Abstract

Semiconductor photodetectors are conventionally optimized for sensing weak optical signals, and they typically saturate at low-to-moderate light intensity. Here, we demonstrate AlN photodetectors that exhibit non-saturating linear response to ultra-bright, sub-bandgap light exceeding 40 W/cm2\mathrm{W/cm^2} (over 400 Suns). The photodetector further shows undistorted linear response at elevated temperature, up to at least 300 ∘C\mathrm{^\circ C}. This exceptional performance originates from photoresponse mediated by point defects with energy levels deep in the bandgap (deep levels) at the metal-AlN Schottky junction. Through dopant design and contact engineering, we demonstrate that a narrow space-charge region is essential for enabling ultra-bright light detection and accurate measurement. These results establish a strategy for engineering ultra-wide bandgap (UWBG) semiconductor devices for reliable operation in extreme conditions to meet emerging needs in industrial process control, thermal and nuclear power generation, and aeronautics and spaceflight.

Main Text

Accurate detection and imaging of intense light are desired for emerging technologies including laser-based manufacturing, plasma and fusion systems, advanced combustion engines, and aerospace and defense platforms. [1, 2, 3] Nonetheless, semiconductor photodetectors have been developed primarily for detection of weak optical signals, with figures of merit such as detectivity and noise-equivalent power (NEP) optimized for sensitivity at low optical power. [4] Under intense (i.e., high-irradiance) illumination, conventional semiconductor photodetectors typically become nonlinear and may ultimately fail because of trap filling, space-charge effects, carrier transport limitations, and overheating. [5, 6, 7, 8, 9] This nonlinearity impedes accurate measurements of irradiance and results in loss of quantitative information. Despite advances in photodetector technologies, semiconductor devices capable of directly and quantitatively sensing bright light remain elusive.

Here, we report a defect-engineered aluminum nitride (AlN) photodetector that features linear, non-saturating response to ultra-bright sub-bandgap illumination exceeding 40 W/cm240\ \mathrm{W}/\mathrm{cm}^{2}, and maintains undistorted operation up to at least 300 °C. These performance levels substantially exceed those of existing semiconductor photodetectors. Sub-bandgap sensitivity results from introducing a point defect (here, Ge) with an energy level deep in the AlN bandgap. Although defect-mediated photoconductivity has long been observed in semiconductors, it is generally considered unsuitable for photodetection because the finite population of defect states can be fully depleted under intense illumination, causing saturated photoresponse. [10, 11, 12, 13, 14, 15] Here, we overturn this conventional expectation and demonstrate that non-saturating sub-bandgap response can be achieved through tunneling-based defect recombination at a suitably-designed metal-AlN heterojunction. This mechanism enables robust optical sensing across operating regimes that are inaccessible to existing semiconductor photodetectors.

These results reveal a route to new optoelectronic functionality in ultra-wide-bandgap (UWBG) semiconductors through the deliberate control of deep-level defects. By overcoming the long-assumed performance limit of defect-mediated photoconductivity, this work establishes a framework for treating defect states as active device elements rather than merely as material imperfections. Because deep-level defects are ubiquitous across WBG and UWBG semiconductors, the underlying principles demonstrated here may be broadly applicable to a wide range of materials and device architectures.

Device concept and performance

We fabricate photodetectors in a lateral configuration, with metal contacts (1 nm Ti / 80 nm Al) deposited on an epitaxial AlN thin film grown by metal-organic chemical vapor deposition (MOCVD, Adroit Materials) with a nominal Ge concentration of 2×1019 cm−32 \times10^{19}\ \mathrm{cm}^{-3}. The contacts are square pads measuring 300×300 μm300 \times300\ \mu\mathrm{m}, separated by 50 μm\mu\mathrm{m}. Ge is expected to be a deep level in AlN because of its high thermal ionization energy. [16, 17] Consistently, the AlN:Ge films are found semi-insulating. To expose the device to high-irradiance light, we use a two-lens optical system to focus light from a blue LED (Thorlabs M450LP2 with a center wavelength 450 nm, Fig. S1).

In Figure 1A we present the device photocurrent (IphI_{\mathrm{ph}}) vs. irradiance (PP) measured between room temperature and 300 °C. We model the photoresponse as a power law Iph∝PθI_{\mathrm{ph}} \propto P^{\theta} and fit the scaling exponent θ\theta at each temperature. According to the consensus statement by Pecunia et al., a photodetector is classified as linear when the exponent θ\theta lies within the range 0.99 - 1.01.[4] The data and fits presented in Figure 1A confirm that the AlN:Ge photodetector maintains a non-saturating, linear response under blue illumination up to 44 W/cm2^2 and temperatures up to 300 °C. These are the limits of our test equipment; the upper limits of the device may be higher. In Figure 1B we present a photocurrent time series for cyclic illumination with decreasing irradiance. The dark current is low at all measurement temperatures, due to the UWBG of AlN and the high ionization energy of Ge deep levels. As a result, the ON/OFF ratio is high at all test conditions.

Image not extracted

Figure 1. Linear and stable photoresponse at high irradiance and elevated temperatures. (A) Photocurrent (IphI_{\mathrm{ph}}) vs. irradiance (PP) measured between 25 – 300 °C. The dashed lines are power-law fits, and dark current levels have been subtracted. All data in panels (A-C) are recorded at a DC voltage of 5 V. Inset: Device structure (not to scale) and incident illumination. (B) Current timeseries data as illumination is cycled on and off in decreasing steps from 44 – 0.009 W/cm2^2. (C) Normalized transient photoresponse under irradiance of 44 W/cm2^2. (D) Comparison of the maximum demonstrated irradiance and operating temperature of our device with the upper limits of previously reported photodetectors at comparable wavelengths, including commercial products (open symbols) and literature reports (filled symbols), all operating in the linear response regime (see Data S1 for underlying data). HP = halide perovskites.

In Figure 1C we present the transient photoresponse of the AlN:Ge device. At 25 °C, both the 90% rise time and 90% fall time are approximately 4 ms, decreasing to 1.5 ms at 300 °C.

Importantly, the AlN:Ge device exhibits excellent operational stability, exhibiting no measurable degradation in photoresponse after 100,000 illumination cycles (20 ms on/20 ms off) at 44 W/cm2^{2}. We compare the irradiance-dependent photoresponse and transient behavior of the AlN:Ge device with those of commercial Si and InGaN photodiodes (Fig. S2). Under bright illumination, the commercial devices are nonlinear and show performance degradation, whereas the AlN:Ge device maintains a stable photoresponse during prolonged exposure. The spectral range of the AlN:Ge photodetector extends over at least 360 - 490 nm (Fig. S3), spanning the ultraviolet (UV) to blue region.

In Figure 1D we benchmark the maximum demonstrated irradiance and operating temperature of our device with the upper limits of previously reported photodetectors at comparable wavelengths, including commercial products and literature reports, all operating in the linear response regime. [18, 19, 20, 21, 22, 23] The AlN:Ge photodetector presented here exceeds prior reports by significant margins in irradiance and operating temperature. Although reports of photodetectors for high temperature operation based on WBG and UWBG semiconductors have increased in frequency in recent years, linear response was not achieved at elevated temperatures. [24, 25, 26, 27, 28, 29]

Device operating principle

To understand the mechanism behind the non-saturating response of our AlN:Ge device, we measured photocurrent IphI_{\mathrm{ph}} vs. DC voltage VDCV_{\mathrm{DC}} for varying irradiance (Figure 2A). Linear response is achieved below approximately 10 V; at higher voltage, IphI_{\mathrm{ph}} increases rapidly and exhibits sub-linear dependence on the irradiance. In the linear response regime, the dependence of IphI_{\mathrm{ph}} on VDCV_{\mathrm{DC}} can be well fit to the form Iph∝VDC+ϕI_{\mathrm{ph}} \propto\sqrt{V_{\mathrm{DC}}+\phi}, where ϕ\phi is a fitting parameter, demonstrated by the dashed lines in Figure 2A. For an applied DC voltage, one of the metal-AlN junctions is under reverse bias VR≈VDCV_{\mathrm{R}} \approx V_{\mathrm{DC}}, while the other junction is under near-zero bias. [14] The width of the space charge region (SCR) WSCRW_{\mathrm{SCR}} at a Schottky junction follows a square root dependence on the reverse bias VRV_{\mathrm{R}}, i.e., WSCR∝VR+ϕbiW_{\mathrm{SCR}} \propto\sqrt{V_{\mathrm{R}}+\phi_{\mathrm{bi}}}, with ϕbi\phi_{\mathrm{bi}} the built-in potential. [30] This suggests that the photocurrent is likely proportional to the space charge region width, Iph∝WSCRI_{\mathrm{ph}} \propto W_{\mathrm{SCR}}.

Image not extracted

Figure 2. Relationship between linear photoresponse and WSCRW_{\mathrm{SCR}}. (A) Photocurrent (IphI_{\mathrm{ph}}) vs. DC voltage (VDCV_{\mathrm{DC}}) at discrete irradiance levels; dark current levels have been subtracted. Linear response is observed below approximately 10 V. Dashed lines are best fits of the data to the form Iph∝VDC+ϕI_{\mathrm{ph}} \propto\sqrt{V_{\mathrm{DC}}+\phi}, where ϕ\phi a fitting parameter (see table S1 for best-fit values). (B) Schematic band diagram illustrating defect ionization by sub-bandgap photoexcitation, and recombination by tunneling injection from the metal contact. Photoexcited carriers drift in the built-in electric field and contribute to IphI_{\mathrm{ph}}.

We further propose that the IphI_{\mathrm{ph}} in the linear response regime originates from defect-to-conduction band excitation within the SCR, as illustrated in Figure 2B. When exposed to sub-bandgap light, photocarriers generated via defect excitation are swept out of the SCR by the internal electric field, contributing to the photocurrent IphI_{\mathrm{ph}}. Besides, a non-saturating response at high irradiance requires that the recombination (carrier recapture) at the photoionized defect states is sufficiently fast, so that the defect states do not become exhausted under illumination.[12] Nonetheless, within the SCR, free carriers are depleted, and there are vanishingly few conduction electrons available for defect recombination.[31] This motivates our hypothesis that carrier injection by tunneling from the metal contact provides sufficiently fast recombination and enables non-saturating photoresponse. Defect-to-band tunneling rates become appreciable for internal electric field strength exceeding 10510^{5} V/cm,[32, 33] which is achieved at the reverse biased junction for VDCV_{\mathrm{DC}} below 10 V (see below).

The mechanism discussed above implies that achieving linear photoresponse requires the presence of a narrow SCR at the reversed biased metal-AlN junction. Device performance should suffer if the SCR is eliminated by forming an ohmic contact, or if the SCR becomes too wide to enable tunneling injection. We test these predictions by designing devices with suppressed and widened SCRs. The SCR can be suppressed by thermal annealing of the metal contact at 950 °C, which promotes interdiffusion at the metal-nitride interface and converts the contact from Schottky to near-ohmic behavior.[34, 35] The SCR can be widened by lowering the Ge concentration, as WSCRW_{\mathrm{SCR}} scales inversely with the square root of the dopant concentration.[30] Accordingly, we fabricate and test an AlN photodetector with a nominal Ge incorporation of 2×1018 cm−32 \times10^{18}\ \mathrm{cm}^{-3}.

To determine WSCRW_{\mathrm{SCR}}, we use capacitance-voltage (CC-VV) profiling and Mott-Schottky analysis to extract the effective defect concentration and estimate WSCRW_{\mathrm{SCR}}. Due to the very low free carrier concentrations in the AlN:Ge, and the inability of deep defects to respond to high frequency modulation (e.g., MHz), low-frequency CC-VV measurements are needed to properly extract WSCRW_{\mathrm{SCR}}.[36, 37, 38] CC-VV profiling data for the device with [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3} are shown in Figure 3A; further details are presented in Supplementary Information and Fig. S4. The extracted WSCRW_{\mathrm{SCR}} are presented in Figure 3B. The junction with a nominal defect concentration [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3} shows a relatively narrow SCR: at VDC=5V_{\mathrm{DC}} = 5 V, WSCR≈132W_{\mathrm{SCR}} \approx132 nm and the peak electric field approaches 7.5×1057.5 \times10^{5} V/cm. After contact annealing, the junction shows near-ohmic behavior (Fig. S5) and the SCR has collapsed to WSCR≈0W_{\mathrm{SCR}} \approx0.[34] Cross-sectional imaging of the annealed contact with scanning transmission electron microscopy (STEM) confirms that annealing-induced interdiffusion is confined to within 2 nm of the metal-AlN interface, without noticeable modification of the AlN bulk (Fig. S6). Meanwhile, lowering [Ge][\mathrm{Ge}] from 2×1019 cm−32 \times10^{19}\ \mathrm{cm}^{-3} to 2×1018 cm−32 \times10^{18}\ \mathrm{cm}^{-3} results in a wider SCR, as expected.

Image not extracted

Figure 3. Illustrating the importance of a narrow SCR for device performance. (A) CC-VV profiling data for device with [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3}, measured with irradiance of 0.455 W/cm2^{2}, for VDCV_{\mathrm{DC}} between 0 and 2.5 V. The dashed line indicates the low-frequency data used for Mott-Schottky analysis. (B) WSCRW_{\mathrm{SCR}} vs. VDCV_{\mathrm{DC}} for three devices with different doping and/or processing. The solid lines represent devices with non-annealed contacts and different [Ge][\mathrm{Ge}]. The dashed line represents a device with annealed contacts and [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3}. (C) Optical responsivity for irradiance from 0.009 - 44 W/cm2^{2} for the same three devices presented in (A). The data are normalized to the responsivity measured at the lowest irradiance (0.009 W/cm2^{2}), to illustrate linearity and deviation from linearity. (D) Arrhenius analysis of photocurrent decay with the activation energy EaE_{\mathrm{a}} extracted for the temperature range from 23 to 90 °C.

In Figure 3C we present the photoresponse of these three devices: one with a narrower SCR ([Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3}), one with a wider SCR ([Ge]=2×1018 cm−3[\mathrm{Ge}] = 2 \times10^{18}\ \mathrm{cm}^{-3}), and one with a negligible SCR (contact annealed). We present the normalized optical responsivity vs. irradiance to assess linearity. The [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3} device exhibits constant responsivity and thereby linear photoresponse. In contrast, the [Ge]=2×1018 cm−3[\mathrm{Ge}] = 2 \times10^{18}\ \mathrm{cm}^{-3} device exhibits response saturation, consistent with exhaustion of defect levels. The annealed contact device shows rapid performance loss with increasing irradiance. These results illustrate that linear, non-saturating photoresponse depends on the existence of a sufficiently narrow SCR.

The SCR determines device performance through the recombination mechanism, as indicated in Figure 2B. The tunneling-based recombination pathway may be thermally-activated, as in thermionic field emission.[30] In contrast, the device with the annealed contact has no Schottky junction, and recombination relies primarily on the cross section for electron recapture from the conduction band, which may be barrier-free (or nearly so) and temperature-independent.[15] To examine the recombination mechanism, we measured photocurrent decay (i.e., persistence) as a function of temperature and extracted the decay rates 1/τdecay1/\tau_{\mathrm{decay}} (Fig. S7), which are presented in the Arrhenius analysis in Figure 3D. In the temperature range of 25 to 90 °C, the [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3} device with non-annealed contacts shows an activation energy of 0.11 eV, whereas in the annealed contact device the decay rate is nearly temperature independent. These results confirm that the SCR determines recombination mechanism and thereby device performance. The measured thermal barrier of 0.11 eV in the photocurrent decay may be further lowered by optimizing the metal contact layer.

Conclusion

We demonstrate that deep-level-mediated photoconductivity can be exploited in a UWBG semiconductor to enable non-saturating response to ultra-bright sub-bandgap light. This runs contrary to decades of accepted wisdom about intrinsically poor performance of devices harnessing defect-mediated photoconductivity. The device presented based on Ge-doped AlN with [Ge]=2×1019 cm−3[\mathrm{Ge}] = 2 \times10^{19}\ \mathrm{cm}^{-3} exhibits linear and robust response for irradiance as high as 44 W/cm² at a center wavelength of 450 nm, and for temperatures as high as 300 °C. Because of lack of free carriers in the AlN, the device exhibits negligible high-frequency capacitance. Thus, the Ge-doped AlN behaves as a low-capacitance current source upon sub-bandgap photoexcitation, which is promising for high-speed operation. Also, devices that rely on tunneling injection are well suited for high-speed switching owing to the intrinsically fast nature of quantum-mechanical tunneling.[39]

The operating principle demonstrated here expands the frontier of UWBG semiconductor optoelectronics. The spectral response to sub-bandgap light can be adjusted through dopant selection and/or alloy design; for instance, literature suggests that Si doping and using high-Al-content AlGaN alloys may enable near-infrared sensitivity.[16, 40] Semiconductor photodetectors capable of linear measurement of high-irradiance light at high temperatures may find many applications in the industrial and defense sectors, including but not limited to laser- and plasma-based materials manufacturing processes, next-generation fusion and fission plants, military sensing and imaging applications, etc.

References

References

  1. [1]Chen, L. et al. In-situ process monitoring and adaptive quality enhancement in laser additive manufacturing: A critical review. Journal of Manufacturing Systems 74, 527–574 (2024).
  2. [2]Stratton, B. C., Bitter, M., Hill, K. W., Hillis, D. L. & Hogan, J. T. Chapter 5: Passive Spectroscopic Diagnostics for Magnetically Confined Fusion Plasmas. Fusion Science and Technology 53, 431–486 (2008).DOI
  3. [3]Jin, Y. & Situ, G. A Survey for 3D Flame Chemiluminescence Tomography: Theory, Algorithms, and Applications. Front. Photon. 3, 845971 (2022).DOI
  4. [4]Pecunia, V. et al. Guidelines for accurate evaluation of photodetectors based on emerging semiconductor technologies. Nat. Photon. 19, 1178–1188 (2025).DOI
  5. [5]Kind, H., Yan, H., Messer, B., Law, M. & Yang, P. Nanowire Ultraviolet Photodetectors and Optical Switches. Adv. Mater. 14, 158–160 (2002).doi.org/10.1002/1521-4095(20020116)14:2<158::aid-adma158>3.0.co;2-w
  6. [6]Stolterfoht, M. et al. Photocarrier drift distance in organic solar cells and photodetectors. Sci Rep 5, 9949 (2015).DOI
  7. [7]Jansen-van Vuuren, R. D., Armin, A., Pandey, A. K., Burn, P. L. & Meredith, P. Organic Photodiodes: The Future of Full Color Detection and Image Sensing. Adv. Mater. 28, 4766–4802 (2016).
  8. [8]Fang, H. & Hu, W. Photogating in Low Dimensional Photodetectors. Advanced Science 4, 1700323 (2017).DOI
  9. [9]Euvrard, J., Revaux, A., Kahn, A. & Vuillaume, D. Photocurrent deviation from linearity in an organic photodetector due to limited hole transport layer conductivity. Organic Electronics 76, 105450 (2020).DOI
  10. [10]Moazzami, K., Murphy, T. E., Phillips, J. D., Cheung, M. C.-K. & Cartwright, A. N. Sub-bandgap photoconductivity in ZnO epilayers and extraction of trap density spectra. Semicond. Sci. Technol. 21, 717–723 (2006).DOI
  11. [11]Casalino, M., Coppola, G., Iodice, M., Rendina, I. & Sirleto, L. Near-Infrared Sub-Bandgap All-Silicon Photodetectors: State of the Art and Perspectives. Sensors 10, 10571–10600 (2010).
  12. [12]Böer, K. W. & Pohl, U. W. Photoconductivity. in Semiconductor Physics 1181–1205 (Springer International Publishing, 2018). doi:10.1007/978-3-319-69150-3_31.DOI
  13. [13]Dong, J. et al. Giant and Controllable Photoplasticity and Photoelasticity in Compound Semiconductors. Phys. Rev. Lett. 129, 065501 (2022).DOI
  14. [14]Dong, J. & Jaramillo, R. A Junction Photoconductive Semiconductor Switch (J-PCSS) in AlN with Sub-Band Gap Responsivity and Accelerated Turn-Off Speed. IEEE Electron Device Lett. 46, 916–919 (2025).DOI
  15. [15]Dong, J. et al. High sub-bandgap response and fast switching enabled by thermal quenching in carbon-doped semi-insulating GaN. Applied Physics Letters 128, 243304 (2026).
  16. [16]Gordon, L., Lyons, J. L., Janotti, A. & Van de Walle, C. G. Hybrid functional calculations of DX centers in AlN and GaN. Phys. Rev. B 89, 085204 (2014).
  17. [17]Blasco, R. et al. Electrical and optical properties of heavily Ge-doped AlGaN. J. Phys. D: Appl. Phys. 52, 125101 (2019).DOI
  18. [18]Dou, L. et al. Solution-processed hybrid perovskite photodetectors with high detectivity. Nat Commun 5, 5404 (2014).DOI
  19. [19]Bao, C. et al. Low-Noise and Large-Linear-Dynamic-Range Photodetectors Based on Hybrid-Perovskite Thin-Single-Crystals. Advanced Materials 29, 1703209 (2017).DOI
  20. [20]Shen, L. et al. A Self-Powered, Sub-nanosecond-Response Solution-Processed Hybrid Perovskite Photodetector for Time-Resolved Photoluminescence-Lifetime Detection. Advanced Materials 28, 10794–10800 (2016).DOI
  21. [21]Li, C. et al. Ultrafast and broadband photodetectors based on a perovskite/organic bulk heterojunction for large-dynamic-range imaging. Light Sci Appl 9, 31 (2020).DOI
  22. [22]Sutherland, B. R. et al. Sensitive, Fast, and Stable Perovskite Photodetectors Exploiting Interface Engineering. ACS Photonics 2, 1117–1123 (2015).DOI
  23. [23]Feng, X., Tan, M., Li, M., Wei, H. & Yang, B. Polyhydroxy Ester Stabilized Perovskite for Low Noise and Large Linear Dynamic Range of Self-Powered Photodetectors. Nano Lett. 21, 1500–1507 (2021).DOI
  24. [24]Hou, S., Hellstrom, P.-E., Zetterling, C.-M. & Ostling, M. 550 °C 4H-SiC p-i-n Photodiode Array With Two-Layer Metallization. IEEE Electron Device Lett. 37, 1594–1596 (2016).DOI
  25. [25]So, H., Lim, J. & Senesky, D. G. Continuous V-Grooved AlGaN/GaN Surfaces for High-Temperature Ultraviolet Photodetectors. IEEE Sensors J. 16, 3633–3639 (2016).DOI
  26. [26]Hou, C., Gazoni, R. M., Reeves, R. J. & Allen, M. W. High-Temperature β-Ga₂O₃ Schottky Diodes and UVC Photodetectors Using RuOₓ Contacts. IEEE Electron Device Lett. 40, 1587–1590 (2019).
  27. [27]Du, F. et al. Demonstration of High-Performance 4H-SiC MISIM Ultraviolet Photodetector With Operation Temperature of 550 °C and High Responsivity. IEEE Trans. Electron Devices 68, 5662–5665 (2021).DOI
  28. [28]Wang, W. et al. High-Temperature Deep Ultraviolet Photodetector Based on a Crystalline Ga₂O₃-Diamond Heterostructure. IEEE Electron Device Lett. 43, 2121–2124 (2022).DOI
  29. [29]Vashishtha, P. et al. Self-Driven UVC–NIR Broadband Photodetector with High-Temperature Reliability Based on a Coco Palm-Like MoS₂/GaN Heterostructure. ACS Appl. Electron. Mater. 5, 1891–1902 (2023).
  30. [30]Sze, S. M. & Ng, K. K. Metal-Semiconductor Contacts. in Physics of Semiconductor Devices 134–196 (John Wiley & Sons, 2006).DOI
  31. [31]Dong, J. & Jaramillo, R. Modeling defect-level switching for nonlinear and hysteretic electronic devices. Journal of Applied Physics 135, 224501 (2024).DOI
  32. [32]Schenk, A. & Krumbein, U. Coupled defect-level recombination: Theory and application to anomalous diode characteristics. Journal of Applied Physics 78, 3185–3192 (1995).DOI
  33. [33]Myers, S. M., Wampler, W. R. & Modine, N. A. Recombination by band-to-defect tunneling near semiconductor heterojunctions: A theoretical model. Journal of Applied Physics 120, 134502 (2016).DOI
  34. [34]Greco, G., Iucolano, F. & Roccaforte, F. Ohmic contacts to Gallium Nitride materials. Applied Surface Science 383, 324–345 (2016).DOI
  35. [35]Cao, H. et al. Low contact resistivity at the 10−4 Ω cm2 level fabricated directly on n-type AlN. Applied Physics Letters 125, 081602 (2024).DOI
  36. [36]Kimerling, L. C. Influence of deep traps on the measurement of free-carrier distributions in semiconductors by junction capacitance techniques. Journal of Applied Physics 45, 1839–1845 (1974).DOI
  37. [37]Huang, J. W., Kuech, T. F., Lu, H. & Bhat, I. Electrical characterization of Mg-doped GaN grown by metalorganic vapor phase epitaxy. Applied Physics Letters 68, 2392–2394 (1996).DOI
  38. [38]Frolov, D. S. & Zubkov, V. I. Frequency dispersion of capacitance–voltage characteristics in wide bandgap semiconductor-electrolyte junctions. Semicond. Sci. Technol. 31, 125013 (2016).DOI
  39. [39]Esaki, L. Discovery of the tunnel diode. IEEE Trans. Electron Devices 23, 644–647 (1976).DOI
  40. [40]Zeisel, R. et al. DX -behavior of Si in AlN. Phys. Rev. B 61, R16283–R16286 (2000).DOI

Paper details

vlnc:W_ndz9wkap
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 5

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents