betaFeedback

WorksPhysics and Astronomy

Optical Spin Sensing and Metamagnetic Phase Control in the 2D Van der Waals Magnet Yb3+-Doped CrPS4

Abstract

The emergence of two-dimensional magnets within the van der Waals toolkit has introduced unprecedented opportunities to develop ultrathin spintronic technologies. Strong coupling between spin and optical properties in such materials can further enable novel spin-photonic capabilities of both fundamental and technological interest. Here, we investigate the optical and spin properties of the air-stable, layered A-type antiferromagnet chromium thiophosphate (CrPS4) when doped with Yb3+. We show that the collective spin properties of CrPS4 are encoded in the sharp f-f luminescence of isolated Yb3+ dopants via strong magnetic superexchange coupling between the two, and that spontaneous magnetic ordering in CrPS4 induces large exchange splittings in the narrow Yb3+ f-f photoluminescence features below TN. Spin reorientation in CrPS4 via a "spin-flop" metamagnetic transition modulates the Yb3+ f-f luminescence energies and exchange splittings. This pronounced link between spin and optical properties enables the demonstration of optically driven spin-flop transitions in CrPS4.

Main Text

The layered van der Waals (vdW) magnet, CrPS4_4, is an emerging material showing exotic magneto-electronic properties including voltage-modulated electron tunneling,[1, 2, 3] spin-polarized transport,[4, 5] and magnetoconductance.[5, 6] Its in-plane anisotropy allows anisotropic tunneling magnetoresistance,[7, 8, 9] anisotropic magnon transport[10] and magnon chirality switching,[11] anisotropic linear- and nonlinear optical responses,[12] and it shows saturable absorption.[13] CrPS4_4 also exhibits rich, structured photoluminescence (PL),[14, 15, 16, 17] but unlike other 2D magnetic materials this PL shows almost no response to applied magnetic fields.[14] Recently, magnetic circularly polarized luminescence (MCPL) was shown to track the out-of-plane magnetization of CrPS4_4,[18] but the polarization response is weak.

The CrPS4\mathrm{CrPS}_{4} lattice consists of highly anisotropic 2D layers involving parallel 1D chains of edge-sharing [CrS6]3−[\mathrm{CrS}_{6}]^{3-} octahedra separated by S-P-S bridges, alternating between two crystallographically distinct Cr3+\mathrm{Cr}^{3+} sites. [19] No other MPS4\mathrm{MPS}_{4} or MPS3\mathrm{MPS}_{3} compound shares this structure.[20, 21] Magnetic susceptibility[22, 23] and neutron diffraction[24] have established that each monolayer orders ferromagnetically with its Cr3+\mathrm{Cr}^{3+} moments nearly perpendicular to the 2D plane, and neighboring monolayers couple antiferromagnetically below a Néel temperature (TNT_{\mathrm{N}}) of ∼\sim36 K, making bulk CrPS4\mathrm{CrPS}_{4} an A-type antiferromagnet. An abrupt metamagnetic spin-flop transition (SFT) is observed with B∥cB \parallel c (out-of-plane) of ∼\sim1 T at 5 K, reorienting all spins into the 2D plane while retaining antiferromagnetic interlayer coupling. Higher magnetic fields progressively cant the Cr3+\mathrm{Cr}^{3+} spins back out of plane until full ferromagnetic (FM) alignment is reached at ∼\sim8 T. Exfoliation down to mono- or few-layer structures reveals layer-dependent magnetism, with even- and odd-layer structures alternating between zero and non-zero magnetic moments, respectively.[25]

Lanthanides doped into crystals have attracted broad attention as phosphors, laser gain media, and more recently, as spin-bearing optical impurities for potential quantum information applications. Screening of their spectroscopically active 4f4f valence electrons imparts trivalent lanthanides with narrow optical linewidths, high PL quantum yields, and long spin- and optical-coherence times,[26, 27] enabling optical quantum memory,[28, 29, 30] microwave-to-optical quantum transduction,[31] and coherent manipulation and optical readout of individual spins.[32] In many instances, magnetic fields are applied to split spin degeneracies for optical spin initialization. Whereas CrPS4\mathrm{CrPS}_{4} doping remains wholly unexplored, lanthanide (Yb3+\mathrm{Yb}^{3+}) doping of other 2D magnets (CrI3\mathrm{CrI}_{3}, CrBr3\mathrm{CrBr}_{3}) was recently established as a route to novel spin-photonic properties,[33, 34] including spontaneous splittings of Yb3+\mathrm{Yb}^{3+} Kramers spin degeneracies via superexchange coupling with the surrounding lattice. This work prompts the investigation of 2D magnets showing exotic metamagnetic properties, such as CrPS4\mathrm{CrPS}_{4}.

Here we demonstrate that doping with even small amounts (<1% vs Cr3+\mathrm{Cr}^{3+}) of Yb3+\mathrm{Yb}^{3+} quenches the native CrPS4\mathrm{CrPS}_{4} PL and generates strong sensitized Yb3+\mathrm{Yb}^{3+} ff-ff PL. Low-temperature PL measurements at zero magnetic field show complex fine structure attributable to Yb3+\mathrm{Yb}^{3+} substituting at the two Cr3+\mathrm{Cr}^{3+} lattice sites, each showing well-resolved spin splittings due to superexchange coupling with surrounding Cr3+\mathrm{Cr}^{3+} ions. These Yb3+\mathrm{Yb}^{3+} dopants show an extraordinarily strong optical response to the CrPS4\mathrm{CrPS}_{4} spin-flop transition, with large PL energy shifts and effective gg values reaching ∼\sim170. Exploiting this strong coupling between optical and magnetic properties, we demonstrate the use of Yb3+\mathrm{Yb}^{3+} PL to detect and quantify photothermally driven CrPS4\mathrm{CrPS}_{4} spin-flop transitions. These results expand upon the spin-photonic functionality known for lanthanides and the optical functionalities known for 2D magnets, with interesting potential ramifications for photo-spintronics and quantum information sciences.

Results and Analysis

CrPS4\mathrm{CrPS}_{4} and Yb3+\mathrm{Yb}^{3+}-doped CrPS4\mathrm{CrPS}_{4} (Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4}) crystals were grown by chemical vapor transport, and Yb3+\mathrm{Yb}^{3+} concentrations were measured by inductively coupled plasma mass spectrometry (ICP-MS, see Methods). Figure 1a shows X-ray diffraction (XRD) data collected on a single-crystal flake of 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} using a powder diffractometer, alongside a reference powder pattern for undoped CrPS4\mathrm{CrPS}_{4}. The XRD peak positions of the doped sample align well with those of the reference. The (00l)(00l) peaks are relatively more intense than in the reference pattern, reflecting orientation of the flake with its cc-axis normal to the substrate. Figure 1b shows the Raman spectrum collected from a 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} flake, with red and blue labels indicating literature peak assignments.[35, 36] The inset shows a photograph of a representative Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} flake. At this low doping level, the XRD, Raman, and crystal morphologies of CrPS4\mathrm{CrPS}_{4} and Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} are essentially indistinguishable.

Image not extracted

Figure 1. (a) XRD data collected on a 0.2%0.2\% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} single crystal using a powder diffractometer. A reference powder diffraction pattern for CrPS4\mathrm{CrPS}_{4} is shown for comparison (red, ICSD Coll. Code 937). The experimental (00l)(00l) peaks are disproportionately strong, consistent with orientation of the 2D planes parallel to the substrate. (b) Raman spectrum collected from a 0.2%0.2\% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} single crystal using unpolarized 532 nm excitation. Peaks are assigned based on refs. [35, 36]. Intensities of the reference Raman lines are scaled arbitrarily to guide the eye. The inset shows a photograph of a representative Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} flake. (c) The 4 K structure of CrPS4\mathrm{CrPS}_{4}, showing alternation between two pseudooctahedral Cr3+\mathrm{Cr}^{3+} sites (Cr1 and Cr2) with different Cr-S bond lengths (from ref. [24]).

The low-temperature PL spectrum of undoped CrPS4\mathrm{CrPS}_{4} has been described in depth previously.[14, 15, 16, 37] This spectrum shows multiple evenly spaced peaks between 10500 and 11000 cm−1\mathrm{cm}^{-1} that have been attributed to vibronic coupling, as well as additional rich fine structure at the lowest temperatures.[14, 15] This spectrum also typically shows a broad trap feature near 9000 cm−1\mathrm{cm}^{-1}, although as emphasized previously,[37] many reports do not adequately account for this low-energy emission.

Figure 2a compares the PL spectrum of a 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} crystal measured at 36 K with that of an undoped CrPS4\mathrm{CrPS}_{4} crystal measured under the same conditions. This temperature was chosen for simplicity because the additional CrPS4\mathrm{CrPS}_{4} PL fine structure observed at lower temperatures is unrelated. In the PL spectrum of 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4}, the signature features of undoped CrPS4\mathrm{CrPS}_{4} are replaced by a series of narrow peaks between 9000 and 10100 cm−1\mathrm{cm}^{-1} that are characteristic of Yb3+\mathrm{Yb}^{3+} ff-ff luminescence. Replotting the high-energy part of the Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} PL spectrum with intensities magnified 2000x reveals that the native PL of CrPS4\mathrm{CrPS}_{4} is still present, just very weak. Integration shows that >99.9% of the PL intensity now comes from Yb3+\mathrm{Yb}^{3+}-centered transitions. With only one Yb3+\mathrm{Yb}^{3+} impurity per ~500 Cr3+\mathrm{Cr}^{3+} ions at 0.2% doping, this result indicates extensive exciton diffusion within CrPS4\mathrm{CrPS}_{4}.

PL spectra of CrPS4 and Yb3+:CrPS4

Figure 2. (a) 36 K PL spectrum of CrPS4\mathrm{CrPS}_{4} (red) and 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} (black) single crystals. The dashed curve plots the same PL spectrum of 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} scaled

up 2000x. (b) 4 K PL spectrum of the Yb3+ 2F5/2→2F7/2\mathrm{Yb}^{3+}\ {}^{2}\mathrm{F}_{5/2} \to{}^{2}\mathrm{F}_{7/2} PL from the 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4_4 crystal plotted on an expanded scale. The brackets denote the primary features identified for two distinct Yb3+\mathrm{Yb}^{3+} doping sites, A and B, using site-selective photoexcitation. All 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4_4 PL data were measured using unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^2. The CrPS4_4 spectrum was measured using unpolarized pulsed 470 nm photoexcitation (6.3 nJ per 3 ns pulse, 40 MHz, average power density of 2.1 W/cm2^2, E⃗⊥c\vec{E} \perp c).

The 2F{}^{2}\mathrm{F} free-ion term of Yb3+\mathrm{Yb}^{3+} (4f13f^{13} configuration) is split into 2F5/2{}^{2}\mathrm{F}_{5/2} and 2F7/2{}^{2}\mathrm{F}_{7/2} terms by strong spin-orbit coupling (~10000 cm−1^{-1}), and each of these is split by the low-symmetry crystal field in CrPS4_4 (~500 cm−1^{-1}) to yield a Kramers-doublet ground state, denoted 2F7/2(0){}^{2}\mathrm{F}_{7/2}(0), and a series of Kramers doublet excited states. Figure 2b plots the 4 K PL spectrum of the Yb3+\mathrm{Yb}^{3+}-doped sample from Figure 2a on an expanded energy scale. This spectrum is complex, showing more peaks than anticipated for a distorted octahedral Yb3+\mathrm{Yb}^{3+} ion. Using site-selective laser excitation of Yb3+\mathrm{Yb}^{3+}, two species could be identified in the PL (A and B, Figure 2b, Figure S1-Figure S2). These species are assigned to substitutional Yb3+\mathrm{Yb}^{3+} in the two distinct Cr3+\mathrm{Cr}^{3+} lattice sites of CrPS4_4. Site B contributes most of the PL intensity, with Site A PL ~10x weaker (Figure 2b), suggesting preferential B-site doping. Yb3+\mathrm{Yb}^{3+} is much larger than Cr3+\mathrm{Cr}^{3+}; the smaller crystal-field splitting for Yb3+\mathrm{Yb}^{3+} in Site B suggests association of this site with the less-constrained Cr1 lattice site illustrated in Figure 1c. These structural differences may also contribute to the shorter 4 K PL decay time of Yb3+\mathrm{Yb}^{3+} in Site A (51 μs) compared to Site B (82 μs) (Figure S1). Even accounting for these two sites, the spectrum shows more peaks than expected. In particular, two peaks are observed at the highest-energy electronic origins of both A- and B-site Yb3+\mathrm{Yb}^{3+} PL (centered at 10075 and 9980 cm−1^{-1} at 4 K, respectively), suggesting that their ground-state Kramers degeneracies are lifted by coupling with the surrounding lattice. Unlike in most materials, Yb3+\mathrm{Yb}^{3+} dopants in CrPS4_4 thus do not possess time-reversal symmetry at 4 K, despite the bulk antiferromagnetism.

Site-selective photoluminescence spectra and decay curves

Figure S1. (a) Site-selective PL spectra of a 0.2% Yb3+^{3+}:CrPS4_4 single crystal (same as Figure 3) measured at 20 K using a tunable, CW Ti:sapphire laser (∼\sim20 mW/cm2^2). The red spectrum was obtained with excitation at 10834 cm−1^{-1} (923 nm) and the black spectrum was obtained with excitation at 10582 cm−1^{-1} (945 nm). (b) Individual PL spectra of Yb3+^{3+} in Sites A and B, obtained by deconvolution of the spectra in panel (a). (c) Site-selective PL decay curves measured for the Yb3+^{3+} 0′→00^\prime\to0 transitions of Sites A (black, 10080 cm−1^{-1}) and B (red, 9980 cm−1^{-1}) with 0.1 nm spectral bandwidth, showing that the two sites have different decay times. Lifetimes are determined by fitting the PL decay curves to a monoexponential decay function. Pulsed photoexcitation was performed using the 532 nm output of a frequency doubled Nd:YAG laser (50 Hz, 30 ps pulse duration, 4 nJ pulse energy) with a 100 cm−1^{-1} bandwidth.

Site-selective PLE and PL spectra of Yb$^{3+}$:CrPS$_4$

Figure S2. (a) Site-selective PLE spectra of a 0.2% Yb3+^{3+}:CrPS4_4 single crystal (same as Figure 3) measured at 4 K. The red spectrum was obtained with detection at 9302.3 cm−1^{-1} and the black spectrum was obtained with detection at 9451.8 cm−1^{-1}. (b) PLE spectra of the individual Yb3+^{3+} Sites A and B, obtained by deconvolution from the spectra presented in panel (a). (c) PL and PLE spectra of the Yb3+^{3+} 0′ ↔ 0 transitions. PL was measured with unpolarized CW 15803 cm−1^{-1} (632.8 nm) photoexcitation at 5 mW/cm2^{2}. PLE was measured using a tunable, CW Ti:Sapphire laser (5-50 mW/cm2^{2}) while monitoring PL at 9451.8 cm−1^{-1}, where both sites emit.

To illustrate, Figure 3 summarizes variable-temperature PL data collected for the 0.2% Yb3+\mathrm{Yb}^{3+}:CrPS4_4 crystal from Figure 2, focusing on the first electronic origins of each Yb3+\mathrm{Yb}^{3+} site. Figure 3a shows PL spectra for Yb3+\mathrm{Yb}^{3+} in Site A collected from 4 to 75 K and plotted spectrally and as a heat map (see Figure S3 for complete data set). At 4 K, two peaks denoted α\alpha and β\beta are observed. With increasing temperature, both peaks broaden and β\beta shifts to higher energy. Concurrently, a pair of hot bands (peaks αH\alpha^{\mathrm{H}} and βH\beta^{\mathrm{H}}) emerges at higher energy, gaining intensity and shifting to lower energy with increasing temperature. Peaks α\alpha and β\beta are assigned as PL transitions to the two spin components of an exchange-split ground 2F7/2(0){}^{2}\mathrm{F}_{7/2}(0) Kramers doublet (denoted 0+0^{+} and 0−0^{-}), as summarized in the inset to Figure 3a. Likewise, peaks αH\alpha^{\mathrm{H}} and βH\beta^{\mathrm{H}} are assigned to PL originating from the thermally populated upper level of the exchange-split 2F5/2(0′){}^{2}F_{5/2}(0^{\prime}) excited-state doublet (denoted 0′+0^{\prime+}). The temperature-dependence of these PL intensities (Figure S4) supports these assignments. Figure 3 shows that the splitting energies between 0+0^{+} and 0−0^{-} (denoted ΔE\Delta E) and between 0′+0^{\prime+} and 0′−0^{\prime-} (denoted ΔE′\Delta E^{\prime}) decrease as the temperature increases from 4 K to the CrPS4_4 Néel temperature, where they abruptly stop being temperature dependent. This result demonstrates a strong sensitivity of the Yb3+^{3+} PL to the spin correlations that emerge spontaneously below TNT_{\mathrm{N}} in CrPS4_4. Figure 3b plots energy differences between select peaks in Figure 3a. Per the peak assignments, E(α)−E(β)E(\alpha)-E(\beta) and E(αH)−E(βH)E(\alpha^{\mathrm{H}})-E(\beta^{\mathrm{H}}) both equal ΔE\Delta E, whereas E(αH)−E(α)E(\alpha^{\mathrm{H}})-E(\alpha) and E(βH)−E(β)E(\beta^{\mathrm{H}})-E(\beta) both equal ΔE′\Delta E^{\prime}. Because no external magnetic field is used, these splittings are solely due to magnetic exchange coupling, such that ΔE=ΔEexch\Delta E=\Delta E_{\mathrm{exch}} and ΔE′=ΔEexch′\Delta E^{\prime}=\Delta E^{\prime}_{\mathrm{exch}}. Figure 3b plots the temperature dependence of ΔEexch\Delta E_{\mathrm{exch}} and ΔEexch′\Delta E^{\prime}_{\mathrm{exch}}. ΔEexch=11 cm−1\Delta E_{\mathrm{exch}}=11\ \mathrm{cm}^{-1} at 4 K and decreases with increasing temperature until TNT_{\mathrm{N}} before becoming independent of temperature at a value of 7.5 cm−17.5\ \mathrm{cm}^{-1}. Similarly, ΔEexch′=27 cm−1\Delta E^{\prime}_{\mathrm{exch}}=27\ \mathrm{cm}^{-1} at 4 K and decreases with temperature until plateauing at 19 cm−119\ \mathrm{cm}^{-1} above TNT_{\mathrm{N}}. As also seen in Yb3+^{3+}:CrBr3_3, [34] ΔEexch\Delta E_{\mathrm{exch}} remains non-zero even in the paramagnetic regime because the dominant Yb3+^{3+}-Cr3+^{3+} exchange interactions are short-range and even random spin disorder leads to net Cr3+^{3+} spin around Yb3+^{3+} dopants. Above ∼75\sim75 K, the Yb3+^{3+} PL intensity and decay time both drop, indicating thermally activated nonradiative losses (Figure S5).

False-color plots, PL spectra, and temperature-dependent splitting energies for Yb$^{3+}$ in Sites A and B

Figure 3. (a) Top: False-color plot of the PL intensity from 4 to 75 K for the 0′ →\to 0 PL peaks of Yb3+^{3+} in Site A of a 0.2% Yb3+^{3+}:CrPS4_4 single crystal. The overlayed data points mark the energies of αH\alpha^{H} and βH\beta^{H} (red) and α\alpha and β\beta (blue) peaks, determined by deconvolution (Figure S6). The dashed white line indicates TN=36T_{\mathrm{N}} = 36 K for CrPS4_4. Bottom: The PL spectra used to make the false-color plot above. The inset illustrates the specific PL transitions observed between exchange-split Yb3+^{3+} states at the 0′ →\to 0 electronic origin. (b) Temperature dependence of ΔEexch\Delta E_{\mathrm{exch}} and ΔEexch′\Delta E'_{\mathrm{exch}} for Yb3+^{3+} at Site A, determined from the data in panel (a) as described in the main text. (c) Same as panel (a) but for Yb3+^{3+} in Site B. (d) Same as panel (b) but for Site B. The red x symbols at 4.6 K in panels (b) and (d) show data points collected in a helium immersion cryostat (Figure 4, Figure S8), which agree well with the data collected in a closed-cycle cryostat and confirm the accuracy of the sample temperature readings in the latter. All PL data were measured using unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^{2} with E⃗⊥c\vec{E} \perp c.

Spectral deconvolution of photoluminescence spectra for Yb$^{3+}$-doped CrPS$_4$

Figure S6. Spectral deconvolution of PL spectra of a 0.2% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 3) in the region of the 0′→00' \to0 transition for each Yb3+^{3+} site, for three sample temperatures (8 K, 24 K, and 50 K). (a) Site A; deconvolution was performed by least-squares fitting to four Lorentzian peaks and a cubic baseline. (b) Site B; deconvolution was performed by least-squares fitting to three Gaussian peaks (β\beta, αH\alpha^{\mathrm{H}}, βH\beta^{\mathrm{H}}) and one Lorentzian peak (α\alpha), with a constant baseline. Peak positions from this fitting are used in the heat maps of Figure 3a,Figure 3c and to determine ΔEexch\Delta E_{\mathrm{exch}} and ΔEexch′\Delta E'_{\mathrm{exch}} energies in Figure 3b,Figure 3d.

Variable-temperature PL spectra of a 0.2% $\mathrm{Yb}^{3+}$-doped $\mathrm{CrPS}_{4}$ single crystal

Figure S3. Variable-temperature PL spectra of a 0.2% Yb3+\mathrm{Yb}^{3+}-doped CrPS4\mathrm{CrPS}_{4} single crystal (same as Figure 3) collected with unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^{2}.

Temperature dependence of hot-band photoluminescence intensities for Site A and Site B

Figure S4. Figure S4. Temperature dependence of hot-band PL intensities from a 0.2% Yb3+Yb^{3+}-doped CrPS4CrPS_4 single crystal (same as Figure 3), plotted as IαH+βH/Iα+βI_{\alpha^{H}+\beta^{H}/I_{\alpha+\beta}} vs temperature. Iα+βI_{\alpha+\beta} represents the integrated area of the combined peaks α\alpha and β\beta (cold bands) for a given Yb3+Yb^{3+} site (Site A or B), and IαH+βHI_{\alpha^{H}+\beta^{H}} represents the integrated area of the combined peaks αH\alpha^{H} and βH\beta^{H} (hot bands) for the same site, as determined by the deconvolution described in Figure S6. (a) Site A data. (b) Site B data.

Temperature dependence of Yb$^{3+}$ photoluminescence intensity and decay time

Figure S5. Temperature dependence of (black) the integrated intensity of the entire Yb3+^{3+} PL spectrum (10200 – 9200 cm−1^{-1}) and (green) the PL decay time measured at 9970 ±\pm 50 cm−1^{-1} (Site B, both α\alpha and β\beta transitions) of a 0.2% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 3). PL was measured with CW 632.8 nm photoexcitation at 5 mW/cm2^2 exciting the CrPS4_4 lattice. PL decay was collected using the 532 nm output of a frequency doubled Nd:YAG laser (50 Hz, 30 ps pulse duration, 4 nJ pulse energy) for excitation. All other major spectroscopic features assigned to Site B were also measured at 4 K and have very similar decay times with slight variation, likely due to partial overlap with Site A features. The divergence between Yb3+^{3+} PL intensities and lifetimes as temperature is lowered below ∼100\sim100K suggests a decreasing quantum efficiency of sensitization at lower temperatures.

Figure 3c,Figure 3d show parallel PL data for the first electronic origin of Yb3+\mathrm{Yb}^{3+} in Site B. The same trends in peak energies, hot-band intensities, and peak broadening are all apparent. Like in Site A, ΔEexch\Delta E_{\mathrm{exch}} and ΔEexch′\Delta E'_{\mathrm{exch}} also decrease from their maximum values (17 and 33 cm−1^{-1}, respectively) at 4 K until TNT_{\mathrm{N}} and then become temperature-independent (at ΔEexch=7.5\Delta E_{\mathrm{exch}} = 7.5 and 16 cm−1^{-1}, respectively). Site B shows larger exchange splittings than Site A despite its smaller 2F7/2{}^{2}F_{7/2} crystal-field splitting, and its discontinuity in ΔEexch′′\Delta E^{\prime\prime}_{\mathrm{exch}} at TNT_{\mathrm{N}} is more abrupt. Because of the similarity between Site A and B data, the rest of this manuscript focuses on characterization of the majority Site B, with additional Site A data provided as Supplementary Material. Overall, the data in Figure 3 demonstrate that the PL of the Yb3+\mathrm{Yb}^{3+} impurities is strongly correlated with the spin properties of the CrPS4\mathrm{CrPS}_{4} lattice, indicating both optical and magnetic integration of this spin-bearing point defect into the material.

To probe this magnetic integration in more detail, PL measurements were performed under applied magnetic fields (B∥cB \parallel c). Figure 4 summarizes data for the α\alpha and β\beta peaks of Site B in 0.02% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} (see Figure S7 for the full data set, Figure S8 for Site A data). Figure 4a plots 4.6 K PL spectra collected at select field strengths between 0 and 6 T. Very little changes at low field until around 0.93 T, where the α\alpha and β\beta peaks broaden and shift to higher energy. By 1.05 T, both peaks have shifted by about +10 cm−1^{-1} and structure appears in the α\alpha peak (Figure S9, S10). At 2 T, the peak broadening has mostly subsided again. The heat map in Figure 4b highlights the abruptness of these spectral changes at low magnetic fields. This unusual field dependence is attributable to the metamagnetic spin-flop transition (SFT) of CrPS4\mathrm{CrPS}_{4}, in which Cr3+\mathrm{Cr}^{3+} spin vectors concertedly rotate from out-of-plane to in-plane orientations while retaining the interlayer antiferromagnetic coupling (A-AFM →\to cAFM). This spin reorientation affects the Yb3+\mathrm{Yb}^{3+} PL energies because of the strong prolate anisotropy of Yb3+\mathrm{Yb}^{3+}. The SFT field (BSFTB_{\mathrm{SFT}}) and its abruptness observed optically are both consistent with magnetic susceptibility results. [22, 38] The peak broadening and resolved structure at intermediate fields reveal the presence of magnetic domains with slightly different BSFTB_{\mathrm{SFT}} values. From 2 to 6 T, α\alpha and β\beta gradually shift to lower energy and sharpen further as Cr3+\mathrm{Cr}^{3+} spins cant out of plane, and by 6 T the spectrum again bears similarity to the 0 T spectrum. These results highlight the high sensitivity of Yb3+\mathrm{Yb}^{3+} PL as an optical probe of CrPS4\mathrm{CrPS}_{4} magnetism.

Variable-field photoluminescence spectra and magnetic-field response

Figure 4. (a) 4.6 K variable-field PL spectra in the region of the α\alpha and β\beta peaks for Yb3+\mathrm{Yb}^{3+} dopants at Site B of an oriented 0.02% Yb3+\mathrm{Yb}^{3+}:CrPS4\mathrm{CrPS}_{4} single crystal. (b) False-color plot of the PL intensities vs magnetic field strength in the region of the α\alpha and β\beta peaks for Site B. (c) Plot of ΔE\Delta E vs magnetic field strength for Site B. Determination of the peak energies is described in Figure S9 and Figure S10. The inset illustrates the Cr3+\mathrm{Cr}^{3+} spin order vs magnetic field strength. For all panels, data were measured at 4.6 K using unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^{2} with E⃗⊥c\vec{E} \perp c and B∥cB \parallel c.

Spectral deconvolution of variable-field PL spectra for Sites A and B

Figure S10. Spectral deconvolution of variable-field PL spectra of a 0.02% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 4) in the region of the α\alpha and β\beta peaks for Sites A and B at 4.6 K. (a) Site A: deconvolution is performed by least-squares fitting to a linear baseline and two Gaussian peaks. (b) Site B: deconvolution is performed by least-squares fitting to a linear baseline and two Gaussian peaks. Peak positions obtained from this fitting are plotted in Figure S9 and used to determine the ΔE\Delta E values plotted in Figure 4c and Figure S8. The same analysis (data not shown) was performed for the data collected at 16 K but with four Gaussian peaks and was used to plot the peak position and ΔE\Delta E and ΔE′\Delta E' splittings in Figure S9 and Figure S11.

Variable-field photoluminescence spectra from 0.00 T to 6.00 T, with PL Intensity (rel.) versus Energy (cm^{-1})

Figure S7. 4.6 K variable-field PL spectra of a 0.02% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 4) measured with unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^{2}. The magnetic field, incident excitation, and emission collection axes are all parallel to the crystallographic cc-axis.

Variable-field photoluminescence spectra and intensity plots for Site A

Figure S8. (a) Variable-field PL spectra in the region of the α\alpha and β\beta peaks for Site A. (b) False-color plot of the PL intensities vs magnetic field strength in the region of the α\alpha and β\beta peaks for Site A. (c) Plot of ΔE\Delta E vs magnetic field strength for Site A. Determination of the peak energies is described in Figure S9 and Figure S10. All panels are for an oriented 0.02% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 4) measured at 4.6 K using CW 632.8 nm unpolarized photoexcitation at 5 mW/cm2^{2} with the incident optical and magnetic-field axes oriented parallel to the crystallographic cc-axis.

Plots of peak energies for Sites A and B at 4.6 K and 16 K

Figure S9. (a) Plots of α\alpha and β\beta peak energies for Site AA vs BB at 4.6 K. (b) Plots of α\alpha and β\beta peak energies for Site BB vs BB at 4.6 K. (c) Plots of α\alpha and β\beta peak energies for Site AA vs BB at 16 K. (d) Plots of αH\alpha^{H} and βH\beta^{H} peak energies for Site AA vs BB at 16 K. (c) Plots of α\alpha and β\beta peak energies for Site BB vs BB at 16 K. (c) Plots of αH\alpha^{H} and βH\beta^{H} peak energies for Site BB vs BB at 16 K. All data sets were collected from a 0.02% Yb3+\mathrm{Yb}^{3+}-doped CrPS4\mathrm{CrPS}_{4} single crystal (same as Figure 4) using CW 632.8 nm unpolarized photoexcitation at 5 mW/cm2\mathrm{mW}/\mathrm{cm}^{2}. Peak energies were determined by spectral deconvolution (see Figure S10).

Applying a magnetic field introduces an additional Zeeman term to each doublet's energy splitting, such that ΔE=ΔEexch+ΔEZ\Delta E = \Delta E_{\mathrm{exch}} + \Delta E_{\mathrm{Z}} (and likewise for ΔE′\Delta E'). Figure 4c plots ΔE\Delta E vs BB for the ground state of Yb3+\mathrm{Yb}^{3+} in Site B, measured at 4.6 K. These data show a dramatic derivative-shaped response at BSFTB_{\mathrm{SFT}}. The initial dip in ΔE\Delta E comes from the β\beta peak shifting at slightly lower BB than the α\alpha peak. ΔE\Delta E then jumps abruptly by ∼+3\sim+3 cm−1^{-1} at BSFTB_{\mathrm{SFT}}. Above 1 T, ΔE\Delta E changes very slowly again up to 6 T. ∂(ΔE)/∂B\partial(\Delta E)/\partial B maximizes at +37+37 cm−1^{-1}/T at BSFTB_{\mathrm{SFT}}, corresponding to an effective gg value of geff=+79g_{\mathrm{eff}} = +79 and indicating a very high sensitivity to the external magnetic field.

Although the excited-state splitting is not measurable by PL at 4.6 K, the αH\alpha^{\mathrm{H}} and βH\beta^{\mathrm{H}} hot bands observed at 16 K allow analysis of both ΔE′\Delta E' and ΔE\Delta E at this temperature (Figure S11). In these data, ΔE′\Delta E' jumps by ca. −21-21 cm−1^{-1} at BSFTB_{\mathrm{SFT}}, compared to ΔE≈+2.5\Delta E \approx+2.5 cm−1^{-1} for the ground state at the same temperature, with (∂(ΔE′)/∂B)max⁡=−80 cm−1/T(\partial(\Delta E')/\partial B)_{\max} = -80\ \mathrm{cm}^{-1}/\mathrm{T} at BSFTB_{\mathrm{SFT}} (geff=−172g_{\mathrm{eff}} = -172) compared to (∂(ΔE)/∂B)max⁡=+17 cm−1/T(\partial(\Delta E)/\partial B)_{\max} = +17\ \mathrm{cm}^{-1}/\mathrm{T} (geff=+40g_{\mathrm{eff}} = +40) for the ground state. The luminescent excited state is thus ca. 5x more sensitive to the SFT than the ground state. The sign change of the exchange splitting reflects Yb3+\mathrm{Yb}^{3+} having oppositely signed spin components along the total angular momentum directions of its 2F7/2(0){}^{2}\mathrm{F}_{7/2}(0) and 2F5/2(0′){}^{2}\mathrm{F}_{5/2}(0') states. [34, 39] A comparison of energy levels and splittings at 4.6 and 16 K is compiled in Figure S13.

Four-panel plots of photoluminescence intensities and energy splittings at Sites A and B

Figure S11. Figure S11. (a) False-color plot of the 16 K PL intensities vs magnetic field strength in the region of the 0′ →\to 0 peaks of Yb3+\mathrm{Yb}^{3+} in Site A. The circular data points plot the energies of the αH\alpha^{\mathrm{H}} and βH\beta^{\mathrm{H}} peaks in red and of the α\alpha and β\beta peaks in blue, as determined by the spectral deconvolution described in Figure S10. (b) Same as panel (a) but at Site B. (c) Magnetic field dependence of ΔE\Delta E and ΔE′\Delta E^{\prime} for Site A, determined from the data in panel (a) as described in the main text (Figure 3) and in Figure S12. (d) Same as panel (c) but for Site B. All data were collected from a 0.02% Yb3+\mathrm{Yb}^{3+}-doped CrPS4\mathrm{CrPS}_{4} single crystal (same as Figure 4), using unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^{2}.

E(0−)≡0 cm−1(1)E(0^-) \equiv0\ \mathrm{cm}^{-1} \tag*{(1)}
E(0+)=E(α)−E(β)=δEexch+δEZ(0+)(2)E(0^+) = E(\alpha)-E(\beta) = \delta E_{\mathrm{exch}}+\delta E_Z(0^+) \tag*{(2)}
E(0′+)=E(α)=E0+δEexch(0′+)+δEZ(0′+)(3)E(0^{\prime+}) = E(\alpha) = E_0+\delta E_{\mathrm{exch}}(0^{\prime+})+\delta E_Z(0^{\prime+}) \tag*{(3)}
E(0′−)=E(αH)=E0+δEexch(0′−)+δEZ(0′−)(4)E(0^{\prime-}) = E(\alpha^{\mathrm{H}}) = E_0+\delta E_{\mathrm{exch}}(0^{\prime-})+\delta E_Z(0^{\prime-}) \tag*{(4)}
ΔEexch=δEexch(0+)−δEexch(0−)≡δEexch(0+)(5)\Delta E_{\mathrm{exch}}=\delta E_{\mathrm{exch}}(0^+)-\delta E_{\mathrm{exch}}(0^-)\equiv\delta E_{\mathrm{exch}}(0^+) \tag*{(5)}
ΔEZ=δEZ(0+)−δEZ(0−)≡δEZ(0+)(6)\Delta E_Z=\delta E_Z(0^+)-\delta E_Z(0^-)\equiv\delta E_Z(0^+) \tag*{(6)}
ΔE=ΔEexch+ΔEZ(7)\Delta E=\Delta E_{\mathrm{exch}}+\Delta E_Z \tag*{(7)}
ΔEexch′=δEexch(0′−)−δEexch(0′+)(8)\Delta E'_{\mathrm{exch}}=\delta E_{\mathrm{exch}}(0^{\prime-})-\delta E_{\mathrm{exch}}(0^{\prime+}) \tag*{(8)}
ΔEZ′=δEZ(0′−)−δEZ(0′+)(9)\Delta E'_Z=\delta E_Z(0^{\prime-})-\delta E_Z(0^{\prime+}) \tag*{(9)}
ΔE′=ΔEexch′+ΔEZ′(10)\Delta E'=\Delta E'_{\mathrm{exch}}+\Delta E'_Z \tag*{(10)}

Figure S12. Figure S12. Energy-level diagram showing PL transitions between exchange-split Yb3+^{3+} states. E(0−)E(0^-) is defined as 0 cm−1^{-1} (eq S1), and E(0+)E(0^+), E(0′+)E(0^{\prime+}), and E(0′−)E(0^{\prime-}) are defined by eqs S2-4 as illustrated in the diagram. E0E_0 represents the combination of spin-orbit and crystal-field energies that place the 2F5/2(0′)^2\mathrm{F}_{5/2}(0') excited state ca. 10,000 cm−1^{-1} above the 2F7/2(0)^2\mathrm{F}_{7/2}(0) ground state in the absence of magnetic-exchange or Zeeman contributions to these energies. ΔEexch\Delta E_{\mathrm{exch}} represents the magnetic-exchange splitting of the 2F7/2(0)^2\mathrm{F}_{7/2}(0) ground state, and ΔEexch′\Delta E'_{\mathrm{exch}} represents the magnetic-exchange splitting of the 2F5/2(0′)^2\mathrm{F}_{5/2}(0') excited state. δEexch\delta E_{\mathrm{exch}} denotes the change in the energy of a given state relative to the ground state due to magnetic-exchange coupling. δEZ\delta E_Z denotes the change in the energy of a given state relative to the ground state due to an external magnetic field oriented perpendicular to the sample plane. The total splitting of the 2F7/2(0)^2\mathrm{F}_{7/2}(0) state resulting from the combined effects of the exchange splitting (ΔEexch\Delta E_{\mathrm{exch}}) and the Zeeman splitting (ΔEZ\Delta E_Z) is ΔE\Delta E (eq S7). The analogous variables for 2F7/2(0′)^2\mathrm{F}_{7/2}(0') (ΔEexch′\Delta E'_{\mathrm{exch}}, ΔEZ′\Delta E'_Z, ΔE′\Delta E') are defined similarly (eq S8-10).

Image not extracted

Figure S13. (a) Magnetic-field dependence of the energies of the Yb3+^{3+} 0−0^{-}, 0+0^{+}, 0′+0^{\prime+}, and 0′−0^{\prime-} states for Site A, measured from PL spectra collected at 4.6 K (circles, 0 – 6 T) and 16 K (diamonds, 0 – 1.5 T). (b) Same as panel (a) but for Site B. (c) ΔE\Delta E and ΔE′\Delta E^{\prime} values plotted vs magnetic field strength for Yb3+^{3+} in Site A, determined from the data in panel (a) following Figure S12. (d) Same as panel (c) but for Site B. All data were collected from a 0.02% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 4).

These results represent a significant improvement in sensitivity over prior optical probes of CrPS4_4 magnetism. CrPS4_4 PL energies appear insensitive to the SFT,[14] but PL polarizations allow detection of this phase transition:[18] the polarization ratio ρ=(σ−−σ+)/(σ−+σ+)\rho= (\sigma^- - \sigma^+)/(\sigma^- + \sigma^+), where σ−\sigma^- and σ+\sigma^+ are the intensities of left and right circularly polarized PL, respectively, increases from 0 to ∼2%\sim2\% crossing BSFTB_{\mathrm{SFT}}. Variable-temperature Raman data at 0 T may also show a small inflection at TNT_{\mathrm{N}} but 5 K data show no discernible inflection at BSFTB_{\mathrm{SFT}}. [18] In contrast, the α\alpha and β\beta PL peaks of Yb3+\mathrm{Yb}^{3+} dopants in CrPS4_4 shift in energy by over one linewidth crossing BSFTB_{\mathrm{SFT}}, providing extremely high sensitivity. To illustrate, Figure 5a plots the PL energy of the combined α\alpha and β\beta center of mass vs BB relative to its zero-field value. This energy shift and the value of BSFTB_{\mathrm{SFT}} both decrease as temperature increases from 4 to 36 K, above which no SFT is detected. Figure 5b summarizes these changes in a magnetic phase diagram, showing a temperature-dependent phase boundary that disappears above TN≈36T_{\mathrm{N}} \approx36 K. This optical result agrees well with analogous phase diagrams obtained from magnetic susceptibility measurements.[22, 23]

Magnetic-field dependence of Site B Yb3+ 0′ → 0 PL energies and optically driven spin-flop transition

Figure 5. (a) Magnetic-field dependence of Site B Yb3+^{3+} 0′ → 0 PL energies plotted relative to their zero-field energies, measured at various temperatures. The energies shown here represent the centers of gravity for the combined α\alpha and β\beta peaks (9940–10040 cm−1^{-1}). Data were collected using 5 mW/cm2^2 of unpolarized CW 632.8 nm photoexcitation with and without co-excitation from an unpolarized 405 nm, 140 W/cm2^2 "control" LED. (b) False-color plot of the data in panel (a). The green data points indicate BSFTB_{\mathrm{SFT}} values at each experimental temperature. Interpolation to create the heatmap was performed using the trendlines shown in Figure S14. The horizontal dashed white line denotes TNT_{\mathrm{N}} of CrPS4_4. (c) PL spectra with and without control LED co-excitation. Black: 0 T, 4.6 K, no control LED. Dark blue: 0 T, 4.6 K, with control LED. Dashed red: 0 T, 17 K, no control LED. Gray: 0.85 T, 4.6 K, no control LED. Light blue: 0.85 T, 4.6 K, with control LED. (d) Reversible optically driven SFT obtained by modulation of the control LED in 10 s on and off intervals, measured probing Yb3+^{3+} PL with the cryostat at 4.6 K. % SFT is defined as the fractional transition from low- to high-field limits of the SFT transition, see Figure S16. (e) Schematic summary of the results from panel (d), showing optical spin-reorientation in CrPS4_4 by the control LED. All panels are for an oriented 0.02% Yb3+^{3+}:CrPS4_4 single crystal (same as Figure 4) with E⃗⊥c\vec{E} \perp c and B∥c\mathbf{B} \parallel c.

Image not extracted

Figure S14. (a) Recast version of the 12 K data in Figure 5a showing the fitting used to determine BSFTB_{\mathrm{SFT}}. The equation of the red dashed line is shown in the inset, where EE denotes the peak center shift, Emax⁡E_{\max} is the maximum shift, rr is a constant that defines the steepness of the sigmoid and is inversely related to the maximum slope, and BSFTB_{\mathrm{SFT}} defines the field at which 0.5 Emax⁡E_{\max} is reached. (b) Plot of the spin-flop field, BSFTB_{\mathrm{SFT}}, from each plot in Figure 5a of the main text, determined by fitting the data to a sigmoidal function as described in panel (a). EE represents the shift in the center of spectral intensity for the combined 0′→00' \rightarrow0 PL peaks and is used to find the field at which the midway point of the SFT occurs (BSFTB_{\mathrm{SFT}}). Plotting the field at which the maximum change in PL energy occurs (obtained from the first derivatives of the data in Figure 5a of the main text) for each temperature gives the same result. The red curve shows a polynomial best fit to BSFTB_{\mathrm{SFT}} data collected between 4.6 and 36 K, yielding the numerical results shown in the inset (units of coefficients are implicit). (c) Plot of the PL energy measured at 1.5 T relative to its value at 0 T and the same temperature for each experimental temperature shown in Figure 5a. The red curve shows a polynomial fit to the data between 4.6 and 36 K, yielding the numerical results shown in the inset (units of coefficients are implicit). The fitted curves in panels b and c were used to generate the interpolated points in the heatmap of Figure 5b.

We now use this sensitivity to demonstrate control of CrPS4_4 magnetism using light. Previously, picosecond photothermal demagnetization has been achieved across the series of analogous MPS3_3 antiferromagnets (M = Co2+^{2+}, Mn2+^{2+}, Fe2+^{2+}, Ni2+^{2+}), [40, 41, 42, 43] demonstrating effective phonon-magnon coupling in such compounds. Photoexcitation above bandgap causes the phonon temperature to increase relative to that of the magnons because of phonon-assisted absorption and nonradiative relaxation. Phonon-magnon coupling then raises the spin temperature and destroys the MPS3_3 magnetic ordering. Such optically driven demagnetization is attractive for both fundamental studies of phonon-magnon interactions and for extremely fast manipulation of correlated spins in layered quantum materials. We therefore sought to demonstrate an analogous optically driven metamagnetic phase transition in CrPS4_4, probed using the high sensitivity of the Yb3+^{3+} PL.

Figure 5c plots Yb3+^{3+}:CrPS4_4 PL spectra obtained with and without an additional "control" CW light-emitting diode (LED) exciting the sample at 405 nm. At 4.6 K and zero magnetic field, introducing the control LED simply broadens the spectrum without shifting the first peak’s energy, consistent with lattice heating. The internal temperature with the control LED on is determined to be ~17 K by comparison with variable-temperature PL spectra collected without the control LED (Figure 5c, Figure S15). Introducing a 0.85 T magnetic field yields markedly different results: the control LED now shifts both peaks to substantially higher energies, a signature of the SFT (Figure 4). Analysis of this shift (Figure S16) indicates the control LED causes a jump from 12.5 to 87% of the full field-induced SFT, and analyses of ΔE\Delta E, E(α)E(\alpha), and E(β)E(\beta) yield similar values (Figure S16). This result is quantitatively consistent with the change in magnetization between 5 and 17 K measured at 0.85 T.[22, 23] Neutron diffraction[22] shows out-of-plane spins at 0 T and 1.7 K oriented θ=9.6∘\theta= 9.6^\circ off of the crystallographic cc-axis, and magnetic susceptibility data[22, 23] suggest θ≈85∘\theta\approx85^\circ at 0.85 T and 17 K. The results in Figure 5c thus show nearly complete out-of-plane to in-plane spin reorientation driven by the control LED. Figure 5d further demonstrates that square-wave modulation of the control LED reversibly switches the CrPS4_4 spin ordering between A-AFM and cAFM phases, as summarized schematically in Figure 5e and highlighted by the blue circles at 0.85 T in Figure 5b. Overall, these results thus demonstrate optical toggling between out-of-plane and in-plane correlated spin orientations in CrPS4_4.

Image not extracted

Figure S15. (a) Variable-temperature Yb3+^{3+} PL spectra for Yb3+^{3+} in Site B, measured in the region of the 0′→00' \to0 transition from 4.6 to 20 K using unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^{2}. The black spectrum was measured at 4.6 K with photothermal heating from an unpolarized CW 405 nm "control" LED operating at 140 W/cm2^{2}. (b) Temperature dependence of the average PL energies in panel (a), obtained by integrating the PL intensities between 9940–10040 cm−1^{-1}. The star indicates the average PL energy for the photothermal (black) spectrum in panel (a), from which an internal temperature of 17 K is deduced. All data were collected from a 0.02% Yb3+^{3+}-doped CrPS4_{4} single crystal (same as Figure 4).

Image not extracted

Figure S16. (a) Magnetic-field dependence of the centers of gravity for the combined α\alpha and β\beta PL peaks for Yb3+\mathrm{Yb}^{3+} in Site B, measured under low (black, 632.8 nm, 5 mW/cm2^{2}) and high (blue, 405 nm, 140 W/cm2^{2} and 632.8 nm, 5 mW/cm2^{2}) unpolarized photoexcitation power densities at 4.6 K (i.e., with or without photothermal heating). The dashed line indicates a field strength of 0.85 T. The peak-center shift was determined from average spectral intensities by integration over the range 9940–10040 cm−1^{-1}. (b) Same as panel (a), but for the PL splitting energy, ΔE=E(α)−E(β)\Delta E = E(\alpha) - E(\beta) (cf. Fig. S12). (c) Same as panel (a), but for the energy of the α\alpha peak. (d) Same as panel (a), but for the energy of the β\beta peak. All data were collected from a 0.02% Yb3+\mathrm{Yb}^{3+}-doped CrPS4\mathrm{CrPS}_{4} single crystal (same as Figure 4).

It is noteworthy that the power density of the control LED at the sample (140 W/cm2^2) here is smaller than those reported in other recent studies of CrPS4_4 (1-400 kW/cm2^2).[15, 17, 37, 44] Even accounting for CrPS4_4 optical densities at different excitation wavelengths (405 nm here, 532 nm,[15, 17, 44] and 633 nm[17, 37]), it is evident that common excitation power densities are sufficient to drive this SFT under an appropriate magnetic field, because only a small temperature jump is required.

In addition to demonstrating excellent in situ optical spin sensitivity of Yb3+^{3+} dopants in CrPS4_4, these findings represent the first demonstration of optical spin control in CrPS4_4. Previously, magnetic switching in 2D magnets has been achieved by application of magnetic fields, electrical biases,[45, 46] and external pressure.[47] Optically induced magnetic ordering[48] and demagnetization[40, 41, 42, 43] have been demonstrated, and circularly polarized excitation has been used to invert spins in CrI3\mathrm{CrI}_{3}[49, 50], but π/2\pi/2 optical spin-reorientation (in-plane vs out-of-plane) is more challenging. The toggled π/2\pi/2 spin-reorientation demonstrated here for CrPS4\mathrm{CrPS}_{4} appears to be a unique example of light-driven correlated spin manipulation in 2D materials.

Conclusion

Doping Yb3+\mathrm{Yb}^{3+} into CrPS4\mathrm{CrPS}_{4} transforms the PL of this material by converting it to narrow sensitized ff-ff emission that is extremely sensitive to lattice spin. Site-selective PL measurements have identified Yb3+\mathrm{Yb}^{3+} dopants substituting at the two distinct Cr3+\mathrm{Cr}^{3+} lattice sites. The Yb3+\mathrm{Yb}^{3+} PL shows pronounced exchange splittings that are highly dependent on magnetic correlations within the surrounding CrPS4\mathrm{CrPS}_{4} lattice. Notably, the CrPS4\mathrm{CrPS}_{4} metamagnetic spin-flop transition induces substantial changes in Yb3+\mathrm{Yb}^{3+} PL energies and exchange splittings, allowing sensitive optical monitoring of lattice magnetism in this part of the magnetic phase diagram. This sensitivity has enabled the first demonstration of an optically driven spin-flop transition in a layered van der Waals magnet. The ability to control in-plane vs out-of-plane spin orientations using light suggests interesting opportunities for optical switching of tunneling magnetoresistance or other photo-spintronics functionality and it could enable dynamic patterning of spatially programmable spin textures with diffraction-limited feature sizes, offering novel paths toward reconfigurable quantum materials.

Methods

Synthesis of CrPS4\mathrm{CrPS}_{4} and Yb3+\mathrm{Yb}^{3+}-doped CrPS4\mathrm{CrPS}_{4} crystals. Crystals of the undoped CrPS4\mathrm{CrPS}_{4} were grown by chemical vapor transport in a manner like that described previously,[51] and Yb3+\mathrm{Yb}^{3+} doping was achieved by addition of ytterbium metal powder to the reaction mixture. A chromium chip (99.995%, lot MKCH4484) was purchased from Sigma Aldrich. The Cr chip was ground to a powder using a mortar and pestle. Red phosphorus powder (>97.0%, lot MKCS0319) was purchased from Sigma Aldrich. Sulfur powder (99.98%, lot STBL3899) was purchased from Sigma Aldrich. Ytterbium metal powder 40 mesh (99.9%) was purchased from BeanTown Chemical. All chemicals were used as received without further purification. In a typical synthesis, Yb metal (xx mmol), Cr metal (2.6 − xx mmol), P powder (2.6 mmol in P), and S8\mathrm{S}_{8} powder (1.3 mmol in S) were loaded (an xx:1−xx:1:4 mole ratio of the elements) into a quartz tube and sealed under an evacuated atmosphere. The quartz tubes were 10 cm long with inner and outer diameters of 14 and 16 mm, respectively. Sealed tubes were placed in an open-ended horizontal tube furnace with the starting materials in the hot zone set at 750 °C and the other end at a temperature of 650 °C. Samples were heated for 5 days and then allowed to cool to room temperature over a period of ca. 6 hr. Once cooled, the tubes were cracked open to yield shiny dark plate-like crystals that had formed at the cold end. Yb3+Yb^{3+} doping was confirmed by inductively coupled plasma mass spectrometry (ICP-MS) using a PerkinElmer NexION 2000B. ICP-MS samples were digested in high-purity concentrated nitric acid, followed by dilution in ultrapure H2O\mathrm{H_2O}. Yb3+Yb^{3+} doping levels are reported as a percentage relative to the total cation contents, [Yb3+]/([Cr3+]+[Yb3+])[Yb^{3+}]/([Cr^{3+}]+[Yb^{3+}]). Analytical Yb3+Yb^{3+} concentrations were ∼50\sim50 times smaller than the nominal ytterbium concentrations used in the synthesis. The Yb3+Yb^{3+} concentrations in the flakes studied here were 0.20±0.05%0.20 \pm0.05\% (Figures 1-3) and 0.020±0.005%0.020 \pm0.005\% (Figures 4-5) with the uncertainty accounting for flake-to-flake variability.

XRD measurements. As-synthesized flakes were characterized by X-ray diffraction using a Bruker D8 Discover powder diffractometer with Iμ\muS microfocus X-ray source for Cu Kα\alpha radiation (5050 kV, 11 mA). Samples were placed onto crystalline silicon substrates and measured under ambient conditions.

Raman scattering measurements. Raman measurements were performed using a Renishaw inVia Raman microscope equipped with a 1200 grooves/mm grating and a Leica DMIRBE inverted optical microscope. A 532 nm laser was used as the excitation source. The collimated monochromatic beam was focused onto the sample through a Leica objective lens. Raman-scattered light was collected by the same objective, directed into the inVia spectrometer, dispersed by the diffraction grating, and focused on a CCD camera.

Photoluminescence (PL) measurements. Single crystals of the material were placed between two sapphire disks and loaded into a closed-cycle helium cryostat. Crystals were exfoliated prior to loading to ensure fresh surfaces, and measurement samples were typically 100100-500500 μm\mu\mathrm{m} thick. Measurements were performed under high vacuum (10−610^{-6} Pa). Sample emission was focused into a monochromator with a spectral bandwidth of 1 nm for the data in Figure 2a and 0.01 nm for all other PL data. The excitation source and collection axes are both normal to the crystal face. Spectra were collected using a LN2\mathrm{LN_2}-cooled silicon CCD camera. All PL spectra were corrected for instrument response. Photoexcitation was performed using either a 632.8 nm helium-neon laser, a tunable Ti:Sapphire laser, a 532 nm Nd:YAG laser, or a 405 nm LED, as specified in the text. Where specified, polarization scrambling was achieved by passing the excitation source and sample emission through fused silica depolarizers. Unless specifically indicated otherwise, crystal orientation was not controlled relative to the excitation polarization.

Photoluminescence excitation (PLE) measurements. PLE measurements were likewise conducted in a closed-cycle helium cryostat under high vacuum. Sample emission was focused into a monochromator with a spectral bandwidth of 5 nm and emission counts were monitored using a Hamamatsu InGaAs/InP NIR photomultiplier tube. Spectra were corrected for intensity of the excitation source, measured simultaneously using a calibrated Si diode.

Magneto-PL measurements. Individual sample flakes were placed between two quartz disks and loaded into a Cryo-Industries SMC-1650 OVT superconducting magneto-optical cryostat oriented in the Faraday configuration. The magnetic field was applied parallel to the crystallographic cc-axis. Sample emission was collected along the magnetic field axis and focused into a fiber-optic cable. Sample emission was then passed through a monochromator with a spectral bandwidth of 0.25 nm and detected using a LN2\mathrm{LN_2}-cooled silicon CCD camera. Field-sweep measurements were performed by measuring sample emission every 1 s while continuously sweeping the magnetic field at a rate of 4 mT/s.

Acknowledgments

This research was primarily supported by the University of Washington Molecular Engineering Materials Center, a U.S. National Science Foundation Materials Research Science and Engineering Center (DMR-2308979). Part of this work was conducted at the Molecular Analysis Facility, which is supported in part by funds from the Molecular Engineering & Sciences Institute, the Clean Energy Institute, the National Science Foundation (NNCI-2025489 and NNCI-1542101).

Contributions

JTB and DRG conceived of this work. JTB led all aspects of experimentation with the support of other authors: KP (magneto-PL, data analysis), NJA (laser PLE, magneto-PL), FH (Raman analysis), TJS (crystal synthesis, ICP-MS, magneto-PL), RB (PL, data analysis). The manuscript was prepared by JTB and DRG in consultation with all other authors. DRG supervised the project. All authors read and commented upon the manuscript.

Data Availability

The original experimental data presented in this work will be made freely available at https://doi.org/10.5281/zenodo upon manuscript acceptance.

Corresponding Authors

Correspondence to Daniel R. Gamelin.

Competing Interests

The authors declare no competing interests.

Supplementary Information

Supplementary Figures S1-S17.

Image not extracted

Figure S17. Recast version of Figure 5a from the main text, showing the centers of PL intensity for the combined α\alpha and β\beta peaks vs magnetic-field strength, measured from 4.6 to 44 K for Yb3+^{3+} in Site B. The dashed lines indicate magnetic-field strengths of -0.85 and 0.85 T. All data were collected from a 0.02% Yb3+^{3+}-doped CrPS4_4 single crystal (same as Figure 4) using unpolarized CW 632.8 nm photoexcitation at 5 mW/cm2^2.

References

  1. [1]Lee, M. J., Lee, S., Lee, S., Balamurugan, K., Yoon, C., Jang, J. T., Kim, S.-H., Kwon, D.-H., Kim, M., Ahn, J.-P., Kim, D. H., Park, J.-G. & Park, B. H. Synaptic devices based on two-dimensional layered single-crystal chromium thiophosphate (CrPS₄). NPG Asia Mater. 10, 23–30 (2018).DOI
  2. [2]Cao, G., Meng, P., Chen, J., Liu, H., Bian, R., Zhu, C., Liu, F. & Liu, Z. 2D Material Based Synaptic Devices for Neuromorphic Computing. Adv. Funct. Mater. 31, 2005443 (2021).DOI
  3. [3]Yu, Z., Zeng, T., Han, Z., Ye, K., Zeng, Y., Kong, C., Fang, B., Zhang, X., Geng, L., Lv, W., Liu, Z., Bian, L. & Zeng, Z. Ultralow Power Artificial Synapses Based on CrPS₄-Floating-Gate Transistor for the Emotional Simulation. ACS Appl. Nano Mater. 8, 1517–1525 (2025).
  4. [4]Deng, J., Guo, J., Hosono, H., Ying, T. & Chen, X. Two-dimensional bipolar ferromagnetic semiconductors from layered antiferromagnets. Phys. Rev. Mater. 5, 034005 (2021).DOI
  5. [5]Yao, F., Liao, M., Gibertini, M., Cheon, C.-Y., Lin, X., Wu, F., Watanabe, K., Taniguchi, T., Gutiérrez-Lezama, I. & Morpurgo, A. F. Switching on and off the spin polarization of the conduction band in antiferromagnetic bilayer transistors. Nat. Nanotechnol., 1–8 (2025).
  6. [6]Wu, F., Gibertini, M., Watanabe, K., Taniguchi, T., Gutiérrez-Lezama, I., Ubrig, N. & Morpurgo, A. F. Gate-Controlled Magnetotransport and Electrostatic Modulation of Magnetism in 2D Magnetic Semiconductor CrPS₄. Adv. Mater. 35, 2211653 (2023).DOI
  7. [7]Wu, R., Ross, A., Ding, S., Peng, Y., He, F., Ren, Y., Lebrun, R., Wu, Y., Wang, Z., Yang, J., Brataas, A. & Kläui, M. Magnetotransport Study of van der Waals CrPS₄/(Pt,Pd) Heterostructures: Spin-Flop Transition and Room-Temperature Anomalous Hall Effect. Phys. Rev. Appl. 17, 064038 (2022).DOI
  8. [8]Fu, Z., Huang, H.-F., Samarawickrama, P., Watanabe, K., Taniguchi, T., Wang, W., Ackerman, J., Zang, J., Yu, J.-X. & Tian, J. Anomalous Tunneling Magnetoresistance Oscillation and Electrically Tunable Tunneling Anisotropic Magnetoresistance in Few-Layer CrPS₄. Adv. Physics Res. 3, 2400052 (2024).DOI
  9. [9]Lin, X., Wu, F., Ubrig, N., Liao, M., Yao, F., Gutiérrez-Lezama, I. & Morpurgo, A. F. Positive Oscillating Magnetoresistance in a van der Waals Antiferromagnetic Semiconductor. Phys. Rev. X 15, 011017 (2025).arxiv.org/abs/2410.17930
  10. [10]Qi, S., Chen, D., Chen, K., Liu, J., Chen, G., Luo, B., Cui, H., Jia, L., Li, J., Huang, M., Song, Y., Han, S., Tong, L., Yu, P., Liu, Y., Wu, H., Wu, S., Xiao, J., Shindou, R., Xie, X. C. & Chen, J.-H. Giant electrically tunable magnon transport anisotropy in a van der Waals antiferromagnetic insulator. Nat. Commun. 14, 2526 (2023).DOI
  11. [11]Li, W., Dai, Y., Ni, L., Zhang, B., Tang, D., Yang, Y. & Xu, Y. Ultrafast Magnon–Magnon Coupling and Chirality Switching in Antiferromagnet CrPS₄. Adv. Funct. Mater. 33, 2303781 (2023).
  12. [12]Yan, L., Gong, Z., He, Q., Shen, D., Ge, A., Liu, Y., Ma, G., Dai, Y., Sun, L. & Zhang, S. Polarization-Dependent Nonlinear Optical Responses of CrPS₄ for Ultrafast All-Optical Switches. Adv. Opt. Mater., 2401723 (2024).DOI
  13. [13]Zhang, W., Zhang, Y., Leng, X., Jing, Q. & Wen, Q. CrPS₄ Nanoflakes as Stable Direct-Band-Gap 2D Materials for Ultrafast Pulse Laser Applications. Nanomater. 13, 1128 (2023).DOI
  14. [14]Gu, P., Tan, Q., Wan, Y., Li, Z., Peng, Y., Lai, J., Ma, J., Yao, X., Yang, S., Yuan, K., Sun, D., Peng, B., Zhang, J. & Ye, Y. Photoluminescent Quantum Interference in a van der Waals Magnet Preserved by Symmetry Breaking. ACS Nano 14, 1003–1010 (2020).DOI
  15. [15]Riesner, M., Fainblat, R., Budniak, A. K., Amouyal, Y., Lifshitz, E. & Bacher, G. Temperature dependence of Fano resonances in CrPS₄. J. Chem. Phys. 156, 054707 (2022).DOI
  16. [16]Multian, V., Wu, F., van der Marel, D., Ubrig, N. & Teyssier, J. Brightened Optical Transition Hinting to Strong Spin–Lattice Coupling in a Layered Antiferromagnet. Adv. Sci., 2408343 (2025).DOI
  17. [17]Hu, L., Dong, S., Pan, Y., Wang, Y., Zhai, Y., Wang, S., Liu, H., Sedmidubský, D., Sofer, Z., Zhou, W., Lou, W., Chang, K. & Xiong, Q. Magnetic Order Induced Suppression of Photoluminescence in van der Waals Magnet CrPS₄. Laser Photonics Rev., 2400862 (2025).DOI
  18. [18]Fąs, T., Wlazło, M., Birowska, M., Rybak, M., Zinkiewicz, M., Oleschko, L., Goryca, M., Gondek, Ł., Camargo, B., Szczytko, J., Budniak, A. K., Amouyal, Y., Lifshitz, E. & Suffczyński, J. Direct Optical Probing of the Magnetic Properties of the Layered Antiferromagnet CrPS₄. Adv. Opt. Mater. 13, 2402948 (2025).
  19. [19]Diehl, R. & Carpentier, C. D. The Crystal Structure of Chromium Thiophosphate, CrPS₄. Acta Cryst. B 33, 1399–1404 (1977).DOI
  20. [20]Du, K.-z., Wang, X.-z., Liu, Y., Hu, P., Utama, M. I. B., Gan, C. K., Xiong, Q. & Kloc, C. Weak Van der Waals Stacking, Wide-Range Band Gap, and Raman Study on Ultrathin Layers of Metal Phosphorus Trichalcogenides. ACS Nano 10, 1738–1743 (2016).DOI
  21. [21]Mayorga-Martinez, C. C., Sofer, Z., Sedmidubský, D., Huber, Š., Eng, A. Y. S. & Pumera, M. Layered Metal Thiophosphite Materials: Magnetic, Electrochemical, and Electronic Properties. ACS Appl. Mater. Inter. 9, 12563–12573 (2017).
  22. [22]Peng, Y., Ding, S., Cheng, M., Hu, Q., Yang, J., Wang, F., Xue, M., Liu, Z., Lin, Z., Avdeev, M., Hou, Y., Yang, W., Zheng, Y. & Yang, J. Magnetic Structure and Metamagnetic Transitions in the van der Waals Antiferromagnet CrPS₄. Adv. Mater. 32, 2001200 (2020).DOI
  23. [23]Bud’ko, S. L., Gati, E., Slade, T. J. & Canfield, P. C. Magnetic order in the van der Waals antiferromagnet CrPS₄: Anisotropic H-T phase diagrams and effects of pressure. Phys. Rev. B 103, 224407 (2021).DOI
  24. [24]Calder, S., Haglund, A. V., Liu, Y., Pajerowski, D. M., Cao, H. B., Williams, T. J., Garlea, V. O. & Mandrus, D. Magnetic structure and exchange interactions in the layered semiconductor CrPS₄. Phys. Rev. B 102, 024408 (2020).DOI
  25. [25]Son, J., Son, S., Park, P., Kim, M., Tao, Z., Oh, J., Lee, T., Lee, S., Kim, J., Zhang, K., Cho, K., Kamiyama, T., Lee, J. H., Mak, K. F., Shan, J., Kim, M., Park, J.-G. & Lee, J. Air-Stable and Layer-Dependent Ferromagnetism in Atomically Thin van der Waals CrPS₄. ACS Nano 15, 16904–16912 (2021).DOI
  26. [26]Zhong, M., Hedges, M. P., Ahlefeldt, R. L., Bartholomew, J. G., Beavan, S. E., Wittig, S. M., Longdell, J. J. & Sellars, M. J. Optically addressable nuclear spins in a solid with a six-hour coherence time. Nature 517, 177–180 (2015).DOI
  27. [27]Ortu, A., Tiranov, A., Welinski, S., Fröwis, F., Gisin, N., Ferrier, A., Goldner, P. & Afzelius, M. Simultaneous coherence enhancement of optical and microwave transitions in solid-state electronic spins. Nat. Mater. 17, 671–675 (2018).
  28. [28]Bussières, F., Clausen, C., Tiranov, A., Korzh, B., Verma, V. B., Nam, S. W., Marsili, F., Ferrier, A., Goldner, P., Herrmann, H., Silberhorn, C., Sohler, W., Afzelius, M. & Gisin, N. Quantum teleportation from a telecom-wavelength photon to a solid-state quantum memory. Nat. Photonics 8, 775–778 (2014).
  29. [29]Saglamyurek, E., Jin, J., Verma, V. B., Shaw, M. D., Marsili, F., Nam, S. W., Oblak, D. & Tittel, W. Quantum storage of entangled telecom-wavelength photons in an erbium-doped optical fibre. Nat. Photonics 9, 83–87 (2015).DOI
  30. [30]Fossati, A., Liu, S., Karlsson, J., Ikesue, A., Tallaire, A., Ferrier, A., Serrano, D. & Goldner, P. A Frequency-Multiplexed Coherent Electro-optic Memory in Rare Earth Doped Nanoparticles. Nano Lett. 20, 7087–7093 (2020).DOI
  31. [31]Fernandez-Gonzalvo, X., Chen, Y.-H., Yin, C., Rogge, S. & Longdell, J. J. Coherent frequency up-conversion of microwaves to the optical telecommunications band in an Er:YSO crystal. Phys. Rev. A 92, 062313 (2015).
  32. [32]Siyushev, P., Xia, K., Reuter, R., Jamali, M., Zhao, N., Yang, N., Duan, C., Kukharchyk, N., Wieck, A. D., Kolesov, R., Wrachtrup, J. Coherent properties of single rare-earth spin qubits. Nat. Commun. 5 (2014).DOI
  33. [33]Pressler, K., Snoeren, T. J., Walsh, K. M. & Gamelin, D. R. Magnetic Amplification at Yb³⁺ “Designer Defects” in the van der Waals Ferromagnet CrI₃. Nano Lett. 23, 1320–1326 (2023).DOI
  34. [34]Snoeren, T. J., Pressler, K. & Gamelin, D. R. Optically resolved exchange splittings in the doped van der Waals ferromagnet CrBr₃:Yb³⁺. Phys. Rev. Mater. 8, 104410 (2024).arxiv.org/abs/2408.14663
  35. [35]Kim, S., Lee, J., Lee, C. & Ryu, S. Polarized Raman Spectra and Complex Raman Tensors of Antiferromagnetic Semiconductor CrPS₄. J. Phys. Chem. C 125, 2691–2698 (2021).
  36. [36]Nguyen, M. H., Son, S., Park, G., Na, W., Park, J.-G. & Cheong, H. Temperature dependent Raman study of antiferromagnetic CrPS₄. J. Mater. Chem. C (2024).DOI
  37. [37]Kim, S., Yoon, S., Ahn, H., Jin, G., Kim, H., Jo, M.-H., Lee, C., Kim, J. & Ryu, S. Photoluminescence Path Bifurcations by Spin Flip in Two-Dimensional CrPS₄. ACS Nano 16, 16385–16393 (2022).
  38. [38]Li, Q., Zhen, W., Wang, N., Shi, M., Yu, Y., Pan, S., Deng, L., Cai, J., Wang, K., Zou, L., Zeng, Z., Wang, Z. & Zhang, J. Magnetism Measurements of Two-Dimensional van der Waals Antiferromagnet CrPS₄ Using Dynamic Cantilever Magnetometry. Chinese Phys. Lett. 41, 107503 (2024).arxiv.org/abs/2404.08521
  39. [39]Kojima, N., Tsushima, K. & Tsujikawa, I. Optical Investigations of YbCrO₃. I. Optical Absorption Spectra of Yb³⁺ Ion. J. Phys. Soc. Jpn. 49 (2013).
  40. [40]Kuntu, D. V., Arkhipova, E. A., Shelukhin, L. A., Mertens, F., Prosnikov, M. A., Eliseyev, I. A., Smirnov, A. N., Davydov, V. Y., Mañas-Valero, S., Coronado, E., Cinchetti, M. & Kalashnikova, A. M. Laser-induced demagnetization in van der Waals XY- and Ising-like antiferromagnets NiPS₃ and FePS₃. Phys. Rev. Mater. 8 (2024).DOI
  41. [41]Zhang, X., Jiang, S., Lee, J., Lee, C., Mak, K. F. & Shan, J. Spin Dynamics Slowdown near the Antiferromagnetic Critical Point in Atomically Thin FePS₃. Nano Lett. 21 (2021).DOI
  42. [42]Matthiesen, M., Hortensius, J. R., Mañas-Valero, S., Kapon, I., Dumcenco, D., Giannini, E., Šiškins, M., Ivanov, B. A., Zant, H. S. J. v. d., Coronado, E., Kuzmenko, A. B., Afanasiev, D. & Caviglia, A. D. Controlling Magnetism with Light in a Zero Orbital Angular Momentum Antiferromagnet. Phys. Rev. Lett. 130 (2023).DOI
  43. [43]Khusyainov, D., Gareev, T., Radovskaia, V., Sampathkumar, K., Acharya, S., Šiškins, M., Mañas-Valero, S., Ivanov, B. A., Coronado, E., Rasing, T., Kimel, A. V. & Afanasiev, D. Ultrafast laser-induced spin–lattice dynamics in the van der Waals antiferromagnet CoPS₃. APL Mater. 11 (2023).DOI
  44. [44]Xing, Y., Chen, H., Zhang, A., Hao, Q., Cai, M., Chen, W., Li, L., Peng, D., Yi, A., Huang, M., Wang, X. & Han, J. Optical Detection of Weak Magnetic Transitions via Photoluminescence in Cr-Doped Van Der Waals Antiferromagnets. Adv. Opt. Mater., 2402549 (2024).DOI
  45. [45]Jiang, S., Shan, J., Mak, K. F., Jiang, S., Shan, J. & Mak, K. F. Electric-field switching of two-dimensional van der Waals magnets. Nat. Mater. 17 (2018).DOI
  46. [46]Gu, K., Zhang, X., Liu, X., Guo, X., Wu, Z., Wang, S., Song, Q., Wang, W., Wei, L., Liu, P., Ma, J., Xu, Y., Niu, W. & Pu, Y. Exchange Bias Modulated by Antiferromagnetic Spin-Flop Transition in 2D Van der Waals Heterostructures. Adv. Sci. 11, 2307034 (2024).DOI
  47. [47]Song, T., Fei, Z., Yankowitz, M., Lin, Z., Jiang, Q., Hwangbo, K., Zhang, Q., Sun, B., Taniguchi, T., Watanabe, K., McGuire, M. A., Graf, D., Cao, T., Chu, J.-H., Cobden, D. H., Dean, C. R., Xiao, D., Xu, X., Song, T., Fei, Z., Yankowitz, M., Lin, Z., Jiang, Q., Hwangbo, K., Zhang, Q., Sun, B., Taniguchi, T., Watanabe, K., McGuire, M. A., Graf, D., Cao, T., Chu, J.-H., Cobden, D. H., Dean, C. R., Xiao, D. & Xu, X. Switching 2D magnetic states via pressure tuning of layer stacking. Nature Materials 2019 18:12 18 (2019).DOI
  48. [48]Wang, X., Wang, Y., Park, J., Zhu, J., Wang, C., Taniguchi, T., Watanabe, K., Yan, J., Xiao, D., Gamelin, D. R., Yao, W. & Xu, X. Light-induced ferromagnetism in moiré superlattices. Nature 604, 468–473 (2022).DOI
  49. [49]Zhang, P., Chung, T.-F., Li, Q., Wang, S., Wang, Q., Huey, W. L. B., Yang, S., Goldberger, J. E., Yao, J. & Zhang, X. All-optical switching of magnetization in atomically thin CrI₃. Nat. Mater. 21, 1373–1378 (2022).DOI
  50. [50]Dąbrowski, M., Guo, S., Strungaru, M., Keatley, P. S., Withers, F., Santos, E. J. G. & Hicken, R. J. All-optical control of spin in a 2D van der Waals magnet. Nat. Commun. 13, 5976 (2022).DOI
  51. [51]Budniak, A. K., Killilea, N. A., Zelewski, S. J., Sytnyk, M., Kauffmann, Y., Amouyal, Y., Kudrawiec, R., Heiss, W. & Lifshitz, E. Exfoliated CrPS₄ with Promising Photoconductivity. Small 16, 1905924 (2020).DOI

Paper details

vlnc:W_n7zr4k8u
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents