WorksPhysics and Astronomy
Evaluation of P3-type layered oxides as K-ion battery cathodes
Abstract
Given increasing energy storage demands and limited natural resources of Li, K-ion batteries (KIBs) could be promising next-generation systems having natural abundance, similar chemistry and energy density. Here, we have investigated the P3-type KTMO (where TM = Ti, V, Cr, Mn, Co, or Ni) systems using density functional theory calculations, as potential positive intercalation electrodes (or cathodes) for KIBs. Specifically, we have identified the ground state configurations, and calculated the average topotactic voltages, electronic structures, on-site magnetic moments, and thermodynamic stabilities of all P3-KTMO compositions and their corresponding depotassiated P3-TMO frameworks. We find that K adopts the honeycomb or zig-zag configuration within each K-layer of all P3 structures considered, irrespective of the TM. In terms of voltages, we find the Co- and Ti-based compositions to exhibit the highest (4.59 V vs. K) and lowest (2.24 V) voltages, respectively, with the TM contributing to the redox behavior upon K (de-)intercalation. We observe all P3-KTMO to be (meta)stable, and hence experimentally synthesizeable according to our 0 K convex hull calculations, while all depotassiated P3-TMO configurations are unstable and may appear during electrochemical cycling. Also, we verified the stability of the prismatic coordination environment of K compared to octahedral coordination at the KTMO compositions using Rouxel and cationic potential models. Finally, combining our voltage and stability calculations, we find P3-KCoO to be the most promising cathode composition, while P3-KNiO is worth exploring. Our work should contribute to the exploration of strategies and materials required to make practical KIBs.
- is worth exploring. Our work should contribute to the exploration of strategies and materials required to make practical KIBs.
Introduction
Lithium-ion batteries (LIBs) have played a pre-eminent role in energy storage for the last three decades.[1, 2, 3] However, our excessive dependence on LIBs raises several challenges on natural abundance of critical elements, fragile supply chains, and cost,[4] which has motivated the search for intercalation chemistries that can be an alternative to LIBs. Notably, K-ion batteries (KIBs) have emerged as a viable alternative for economic grid-scale storage applications owing to the natural abundance of K, reversible (de)intercalation into graphite (as anode), and lower standard redox potential (K/K, -2.936 V vs. standard hydrogen electrode –SHE).[5, 6, 7] Despite several advantages over Li (and Na), the practical development of KIB is constrained by the need for robust cathode materials that can (de)intercalate K reversibly. Several classes of materials have been explored as K-intercalation cathodes, namely layered oxides, polyanionic frameworks, Prussian blue analogous, and organic compounds.[5] Out of these, layered transition metal oxides (TMOs), similar to those used for Li and Na (de)intercalation, are promising in terms of their high theoretical energy density, high rate capability owing to the large two-dimensional K diffusion pathways, and possible structural stability during cycling due to the large slab spacing that can suppress detrimental transition metal (TM) migration into K-layers.[8]
Typical K-containing layered structures, of composition (, TM = transition metal), exhibit a variety of stacking sequences, including prismatic-based P3 or P2, and octahedral-based O3 or O2, where the P3, P2, O3, and O2 notations are defined as per the nomenclature of Delmas and co-workers.[9] The type of coordination environment preferred by K (i.e., octahedral vs. prismatic, see Figure S1 of the supporting information –SI, for an illustration) in a given framework, which in turn determines the type of stacking sequence of the structure, is primarily determined by the TM itself, the oxidation state(s) of the TM, and the K-concentration. For example, KScO and KCrO exhibit the O3 framework, while KMnO adopts the P3 framework.[10, 11, 12, 13, 14, 15] The relative stability of octahedral and prismatic coordination can also be quantified via the “cationic potential” model and/or the Rouxel diagram.[9, 16] Notably, prismatic coordination is often stabilized at intermediate (x∼0.5) or non-stoichiometric (x < 1) K-concentrations in layered frameworks, similar to observations in analogous Na-containing layered systems,[17, 18, 19, 20] as illustrated by KCrO, KMnO, and KCoO systems.[11, 19] Indeed, Hagenmuller and co-workers’ experiment-derived phase diagram of (A = Na or K; M = Cr, Mn, or Co), indicates that either the P3 or the P’3 is the stable phase at intermediate Na or K concentrations, irrespective of the TM.[11]
Experimentally, stoichiometric (x=1) has been synthesized only in , , , and systems, with limitations on the observable electrochemical capacity.[10, 11, 12, 13, 14, 15] As a result, previous studies have investigated non-stoichiometric frameworks, often dealing with prismatic phases. For example, Vaalma et al. demonstrated as a possible K-intercalation host,[21] which was followed by Kim et al.’s report that found P3- as a viable candidate as well.[22] Interestingly, the analogous P3- compound is metastable and cannot be trivially synthesized.[23, 24] Hironaka et al. showed P3- as an efficient reversible K-intercalation host,[25] while Hwang et al. developed P3- via electrochemical ion exchange from the parent O3- compound.[26] Notably, previous computational studies have revealed that the diffusivity of in prismatic stacking is higher than in octahedral stacking.[24, 26, 27] Thus, the existing literature indicates that K-containing layered TMOs with prismatic stacking sequences can be easily synthesized, exhibit reasonable cyclability, and good rate performance. However, systematic computational or experimental studies of P3-type K-containing layered TMOs are missing, so far.
Here, we have used density functional theory (DFT[28, 29]) calculations to systematically evaluate various K-ion containing P3-layered oxides as candidate electrodes for KIBs. Specifically, we have calculated the lattice parameters, average intercalation voltage, thermodynamic stability, electronic properties, and on-site magnetic moments in systems, where TM = Ti, V, Cr, Mn, Co, or Ni. We enumerate the possible in-plane K-ion orderings for compositions, and determine the ground states using DFT. Subsequently, we evaluate the aforementioned properties for the ground state configuration and its corresponding depotassiated composition, namely . Notably, we observe that all P3-type systems are thermodynamically stable, except V and Cr, with Co (Ti) system exhibiting the highest (lowest) predicted voltage of 4.59 V (2.24 V) vs. K. The ground state configurations for all systems are identical, with K exhibiting a honeycomb or zig-zag ordering in each K-layer. Based on calculated projected density of states (pDOS) and on-site magnetic moments, we expect the TM to be redox-active upon K (de)intercalation in P3-. Also, we demonstrate the stability of prismatic over octahedral coordination in the systems considered, via the Rouxel and cationic potential model approaches. Finally, based on voltage and stability metrics, we expect P3 and to be promising candidates. We hope that our study will reinvigorate the computational and experimental investigations of - systems as K-intercalating hosts.
Computational Methods
We used the Vienna Ab Initio Simulation Package[30, 31, 32] to perform the DFT calculations, using the plane wave basis set with a kinetic energy cut-off of 520 eV and the projected-augmented wave (PAW[32, 33]) potentials to model the ionic cores, consistent with our previous work.[34, 35] We sampled the irreducible Brillouin zone using -centered Monkhorst-Pack[36] -point meshes with a density of 32 points per Å, and we integrated the Fermi surface with a Gaussian smearing of width 0.05 eV. We relaxed the cell volume, shape, and ionic positions of all our structures without any symmetry constraints, till the atomic forces and the total energy were converged within eV/Å and eV, respectively.[37] All our calculations were spin-polarized, and we initialized the magnetic moments of all TM metals in a high-spin ferromagnetic ordering, except Co and Ni where we initialized with a low-spin ferromagnetic ordering for both the and oxidation states. For describing the electronic exchange-correlation, we utilized the Hubbard corrected, strongly constrained and appropriately normed (SCAN[38]) functional, i.e., SCAN+. As derived in previous work, we used Hubbard corrections[39] of 2.5, 1.0, 2.7, 3.0, and 2.5 eV for Ti, V, Mn, Co, and Ni, respectively.[34, 35] All pDOS calculations with the ‘fake-self-consistent-field’ procedure, as detailed in previous work.[40, 41]
The starting structure for Ti, V, Mn, and Ni compositions was the -, as obtained from the inorganic crystal structure database (ICSD[42]), where we created the Ti, V, and Ni structures via ionic substitution of Mn in -. We constructed the Cr- and Co-based structures based on previous reports.[10, 25] Since several K-vacancy configurations are possible at the target composition, we used the pymatgen package to enumerate all symmetrically distinct orderings[43] within each supercell of size . We used VESTA for the visualization and illustration of structures used in our calculations.[44]
The redox reaction of topotactic (de-)intercalation of in a P3-type can be represented as:
and represent the potassiated and depotassiated structures, respectively. The average intercalation voltage can be calculated via the Nernst equation from the difference in the Gibbs energies () of the potassiated and depotassiated compositions. We approximated the Gibbs energies with the DFT calculated total energies (i.e., ), thus ignoring the – and entropic contributions.[45, 46] Within this approximation and with being the Faraday’s constant, the average K-intercalation voltage K/K is:
, , and are the DFT-calculated total energies of the ground state potassiated configuration, depotassiated composition, and the body-centered-cubic phase of pure K, respectively.
In order to assess the thermodynamic stability of the P3-type and compositions, we computed the 0 K phase diagram (or the convex hull) of each ternary K-TM-O system, based on the DFT-calculated total energies of all elements, and compounds (i.e., binary and ternaries), whose experimentally reported structures are available in the ICSD. We used the pymatgen package to construct the phase diagrams.[43] We quantify the instability (stability) of and by calculating the energy above (below) the hull, denoted by , based on the 0 K phase diagrams.[47, 48, 49] Note that we used a meV/atom as a threshold value for a structure being experimentally synthesizeable, but this threshold is arbitrary and is highly chemistry-dependent.[49]
Results
Structure, K-ordering, and lattice parameters
Figure 1a illustrates the typical unit cell of P3-, consisting of three layers, denoted by the brown polyhedra. The topologically distinct prismatic sites of K are shown by the blue and orange polyhedra in Figure 1a and equivalently by the blue and orange spheres in Figure 1b. Combined, the two prismatic sites arrange themselves in a hexagonal lattice, as shown by the black guidelines in panels b and c of Figure 1. Each prism shares one of its triangular faces with one octahedra, thus violating the third Pauling’s rule,[50, 51] while the other triangular face shares its three edges with three different octahedra. The oxygen packing in P3 compounds follows the ABBCCA sequence.

Figure 1. (a) Unit cell of typical P3- structure. (b) Visualization of different types of prismatic sites (blue and orange spheres) that are available for K-occupation, per K-layer in P3-. The blue and orange spheres are equivalent to the blue and orange polyhedra shown in panel a. (c) Honeycomb or zig-zag ordering in each K-layer that constitutes the ground state configuration for all P3- considered. Pink guidelines in panels b and c connect identical K-sites.
The K-vacancy arrangement in each K-layer is an optimization of the steric and electrostatic interactions between the K-ions for any . Interestingly, we found the ground state K-vacancy configuration of all systems to be identical, as indicated in Figure 1c by the honeycomb or zig-zag ordering of in each K-layer. Specifically, in each of the blue+orange hexagon of Figure 1b, occupies the farthest possible combination of one blue and one orange site, resulting in the honeycomb ordering of Figure 1c. This is equivalent to a K-K distance of if the side-length of the hexagon in Figure 1b is . Also, our in-plane K-ordering is similar to previous experimental and theoretical studies,[52, 53, 54, 55] with marginal differences in the construction of the honeycomb ordering. Note that the scale of panels b and c in Figure 1 are different, where the pink guidelines in both panels connect identical set of K-sites.
The SCAN+-calculated lattice parameters for the ground state configurations of all systems considered are compiled in Table S1. The computed lattice parameters are in good agreement with available experimental values,[22, 25, 26] with the maximum overestimation (underestimation) of the parameter of 4.69% (2.79%). Increase in the atomic number of the TM monotonically decreases the and lattice parameters (see trendlines in Figure 2a), caused primarily by a decrease in TM-O bonds, except for Mn and Ni which can be attributed to the Jahn-Teller distortion of and (Figure S2). As shown in Figure 2a and Table S1, the Jahn–Teller distortion also causes a decrease in the parameter for Mn compared to Cr and Co, whereas in Ni, the parameter remains similar to Co.

Figure 2. SCAN+ calculated (a) lattice parameters in various KTMO systems, and (b) average K-intercalation voltage across the different KTMO-TMO compositions. Average voltage values in (b) are also indicated by the text annotations.
Average Voltages
Figure 2b presents the calculated average topotactic intercalation voltage, referenced against K/K, for the P3-type KTMO-TMO systems considered in this work. Notably, the predicted voltages range from 2.24 V for the KTiO-TiO system to 4.59 V for the KCoO-CoO system, which is within the stable window of typical electrolytes used for KIBs.[5] The calculated intercalation voltage increases progressively as we move from Ti to Co, in accordance with the standard reduction potentials of the corresponding TMs, as noted in a previous study.[40]
Importantly, Mn and Ni systems show markedly lower voltages compared to their neighboring TMs, which can be partly attributed to the Jahn–Teller distortions of Mn and Ni. Also, the predicted voltage drop from Co to Ni is similar to the observation in Li-containing layered oxides, caused by the filling of the antibonding orbital of NiO.[40] Finally, the lower intercalation voltage of 2.24 V for the KTiO system suggest that this system can be explored as an anode for KIBs.
Electronic Structure and Magnetic Moments
The calculated pDOS of all KTMO ground state structures are displayed in Figure 3, with Figure S3 compiling the pDOS of all TMO structures. The red, blue, orange, dotted blue, and dashed black lines represent K states, O states, TM states, band edges, and Fermi level, respectively, with the numbers in each panel indicating band gaps. Except KCrO, KVO and CrO, all KTMO and TMO structures are predicted to be semiconductors by SCAN+. The calculated band gaps exhibit a non-monotonic trend as we move along the series in KTMO, decreasing from 0.49 eV in Ti to 0 eV in Cr, subsequently increasing up to 1.66 eV in Co and further decreasing to 0.30 eV in Ni. Band gap trends in TMO structures (Figure S3) are similar to KTMO, with the gap decreasing from 2.85 eV to 0 eV from Ti to Cr, then increasing to 2.40 eV in Mn and finally decreasing to 1.39 eV in Ni.

Figure 3. SCAN+-calculated pDOS for all P3-KTMO systems. Blue, orange, and red curves correspond to TM , O , and K states, respectively. Positive (negative) values of pDOS correspond to up (down) spin electrons. Dotted blue lines represent the valence and conduction band edges, with the numbers indicating band gap values. Dashed black lines signify Fermi level. The zero on the energy scale in each panel is referenced either to the valence band maximum or to the Fermi level.
While TM states dominate the valence band edge (VBE) or the Fermi level in Ti, V, and Cr versions of KTMO (Figure 3), both O and TM states contribute equally in the case of Mn, Co, and Ni analogs, attributed to increased hybridization of the TM-O bonds as we move across the series. In the case of conduction band edges (CBEs), the TM states dominate from Ti to Mn, while O states contribute significantly alongside TM states in Co and Ni structures. In the case of depotassiated TMO structures (Figure S3), O states dominate the VBE in TiO, CoO, and NiO, TM states dominate VBE in VO, while a mixture of O and TM states contribute to the VBE/Fermi level in MnO and CrO. The CBE of TMO structures are dominated by TM states, with the exception of NiO, where a mixture of O and Ni states contribute. Given that TM states contribute significantly to the VBE/Fermi level (responsible for oxidation) of all KTMO and the CBE/Fermi level (responsible for reduction) of all TMO structures (except NiO), we expect the TM to be predominantly redox-active during K (de)intercalation across all P3 systems (with Ni being a possible exception).
To further probe the possible origins of redox activity in the P3 frameworks, we analysed the calculated on-site magnetic moments of the TM in each system, as tabulated in Table S2. In all ground state KTMO configurations, we observe that half the TM ions are in 3+, and the rest in 4+ oxidation state, except KCrO, where the electrons appear delocalized across Cr centers due to its metallic nature. Upon K-removal, all the transition metals in all TMO structures are in a uniform 4+ oxidation state, as suggested by the calculated magnetic moments (see Table S2), highlighting that the TM exclusively contributes to the redox activity with K (de)intercalation. Also, we observe from the magnetic moments that each K in KTMO shares the triangular face with a TM octahedra and the triangular edges with three TM octahedra.
Thermodynamic stability
The for the KTMO and TMO compositions are displayed as a heatmap in Figure 4, where blue (red) tiles indicate compositions that are stable (unstable). The solid green line across the legend bar in Figure 4 signifies the 50 meV/atom stability threshold. The 0 K convex hulls of the K-TM-O ternaries (relevant for potassiated compositions) and TM-O binaries (relevant for depotassiated compositions) are compiled in Figures S4 and S5, respectively. Importantly, the data indicates high degree of stability for all KTMO frameworks, with the exception of KVO and KCrO, which are metastable with of 47 and 13 meV/atom, respectively, below the 50 meV/atom threshold. Thus, we expect all P3-type potassiated compositions considered in this work to be experimentally synthesizable.

Figure 4. DFT-calculated for P3-KTMO (top row) and P3-TMO (bottom row) compositions. Each column represents a given TM. Blue (red) squares indicate high degrees of stability (instability), with the specific value of each composition listed as a text annotation in the corresponding square. The green line on the legend bar indicates the rule-of-thumb meV/atom threshold for experimental synthesizability.
In case of depotassiated compositions, we find all P3-TMO structures to be unstable, with more than 50 meV/atom. Thus, we don’t expect the synthesis of P3-TMO configurations to be facile. However, during electrochemical cycling, the P3-TMO structures may exist in a metastable manner, due to kinetic barriers to transform to the corresponding stable states. Notably, the lower extent of instability displayed by P3-CoO and P3-MnO ( meV/atom) is more promising than the other frameworks in terms of their ability to appear during electrochemical cycling and not decompose to other stable compositions. Finally, combining both stability and voltage metrics, we find P3-KCoO to be the most promising cathode composition, while P3-KNiO can also be explored as a candidate.
Discussion
Using DFT-based calculations, we have explored the P3-KTMO frameworks as potential intercalation hosts for KIBs in this work. Specially, we have computed the lattice parameters, ground state K-vacancy configurations, average K-interaction voltage, electronic structure, on-site magnetic moments, and 0 K thermodynamic stability for P3-KTMO and the corresponding depotassiated-TMO structures, where TM is Ti, V, Cr, Mn, Co, or Ni. We found that all KTMO ground states adopted the honeycomb or zig-zag ordering of K-ions. With respect to voltage predictions, we observed the highest (lowest) voltages to arise from the Co (Ti) system, consistent with trends in standard reduction potentials. While we found all potassiated P3- compositions to be stable or metastable (i.e., meV/atom) highlighting experimental synthesizability, all depotassiated P3- compositions were unstable, indicating that they may not be synthesizable experimentally but may appear during electrochemical cycling due to kinetic barriers for decomposition. Also, we observed the TM to be the primary participant in the redox process, characterized by the electronic structure and on-site magnetic moments of the potassiated and depotassiated compositions. Finally, combining voltage and stability metrics, we find the P3 frameworks of , and to be promising cathode candidates, while P3- may be explored as an anode.
Typically, in layered oxide frameworks, K can occupy either prismatic or octahedral coordination (Figure S1), depending on the K-concentration, and associated steric and electrostatic interactions within the structure. The relative stability of prismatic vs. octahedral coordination environment of K (and hence the stacking sequence of the layered structure) can be modelled via the modified Rouxel diagram[9] and the cationic potential[16] phase map, which are displayed in panels a and b of Figure 5, respectively. Numerical details of the Rouxel diagram and cationic potential frameworks are described in the SI, with Tables S3-S6 compiling relevant parameters or values.

Figure 5. (a) Rouxel diagram and (b) cationic potential phase map for various compositions. The dashed line in both panels separates the region of stability of octahedral-coordinated phases from prismatic-coordinated phases. Each column of data points in panel a represents a distinct TM while the symbols represent various K compositions (x). In panel b, each row of data points corresponds to a unique x while the symbols distinguish the TMs.
In the Rouxel diagram framework, the critical parameter () is used a classifier of prismatic and octahedral phases (see formulation provided in SI). depends on the ionic or covalent nature of the bonds between the cations (K and TM) and anions (O), and the K concentration (x). Figure 5a plots at different K compositions (x = 1/4, 1/3, 1/2, 2/3, 3/4, and 1) as the TM is varied in . Importantly, we observe that all compositions prefer prismatic coordination, while several compositions (except , , and ) also favour the prismatic coordination for any K content.
Cationic potential () is a descriptor of interslab interactions, i.e., higher the cationic potential of a metal higher is the ionic polarizability and more covalent is the bond between the metal and an anion. Higher cationic potential also indicates stronger repulsion between adjacent octahedra (resulting from larger electrostatic repulsion of higher oxidation state metals) and weaker interaction between adjacent slabs. The larger interlayer distance in a prismatic structure usually coincides with a higher cationic potential implying more covalent TM-O bonds. Conversely, the smaller interlayer distances in O3 structures (at similar compositions as corresponding P3 structures) coincide with a lower cationic potential.
Apart from interlayer distances, is also dependent on K-concentration. For example, at low x in (or equivalently lower mean ionic potential of K, ), binding of layers by K via electrostatic attraction between and is weaker resulting in larger interlayer spacings and prismatic stacking, which is what we observe in Figure 5b. Additionally, the variations in and for various compositions indicate that prismatic structures should be observed at x = 1/2 for all TM, consistent with the Rouxel diagram framework as well (Figure 5a). Trends in panels a and b of Figure 5 are also in agreement with the literature reported so far for the K-based layered oxides,[5] highlighting the utility of such empirical frameworks. Additionally, can be tuned by the addition/doping of multiple TMs within the same layered oxide, thereby stabilizing either octahedral or prismatic coordination for the K-ions.
We find the honeycomb or zig-zag arrangement of to be the ground state configuration of all compositions, as displayed in Figure 1c. Owing to the larger size and higher ionicity of , there is strong in-plane electrostatic and steric repulsion that tends to maximize the - distance, irrespective of the TM. Thus, can be considered to screen effectively TM-TM interactions across the layers (at x=0.5), which can be a cause of our observation of identical ground states. Additionally, we find that each shares its triangular face and three triangular edges with and , respectively, which may be a result of electrostatic interactions as well. Another consequence of the large size and higher ionicity of is the observed lower intercalation voltages than analogous Na-layered compounds, despite exhibiting a more negative standard reduction potential than . [5, 40, 56] Specifically, the stronger electrostatic interactions between and the TM ions can result in increasing the interlayer distance, and could weaken the TM-O bonds by increasing the TM-O bond lengths compared to the Na-analogues.[57]
While we have used the SCAN+ framework for describing the electronic exchange and correlation, recent studies have reported that SCAN+ overestimates average voltages in Li-intercalation electrodes.[40, 41] Indeed, we observe a similar overestimation of average voltages in P3-CrO, MnO and CoO, where our predicted values are V, V and V vs. K, respectively (Figure 2b), compared to the experimental V in Cr (cathode composition was CrO), V in Mn (MnO), and V in Co (CoO).[22, 25, 26] Such overestimation of voltages may arise from an underestimation of energies (i.e., total DFT-calculated energies are less negative) of metastable/unstable phases, such as depotassiated-TMO structures.[40] Note that all our calculated voltages, despite being overestimated by SCAN+, are within the stability window of the commonly used electrolyte, KPF in ethylene carbonate: diethyl carbonate.
Finally, when it comes to phase stability, SCAN+ frequently doesn’t provide quantitative precision owing to underestimation of total energies of metastable phases. Yet, our calculations predicts that the traditional chemical synthesis pathway can produce P3-TMO, owing to the calculated (meta)stability of P3-TMO, whereas the depotassiated P3-TMO may appear during electrochemical cycling. Apart from the single transition metal-based system, investigating possible inclusion of multiple TMs within the P3 framework could be result in better insertion host(s) for KIBs, where higher voltages arising from the presence of one TM can be combined with the stability contributed by another TM.
Conclusion
We explored the K-containing P3-type layered TMOs as potential intercalation hosts for KIBs using DFT calculations and the SCAN+ framework for describing electronic exchange and correlation. We considered six different TMOs, namely, TiO, VO, CrO, MnO, CoO, and NiO, and their corresponding depotassiated compositions, as the candidate K-intercalation hosts. Apart from estimating the ground state K-vacancy configuration in each TMO system considered, we evaluated the DFT-relaxed lattice parameters, topotactic average intercalation voltage, and 0 K thermodynamic stability. Additionally, we probed the nature of redox activity upon K (de)intercalation in these compounds by analysing the electronic structure and on-site TM magnetic moments in the potassiated and depotassiated structures. Importantly, we find that prefers the honeycomb or zig-zag ordering in , irrespective of the TM, highlighting the dominance of electrostatic interactions between ions within the same layer. Our calculated voltages follow the general trend of standard reduction potentials of the TMs involved, with the low-voltage - framework being more suitable as an anode, and - exhibiting the highest predicted voltage. Notably, we find the redox activity to be centered on the TM sites in all systems, with negligible contribution from redox on the anionic sites. In terms of thermodynamic stability, we find all - frameworks considered to be below the meV/atom threshold, indicating that synthesis of such compounds is likely to be facile. Finally, given the combination of our thermodynamic stability and average voltage estimates, we find -, and as potential candidates as KIB cathodes.
Conflicts of interest
There are no conflicts of interest to declare.
Acknowledgments
G.S.G. acknowledges financial support from the Indian Institute of Science (IISc) Seed Grant, SG/MHRD/20/0020 and SR/MHRD/20/0013, and support from the Science and Engineering Research Board (SERB) of Government of India, under sanction numbers SRG/2021/000201 and IPA/2021/000007. P.B. is grateful to the Alexander von Humboldt Foundation (Bonn, Germany) for a 2022 Humboldt fellowship for experienced researchers. P.B. acknowledges financial support from the HP Green R&D Centre (Bangalore). P.K.J. and S.N.T. would like to thank the Ministry of Human Resource Development (MHRD), Government of India, for financial assistance. We also acknowledge the computational resources provided by the Supercomputer Education and Research Centre (SERC), IISc.
References
- [1]Armand, M.; Tarascon, J. M., Building better batteries. Nature 2008, 451, 652-657.DOI
- [2]Dunn, B.; Kamath, H.; Tarascon, J. M., Electrical energy storage for the grid: a battery of choices. Science (New York, N.Y.) 2011, 334, 928-935.
- [3]Whittingham, M. S., History, Evolution, and Future Status of Energy Storage. Proc. IEEE 2012, 100, 1518-1534.DOI
- [4]Whittingham, M. S., Ultimate Limits to Intercalation Reactions for Lithium Batteries. Chem. Rev. 2014, 114, 11414-11443.DOI
- [5]Hosaka, T.; Kubota, K.; Hameed, A. S.; Komaba, S., Research Development on K-Ion Batteries. Chem. Rev. 2020, 120, 6358-6466.DOI
- [6]Hwang, J.-Y.; Myung, S.-T.; Sun, Y.-K., Recent Progress in Rechargeable Potassium Batteries. Adv. Funct. Mater. 2018, 28, 1802938.DOI
- [7]Kim, H.; Kim, J. C.; Bianchini, M.; Seo, D.-H.; Rodriguez-Garcia, J.; Ceder, G., Recent Progress and Perspective in Electrode Materials for K-Ion Batteries. Adv. Energy Mater. 2018, 8, 1702384.DOI
- [8]Zhang, X.; Wei, Z.; Dinh, K. N.; Chen, N.; Chen, G.; Du, F.; Yan, Q., Layered Oxide Cathode for Potassium-Ion Battery: Recent Progress and Perspective. small 2020, 16, 2002700.DOI
- [9]Delmas, C.; Fouassier, C.; Hagenmuller, P., Structural classification and properties of the layered oxides. Physica B+C 1980, 99, 81-85.DOI
- [10]Delmas, C.; Devalette, M.; Fouassier, C.; Hagenmuller, P., Les phases KₓCrO₂ (X ≤ 1). Mater. Res. Bull. 1975, 10, 393-398.DOI
- [11]Fouassier, C.; Delmas, C.; Hagenmuller, P., Evolution structurale et proprietes physiques des phases AₓMO₂ (A = Na, K; M = Cr, Mn, Co) (x ≤ 1). Mater. Res. Bull. 1975, 10, 443-449.DOI
- [12]Han, S. C.; Park, W. B.; Sohn, K.-S.; Pyo, M., KFeO₂ with corner-shared FeO₄ frameworks as a new type of cathode material in potassium-ion batteries. J. Solid State Electrochem. 2019, 23, 3135-3143.DOI
- [13]Hoppe, R.; Sabrowsky, H., Oxosandate der Alkalimetalle: KSCoO₂ und RbSCoO₂. Z. anorg. allg. Chem. 1965, 339, 144-154.
- [14]Jansen, M.; Chang, F. M.; Hoppe, R., Zur Kenntnis von KMnO₂. Z. anorg. allg. Chem. 1982, 490, (1), 101-110.DOI
- [15]Kim, H.; Seo, D.-H.; Urban, A.; Lee, J.; Kwon, D.-H.; Bo, S.-H.; Shi, T.; Papp, J. K.; McCloskey, B. D.; Ceder, G., Stoichiometric Layered Potassium Transition Metal Oxide for Rechargeable Potassium Batteries. Chem. Mater. 2018, 30, 6532-6539.DOI
- [16]Zhao, C.; Wang, Q.; Yao, Z.; Wang, J.; Sánchez-Lengeling, B.; Ding, F.; Qi, X.; Lu, Y.; Bai, X.; Li, B.; Li, H.; Aspuru-Guzik, A.; Huang, X.; Delmas, C.; Wagemaker, M.; Chen, L.; Hu, Y. S., Rational design of layered oxide materials for sodium-ion batteries. Science (New York, N.Y.) 2020, 370, 708-711.DOI
- [17]Lei, Y.; Li, X.; Liu, L.; Ceder, G., Synthesis and Stoichiometry of Different Layered Sodium Cobalt Oxides. Chem. Mater. 2014, 26, 5288-5296.DOI
- [18]Parant, J.-P.; Olazcuaga, R.; Devalette, M.; Fouassier, C.; Hagenmuller, P., Sur quelques nouvelles phases de formule NaxMnO2 (x ≤ 1). J. Solid State Chem. 1971, 3, 1-11.DOI
- [19]Claude Delmas, M. M.; Fouassier, C.; Hagenmuller, P., Stabilite relative des environnements octaedrique et prismatique triangulaire dans les oxydes lamellaires alcalins AₓMO₂ (x ≤ 1). Mater. Res. Bull. 1976, 11, 1483-1488.DOI
- [20]Radin, M. D.; Van der Ven, A., Stability of Prismatic and Octahedral Coordination in Layered Oxides and Sulfides Intercalated with Alkali and Alkaline-Earth Metals. Chem. Mater. 2016, 28, 7898-7904.DOI
- [21]Vaalma, C.; Giffin, G. A.; Buchholz, D.; Passerini, S., Non-Aqueous K-Ion Battery Based on Layered K0.3MnO2 and Hard Carbon/Carbon Black. J. Electrochem. Soc. 2016, 163, A1295.DOI
- [22]Kim, H.; Seo, D.-H.; Kim, J. C.; Bo, S.-H.; Liu, L.; Shi, T.; Ceder, G., Investigation of Potassium Storage in Layered P3-Type K₀.₅MnO₂ Cathode. Adv. Mater. 2017, 29, 1702480.
- [23]Bianchini, M.; Wang, J.; Clément, R. J.; Ouyang, B.; Xiao, P.; Kitchaev, D.; Shi, T.; Zhang, Y.; Wang, Y.; Kim, H.; Zhang, M.; Bai, J.; Wang, F.; Sun, W.; Ceder, G., The interplay between thermodynamics and kinetics in the solid-state synthesis of layered oxides. Nat. Mater. 2020, 19, (10), 1088-1095.
- [24]Kubota, K.; Kumakura, S.; Yoda, Y.; Kuroki, K.; Komaba, S., Electrochemistry and Solid-State Chemistry of NaMeO₂ (Me = 3d Transition Metals). Adv. Energy Mater. 2018, 8, 1703415.DOI
- [25]Hironaka, Y.; Kubota, K.; Komaba, S., P2- and P3-KₓCoO₂ as an electrochemical potassium intercalation host. Chem. Comm. 2017, 53, 3693-3696.DOI
- [26]Hwang, J.-Y.; Kim, J.; Yu, T.-Y.; Myung, S.-T.; Sun, Y.-K., Development of P3-K₀.₆₉CrO₂ as an ultra-high-performance cathode material for K-ion batteries. Energy Environ. Sci. 2018, 11, 2821-2827.
- [27]Kaufman, J. L.; Van der Ven, A., Antiphase boundary migration as a diffusion mechanism in a P3 sodium layered oxide. Phys. Rev. Materials 2021, 5, 055401.DOI
- [28]Kohn, W.; Sham, L. J., Self-Consistent Equations Including Exchange and Correlation Effects. Phys. Rev. 1965, 140, A1133-A1138.DOI
- [29]Hohenberg, P.; Kohn, W., Inhomogeneous Electron Gas. Phys. Rev. 1964, 136, B864-B871.
- [30]Kresse, G.; Furthmüller, J., Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set. Phys. Rev. B 1996, 54, 11169-11186.pubmed.ncbi.nlm.nih.gov/9984901
- [31]Kresse, G.; Furthmüller, J., Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set. Comput. Mater. Sci. 1996, 6, 15-50.DOI
- [32]Kresse, G.; Joubert, D., From ultrasoft pseudopotentials to the projector augmented-wave method. Phys. Rev. B 1999, 59, 1758-1775.DOI
- [33]Blöchl, P. E., Projector augmented-wave method. Phys. Rev. B 1994, 50, (24), 17953-17979.pubmed.ncbi.nlm.nih.gov/9976227
- [34]Sai Gautam, G.; Carter, E. A., Evaluating transition metal oxides within DFT-SCAN and SCAN+U frameworks for solar thermochemical applications. Phys. Rev. Mater. 2018, 2, 095401.DOI
- [35]Long, O. Y.; Sai Gautam, G.; Carter, E. A., Evaluating optimal U for 3d transition-metal oxides within the SCAN+U framework. Phys. Rev. Mater. 2020, 4, 045401.DOI
- [36]Monkhorst, H. J.; Pack, J. D., Special points for Brillouin-zone integrations. Phys. Rev. B 1976, 13, 5188-5192.DOI
- [37]Ho, K. M.; Fu, C. L.; Harmon, B. N.; Weber, W.; Hamann, D. R., Vibrational Frequencies and Structural Properties of Transition Metals via Total-Energy Calculations. Phys. Rev. Lett. 1982, 49, 673-676.DOI
- [38]Sun, J.; Ruzsinszky, A.; Perdew, J. P., Strongly Constrained and Appropriately Normed Semilocal Density Functional. Phys. Rev. Lett. 2015, 115, 036402.arxiv.org/abs/1504.03028
- [39]Anisimov, V. I.; Zaanen, J.; Andersen, O. K., Band theory and Mott insulators: Hubbard U instead of Stoner I. Phys. Rev. B 1991, 44, (3), 943-954.
- [40]Long, O. Y.; Sai Gautam, G.; Carter, E. A., Assessing cathode property prediction via exchange-correlation functionals with and without long-range dispersion corrections. Phys. Chem. Chem. Phys. 2021, 23, 24726-24737.DOI
- [41]Jha, P. K.; Singh, S.; Shrivastava, M.; Barpanda, P.; Sai Gautam, G., First principles investigation of anionic redox in bisulfate lithium battery cathodes. Phys. Chem. Chem. Phys. 2022, 24, 22756-22767.DOI
- [42]Hellenbrandt, M., The Inorganic Crystal Structure Database (ICSD)—Present and Future. Crystallogr. Rev. 2004, 10, 17-22.DOI
- [43]Ong, S. P.; Richards, W. D.; Jain, A.; Hautier, G.; Kocher, M.; Cholia, S.; Gunter, D.; Chevrier, V. L.; Persson, K. A.; Ceder, G., pymatgen Materials Genomics (pymatgen): A robust, open-source python library for materials analysis. Comput. Mater. Sci. 2013, 68, 314-319.
- [44]Momma, K.; Izumi, F., VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data. J. Appl. Cryst. 2011, 44, 1272-1276.DOI
- [45]Aydinol, M. K.; Kohan, A. F.; Ceder, G.; Cho, K.; Joannopoulos, J., Ab initio study of lithium intercalation in metal oxides and metal dichalcogenides. Phys. Rev. B 1997, 56, 1354-1365.DOI
- [46]Aydinol, M. K.; Kohan, A. F.; Ceder, G., Ab initio calculation of the equilibrium voltage of lithium-transition-metal oxide electrodes for rechargeable batteries. J. Power Sources 1997, 68, 664-668.DOI
- [47]Sai Gautam, G.; Stechel, E. B.; Carter, E. A., Exploring Ca–Ce–M–O (M = 3d Transition Metal) Oxide Perovskites for Solar Thermochemical Applications. Chem. Mater. 2020, 32, 9964-9982.DOI
- [48]Tekliye, D. B.; Kumar, A.; Weihang, X.; Mercy, T. D.; Canepa, P.; Sai Gautam, G., Exploration of NaSiCON Frameworks as Calcium-Ion Battery Electrodes. Chem. Mater. 2022, 34, 10133-10143.DOI
- [49]Sun, W.; Dacek, S. T.; Ong, S. P.; Hautier, G.; Jain, A.; Richards, W. D.; Gamst, A. C.; Persson, K. A.; Ceder, G., The thermodynamic scale of inorganic crystalline metastability. Sci. Adv. 2016, 2, e1600225.
- [50]Pauling, L., The nature of the chemical bond and the structure of molecules and crystals; an introduction to modern structural chemistry. Cornell University Press: 1960.
- [51]Pauling, L., The principles determining the structure of complex ionic crystals. J. Am. Chem. Soc. 1929, 51, 1010-1026.DOI
- [52]Kubota, K.; Asari, T.; Yoshida, H.; Yaabuuchi, N.; Shiiba, H.; Nakayama, M.; Komaba, S., Understanding the Structural Evolution and Redox Mechanism of a NaFeO₂–NaCoO₂ Solid Solution for Sodium-Ion Batteries. Adv. Funct. Mater. 2016, 26, 6047-6059.DOI
- [53]Kaufman, J. L.; Van der Ven, A., NaₓCoO₂ phase stability and hierarchical orderings in the O3/P3 structure family. Phys. Rev. Materials 2019, 3, 015402.DOI
- [54]Toriyama, M. Y.; Kaufman, J. L.; Van der Ven, A., Potassium Ordering and Structural Phase Stability in Layered KₓCoO₂. ACS Appl. Energy Mater. 2019, 2, 2629-2636.DOI
- [55]Kaufman, J. L.; Van der Ven, A., Ordering and Structural Transformations in Layered KₓCrO₂ for K-Ion Batteries. Chem. Mater. 2020, 32, 6392-6400.DOI
- [56]Yabuuchi, N.; Kubota, K.; Dahbi, M.; Komaba, S., Research Development on Sodium-Ion Batteries. Chem. Rev. 2014, 114, 11636-11682.DOI
- [57]Goodenough, J. B.; Mizushima, K.; Takeda, T., Solid-Solution Oxides for Storage-Battery Electrodes. Jpn. J. Appl. Phys. 1980, 19, 305.DOI