Multi-kV class ββ-Ga2_2O3_3 MESFETs with a Lateral Figure of Merit up to 355 MW/cm2^2

Abstract

We demonstrate over 3 kV gate-pad-connected field plated (GPFP) ββ-Ga2_2O3_3 lateral MESFETs with high lateral figure of merit (LFOM) using metalorganic vapor phase epitaxy (MOVPE) grown channel layers and regrown ohmic contact layers. Using an improved low-temperature MOVPE selective area epitaxy process, we show that a total contact resistance to the channel as low as 1.4 ΩΩ.mm can be achieved.The GPFP design adopted here using PECVD (plasma-enhanced chemical vapor deposition) deposited SiNx_x dielectric and SiNx_x/SiO2_2 wrap-around passivation exhibits up to ~14% improved RON_{ON}, up to ~70% improved breakdown voltage (VBR_{BR} = VDS_{DS} - VGS_{GS}) resulting in up to ∼\sim3×\times higher LFOM compared to non-FP ββ-Ga2_2O3_3 lateral MESFETs. The VBR_{BR} (~2.5 kV) and LFOM (355 MW/cm2^2) measured simultaneously in our GPFP ββ-Ga2_2O3_3 lateral MESFET (with LGD_{GD} = 10 μμm) is the highest value achieved in any depletion-mode ββ-Ga2_2O3_3 lateral device.

This material is based upon work supported by the II-VI foundation Block Gift Program 2020-2021 and the DoD SBIR Phase I – AF203-CS01 (Contract #: FA864921P0304). This work was performed in part at the Utah Nanofab sponsored by the College of Engineering and the Office of the Vice President for Research (The University of Utah).

A. Bhattacharyya, P. Ranga, S. Roy, C. Peterson and S. Krishnamoorthy are with the Department of Electrical and Computer Engineering, University of Utah, Salt Lake City, Utah, USA 84112. (email: [email protected])

Sriram Krishnamoorthy is also with Materials Department, University of California, Santa Barbara, California, USA 93106. (email: [email protected])

F. Alema, G. Seryogin and A. Osinsky are with Agnitron Technology Incorporated, Chanhassen, Minnesota 55317, USA.

Introduction

Ga₂O₃-based devices have increasingly gained momentum as a potential technology that demonstrates numerous strengths for high voltage/power applications. The high projected breakdown field (~8 MV/cm) of β-Ga₂O₃ and the availability of high-quality melt-grown β-Ga₂O₃ bulk substrates offers compelling promise for high efficiency power devices[1, 2, 3, 4, 5, 6]. The β-Ga₂O₃–based device performance has rapidly progressed in both lateral and vertical geometries thanks to the simultaneous progress in high-quality epilayer growth technologies that includes mainly molecular beam epitaxy (MBE), metalorganic vapor phase epitaxy (MOVPE), halide vapor phase epitaxy (HVPE) and low-pressure chemical vapor deposition (LPCVD) as well as device processing techniques [7, 8, 9, 10, 11, 12, 13, 14, 15, 16]. Of all these epitaxial growth techniques, MOVPE has captivated widespread attention due to its versatility and ability to grow comparatively higher-quality epilayers that enables high room-temperature electron mobility values (close to the theoretical limit) and could be promising for fabricating Ga₂O₃ lateral FETs with high current densities as well as high breakdown voltages [8, 17, 18, 19].

Many new field management techniques have been successfully demonstrated in lateral β-Ga₂O₃-based devices that enabled high-breakdown voltages, high average breakdown fields, and high (VBR²/RON,sp) lateral figures of merit but not simultaneously in the same device [3, 4, 20]. In other words, VBR > 2kV, lateral VBR²/RON,sp > 300MW/cm², and EBR,AVG > 2MV/cm could not be achieved simultaneously in the same device. This could be due to a combination of factors such as device design, device processing techniques (bulk or surface leakage paths) and more importantly the epilayer material quality. In this work, we address these issues using a gate-pad connected field plate (GPFP) design using a PECVD deposited SiNₓ dielectric in a β-Ga₂O₃ MESFET with MOVPE-grown channel and contact layers.

device growth and fabrication

The epitaxial structure shown in Figure 1(a) consists of a β-Ga₂O₃ channel (230 nm thick Si-doped ~3.6×10¹⁷ cm⁻³) on a Fe-doped (010) bulk substrate grown using Agnitron Technology’s Agilis 700 MOVPE reactor with TEGa, O₂, and silane (SiH₄) as precursors and argon as carrier gas. The 10×15 mm² edge-defined film fed grown (EFG) semi-insulating Fe-doped (010) Ga₂O₃ bulk substrate was acquired from Novel Crystal Technology (NCT), Japan. Before the channel layer growth, the substrate was cleaned using HF for 30 mins. From Hall measurement, the channel charge and mobility were measured to be 5.7×10¹² cm⁻² and 95 cm²/Vs respectively, yielding a channel sheet resistance, Rₛ,ₕ = 11.7 kΩ/□. The device mesa isolation and the source/drain ohmic contacts were selectively regrown by MOVPE technique using a Ni/SiO₂ mask pattern [21]. The contact recess etch was performed using a low power SF₆/Ar ICP-RIE dry etching, followed by a quick dip in a diluted BOE solution. The etching in the contact regions was extended down to the Ga2_2O3_3 epitaxial layer with an estimated Ga2_2O3_3 trench depths of 10–20 nm (Ga2_2O3_3 etch rate ∼1.5\sim1.5 nm/min). The Si-doping in the regrown n+n^{+} layer was ∼2.6×1020\sim2.6 \times10^{20} cm−3^{-3}. Following the contact regrowth process, ohmic metal stack Ti/Au/Ni (20 nm/100 nm/30 nm) was evaporated on the regrown contact regions using photolithography patterning and lift off, followed by a 450°C anneal in N2_2 for 1.5 mins. Ni/Au/Ni (30 nm/100 nm/30 nm) metal stack was then evaporated to form the Schottky gate for the MESFET structure.

Schematic of the GPFP β-Ga₂O₃ MESFET with a SiNₓ/SiO₂ wrap-around passivation and top-view optical image of a fabricated GPFP MESFET

Figure 1. (a) Schematic of the GPFP β-Ga₂O₃ MESFET with a SiNₓ/SiO₂ wrap-around passivation. The FP metal is electrically connected to the gate pad outside the mesa (not shown). (b) top-view optical image of a fabricated GPFP MESFET.

The gate field plate design used in this work is shown in Figure 1(a), where the gate field plate metal was electrically connected to the gate pad (shorted) outside the device mesa, hence, named gate-pad-connected field plate (GPFP). This design was adopted to protect the channel region from the dry-etching plasma damage that occurs in the conventional gate field plate etch process flow and has been reported to cause plasma-damage induced RONR_{\mathrm{ON}} increase [4, 22]. Unlike MOSFETs, due to the absence of any gate dielectric that can act as etch stop/protective layer, avoiding the etch step in the active region played a key role to maintain RONR_{\mathrm{ON}} in our FP MESFETs as discussed later. The gate field plate metal was deposited following a SiNx_x (170 nm thick) passivation layer deposited using plasma-enhanced chemical vapor deposition (PECVD at 300°C). The field plate extension (LFPL_{\mathrm{FP}}) was varied from ∼0.3\sim0.3 to 3.5 μ\mum as the gate-to-drain distance (LGDL_{\mathrm{GD}}) varied from 2 to 45 μ\mum. Finally, the whole active region was passivated using an SiNx_x/SiO2_2 (50 nm/50nm) bilayer dielectric deposited using the same PECVD (300°C) technique. The SiNx_x/SiO2_2 wrap-around bi-layer allowed for a thicker overall dielectric passivation with lower SiNx_x thickness to prevent excessive stress in the SiNx_x film. The final device optical image is shown in Figure 1(b). The non-FP MESFET devices had no dielectric surface passivation.

RESULTS AND DISCUSSIONS

Fig. 2(a) & 2(b) show the DC output and transfer curves for the GPFP MESFET (solid lines) and the unpassivated non-FP MESFET (dashed lines) for device with dimensions LGS/LG/LGD=1.0/2.8/2.4 μL_{\mathrm{GS}}/L_{\mathrm{G}}/L_{\mathrm{GD}} = 1.0/2.8/2.4\ \mum. No hysteresis was observed in the DC current-voltage dual sweeps. The ID,MAXI_{\mathrm{D,MAX}} (at VGS=0V_{\mathrm{GS}} = 0V) measured was 88 mA/mm for the passivated GPFP MESFET and 81 mA/mm for the un-passivated non-FP MESFET. The ON resistance (RONR_{\mathrm{ON}}) @ VGS=0V_{\mathrm{GS}} = 0V extracted from the linear region of the output curves were found to be 55.8 Ω\Omega.mm for the GPFP MESFET and 63.2 Ω\Omega.mm for the non-FP MESFET. From TLM measurements, the total RCR_{\mathrm{C}} (contact resistance) measured was 1.4 Ω\Omega.mm (<3%< 3\% of the total device RONR_{\mathrm{ON}}) as shown in Figure 2(c). This total RCR_{\mathrm{C}} value consists of metal/n+n^{+} regrown Ga2_2O3_3 interface contact resistance, resistance of the regrown n+n^{+}-Ga2_2O3_3 region and the n+n^{+} regrown Ga2_2O3_3/lightly doped Ga2_2O3_3 channel interface resistance. Compared to our previous work, the ten-fold improvement in RCR_{\mathrm{C}} was achieved using a low etch rate SF6_6/Ar dry etching during the contact region recessing [21]. The transfer curves show that both devices have low leakage (∼10−12\sim10^{-12} A/mm) and high ION/IOFFI_{\mathrm{ON}}/I_{\mathrm{OFF}} ratio ∼1010\sim10^{10}. The passivated GPFP MESFETs show ∼\sim14% lower RONR_{\mathrm{ON}}, ∼\sim8% higher ON currents, and ∼\sim13% higher transconductance compared to the non-FP MESFETs clearly indicating the FP design used here not only preserves the RONR_{\mathrm{ON}} in these devices, rather improves it possibly due to reduction

DC output, transfer, resistance, breakdown, and reverse leakage characteristics of GPFP and non-FP MESFETs

Figure 2. (a) Output and (b) transfer curves for the GPFP (solid lines) and non-FP (dashed lines) β\beta-Ga2_2O3_3 MESFETs. (c) Total resistance vs spacing for the TLM patterns (schematic shown in inset). (d) Breakdown characteristics of the non-FP (top) and GPFP (bottom) β\beta-Ga2_2O3_3 MESFETs with various LGDL_{\mathrm{GD}} values. Reverse leakage plots for the (e) non-FP MESFET with LGDL_{\mathrm{GD}} of 10 μ\mum and (f) GPFP MESFET with LGDL_{\mathrm{GD}} of 10 μ\mum.

of upward surface band-bending in the open access regions due to the SiNx_x passivation [23].

Fig. 2(d) shows the three-terminal breakdown characteristics (at VGS=−20V_{\mathrm{GS}} = -20 V) for the non-FP MESFETs and the GPFP MESFET with various LGDL_{\mathrm{GD}} values. All the breakdown measurements were performed with the wafer submerged in FC-40 Fluorinert dielectric liquid. Comparing devices with identical LGDL_{\mathrm{GD}} values, the GPFP MESFETs show significant improvement in breakdown voltage (VBR=VDS−VGSV_{\mathrm{BR}} = V_{\mathrm{DS}} - V_{\mathrm{GS}}) over the non-FP MESFETs. The highest measurable VBRV_{\mathrm{BR}} recorded was 2462V (LGD=10μL_{\mathrm{GD}} = 10\mum) for the GPFP MESFET, which is ∼\sim70% higher compared to the non-FP MESFET (1462V) of the same dimensions showing the efficacy of the FP design demonstrated here. The reverse leakage current rise was mainly due to gate leakage for both types of MESFETs. Fig. 2(e) and 2(f) show the OFF-state gate and drain terminal currents of the non-FP and GPFP MESFETs respectively with LGDL_{\mathrm{GD}} of 10 μ\mum, showing that the leakage current is dominated by the gate leakage before the catastrophic breakdown.

It can be seen that for the GPFP MESFET, the VBRV_{\mathrm{BR}} scales more linearly with LGDL_{\mathrm{GD}} compared to the non-FP MESFETs (Figure 3(a)). Even though the E-field profile is highly non-uniform in the gate-drain region of a lateral device, an effective average lateral field (EAVG=VBR/LGDE_{\mathrm{AVG}} = V_{\mathrm{BR}}/L_{\mathrm{GD}}) can be defined to be used as a metric to understand the scaling of breakdown voltage vs spacing and helps with lateral device design. Non-linear scaling of field peaking around the contact edges and transition from punch through to non-punch field profile occurs with increasing LGDL_{\mathrm{GD}}. This reduces EBR,AVGE_{\mathrm{BR,AVG}} values and, therefore, results in non-linear VBRV_{\mathrm{BR}} vs LGDL_{\mathrm{GD}} relationship. However, the calculated EAVGE_{\mathrm{AVG}} values remained uniform ∼\sim2.5 MV/cm for GPFP MESFETs with LGDL_{\mathrm{GD}} up to 10 μ\mum. This combination of EAVGE_{\mathrm{AVG}} (∼\sim2.5 MV/cm) and VBRV_{\mathrm{BR}} (∼\sim2.5 kV) demonstrated here for a MESFET with LGDL_{\mathrm{GD}} = 10 μ\mum is the highest to date for any depletion-mode Ga2_2O3_3 lateral device. GPFP MESFETs with LGDL_{\mathrm{GD}} 20 μ\mum and above did not breakdown and were measured repeatedly up to 3 kV (our measurement tool limit) without showing any degradation, demonstrating the robustness of these devices to high voltage stresses. It should be noted that all the devices in this work exhibit catastrophic breakdown.

VBR as a function of LGD and LFOM as a function of LGD

Figure 3. (a) VBRV_{\mathrm{BR}} as a function of LGDL_{\mathrm{GD}} for the non-FP and GPFP MESFETs showing the increase in EBR,AVGE_{\mathrm{BR,AVG}}, and improved VBRV_{\mathrm{BR}} vs LGDL_{\mathrm{GD}} linearity. (b) LFOM of the MESFETs as a function of LGDL_{\mathrm{GD}}.

The lateral figures of merit (VBR2/Ron,spV_{\mathrm{BR}}^{2}/R_{\mathrm{on,sp}}) of the GPFP MESFETs were calculated, where Ron,spR_{\mathrm{on,sp}} is RONR_{\mathrm{ON}} normalized to the device length (LSD+2LTL_{\mathrm{SD}}+2L_{\mathrm{T}}). The LFOM values for the GPFP and non-FP MESFETs are plotted as a function of LGDL_{\mathrm{GD}} (Figure 3(b)). The highest LFOM of 355 MW/cm2^{2} was calculated for GPFP MESFET (VBRV_{\mathrm{BR}} = 2462V, Ron,spR_{\mathrm{on,sp}} = 17.05 mΩ\Omega.cm2^{2} with an LGDL_{\mathrm{GD}} of 10 μ\mum which is more than 3×\times higher compared to the non-FP MESFET (LFOM = 115 MW/cm2^{2}, VBRV_{\mathrm{BR}} = 1466V, Ron,spR_{\mathrm{on,sp}} = 18.6 mΩ\Omega.cm2^{2}). Overall, the GPFP design is found to have 2-3 times higher LFOM compared to the non-FP design. This is because of the improved Ron,spR_{\mathrm{on,sp}} (up to 14% lower) and VBRV_{\mathrm{BR}} (up to 70% higher) values simultaneously with the GPFP design. Given the GPFP MESFET with LGDL_{\mathrm{GD}} = 20 μ\mum have VBRV_{\mathrm{BR}} >3 kV, these devices can demonstrate LFOM >200 MW/cm2^{2} for >3kV class transistors.

To understand the electric field profiles, the device structures were simulated using Sentaurus TCAD under the breakdown condition. For the GPFP design, the EpeakE_{\mathrm{peak}} was found to be at the FP edge as expected (Figure 4(d)). The sharp metal edges used in the simulation act as points of singularity in the Poisson solver and may overestimate actual peak field values in real devices. From the simulated lateral field profile under the gate, the GPFP MESFET with an LGDL_{\mathrm{GD}} of 10 μ\mum was found to have a punchthrough field profile for the reported breakdown voltage.The electric field under the gate was found to be < 2 MV/cm, but the EpeakE_{\mathrm{peak}} values in the SiNx_x at the FP edge were found to be much higher (1.4 – 1.8×\times higher) than in Ga2_2O3_3 under the FP edge. Therefore, it is possible that the dielectric breakdown could also be the dominant breakdown mechanism for large LGDL_{\mathrm{GD}} values rather than just the gate (tunneling) leakage in the GPFP design.

Simulated 2D electric field contours and lateral E-field profiles

Figure 4. (a) Simulated 2D electric field contour and (b) Lateral E-field profile in Ga2_2O3_3 under the gate along cutline A-A’ and for a device with LGDL_{\mathrm{GD}} = 10μ\mum at the experimental breakdown condition of VDGV_{\mathrm{DG}} = 1466V for the non-FP MESFET. (c) Simulated 2D electric field contour and (d) Lateral E-field profile along cutline A-A’ & B-B’ for a device with LGDL_{\mathrm{GD}} = 10μ\mum at the experimental breakdown condition of VDGV_{\mathrm{DG}} = 2462V for the GPFP MESFET.

Figure 5 benchmarks our VBRV_{\mathrm{BR}}-Ron,spR_{\mathrm{on,sp}} values with the existing literature reports showing that the reported GPFP β\beta-Ga2_2O3_3 MESFET shows the highest LFOM for VBRV_{\mathrm{BR}} > 2 kV, outperforming the likes of Ga2_2O3_3 MOSFETs and even advanced device designs like (AlGa)2_2O3_3/Ga2_2O3_3 HFETs and NiOx_x/Ga2_2O3_3 p-n hetero-Junction FETs (hJFETs) [3, 20]. With the implementation of a gate dielectric, we expect the LFOM values could be further improved, provided gate dielectrics with low-leakage, cleaner interface and more importantly, dielectrics with high breakdown fields could be deposited along with high-quality β\beta-Ga2_2O3_3 epitaxial layers.

Differential Ron,sp-VBR benchmark plot

Figure 5. Differential Ron,spR_{\mathrm{on,sp}}-VBRV_{\mathrm{BR}} benchmark plot of our β\beta-Ga2_2O3_3 MESFETs with the lateral β\beta-Ga2_2O3_3 MESFETs in the literature [3, 20, 24, 25, 26, 27, 28, 29, 30].

Conclusion

We demonstrate gate-pad connected field plated MOCVD-grown kV-class β\beta-Ga2_2O3_3 lateral MESFETs with high LFOM and EBR,AVGE_{\mathrm{BR,AVG}} using PECVD deposited SiNx_x and SiO2_2 field/passivation dielectrics. A record high LFOM of 355 MW/cm2^{2} with a VBRV_{\mathrm{BR}} of ∼\sim2.5 kV and EAVGE_{\mathrm{AVG}} of ∼\sim2.5 MV/cm simultaneously is demonstrated in a GPFP β\beta-Ga2_2O3_3 MESFET with LGDL_{\mathrm{GD}} = 10 μ\mum. This LFOM value is the highest for any β\beta-Ga2_2O3_3 lateral device with VBRV_{\mathrm{BR}} > 2kV. These devices show great potential of MOCVD-grown β\beta-Ga2_2O3_3 FETs for future power device applications in the low to medium voltage range.

References

References

  1. [1]M. Higashiwaki and G. H. Jessen, “Guest Editorial: The dawn of gallium oxide microelectronics,” Appl. Phys. Lett., vol. 112, no. 6, p. 060401, Feb. 2018, doi: 10.1063/1.5017845.
  2. [2]S. J. Pearton, J. Yang, P. H. Cary, F. Ren, J. Kim, M. J. Tadjer, and M. A. Mastro, “A review of Ga2O3 materials, processing, and devices,” Applied Physics Reviews, vol. 5, no. 1, p. 011301, Mar. 2018, doi: 10.1063/1.5006941.DOI
  3. [3]N. K. Kalarickal, Z. Xia, H.-L. Huang, W. Moore, Y. Liu, M. Brenner, J. Hwang, and S. Rajan, “β-(Al0.18Ga0.82)2O3/Ga2O3 Double Heterojunction Transistor with Average Field of 5.5 MV/cm,” IEEE Electron Device Letters, pp. 1–1, 2021, doi: 10.1109/LED.2021.3072052.
  4. [4]S. Sharma, K. Zeng, S. Saha, and U. Singisetti, “Field-Plated Lateral Ga2O3 MOSFETs With Polymer Passivation and 8.03 kV Breakdown Voltage,” IEEE Electron Device Letters, vol. 41, no. 6, pp. 836–839, Jun. 2020, doi: 10.1109/LED.2020.2991146.DOI
  5. [5]S. Roy, A. Bhattacharyya, P. Ranga, H. Splawn, J. Leach, and S. Krishnamoorthy, “High-Oxide Field-Plated Vertical (001) β-Ga2O3 Schottky Barrier Diode with Baliga’s Figure of Merit Over 1 GW/cm2,” IEEE Electron Device Letters, pp. 1–1, 2021, doi: 10.1109/LED.2021.3089945.DOI
  6. [6]A. J. Green, K. D. Chabak, E. R. Heller, R. C. Fitch, M. Baldini, A. Fiedler, K. Irmscher, G. Wagner, Z. Galazka, S. E. Tetlak, A. Crespo, K. Leedy, and G. H. Jessen, “3.8-MV/cm Breakdown Strength of MOVPE-Grown Sn-Doped β-Ga2O3 MOSFETs,” IEEE Electron Device Letters, vol. 37, no. 7, pp. 902–905, Jul. 2016, doi: 10.1109/LED.2016.2568139.DOI
  7. [7]K. Sasaki, M. Higashiwaki, A. Kuramata, T. Masui, and S. Yamakoshi, “MBE grown Ga2O3 and its power device applications,” Journal of Crystal Growth, vol. 378, pp. 591–595, 2013.DOI
  8. [8]Z. Feng, A. F. M. Anhar Uddin Bhuiyan, M. R. Karim, and H. Zhao, “MOCVD homoepitaxy of Si-doped (010) β-Ga2O3 thin films with superior transport properties,” Appl. Phys. Lett., vol. 114, no. 25, p. 250601, Jun. 2019, doi: 10.1063/1.5109678.DOI
  9. [9]S. Bin Anooz, R. Grüneberg, C. Wouters, R. Schewski, M. Albrecht, A. Fiedler, K. Irmscher, Z. Galazka, W. Miller, G. Wagner, J. Schwarzkopf, and A. Popp, “Step flow growth of β-Ga2O3 thin films on vicinal (100) β-Ga2O3 substrates grown by MOVPE,” Appl. Phys. Lett., vol. 116, no. 18, p. 182106, May 2020, doi: 10.1063/5.0005403.
  10. [10]J. H. Leach, K. Udawary, J. Rumsey, G. Dodson, H. Splawn, and K. R. Evans, “Halide vapor phase epitaxial growth of β-Ga2O3 and α-Ga2O3 films,” APL Materials, vol. 7, no. 2, p. 022504, Feb. 2019, doi: 10.1063/1.5055680.DOI
  11. [11]H. Murakami, K. Nomura, K. Goto, K. Sasaki, K. Kawara, Q. T. Thieu, R. Togashi, Y. Kumagai, M. Higashiwaki, A. Kuramata, S. Yamakoshi, B. Monemar, and A. Koukitou, “Homoepitaxial growth of β-Ga2O3 layers by halide vapor epitaxy,” Appl. Phys. Express, vol. 8, no. 1, p. 015503, Dec. 2014, doi: 10.7567/APEX.8.015503.DOI
  12. [12]P. Ranga, A. Rishinaramangalam, J. Varley, A. Bhattacharyya, D. Feezell, and S. Krishnamoorthy, “Si-doped β-(Al0.26Ga0.74)2O3 thin films and heterostructures grown by metalorganic vapor-phase epitaxy,” Applied Physics Express, vol. 12, no. 11, p. 111004, Oct. 2019, doi: 10.7567/1882-0786/abad7b8.DOI
  13. [13]P. Ranga, A. Bhattacharyya, A. Rishinaramangalam, Y. K. Ooi, M. A. Scarpulla, D. Feezell, and S. Krishnamoorthy, “Delta-doped β-Ga2O3 thin films and β-(Al0.26Ga0.74)2O3/β-Ga2O3 heterostructures grown by metalorganic vapor-phase epitaxy,” Appl. Phys. Express, vol. 13, no. 4, p. 045501, Mar. 2020, doi: 10.35848/1882-0786/ab7712.DOI
  14. [14]P. Ranga, A. Bhattacharyya, A. Chmielewski, S. Roy, N. Alem, and S. Krishnamoorthy, “Delta-doped β-Ga2O3 films with narrow FWHM grown by metalorganic vapor-phase epitaxy,” Applied Physics Letters, vol. 117, no. 17, p. 172105, 2020, doi: 10.1063/5.0027827.DOI
  15. [15]P. Ranga, A. Bhattacharyya, A. Chmielewski, S. Roy, R. Sun, M. A. Scarpulla, N. Alem, and S. Krishnamoorthy, “Growth and characterization of metalorganic vapor-phase epitaxy-grown β-(AlxGa1-x)2O3/β-Ga2O3 heterostructure channels,” Appl. Phys. Express, vol. 14, no. 2, p. 025501, Jan. 2021, doi: 10.35848/1882-0786/abd675.DOI
  16. [16]P. Ranga, A. Bhattacharyya, L. Whittaker-Brooks, M. A. Scarpulla, and S. Krishnamoorthy, “N-type doping of low-pressure chemical vapor deposition grown β-Ga2O3 thin films using solid-source germanium,” Journal of Vacuum Science & Technology A, vol. 39, no. 3, p. 030404, May 2021, doi: 10.1116/6.0001004.DOI
  17. [17]A. Bhattacharyya, P. Ranga, S. Roy, J. Ogle, L. Whittaker-Brooks, and S. Krishnamoorthy, “Low temperature homoepitaxy of (010) β-Ga2O3 by metalorganic vapor phase epitaxy: Expanding the growth window,” Appl. Phys. Lett., vol. 117, no. 14, p. 142102, Oct. 2020, doi: 10.1063/5.0023778.DOI
  18. [18]Y. Zhang, F. Alema, A. Mauze, O. S. Koksalldi, R. Miller, A. Osinsky, and J. S. Speck, “MOCVD grown epitaxial β-Ga2O3 thin film with an electron mobility of 176 cm2/V s at room temperature,” APL Materials, vol. 7, no. 2, p. 022506, Dec. 2018, doi: 10.1063/1.5058059.DOI
  19. [19]G. Seryogin, F. Alema, N. Valente, H. Fu, E. Steinbrunner, A. T. Neal, S. Mou, A. Fine, and A. Osinsky, “MOCVD growth of high purity Ga2O3 epitaxial films using trimethylgallium precursor,” Appl. Phys. Lett., vol. 117, no. 26, p. 262101, Dec. 2020, doi: 10.1063/5.0031484.DOI
  20. [20]C. Wang, H. Gong, W. Lei, Y. Cai, Z. Hu, S. Xu, Z. Liu, Q. Feng, H. Zhou, J. Ye, J. Zhang, R. Zhang, and Y. Hao, “Demonstration of the p-NiOx/n-Ga2O3 Heterojunction Gate FETs and Diodes With BV2R,on Figures of Merit of 0.39 GW/cm2 and 1.38 GW/cm2,” IEEE Electron Device Letters, vol. 42, no. 4, pp. 485–488, Apr. 2021, doi: 10.1109/LED.2021.3062851.DOI
  21. [21]A. Bhattacharyya, S. Roy, P. Ranga, D. Shoemaker, Y. Song, J. S. Lundh, S. Choi, and S. Krishnamoorthy, “130 mA mm-1 β-Ga2O3 metal semiconductor field effect transistor with low-temperature metalorganic vapor phase epitaxy-regrown ohmic contacts,” Appl. Phys. Express, vol. 14, no. 7, p. 076502, Jun. 2021, doi: 10.35848/1882-0786/ac07ef.DOI
  22. [22]C. Joishi, Z. Xia, J. S. Jamison, S. H. Sohel, R. C. Myers, S. Lodha, and S. Rajan, “Deep-Recessed β-Ga2O3 Delta-Doped Field-Effect Transistors With In Situ Epitaxial Passivation,” IEEE Transactions on Electron Devices, vol. 67, no. 11, pp. 4813–4819, Nov. 2020, doi: 10.1109/TED.2020.3023679.DOI
  23. [23]C. Joishi, Y. Zhang, Z. Xia, W. Sun, A. R. Arehart, S. Ringel, S. Lodha, and S. Rajan, “Breakdown Characteristics of β-(Al0.22Ga0.78)2O3/Ga2O3 Field-Plated Modulation-Doped Field-Effect Transistors,” IEEE Electron Device Letters, vol. 40, no. 8, pp. 1241–1244, Aug. 2019, doi: 10.1109/LED.2019.2921116.
  24. [24]K. Zeng, A. Vaidaya, and U. Singisetti, “1.85 kV Breakdown Voltage in Lateral Field-Plated Ga2O3 MOSFETs,” IEEE Electron Device Letters, vol. 39, no. 9, pp. 1385–1388, Sep. 2018, doi: 10.1109/LED.2018.2859049.DOI
  25. [25]Y. Lv, H. Liu, X. Zhou, Y. Wang, X. Song, Y. Cai, Q. Yan, C. Wang, S. Liang, J. Zhang, Z. Feng, H. Zhou, S. Cai, and Y. Hao, “Lateral β-Ga2O3 MOSFETs With High Power Figure of Merit of 277 MW/cm2,” IEEE Electron Device Letters, vol. 41, no. 4, pp. 537–540, Apr. 2020, doi: 10.1109/LED.2020.2974515.
  26. [26]K. Tetzner, E. Bahat Treidel, O. Hilt, A. Popp, S. Bin Anooz, G. Wagner, A. Thies, K. Ickert, H. Gargouri, and J. Würfl, “Lateral 1.8 kV β-Ga2O3 MOSFET With 155 MW/cm2 Power Figure of Merit,” IEEE Electron Device Letters, vol. 40, no. 9, pp. 1503–1506, Sep. 2019, doi: 10.1109/LED.2019.2930189.DOI
  27. [27]N. K. Kalarickal, Z. Feng, A. F. M. Anhar Uddin Bhuiyan, Z. Xia, W. Moore, J. F. McGlone, A. R. Arehart, S. A. Ringel, H. Zhao, and S. Rajan, “Electrostatic Engineering Using Extreme Permittivity Materials for Ultra-Wide Bandgap Semiconductor Transistors,” IEEE Transactions on Electron Devices, vol. 68, no. 1, pp. 29–35, Jan. 2021, doi: 10.1109/TED.2020.3037271.DOI
  28. [28]K. Zeng, A. Vaidya, and U. Singisetti, “A field-plated Ga2O3 MOSFET with near 2-kV breakdown voltage and 520 mΩ.cm2,” Appl. Phys. Express, vol. 12, no. 8, p. 081003, Jul. 2019, doi: 10.7567/1882-0786/ab2e86.DOI
  29. [29]Y. Lv, X. Zhou, S. Long, X. Song, Y. Wang, S. Liang, Z. He, T. Han, X. Tan, Z. Feng, H. Dong, X. Zhou, Y. Su, S. Cai, and M. Liu, “Source-Field-Plated β-Ga2O3 MOSFET With Record Power Figure of Merit of 50.4 MW/cm2,” IEEE Electron Device Letters, vol. 40, no. 1, pp. 83–86, Jan. 2019, doi: 10.1109/LED.2018.2881274.DOI
  30. [30]K. D. Chabak, J. P. McCandless, N. A. Moser, A. J. Green, K. Mahalingam, A. Crespo, N. Hendricks, B. M. Howe, S. E. Tetlak, K. Leedy, R. C. Fitch, D. Wakimoto, K. Sasaki, A. Kuramata, and G. H. Jessen, “Recessed-Gate Enhancement-Mode β-Ga2O3 MOSFETs,” IEEE Electron Device Letters, vol. 39, no. 1, pp. 67–70, Jan. 2018, doi: 10.1109/LED.2017.2779867.DOI

Paper details

vlnc:W_m32awaed
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents