is much longer than the spin diffusion length. In terms of magnitude, the ξDL\xi_{\mathrm{DL}} of +0.174+0.174 for the WO2\mathrm{WO}_{2} is about two thirds of that for the W, reinforcing the validity of WO2\mathrm{WO}_{2} as the spintronic material; the ξDL\xi_{\mathrm{DL}} is indeed comparable to those for Pt[4, 6, 22, 23], Ta[5, 11, 13], and amorphous IrO2\mathrm{IrO}_{2}[22, 23]. Regarding the FL-SOT, we obtain ξFL=+0.042±0.003\xi_{\mathrm{FL}}=+0.042\pm0.003 for WO2\mathrm{WO}_{2} and −0.018±0.002-0.018\pm0.002 for W. The smaller ξFL\xi_{\mathrm{FL}} with the same sign compared to their ξDL\xi_{\mathrm{DL}} is likely to stem from the bulk SHE; the similar trend on the magnitude and sign is found in typical 5d5d TMs[4, 5, 6, 13, 16, 23] as well. The larger ξDL\xi_{\mathrm{DL}} than ξFL\xi_{\mathrm{FL}} is helpful for demonstrating the magnetization switching since the DL-SOT plays an important role in magnetization control.

We then focus on the observed positive sign of ξDL\xi_{\mathrm{DL}} for WO2\mathrm{WO}_{2}. This contrasts with the negative sign of ξDL\xi_{\mathrm{DL}} for W, reflecting the difference of the electronic structure between WO2\mathrm{WO}_{2} and W. The 5d5d electron solely dominates the density of states at EFE_{\mathrm{F}} in WO2\mathrm{WO}_{2} and hence the spintronic behavior of WO2\mathrm{WO}_{2} can be totally different with W and/or slightly oxidized W. For 4d4d and 5d5d TMs, the theoretical study concludes that the spin Hall conductivity is proportional to the SOC constant (λ\lambda)[44]; the spin Hall conductivities of TMs show a change from the negative to positive signs with increasing electron numbers since the sign of the λ\lambda is reversed between more-than half and less-than half filling in 5d5d orbitals; this sign change is experimentally confirmed[45]. In contrast, the spin Hall conductivity of 4d4d TMOs is theoretically predicted to be dominated by the quadratic term of the λ\lambda[46], conveying that the 4d4d TMOs keeps the same sign irrespective of the sign of the λ\lambda which depends on the 5d5d electron number. Since the positive sign is observed in the rutile IrO2_2[21], the positive sign of the WO2_2 is plausible by assuming that the quadratic term of the λ\lambda is dominant in the 5d5d oxides as theoretically predicted in 4d4d oxides. Thus, the WO2_2 would be an attractive spintronic material, motivating us to gain further insight from both experimental and theoretical aspects. For instance, the anisotropic effect on the SOT may bring rich information about the relationship between the electronic structure and the spin-current properties since the anisotropic electronic structure is expected in the rutile compounds. At current stage, while we cannot pin down the positive sign for WO2_2 in detail, our finding is a good starting point to clarify the spin current physics behind the unique electronic structure inherent to 5d5d TMOs.

In conclusion, we studied an efficient room temperature generation of spin current in Py/WO2_2 bilayer, where the distorted rutile type WO2_2 is epitaxially grown on Al2_2O3_3 substrate by reactive sputtering method. By tuning the sputtering power and oxygen ratio, we obtained the monoclinic WO2_2 (010) characterized by the XRD. Further film characterization revealed the metallic character and the 5d25d^2 electron configuration of WO2_2, supported by the resistivity and XPS measurements. By performing the harmonic Hall measurement, we estimated that the ξDL\xi_{\mathrm{DL}} (+0.174) of the WO2_2 is roughly two thirds of that (−0.281) of W control sample in terms of magnitude and is as large as those values in typical Pt and Ta, and IrO2_2, demonstrating efficient spin current generation from the WO2_2. The positive sign of ξDL\xi_{\mathrm{DL}} for WO2_2 in contrast to the negative one for W, is the same with that for IrO2_2, which is consistent with theoretical prediction based on the 4d4d oxides. Our findings indicate that WO2_2 is a promising spintronic material, which may be a component of magnetic memory device driven by SOT switching.

Acknowledgement

The authors thank H. Kontani for fruitful discussion, K. Omura for the XPS measurement, and T. Arakawa for technical support. This work was carried out at the Center for Advanced High Magnetic Field Science in Osaka University under the Visiting Researcher’s Program of the Institute for Solid State Physics, the University of Tokyo. This work was supported by Nanotechnology Platform of MEXT, Grant Number JPMXP09S21OS0027, the JSPS KAKENHI (Grant Nos. JP19K15434, JP19H05823, and 22H04478), JPMJCR1901 (JST-CREST), the Spintronics Research Network of Japan (Spin-RNJ), Nippon Sheet Glass foundation for Materials Science and Engineering, and Iketani Science and Technology Foundation. We acknowledge stimulating discussions at the meeting of the Cooperative Research Project of the Research Institute of Electrical Communication, Tohoku University

References

  1. [1]1) A. Hoffmann, IEEE Trans. Magn. 49, 5172 (2013).
  2. [2]2) X. Han, X. Wang, C. Wan, G. Yu, and X. Lv, Appl. Phys. Lett. 118, 120502 (2021).
  3. [3]3) I. M. Miron, K. Garello, G. Gaudin, P. J. Zermatten, M. V. Costache, S. Auffret, S. Bandiera, B. Rodmacq, A. Schuhl and P. Gambardella, Nature 476, 189 (2011).
  4. [4]4) K. Garello, I. M. Miron, C. O. Avci, F. Freimuth, Y. Mokrousov, S. Blügel, S. Auffret, O. Boulle, G. Gaudin and P. Gambardella, Nat. Nanotechnol. 8, 587, (2013).
  5. [5]5) C. O. Avci, K. Garello, M. Gabureac, A. Ghosh, A. Fuhrer, S. F. Alvarado, and P. Gambardella, Phys. Rev. B 90, 224427 (2014).
  6. [6]6) T. Nan, S. Emori, C. T. Boone, X. Wang, T. M. Oxholm, J. G. Jones, B. M. Howe, G. J. Brown, and N. X. Sun, Phys. Rev. B 91, 214416 (2015).
  7. [7]7) C. F. Pai, Y. X. Ou, L. H. Vilela-Leao, D. C. Ralph, and R. A. Buhrman, Phys. Rev. B 92, 064426 (2015).
  8. [8]8) W. Zhang, W. Han, X. Jiang, S.-H. Yang, and S. S. P. Parkin, Nat. Phys. 11, 496 (2015).
  9. [9]9) K. Kondou, H. Sukegawa, S. Kasai, S. Mitani, Y. Niimi, and Y. Otani, Appl. Phys. Express 9, 023002 (2016).
  10. [10]10) S. Jeong, J. Lee, S. Lee, J. Park, D. Lee, J. Jeong, H. Jang, E. Park, Y. Jo, N. J. Lee, K.-W. Kim, B.-G. Park, S. Lee, T. H. Kim, and S. Kim, Appl. Phys. Lett. 119, 212402 (2021).
  11. [11]11) L. Liu, C.-F. Pai, Y. Li, H. W. Tseng, D. C. Ralph, and R. A. Buhrman, Science 336, 555 (2012).
  12. [12]12) J. Kim, J. Sinha, M. Hayashi, M. Yamanouchi, S. Fukami, T. Suzuki, S. Mitani and H. Ohno, Nat. Mater. 12, 240 (2013).
  13. [13]13) K. Ueda, M. Mann, P. W. P. de Brouwer, D. Bono, and G. S. D. Beach, Phys. Rev. B 96, 064410 (2017).
  14. [14]14) C. F. Pai, L. Liu, Y. Li, H. W. Tseng, D. C. Ralph, and R. A. Buhrman, App. Phys. Lett. 101, 122404 (2012).
  15. [15]15) J. Liu, T. Ohkubo, S. Mitani, K. Hono, and M. Hayashia, Appl. Phys. Lett. 107, 232408 (2015).
  16. [16]16) Y. Takeuchi, C. Zhang, A. Okada, H. Sato, S. Fukami,,and H. Ohno, on: Appl. Phys. Lett. 112, 192408 (2018).
  17. [17]17) T. Nan, T. J. Anderson, J. Gibbons, K. Hwang, N. Campbell, H. Zhou, Y. Q. Dong, G. Y. Kim, D. F. Shao, T. R. Paudel, N. Reynolds, X. J. Wang, N. X. Sun, E. Y. Tsymbal, S. Y. Choi, M. S. Rzchowski, Yong Baek Kim, D. C. Ralph, and C. B. Eom, Proc. Natl. Acad. Sci. 116, 33 (2018).
  18. [18]18) L. Liu, Q. Qin, W. Lin, C. Li, Q. Xie, S. He, X. Shu, C. Zhou, Z. Lim, J. Yu, W. Lu, M. Li, X. Yan, S. J. Pennycook, and J. Chen Nat. Nanotechnol. 14, 939 (2019).
  19. [19]19) X. Huang, S. Sayed, J. Mittelstaedt, S. Susarla, S. Karimedddiny, L. Caretta, H. Zhang, V. A. Stoica, T. Gosavi, F. Mahfouzi, Q. Sun, P. Ercius, N. Kioussis, S. Salahuddin, D. C. Ralph, R. Ramesh, Adv. Mater. 33, 2008269 (2021).
  20. [20]S. Hori, K. Ueda, T. Kida, M. Hagiwara, J. Matsuno, Appl. Phys. Lett. 121, 022402 (2022).
  21. [21]A. Bose, J. N. Nelson, X. S. Zhang, P. Jadaun, R. Jain, D. G. Schlom, D. C. Ralph, D. A. Muller, K. M. Shen, and R. A. Buhrman, ACS Appl. Mater. Interfaces 12, 55411 (2020).
  22. [22]K. Ueda, N. Moriuchi, K. Fukushima, T. Kida, M. Hagiwara, and J. Matsuno, Phys. Rev. B 102, 134432 (2020).
  23. [23]K. Ueda, N. Moriuchi, K. Fukushima, T. Kida, M. Hagiwara, and J. Matsuno, Phys. Rev. Appl. 16, 034039 (2021).
  24. [24]J. Matsuno, K. Ihara, S. Yamamura, H. Wadati, K. Ishii, V. V. Shankar, H.-Y. Kee, and H. Takagi, Phys. Rev. Lett. 114, 247209 (2015).
  25. [25]D. J. Groenendijk, C. Autieri, J. Girovsky, M. C. Martinez-Velarte, N. Manca, G. Mattoni, A. M. R. V. L. Monteiro, N. Gauquelin, J. Verbeeck, A. F. Otte, M. Gabay, S. Picozzi, and A. D. Caviglia, Phys. Rev. Lett. 119, 256403 (2017).
  26. [26]Y. Kozuka, S. Isogami, K. Masuda, Y. Miura, Saikat Das, J. Fujioka, T. Ohkubo, and S. Kasai, Phys. Rev. Lett. 126, 236801 (2021).
  27. [27]D.J. Palmer and P.G. Dickens, Acta Crystallogr., Sect. B: Struct. Sci. 35, 2199 (1979).
  28. [28]A. Gulino, S. Parker, F. H. Jones, and R. G. Egdell, J. Chem. Soc. Faraday Trans. 92, 2137 (1996).
  29. [29]F.H. Jones, R.G. Egdell, A. Brown, F.R. Wondre, Sur. Sci. 374, 80 (1997).
  30. [30]F. J. Wong and S. Ramanathan, J. Mater. Res. 28, 18 (2013).
  31. [31]K. Fujiwara and A. Tsukazaki, J. Appl. Phys. 125, 085301 (2019).
  32. [32]E. Gebert and R. J. Ackermann, Inor. Chem. 5, 1, (1966).
  33. [33]J. M. Berak and M. J. Sienko, J. Solid State. Chem. 2, 109, (1970).
  34. [34]T. Vogt, P. M. Woodward, and B. A. Hunter, Jour. Solid State Chem. 144, 209, (1999).
  35. [35]L. Cao, X. Zhang, J. Yuan, L. Guo, T. Hong, W. Hang, and Y. Ma, Appl. Sci. 10, 8065 (2020).
  36. [36]M. Negishi, K. Fujiwara, and A. Tukazaki, AIP Advances 11, 125125 (2021).
  37. [37]A. Manchon, I. M. Miron, T. Jungwirth, J. Sinova, J. Železny, A. Thiaville, K. Garello, and P. Gambardella, Rev. Mod. Phys. 91, 035004 (2019).
  38. [38]G. E. Bauer, E. Saitoh, and B. J. van Wees, Nat. Mater. 11, 391 (2012).
  39. [39]K. Uchida, S. Takahashi, K. Harii, J. Ieda, W. Koshibae, K. Ando, S. Maekawa, and E. Saitoh, Nature (London, UK) 455, 778 (2008).
  40. [40]A. V. Khvalkovskiy, V. Cros, D. Apalkov, V. Nikitin, M. Krounbi, K. A. Zvezdin, A. Anane, J. Grollier, and A. Fert, Phys. Rev. B 87, 020402(R) (2013).
  41. [41]A. Tsukahara, Y. Ando, Y. Kitamura, H. Emoto, E. Shikoh, M. P. Delmo, T. Shinjo, and M. Shiraishi, Phys. Rev. B 89, 235317 (2014).
  42. [42]42) Y. Du, R. Thompson, M. Kohda, and J. Nitta, AIP Adv. 11, 025033 (2021).
  43. [43]43) T. Seki, Y. Ch. Lau, S. Iihama, and K. Takanashi, Phys. Rev. B 104, 094430 (2021).
  44. [44]44) T. Tanaka, H. Kontani, M. Naito, T. Naito, D. S. Hirashima, K. Yamada, and J. Inoue, Phys. Rev. B 77, 165117 (2008).
  45. [45]45) M. Morota, Y. Niimi, K. Ohnishi, D. H. Wei, T. Tanaka, H. Kontani, T. Kimura, and Y. Otani, Phys. Rev. B 83, 174405 (2011).
  46. [46]46) H. Kontani, T. Tanaka, D. S. Hirashima, K. Yamada, and J. Inoue, Phys. Rev. Lett. 100, 096601 (2008).

Paper details

vlnc:W_j6y8sjx9
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents