Dual function spin-wave logic gates based on electric field control magnetic anisotropy boundary

Abstract

Spin waves (SWs) have been considered a promising candidate for encoding information with lower power consumption. Here, we propose the dual function SW logic gates based on the electric field controlling the SW propagation in the Fe film of Fe/BaTiO3 heterostructure with the motion of magnetic anisotropy boundary (MAB). We show micromagnetic simulations to validate the AND-OR and NAND-NOR logic gates. Our research may find a path for simplifying integrated logic circuits using such dual function SW logic gates.

With the rapid development in the miniaturization of electronic devices, power consumption has become one important issue because of the unbearable Joule heating.[1, 2] To overcome this issue, seeking new charge-neutral information carriers has spurred great attention. One representative charge-neutral information carrier is spin angular momentum, the electron’s another degree of freedom. Spin waves (SWs), the collective spin angular momentum excitations in magnetically ordered material and their associated quanta, magnons, are considered the promising information carrier for the next-generation lower power consumption, higher speed, and higher density devices. The phase[3, 4, 5, 6], amplitude[7, 8, 9, 10], and polarization[11, 12] of SWs can be employed to encode information. Generally, the nanostructured SW logic gates are designed on the uniform magnetized ferromagnetic materials by using all kinds of methods to control the propagation of SWs, including magnetic field[10], electric current[7, 8, 9] and voltage[13, 14].

The logic gates based on electric field or voltage can be easily programmable and compatible with nanoscale microwave devices[15]. Rana et al.[14] have proposed SW XNOR and universal NAND logic gates based on the voltage-controlled magnetic anisotropy (VCMA), which mainly arises from the change of electronic occupation state near the interface between the magnetic films and nonmagnetic heavy metals controlled by the voltage[15, 16, 17]. Magnetoelectric effects[18, 19, 20] provide another path for electric-field control of SWs in multiferroic materials[21, 22]. The most representative multiferroic system is artificial multiferroic materials. Just recently, electric field controlled spin wave propagation had been experimentally demonstrated in artificial multiferroic heterostructure.[23] Magnetoelectric effects could help us to design much more functional SW logic gates based on multiferroic structure. Here, the dual function SW logic gates are proposed by controlling the motion of magnetic anisotropy boundary (MAB) in epitaxial Fe film on ferroelectric BaTiO3\mathrm{BaTiO}_{3} substrate with altering in-plane and out-of-plane polarization domains. The AND-OR gate and NAND-NOR gate are validated by micromagnetic simulation.

We perform micromagnetic simulations by MuMax3[24] to study the propagation of Damon-Eshbach (DE) SWs[25] in the epitaxial Fe film on ferroelectric BaTiO3\mathrm{BaTiO}_{3} substrate. Figure 1(a) shows one unit structure in our simulation, including one 2 nm thick Fe layer, 100 nm thick BaTiO3\mathrm{BaTiO}_{3}, and the bottom electrode layer. The width and length of the structure are 800 nm and 2000 nm, respectively. The magnetic Fe layer includes uniaxial and cubic magnetic anisotropy regions via inverse magnetostriction owning to the different strains between Fe film and two kinds of domains in BaTiO3_3 layer[26]. The easy axis of uniaxial magnetic anisotropy on the top of in-plane ferroelectric a-domain is along the yy axis, while the easy axes of cubic anisotropy on the top of out-of-plane ferroelectric c-domain are along the direction with 45∘45^\circ to the xx axis, as shown by the white double head arrows. The MAB is at the middle of the Fe film (x=0x = 0, along yy axis) and is pinned on the ferroelectric domain wall of the BaTiO3_3 substrate. The width of MAB in Fe film is same to the ferroelectric domain wall in BaTiO3_3 (22–55 nm[27, 28, 29]), which is far smaller than the wavelength of SWs (several hundred nanometers). So, we neglect the width of the MAB in simulation. The parameters of Fe film used in simulation are the following[30]: saturation magnetization Ms=1.7×106M_\mathrm{s} = 1.7 \times10^{6} A/m, exchange stiffness constant Aex=2.1×10−11A_\mathrm{ex} = 2.1 \times10^{-11} J/m, Gilbert damping constant α=0.01\alpha= 0.01. The uniaxial and cubic magnetic anisotropy constants are the experiment values[23] of Ku=1.5×104K_\mathrm{u} = 1.5 \times10^{4} J/m3^{3} and Kc=4.4×104K_\mathrm{c} = 4.4 \times10^{4} J/m3^{3}. The cell size is 2×2×22 \times2 \times2 nm3^{3}, which is smaller than the exchange length (lex≈3.4l_\mathrm{ex} \approx3.4 nm). In order to avoid SWs’ reflection at the boundary, the damping is set to 1 at both ends (width = 100 nm) of the Fe film. An external magnetic field μ0Hext=100\mu_{0}H_\mathrm{ext} = 100 mT is applied to avoid the formation of magnetic domain wall and magnetize the Fe film along yy axis. To obtain the dispersion relation of the DE SWs in uniaxial and cubic anisotropy regions, a sinc based exciting field, h(t)=h0sinc⁡(2πfc(t−t0))e^z\mathbf{h}(t) = h_{0}\operatorname{sinc}(2\pi f_\mathrm{c}(t - t_{0}))\hat{\mathbf{e}}_{z}, with μ0h0=10\mu_{0}h_{0} = 10 mT, fc=50f_\mathrm{c} = 50 GHz, t0=5t_{0} = 5 ns, is applied locally to a 2×800×22 \times800 \times2 nm3^{3} central section of the Fe film, which is the SW source port (S) as

Image not extracted

Figure 1. (a) Schematic of the simulation model. Fe film is grown on the BaTiO3_3 with alternating in-plane polarization a-domain and out-of-plane polarization c-domain. The origin of the coordinate system is set at the center of the Fe film. (b) The image plot of the dispersion relation of the SWs. The dash lines are theoretically calculated results. (c) A snapshot of the MxM_x component of the magnetization taken at t=4t = 4 ns, y=−1y = -1 nm with a fixed f=12.6f = 12.6 GHz.

indicated by the red region in Figure 1(a). The dispersion relation[31, 32] of SWs can be obtained by performing a two-dimensional Fourier transform on mxm_x (mx=Mx/Msm_x = M_x/M_s), as shown in Figure 1(b). The curve of the left branch is the dispersion relation of SWs propagating along the the negative direction of xx axis in the uniaxial anisotropy region and the right branch is the dispersion relation of SWs propagating along the positive direction of xx axis in the cubic anisotropy region. The theory curves of SW dispersion relations are calculated by adopting the Eq. (4) and Eq. (5). It is clear to show that the SWs are only excited in the cubic anisotropy region in the frequency range of 9.5 GHz <f<< f < 14.5 GHz. To further clarify the property, we excite SWs at the source port with a sinusoidal field h(t)=h0sin⁡(2πft)e^z\mathbf{h}(t) = h_0\sin(2\pi f t)\hat{\mathbf{e}}_z with μ0h0=10\mu_0h_0 = 10 mT and a fixed f=12.6f = 12.6 GHz. A snapshot of the MxM_x component of the magnetization taken at t=4t = 4 ns is presented in Figure 1(c). SWs only propagate in the region with cubic anisotropy.

An out-of-plane electric field controlling ferroelectric domain wall motion can realize the movement of the MAB[30]. When the electric field is along the direction of the polarization in the c-domain, the c-domain will expand while the a-domain shrinks by the lateral domain wall motion. Suppose the electric field is inverse to the direction of the polarization in the c-domain. In that case, the c-domain will shrink and the a-domain expands. So, the electric field can drive the ferroelectric domain wall’s motion, thus driving the concurrent motion of the MAB. The velocity of MAB, that is, the velocity of ferroelectric domain wall driven by electric field pulse, can be up to 1000 m/s[33, 34]. Because the wall velocity is still smaller than the speed of sound in BaTiO3_3 (vsound=2000v_{\mathrm{sound}} = 2000 m/s[35]), the strain state can be considered quasistatic during the motion of ferroelectric domain wall and the strength and symmetry of the magnetic anisotropy are invariant during the MAB back and forth. The velocity vv of the MAB is implemented by shifting the MAB over one discretization cell (δx=2\delta x = 2 nm) during each time window δt=δx/v\delta t = \delta x/v. In the simulation, the velocity of MAB is 1000 m/s under the electric field 31.4 MV/m obtained by applying 3.14 V perpendicular voltage, which is inferred from previous experimental results[33].

Figure 2(a) shows the motion of MAB driven by voltage pulse and Figure 2(b)–(Figure 2d) shows the schematics of model and the snapshots of MxM_x when MAB at x=−600x = -600 nm, −100-100 nm and 400 nm, respectively. The SWs with f=12.6f = 12.6 GHz are excited from the source port. The position of MAB is driven to x=−600x = -600 nm by using the positive electric voltage (1.4 ns – 2 ns) shown in Figure 2(a). As expected, the SWs are blocked in uniaxial anisotropy region shown by the snapshot of SWs taken at t=5t=5 ns in Figure 2(b). After applying one negative pulse voltage (7 ns – 7.5 ns), the MAB moves to the position x=−100x=-100 nm. And, the SWs only propagate in the cubic anisotropy region from the snapshot of MxM_x taken at t=10.5t=10.5 ns, shown in Figure 2(c). When another 0.5 ns negative voltage pulse is applied (12.5 ns – 13 ns), the MAB moves to the position x=400x=400 nm, and the SW source port is out-of cubic anisotropy region. There are no SWs in Fe film. Thus, the transmission and block of SWs in Fe film can be controlled by voltage through driving the motion of MAB. Based on this unique property, we propose the design of dual function SW logic gates.

Image not extracted

Figure 2. (a) The position variation of the MAB with voltage pulse. (b), (c) and (d) are the schematics of model and the snapshots of MxM_x taken at y=−1y=-1 nm when MAB at x=−600x=-600 nm, −100-100 nm and 400400 nm (adopting the coordinate system in Figure 1(a)), respectively. The dashed lines mark the position of MAB.

Figure 3(a) is the schematic of the dual function AND-OR gate, which includes two input ports (A and B), two output ports (C and D), and a source port of SWs. Initially, the MAB is set at x=400x = 400 nm parallel to yy axis. The position of input A and B ports are arbitrary on the top of the Fe film. In order to make the two input ports independent, the B port includes a time delay unit, which can delay the voltage pulse for 0.5 ns. The output ports C and D take the xx component of magnetization at region (498498 nm <x<500< x < 500 nm, −2-2 nm <y<0< y < 0 nm) and (−500-500 nm <x<−498< x < -498 nm, −2-2 nm <y<0< y < 0 nm), respectively, as indicated by the black square regions. Magnetic tunnel junctions can perform this function and convert SW signals to electrical signals. An external magnetic field μ0Hext=100\mu_0 H_{\mathrm{ext}} = 100 mT is applied to magnetize the Fe film along yy axis and a sinusoidal field h(t)=h0sin⁡(2πft)e^z\mathbf{h}(t) = h_0 \sin(2\pi f t)\hat{\mathbf{e}}_z with μ0h0=10\mu_0 h_0 = 10 mT and f=12.6f = 12.6 GHz is set at the source port. The bottom electrode is grounding.

Image not extracted

Figure 3. (a) Schematic diagram of the AND-OR gate. Initially, the MAB is set at x=400x = 400 nm. Input A and B are the input ports and input B includes a time delay unit that can delay the input signal for 0.5 ns. C and D ports are output ports. The bottom electrode is grounding. The simulation results of the AND-OR gate with different inputs are shown in (b) – (e), respectively. The amplitudes of SWs in 11 ns – 11.5 ns are the logic operation results and the time domain is marked by the red dash lines. Finishing one logic operation needs 4.5 ns. (f) The truth table of the AND-OR gate.

The simulation results of the AND-OR gate with different inputs are shown in Figure 3(b)–(e). The simulation result of A = 0 and B = 0 is shown in Figure 3(b). Obviously, the MAB keeps still at position x=400x = 400 nm, because there is no electric field across BaTiO3_3. The outputs of C and D are both small amplitudes representing ’0’ due to the blocking of SWs shown in Figure 2(d). The simulation result of A = 1 and B = 0 is shown in Figure 3(c). The input ’1’ signal includes one 0.5 ns positive voltage pulse and 0.5 ns negative voltage pulse as shown in Figure 3(c). The positive pulse is used to start logical operation by driving the MAB moving 500 nm along the negative direction of xx axis in 0.5 ns, while the negative pulse is used to reset the position of MAB. The related motion of MAB and output signals of the two ports are also shown in Figure 3(c). In 9 ns – 9.5 ns, the MAB is driven from x=400x = 400 nm to x=−100x = -100 nm. After oscillation in 9.5 ns – 11 ns, the amplitudes of SWs at C and D represent C = 1 and D = 0 in the time range of 11 ns – 11.5 ns, marked by the red dash lines. After that, the negative pulse drives the MAB back to x=400x = 400 nm during 11.5 ns – 12 ns. The outputs will be the same as the initial and one whole logical operation is finished. Figure 3(d) shows the simulation result of A = 0 and B = 1. It’s very similar to the previous operation. The only difference is the 0.5 ns delay of the voltage pulse in B port. But the outputs of ports C and D are still ’1’ and ’0’, respectively. If A and B ports are both ’1’, the driving time of MAB will be 1 ns due to the 0.5 ns delay between A and B shown in Figure 3(e). The MAB is driven to x=−600x = -600 nm from x=400x = 400 nm during the period of 9 ns – 10 ns. And the amplitudes of SWs for ports C and D are over 1000 A/m at the time range of 11 ns – 11.5 ns. The operation results of C and D are both ’1’. Then,

MAB is driven back to x=400x = 400 nm during 11.5 ns – 12.5 ns. It should be mentioned that the amplitude of the SWs in C port at 11 ns – 11.5 ns is a bit larger than that in Figure 3(c) and (d), which mainly arises from the weaker interference between the reflected SWs from the MAB and the initial SWs. In short summary, the logic operation of the AND-OR gate can be divided into three stages, preparation before output (9 ns – 11 ns), output (11 ns – 11.5 ns) and reset (11.5 ns – 13.5 ns). The truth table of the AND-OR gate is shown in Figure 3(f). The input A, B and output C compose an OR gate while the input A, B and output D compose an AND gate.

In order to implement full Boolean logic operation, we also need the NAND and NOR gates. Figure 4(a) is the schematic of the dual function NAND-NOR gate. Here, the initial MAB is set at x=−600x = -600 nm. The main change of the NAND-NOR gate is that the two input ports A and B are connected with the bottom electrode and the Fe layer is grounding. The output ports and source port are the same with the AND-OR gate. When A and B are both ’0’, the MAB keeps still at x=−600x = -600 nm. When only one of A and B is ’1’, the MAB is driven to x=−100x = -100 nm for logic operation and then driven back to reset. When A and B are both ’1’, the MAB is driven to x=400x = 400 nm for logic operation and then driven back to reset. The simulation results of the NAND-NOR logic gate with different inputs are shown in Figure 4(b)–(Figure 4e), respectively. The output result of A = 0 and B = 0 is shown in Figure 4(b). The MAB is still at x=−600x = -600 nm because of the zero-field force. The amplitudes of the SWs are over 1000 A/m, both for C and D ports. This indicates that the output ports C and D are both ’1’. The simulation result of A = 1 and B = 0 is shown in Figure 4(c). The MAB is driven from x=−600x = -600 nm to x=−100x = -100 nm for positive pulse during 9 ns – 9.5 ns. Then, the amplitude of the SWs at C port is slightly reduced before the negative reset pulse, which can be explained by the interference between the reflected SWs from MAB and the initial SWs. For the D port, the amplitude of the SWs is almost vanishing. So we can recognize the output C = 1 and D = 0 before the reset of the MAB. Figure 4(d) shows the simulation result for A = 0 and B = 1. The output is same as A = 1 and B = 0. The last configuration of A = 1 and B = 1 is shown in Figure 4(e). In 9 ns – 10 ns, the MAB is driven to x=400x = 400 nm from x=−600x = -600 nm. After oscillation in 10 ns – 11 ns, the amplitudes of C and D in 11 ns – 11.5 ns are the operation result representing C = 0 and D = 0. In 11.5 ns – 12.5 ns, the MAB is driven back to x=−600x = -600 nm. After oscillation in 12.5 ns – 13.5 ns, one logic operation is finished. The logic operation of the NAND-NOR gate can also be divided into three stages, preparation before output (9 ns – 11 ns), output (11 ns – 11.5 ns) and reset (11.5ns – 13.5 ns). One circle logic operation needs 4.5 ns. The truth table of the NAND-NOR gate is listed in Figure 4(f). The input A, B and output C compose a NAND gate, while the input A, B and output D compose a NOR gate.

Image not extracted

Figure 4. (a) Schematic diagram of the NAND-NOR gate. Initially, the MAB is set at x=−600x = -600 nm. The Fe film is grounding and the input voltage signals are injected from bottom electrode. Other configurations and the input signals are same to the AND-OR gate. The simulation results of the NAND-NOR gate with different inputs are shown in (b) – (e), respectively. The amplitudes of SWs in 11 ns – 11.5 ns are the logic operation results and the time domain is marked by the red dash lines. Finishing one logic operation needs 4.5 ns. (f) The truth table of the NAND-NOR gate.

In conclusion, we propose dual function SW logic gates based on the motion of MAB controlled by electric field. AND-OR gate and NAND-NOR gate are validated by micro-magnetic simulation. Owning to the inherent dual function, the proposed SW logic gates have potential of building low power consumption and high density devices. Our results will also motivate further experimental studies for the development of dual function SW devices.

Acknowledgments

This work is partially supported by National Key Research Program of China (Grant No. 2017YFA0206202), International Postdoctoral Exchange Fellowship Program (20190083), Natural Science Foundation of Shaanxi Province (2021JM-022).

Dispersion relation of SWs

Kalinikos et al [36] developed the theory of dispersion relation of SWs taking into account both dipole-dipole and exchange interactions. The general formula of dispersion relation of DE SWs is:

f=γμ02π(Hi+2Aexμ0Msk2)(Hi+Ms+2Aexμ0Msk2)+Ms2F(1)f = \frac{\gamma\mu_{0}}{2\pi}\sqrt{\left(H_i+\frac{2A_{\mathrm{ex}}}{\mu_{0}M_s}k^2\right)\left(H_i+M_s+\frac{2A_{\mathrm{ex}}}{\mu_{0}M_s}k^2\right)+M_s^2F} \tag*{(1)}

where γ\gamma is the gyromagnetic ratio, μ0\mu_0 is vacuum permeability, HiH_i is the internal static magnetic field, AexA_{\mathrm{ex}} is exchange stiffness constant, MsM_s is saturation magnetization, kk is the wave vector of SWs, F=1−e−kdkd(1−1−e−kdkd)F=\frac{1-e^{-kd}}{kd}\left(1-\frac{1-e^{-kd}}{kd}\right), dd is the thickness of the film. This formula doesn’t include magnetic anisotropy field. So we need calculate magnetic anisotropy field and give the formula of dispersion relation in uniaxial and cubic anisotropy region, respectively.

The dynamic unit magnetization can be written as: m=MMs≈e^y+mxe^x+mze^z\mathbf{m}=\frac{\mathbf{M}}{M_s}\approx\hat{e}_y+m_x\hat{e}_x+m_z\hat{e}_z, where mx,mz≪1m_x,m_z\ll1. The magnetic anisotropy fields in uniaxial and cubic anisotropy regions can be calculated by equation (A2) and (A3) (ignore high-order mxm_x and mzm_z terms for linear approximation).

Hu=2Kuμ0Ms(u⋅m)u=2Kuμ0Mse^y(2)\mathbf{H}_u=\frac{2K_u}{\mu_0M_s}(\mathbf{u}\cdot\mathbf{m})\mathbf{u}=\frac{2K_u}{\mu_0M_s}\hat{e}_y \tag*{(2)}

where Hu\mathbf{H}_u is the uniaxial anisotropy field, KuK_u is the uniaxial anisotropy constant, u\mathbf{u} is the unit vector of the easy axis of uniaxial anisotropy, along yy axis.

Hc=−2Kcμ0Ms(((c2⋅m)2+(c3⋅m)2)((c1⋅m)c1)+((c1⋅m)2+(c3⋅m)2)((c2⋅m)c2)+((c1⋅m)2+(c2⋅m)2)((c3⋅m)c3))=Kcμ0Msmxe^x−Kcμ0Mse^y−2Kcμ0Msmze^z(3)\begin{aligned} \mathbf{H}_c={}&-\frac{2K_c}{\mu_0M_s}\bigl(((\mathbf{c}_2\cdot\mathbf{m})^2+(\mathbf{c}_3\cdot\mathbf{m})^2)((\mathbf{c}_1\cdot\mathbf{m})\mathbf{c}_1) \\ &+((\mathbf{c}_1\cdot\mathbf{m})^2+(\mathbf{c}_3\cdot\mathbf{m})^2)((\mathbf{c}_2\cdot\mathbf{m})\mathbf{c}_2) \\ &+((\mathbf{c}_1\cdot\mathbf{m})^2+(\mathbf{c}_2\cdot\mathbf{m})^2)((\mathbf{c}_3\cdot\mathbf{m})\mathbf{c}_3)\bigr) \\ ={}&\frac{K_c}{\mu_0M_s}m_x\hat{e}_x-\frac{K_c}{\mu_0M_s}\hat{e}_y-\frac{2K_c}{\mu_0M_s}m_z\hat{e}_z \tag*{(3)} \end{aligned}

where Hc\mathbf{H}_{\mathrm{c}} is the cubic anisotropy field, KcK_{\mathrm{c}} is the cubic anisotropy constant, c1\mathbf{c}_1, c2\mathbf{c}_2 and c3\mathbf{c}_3 are (2/2,2/2,0)(\sqrt{2}/2,\sqrt{2}/2,0), (−2/2,2/2,0)(-\sqrt{2}/2,\sqrt{2}/2,0) and (0,0,1)(0,0,1), respectively, the unit vector of the easy axes of cubic anisotropy.

So, the formulas of dispersion relation of DE SWs in uniaxial and cubic anisotropy region are

f=γμ02π(Hext+2Kuμ0Ms+2Aexμ0Msk2)(Hext+2Kuμ0Ms+Ms+2Aexμ0Msk2)+Ms2F(4)f=\frac{\gamma\mu_0}{2\pi}\sqrt{\left(H_{\mathrm{ext}}+\frac{2K_{\mathrm{u}}}{\mu_0M_{\mathrm{s}}}+\frac{2A_{\mathrm{ex}}}{\mu_0M_{\mathrm{s}}}k^2\right)\left(H_{\mathrm{ext}}+\frac{2K_{\mathrm{u}}}{\mu_0M_{\mathrm{s}}}+M_{\mathrm{s}}+\frac{2A_{\mathrm{ex}}}{\mu_0M_{\mathrm{s}}}k^2\right)+M_{\mathrm{s}}^2F} \tag*{(4)}

and

f=γμ02π(Hext−2Kcμ0Ms+2Aexμ0Msk2)(Hext+Kcμ0Ms+Ms+2Aexμ0Msk2)+Ms2F(5)f=\frac{\gamma\mu_0}{2\pi}\sqrt{\left(H_{\mathrm{ext}}-\frac{2K_{\mathrm{c}}}{\mu_0M_{\mathrm{s}}}+\frac{2A_{\mathrm{ex}}}{\mu_0M_{\mathrm{s}}}k^2\right)\left(H_{\mathrm{ext}}+\frac{K_{\mathrm{c}}}{\mu_0M_{\mathrm{s}}}+M_{\mathrm{s}}+\frac{2A_{\mathrm{ex}}}{\mu_0M_{\mathrm{s}}}k^2\right)+M_{\mathrm{s}}^2F} \tag*{(5)}

References

References

  1. [1]E. Vogel, Nature Nanotechnology, 2007, 2, 25–32.
  2. [2]T. N. Theis and H. P. Wong, Computing in Science & Engineering, 2017, 19, 41–50.
  3. [3]A. Khitun and K. L. Wang, Superlattices and Microstructures, 2005, 38, 184–200.
  4. [4]S. Klingler, P. Pirro, T. Brächer, B. Leven, B. Hillebrands and A. V. Chumak, Applied Physics Letters, 2014, 105, 152410.
  5. [5]S. Klingler, P. Pirro, T. Brächer, B. Leven, B. Hillebrands and A. V. Chumak, Applied Physics Letters, 2015, 106, 212406.
  6. [6]T. Fischer, M. Kewenig, D. A. Bozhko, A. A. Serga, I. I. Syvorotka, F. Ciubotaru, C. Adelmann, B. Hillebrands and A. V. Chumak, Applied Physics Letters, 2017, 110, 152401.
  7. [7]M. P. Kostylev, A. A. Serga, T. Schneider, B. Leven and B. Hillebrands, Applied Physics Letters, 2005, 87, 153501.
  8. [8]T. Schneider, A. A. Serga, B. Leven, B. Hillebrands, R. L. Stamps and M. P. Kostylev, Applied Physics Letters, 2008, 92, 022505.
  9. [9]K.-S. Lee and S.-K. Kim, Journal of Applied Physics, 2008, 104, 053909.
  10. [10]M. Jamali, J. H. Kwon, S. M. Seo, K. J. Lee and H. Yang, Sci Rep, 2013, 3, 3160.
  11. [11]J. Lan, W. Yu and J. Xiao, Nat Commun, 2017, 8, 178.
  12. [12]W. Yu, J. Lan and J. Xiao, Phys. Rev. Applied, 2020, 13, 024055.
  13. [13]Q. Wang, A. V. Chumak, L. Jin, H. Zhang, B. Hillebrands and Z. Zhong, Phys. Rev. B, 2017, 95, 134433.
  14. [14]B. Rana and Y. Otani, Phys. Rev. Applied, 2018, 9, 014033.
  15. [15]B. Rana and Y. Otani, Communications Physics, 2019, 2, 90.
  16. [16]C.-G. Duan, J. P. Velev, R. F. Sabirianov, Z. Zhu, J. Chu, S. S. Jaswal and E. Y. Tsymbal, Phys. Rev. Lett., 2008, 101, 137201.
  17. [17]M. Tsujikawa and T. Oda, Phys. Rev. Lett., 2009, 102, 247203.
  18. [18]N. A. Spaldin and M. Fiebig, Science, 2005, 309, 391–392.
  19. [19]T. Taniyama, J Phys Condens Matter, 2015, 27, 504001.
  20. [20]C. Song, B. Cui, F. Li, X. Zhou and F. Pan, Progress in Materials Science, 2017, 87, 33–82.
  21. [21]M. Balinskiy, A. C. Chavez, A. Barra, H. Chiang, G. P. Carman and A. Khitun, Sci Rep, 2018, 8, 10867.
  22. [22]A. V. Sadovnikov, A. A. Grachev, S. E. Sheshukova, Y. P. Sharaevskii, A. A. Serdobintsev, D. M. Mitin and S. A. Nikitov, Phys Rev Lett, 2018, 120, 257203.
  23. [23]H. Qin, R. Dreyer, G. Woltersdorf, T. Taniyama and S. van Dijken, Advanced Materials, 2021, 33, 2100646.
  24. [24]A. Vansteenkiste, J. Lelaiert, M. Dvornik, M. Helsen, F. Garcia-Sanchez and B. Van Waeyenberge, AIP Advances, 2014, 4, 107133.
  25. [25]R. W. Damon and J. R. Eshbach, Journal of Physics and Chemistry of Solids, 1961, 19, 308–320.
  26. [26]T. H. E. Lahtinen, Y. Shirahata, L. Yao, K. J. A. Franke, G. Venkataiah, T. Taniyama and S. van Dijken, Applied Physics Letters, 2012, 101, 262405.
  27. [27]X. Zhang, T. Hashimoto and D. C. Joy, Applied Physics Letters, 1992, 60, 784–786.
  28. [28]J. Hlinka and P. Márton, Phys. Rev. B, 2006, 74, 104104.
  29. [29]Q. Zhang and W. A. Goddard, Applied Physics Letters, 2006, 89, 182903.
  30. [30]K. J. A. Franke, B. Van de Wiele, Y. Shirahata, S. J. Hämäläinen, T. Taniyama and S. van Dijken, Phys. Rev. X, 2015, 5, 011010.
  31. [31]D. Kumar, O. Dmytriiev, S. Ponraj and A. Barman, Journal of Physics D: Applied Physics, 2011, 45, 015001.
  32. [32]G. Venkat, D. Kumar, M. Franchin, O. Dmytriiev, M. Mruczkiewicz, H. Fangohr, A. Barman, M. Krawczyk and A. Prabhakar, IEEE Transactions on Magnetics, 2013, 49, 524–529.
  33. [33]H. L. Stadler and P. J. Zachmanidis, Journal of Applied Physics, 1963, 34, 3255–3260.
  34. [34]V. Boddu, F. Endres and P. Steinmann, Sci Rep, 2017, 7, 806.
  35. [35]A. K. Tagantsev, L. E. Cross and J. Fousek, Domains in Ferroelectric Crystals and Thin Films, Springer, New York, NY, 2010, p. 369.
  36. [36]B. A. Kalinikos and A. N. Slavin, Journal of Physics C: Solid State Physics, 1986, 19, 7013–7033.

Paper details

vlnc:W_jznrd4m9
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents