Humidity-modulated Ostwald Step Rule in FAPbI3\rm FAPbI_3 Martensitic Transitions

Abstract

Experimental observations reveal a dual role of moisture in FAPbI3\rm FAPbI_3 phase transitions. During fabrication at high temperatures, humidity improves the quality of the perovskite (αα phase) films, whereas at low service temperatures, humidity accelerates degradation of the photoactive αα phase into the photo-inactive hexagonal δδ phase. Despite extensive experimental evidence, the microscopic mechanisms by which moisture modulates phase stability and transition pathways remain unknown. Here, using large-scale atomistic simulations powered by an ab initio machine-learned potential, we reproduce the experimentally observed increase in the δδ-to-αα transition temperature under increased humidity. Our simulations reveal a layered metastable intermediate along the Burgers transition pathway that exhibits a strong affinity for water. The competing water uptake of this intermediate and the δδ phase governs the humidity dependence of transition kinetics. These findings elucidate the dual role of moisture in perovskite phase transitions and demonstrate how environmental species can stabilize metastable intermediates and reshape transition pathways, providing an environment-dependent perspective on Ostwald's step rule.

Moisture has long been recognized as a double-edged sword in the phase stability and synthesis of FAPbI3. On the one hand, a sharp decline in optical absorptance has been repeatedly observed when the relative humidity exceeds approximately 45% [1, 2], indicating moisture-induced degradation of the photoactive perovskite (α\alpha) phase. On the other hand, moisture exposure has been shown to accelerate the δ\delta-to-α\alpha phase transition and improve the perovskite film quality during fabrication [3, 4, 5, 6, 7]. Despite extensive experimental investigations, the microscopic mechanisms underlying these effects remain poorly understood. Elucidating how moisture influences the relative phase stability and transition pathways of FAPbI3 could therefore not only guide the development of more stable perovskite photovoltaics but also provide broader insights into the role of humidity in solid-state phase transitions.

Here, we unravel the humidity-dependent phase behavior of FAPbI3 through large-scale atomistic simulations powered by a machine-learned interatomic potential with ab initio accuracy. By calculating and comparing the free energies of α\alpha and δ\delta phases across a broad range of temperatures and relative humidities, we establish a thermodynamic phase diagram that reveals an increasing δ→α\delta\to\alpha transition temperature under higher humidity, in good agreement with experimental observations. More importantly, we identify a layered metastable intermediate along the transition path that exhibits a pronounced affinity for water uptake. The competition of humidity-dependent water uptake between this intermediate and the δ\delta phase modulates the transition kinetics and controls the speed of α→δ\alpha\to\delta degradation. These findings provide a microscopic understanding of how moisture affects solid-solid phase transitions by modulating the formation and stability of metastable intermediates, providing new insights into the role of environmental species in Ostwald’s step rule.

α−δ\alpha- \delta transition under humidity

To predict the phase transition temperature under different humidity, we first use thermal integration to calculate the free energies of α\alpha and δ\delta phases at different temperatures, then run grand canonical Monte Carlo of water insertion to establish a relation between the grand canonical free energy Ω\Omega and relative humidity (RH). The δ\delta phase equilibrates with high water uptake at increased RH, while the α\alpha phase shows almost zero water uptake. As a result, the transition temperature rises with increased RH (Figure 1a). Here, we used the relationship between Ω\Omega and RH determined at 76.85 °C (350 K) as an approximation for higher temperatures.

Phase diagram of $\mathrm{FAPbI}_{3}$

Figure 1. Phase diagram of FAPbI3\mathrm{FAPbI}_{3}. (A) Temperature-humidity phase diagram of FAPbI3\mathrm{FAPbI}_{3} and comparison with experimental observations. The colour map represents the normalized Gibbs free-energy difference between the α\alpha and δ\delta phases as a function of temperature and relative humidity (RH). The solid white curve marks the predicted phase boundary, where the two phases have equal free energies, while the dashed white curves delimit the uncertainty in the predicted boundary. Experimental observations from six studies are overlaid for comparison. The experimental results are taken from refs. [3, 4, 8, 9, 10, 11, 12]. (B) Illustration of the Burgers path of the FAPbI3\mathrm{FAPbI}_{3} α↔δ\alpha\leftrightarrow\delta transition.

We compare the predicted phase boundary with experimental observations from six studies in Figure 1A, finding excellent agreement overall. Cordero et al. [8, 9] reported thermal hysteresis in the α↔δ\alpha\leftrightarrow\delta transition, spanning 77 °C upon cooling and 127 °C upon heating. They further demonstrated increased transition temperature under trace humidity. Lin et al. [3] investigated humidity treatments at RH values 30% and 80%, followed by annealing at 150 °C, and reported improved photovoltaic performance under the higher-humidity treatment owing to reduced side-products. Liu et al. [10] demonstrated reversible phase transitions through “humidity aging-heat healing” cycles, in which the α\alpha phase transformed into the δ\delta phase at RH ≈60\approx60% and subsequently reverted to the α\alpha phase upon annealing at 150 °C. Kumar et al. [11] achieved a stable α\alpha phase by annealing δ\delta-phase films at 150 °C under RH 25%. Similarly, Jheng et al. [4] obtained high-quality, phase-pure α\alpha-FAPbI3_3 films with enhanced power conversion efficiency through annealing at 170 °C under RH as high as 55% and 99%. During film deposition, Hossain et al. [12] observed the emergence of the kinetically favored α\alpha phase at approximately 60 °C and the disappearance of δ\delta-phase at approximately 75 °C across a range of humidity levels.

Kinetics modulation by water uptake of an intermediate phase

FAPbI3_3 perovskite assumes a body-centered cubic (bcc) lattice structure, with Pb and FA occupying the edge and body-center, respectively (Figure 1b). A classic mechanism of the transition between bcc and hexagonal lattices is the Burgers path. This pathway involves two steps: the first step is an orthorhombic lattice deformation, where the lattice is stretched in the [110][110] direction and compressed in the [001][001] direction, and the second step is a cooperative atom shuffling in the [110][110] direction with atoms in the adjacent planes shifting in opposite directions. The first step of lattice deformation transforms the geometry of the {110}\{110\} planes of the bcc lattice into the basal planes of the hcp lattice, with mild atomic displacements. The second step shifts the lattice from orthorhombic to hexagonal. For FAPbI3_3, the Burgers path is accompanied by breaking and reforming of Pb – I bonds, as illustrated in Figure 1B.

The crystallographic anisotropy associated with the Burgers path is reflected in two complementary experimental observations. First, moisture-induced degradation of the α\alpha phase exhibits a pronounced facet dependence, with the {100}\{100\} facet being more susceptible to degradation than the {111}\{111\} facet [13]. Second, termination of the δ\delta phase along its {110}\{110\} planes by introducing two-dimensional perovskitoid materials into the perovskite matrix has been demonstrated as an effective strategy for stabilizing FA-based perovskite solar cells [14] by suppressing the Burgers path.

More intriguingly, the first step along the Burgers pathway gives rise to a layered metastable intermediate phase (PbI3⋅FA\mathrm{PbI_3}\cdot\mathrm{FA}) with a pronounced affinity for water uptake. As shown in Figure 2A, at room temperature, water uptake of the intermediate increases sharply with increasing RH, whereas that of the δ\delta phase increases more gradually but eventually surpasses that of the intermediate at RH ≳45%\gtrsim45\%. At the elevated temperature of 76.28 °C, however, the intermediate exhibits greater water uptake than the δ\delta phase across a much wider RH range (Figure 2B). This temperature-dependent contrast provides a possible explanation for the dual effects of humidity on phase transitions observed experimentally.

Water uptake of the $\delta$ and intermediate $\mathrm{PbI_3}\cdot\mathrm{FA}$ phases

Figure 2. Water uptake of the δ\delta and intermediate PbI3⋅FA\mathrm{PbI_3}\cdot\mathrm{FA} phases. (A) Water uptake per formula unit in the δ\delta and intermediate PbI3⋅FA\mathrm{PbI_3}\cdot\mathrm{FA} phases obtained at 26.85 °C (300 K). The dashed portion of the line is extrapolated from sampling results obtained at lower RH values. The α\alpha phase exhibits negligible water uptake in all grand canonical Monte Carlo (GCMC) simulations and is therefore omitted. Experimentally reported α→δ\alpha\to\delta transition times at different humidity levels are marked for comparison [1, 2, 15]. (B) Water uptake per formula unit in the δ\delta and intermediate PbI3⋅FA\mathrm{PbI_3}\cdot\mathrm{FA} phases obtained at 76.85 °C (350 K). The α\alpha phase exhibits negligible water uptake and is omitted. (C) Burgers transition pathway connecting the α\alpha and δ\delta phases via the intermediate PbI3⋅FA\mathrm{PbI_3}\cdot\mathrm{FA} phase, optimized using the nudged elastic band (NEB) method. The first diffraction peak positions and corresponding interplanar spacings are annotated for each phase.

First, multiple studies have reported a drastic drop in the lifetime of α\alpha-FAPbI3_3 from several months to only a few days, once RH levels exceed approximately 45% (Figure 2A) [1, 2, 15, 16]. This can be explained by the competition for water uptake between the intermediate and δ\delta phases shown in Figure 2A. At RH < 45%, the intermediate phase adsorbs more water than the δ\delta phase. Therefore, the second step of the Burgers path from the intermediate phase to the δ\delta phase involves expulsion of the water interstitials settled in the lattice. This creates an extra barrier and stalls the formation of the δ\delta phase, resulting in a longer α\alpha phase lifetime. When RH > 45%, on the other hand, water uptake of the δ\delta phase surpasses that of the intermediate phase, and the α→δ\alpha\to\delta phase degradation is accelerated drastically. Second, a trace XRD peak at Q≈0.7Q \approx0.7 \AA−1^{-1} has been repeatedly observed at medium RH but disappears at higher RH [10, 17, 18, 19]. The corresponding interplanar spacing of approximately 8.95 \AA{} is consistent with the {001}\{001\} planes of the metastable intermediate phase, suggesting its transient formation during humidity-driven phase transition (Figure 2C).

Conversely, during fabrication, humidity has been widely employed to help accelerate the α\alpha phase formation and improve the quality of the perovskite film [3, 4, 5, 6, 7]. At the elevated fabrication temperatures (≳150\gtrsim150 °C), the water uptake is always higher in the intermediate phase (Figure 2B), promoting the second step of the Burgers path from δ\delta to the intermediate phase and reducing the leftover δ\delta phase impurities in the perovskite film. Therefore, even RH as high as 99% has been reported to improve the lifetime of the produced perovskite films [4].

Together, these findings support the dual effect of humidity, where humidity can either accelerate α→δ\alpha\to\delta degradation or assist δ→α\delta\to\alpha phase conversion and reduce δ\delta phase impurities in the fabricated perovskite film, depending on temperature and the relative water affinities of the competing intermediate and δ\delta phases.

The implications of this mechanism extend beyond perovskites. Layered polymorphs are widespread among ionic solids, including halides, oxides, sulfides, and hydrated minerals, where environmental species such as water can intercalate into and stabilize layered structures. We therefore propose that humidity-mediated stabilization of metastable intermediates may represent a broader mechanism governing phase transitions in ionic solids. Our findings suggest an environment-mediated extension of Ostwald’s step rule, in which external species actively reshape the free-energy landscape, stabilize otherwise transient intermediates, and modulate transition dynamics.

References and Notes

Acknowledgments

The authors acknowledge the research computing facilities provided by the Bohrium Cloud Platform and the Savio computational cluster resource provided by the Berkeley Research Computing program at the University of California, Berkeley (supported by the UC Berkeley Chancellor, Vice Chancellor for Research, and Chief Information Officer). P.T. acknowledges valued discussions with Dr. Linfeng Zhang, Dr. Michele Invernizzi, Dr. Haiyang Niu, Dr. Manyi Yang, Dr. Fuzhi Dai, and Dr. Han Wang.

Funding: P.T. acknowledges funding from the BIDMaP Postdoctoral Fellowship.

References

  1. [1]P. Raval, et al., Understanding instability in formamidinium lead halide perovskites: kinetics of transformative reactions at grain and subgrain boundaries. ACS Energy Letters 7 (4), 1534–1543 (2022).DOI
  2. [2]J. S. Yun, et al., Humidity-induced degradation via grain boundaries of HC(NH₂)₂PbI₃ planar perovskite solar cells. Advanced Functional Materials 28 (11), 1705363 (2018).DOI
  3. [3]D. Lin, et al., Vapor deposited pure α-FAPbI₃ perovskite solar cell via moisture-induced phase transition strategy. Advanced functional materials 32 (48), 2208392 (2022).DOI
  4. [4]Y.-S. Jheng, et al., Realizing High-Performance Vacuum-Deposited Inverted α-FAPbI₃ Perovskite Solar Cells through Saturated-Humidity Annealing. ACS Applied Materials & Interfaces 18 (12), 18049 (2026).DOI
  5. [5]K. Liu, et al., Moisture-triggered fast crystallization enables efficient and stable perovskite solar cells. Nature Communications 13 (1), 4891 (2022).DOI
  6. [6]Y. Ma, et al., Crystallization-activated moisture barrier for high-tolerance manufacturing of perovskite solar cells. Science Advances 11 (43), eady5703 (2025).DOI
  7. [7]J. Cao, et al., Interactions between H₂O and lead halide perovskites: Recent progress and applications. Matter 7 (11), 3728–3755 (2024).DOI
  8. [8]F. Cordero, et al., Influence of temperature, pressure, and humidity on the stabilities and transition kinetics of the various polymorphs of FAPbI₃. The Journal of Physical Chemistry C 124 (42), 22972–22980 (2020).DOI
  9. [9]F. Cordero, F. Craciun, A. M. Paoletti, G. Zanotti, Structural transitions and stability of FAPbI₃ and MAPbI₃: The role of interstitial water. Nanomaterials 11 (6), 1610 (2021).DOI
  10. [10]H. Liu, et al., Reversible Phase Transition for Durable Formamidinium-Dominated Perovskite Photovoltaics. Advanced Materials 34 (39), 2204458 (2022).DOI
  11. [11]A. Kumar, et al., Superior stabilized α-FAPbI₃ perovskite solar cells with efficiency exceeding 24%. Organic Electronics 135, 107143 (2024).DOI
  12. [12]M. Hossain, et al., Balancing moisture and oxygen can match the crystallization dynamics of inert halide perovskite processing. EES Solar 2 (3), 715–723 (2026).DOI
  13. [13]C. Ma, et al., Unveiling facet-dependent degradation and facet engineering for stable perovskite solar cells. Science 379 (6628), 173–178 (2023).DOI
  14. [14]C. Xing, et al., Mechanistic insight into α-to-δ phase transition and stabilizing α-phase FAPbI₃ via regulating δ-phase orientation. Nature Communications (2026).DOI
  15. [15]E. M. Wall, Y.-K. Lin, M. Bawendi, Q. C. Burlingame, Y.-L. Loo, Impact of Processing Environment on Anti-Solvent Free FAPbI₃ Films and Solar Cells. Advanced Energy Materials 16 (7), e03828 (2026).DOI
  16. [16]M. Wang, F. Cao, L. Meng, M. Wang, L. Li, Phase-Transition-Cycle-Induced Recrystallization of FAPbI₃ Film in An Open Environment Toward Excellent Photodetectors with High Reproducibility. Advanced Science 9 (34), 2204386 (2022).DOI
  17. [17]R. T. Wang, A. F. Xu, W. Li, Y. Li, G. Xu, Moisture-stable FAPbI₃ perovskite achieved by atomic structure negotiation. The Journal of Physical Chemistry Letters 12 (22), 5332–5338 (2021).DOI
  18. [18]R. T. Wang, et al., Stable FAPbI₃ hydrate structure by kinetics negotiation for solar cells. Sustainable Energy & Fuels 7 (8), 1974–1980 (2023).DOI
  19. [19]F. Ma, et al., Stable α/δ phase junction of formamidinium lead iodide perovskites for enhanced near-infrared emission. Chemical science 8 (1), 800–805 (2016).DOI

Paper details

vlnc:W_r3w3myz3
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 7

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents