Atomic ironing for conformal interfaces in freestanding oxide nanomembranes

Abstract

Atomically well-defined interfaces are essential for realizing functional interlayer coupling in stacked and twisted oxide heterostructures, yet transferred freestanding oxides can develop structural inhomogeneities, including local curvatures, interfacial voids, and incomplete contacts with substrates. Here, we demonstrate that these transfer-induced structural disorders and imperfections evolve substantially and can be suppressed by post-transfer thermal treatments, yielding bulk-like crystalline freestanding oxide nanomembranes. Using freestanding SrTiO3 membranes as a model system, we report a systematic understanding of the role of "atomic ironing" and the associated evolution of lattice mosaicity, interfacial roughness, and optical bandgap. We further demonstrate atomically bonded conformal interfaces in twisted SrTiO3 heterostructures, highlighting the importance of post-transfer thermal processes. These results establish a synthetic strategy to restore the structural integrity and intrinsic bulk-like functionality of freestanding oxide nanomembranes, enabling stacked, twisted, and heterogeneously integrated oxide architectures with atomically well-defined interfaces for emerging quantum functionalities.

Correspondence to: [email protected]

Notice: This manuscript has been authored by UT-Battelle, LLC, under contract DE-AC05-00OR22725 with the US Department of Energy (DOE). The US government retains and the publisher, by accepting the article for publication, acknowledges that the US government retains a nonexclusive, paid-up, irrevocable, worldwide license to publish or reproduce the published form of this manuscript, or allow others to do so, for US government purposes. DOE will provide public access to these results of federally sponsored research in accordance with the DOE Public Access Plan (http://energy.gov/downloads/doe-public-access-plan).

Introduction

The emergence of cleavable or weakly bonded two-dimensional (2D) materials and freestanding membranes has transformed the design of electronic and quantum systems by enabling heterostructures beyond conventional thermodynamic and epitaxial constraints. In particular, stacking, twisting, and stretching atomically thin layers introduce new structural degrees of freedom that can generate moiré superlattices, correlated electronic states, and tunable optical responses[1, 2, 3, 4, 5, 6, 7] that are absent in their bulk counterparts. Extending these concepts to complex oxides is particularly attractive because their intertwined charge, spin, orbital, and lattice degrees of freedom offer a broader landscape of emergent functionalities[8, 9, 10, 11, 12, 13, 14, 15]. However, unlike van der Waals materials, most oxides cannot be readily exfoliated because of their strong ionic and covalent bondings[16, 17], limiting access to stacked artificial oxide heterostructures.

Recent advances in remote epitaxy and sacrificial-layer liftoff techniques have enabled the fabrication of freestanding oxide membranes, providing a pathway to overcome this limitation[18, 19, 20, 21, 22, 23]. By releasing epitaxial oxides from their parent substrates, these membranes can be heterogeneously integrated with other materials platforms, including silicon and flexible supports, enabling deliberate manipulation through bending[24, 25], stacking[26], and twisting[27, 28, 29, 30, 31]. Moreover, such approaches further enable the monolithic three-dimensional integration of diverse oxide functionalities, including ferroelectricity, magnetism, ionicity, and superconductivity, into microelectronic and quantum-device architectures. Thus, freestanding oxide membranes have emerged as a promising platform for a wide range of technological applications, including flexible electronics, oxide photonics, and moiré heterostructures with novel quantum functionalities.

Realizing this potential, however, requires precise control of the membrane interface after release and transfer. In contrast to the dry-transfer processes commonly used for van der Waals materials[32], sacrificial-layer-based release generally involves wet chemical etching, during which freestanding oxides can develop microscopic and macroscopic imperfections, such as wrinkles, local curvature, interfacial voids, and incomplete contact with the underlying substrate[21, 33, 34]. Their effects are particularly consequential in stacked and twisted oxide heterostructures, where atomically flat and conformal interfaces are essential for controlling interlayer coupling, local atomic registry, charge transfer, and moiré potentials. Yet how transferred oxide membranes can be reconstructed toward atomically conformal interfaces remains poorly understood.

Here, using freestanding SrTiO3\mathrm{SrTiO}_{3} membranes (m-STO) as a model system, we show how the structure and property of oxide membranes, including membrane curvature, lattice mosaicity, interfacial roughness, and optical bandgap, evolve upon a post-transfer thermal treatment, yielding atomically flat, conformal membrane-substrate interfaces. This structural improvement restores the intrinsic optical response without introducing detectable low-energy in-gap states. We further demonstrate that a proper thermal treatment eliminates discernible interfacial gaps in a twisted m-STO heterostructure.

Results and Discussion

To examine the structural changes introduced during membrane release and transfer, we first fabricated freestanding m-STO using a sacrificial-layer-based approach. STO/Sr4Al2O7\mathrm{STO}/\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} (SAO) thin films were epitaxially grown on (001)-oriented TiO2\mathrm{TiO}_{2}-terminated STO substrates by pulsed laser deposition. The SAO sacrificial layer was then selectively dissolved in water, releasing the epitaxial m-STO from the parent substrate (Figure 1a–Figure 1c). The released m-STO was successfully transferred onto a (001)-oriented SiO2/SiSiO_{2}/Si substrate (Figure 1d). The transferred membrane exhibits a continuous and well-defined square geometry without macroscopic tearing or delamination over the SiO2/SiSiO_{2}/Si substrate, indicating the successful release and transfer of the m-STO. During release and transfer, however, freestanding membranes can develop structural inhomogeneities[21, 33], such as local curvature, wrinkles, and interfacial voids, resulting in non-uniform membrane–substrate contacts (Figure 1b). To mitigate these transfer-induced disorders, thermal annealing was employed to promote atomic interface formation between the transferred membrane and the receiving substrate (Figure 1c).

Fabrication and transfer-induced structural evolution of freestanding STO membranes

Figure 1. Fabrication and transfer-induced structural evolution of freestanding STO membranes. (a-c) Schematic illustration of the sacrificial-layer lift-off process. (a) An epitaxial STO membrane (m-STO) grown on a water-soluble Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} (SAO) sacrificial layer is released by dissolving SAO in water. (b) The membrane is then transferred onto a target substrate. (c) Thermal “ironing” is used to flatten the transferred membrane. (d) Optical image of an m-STO transferred onto SiO2\mathrm{SiO}_{2}/Si. (e) X-ray diffraction patterns of the as-grown STO/SAO/STO heterostructure (gray) and m-STOs transferred onto SiO2\mathrm{SiO}_{2}/Si (blue) and Al2O3\mathrm{Al}_{2}\mathrm{O}_{3} (red). (f) X-ray rocking curves (ω\omega) of the as-transferred (AT) m-STO (blue) and the as-grown epitaxial STO film (gray), showing a substantial increase in mosaicity after membrane transfer.

The structural properties of the membranes were first examined by X-ray diffraction (XRD). As shown in Figure 1e, the as-grown STO/SAO/STO heterostructure exhibits sharp diffraction peaks with pronounced Laue oscillations, indicating high-crystalline quality. After transfer, m-STO on both SiO2/SiSiO_{2}/Si and Al2O3Al_{2}O_{3} retain the characteristic STO 001 and 002 reflections near 22.8∘22.8^{\circ} and 46.5∘46.5^{\circ}, respectively, confirming preservation of the structural integrity and crystallinity. However, the diffraction features become significantly broadened compared to the as-grown thin film, suggesting increased structural disorder. Consequently, XRD rocking curve measurements (Figure 1f) reveal a substantial increase in full width at half maximum (FWHM) from ∼0.08∘\sim0.08^{\circ} in the as-grown state to ∼1.0∘\sim1.0^{\circ} after transfer. This peak broadening indicates enhanced mosaicity arising from local bending, lattice tilt variations, and wrinkle formation introduced during the release and transfer processes. In other words, these results indicate that although the SAO-assisted process enables successful release and transfer of crystalline m-STO, the transfer process introduces pronounced structural inhomogeneities[19, 35] that require additional processes to recover atomically uniform membrane–substrate interface.

We next examine the effect of thermal annealing on structural recovery. Figure 2a displays XRD 2θ2\theta–θ\theta scans of m-STO annealed at different temperatures ranging from 300 to 700 °C. While the position of the 002 reflection remains nearly unchanged, the diffraction features become progressively pronounced with increasing annealing temperature, suggesting improved crystallographic coherence and reduced structural disorder. Low-angle X-ray reflectivity (XRR) measurements further reveal the systematic evolution of membrane thickness and surface/interface roughness. As shown in Figure 2b, the XRR oscillations become more pronounced and persist to higher angles with increasing annealing temperature, consistent with improved thickness uniformity and reduced roughness. Quantitative fitting using a multilayer model shows that the effective membrane thickness decreases from ∼13.9\sim13.9 nm at 300 °C to ∼13.0\sim13.0 nm at 600 °C, while the interface roughness is substantially reduced from ∼4.4\sim4.4 to ∼2.9\sim2.9 Å.

Structural evolution upon thermal annealing

Figure 2. Structural evolution upon thermal annealing. (a) XRD 2θ2\theta–θ\theta scans of m-STO samples on SiO2_2/Si after thermal annealing from 300 to 700 °C. The asterisk denotes reflections from the SiO2_2/Si substrate. (b) Low-angle X-ray reflectivity (XRR) profiles of annealed m-STO, along with corresponding fitting results. (c) XRD rocking curves (ω\omega) of the as-transferred and annealed m-STO, showing progressive narrowing of the peak width with increasing annealing temperature. (d) Extracted membrane thickness (deffd_{\mathrm{eff}}), surface/interface roughness (rr), and full width at half maximum (FWHM) of the rocking curve as a function of annealing temperature. The reduction in roughness and FWHM indicates enhanced membrane flattening and improved structural coherence.

Rocking curve analysis of the STO 002 reflection further confirms the annealing-induced structural recovery (Figure 2c). The rocking-curve FWHM decreases from ∼1.0∘\sim1.0^\circ in the as-transferred state to ∼0.1∘\sim0.1^\circ after annealing, approaching the crystallinity of the as-grown film. Figure 2d summarizes the evolution of effective membrane thickness, interface roughness, and rocking-curve FWHM as a function of annealing temperature. Collectively, these results demonstrate that post-transfer thermal annealing effectively recovers the structural uniformity of m-STO by reducing interfacial roughness, mosaicity, and lattice misorientation while improving the membrane–substrate contact.

We next examined whether this structural recovery is accompanied by a corresponding recovery of the intrinsic optical response of the m-STO. STO is a wide bandgap oxide (∼3.2\sim3.2 eV) exhibiting a strong optical absorption in the ultraviolet region associated with O–2p to Ti– 3d3d electronic transitions. Figure 3a illustrates the transmission measurement geometry for m-STO samples on double-side polished Al2O3\mathrm{Al_2O_3} substrates. Transmission spectrum (Figure 3b) show that while the visible-range transmission remains nearly unchanged, the ultraviolet transmission decreases systematically with increasing annealing temperature. The absorption edge becomes sharper and approaches that of single-crystalline STO, indicating an improved optical response.

Optical responses of m-STO following thermal ironing

Figure 3. Optical responses of m-STO following thermal ironing. (a) Schematic illustration of the optical transmission measurement geometry for an m-STO transferred onto a double-side polished sapphire substrate. Incident light (TiT_i) passes through the m-STO and sapphire substrate, while transmitted light (ToT_o) is collected from the opposite side. (b) Optical transmission spectra of as-transferred and annealed m-STO measured from 200 to 800 nm. The transmission becomes closer to that of single-crystalline STO with increasing the annealing temperature. (c) Extracted absorption coefficient (α\alpha) spectra of m-STO. (d) Tauc plots of (αhν)0.5(\alpha h\nu)^{0.5} versus photon energy for the as-transferred and 600 °C annealed membranes. Linear extrapolation indicates that the optical band gap remains unchanged after annealing. (e) Absorption coefficient at 4.8 eV and extracted optical band gap as a function of the annealing temperature.

These observations indicate a correlation between improved structural uniformity and the recovery of the intrinsic optical response of m-STO. Note that we have measured transmission spectrum of the polymer support on double-side polished Al2O3\mathrm{Al_2O_3} substrates to compare with that of STO, which shows distinctive transmission spectra allowing it to be selectively excluded from the data (Figure S1). The extracted absorption coefficient spectra shown in Figure 3c reveal distinct features near 3.8, 4.2, and 4.8 eV, corresponding to intrinsic interband transitions[36, 37, 38]. Notably, the absorption coefficient increases with increasing annealing temperature, particularly in the 4 – 5 eV range, while the peak positions remain unchanged. This behavior indicates that thermal annealing enhances the strength and clarity of intrinsic optical transitions without altering the underlying electronic structure.

To confirm the enhancement of optical absorption without changes in electronic structure, Tauc analysis was performed (Figure 3d and Figure S2). Despite the substantial increase in absorption intensity, the optical band gap remains nearly constant at ∼3.2\sim3.2 eV. This indicates that thermal annealing enhances the optical transition strength without substantially modifying the intrinsic band structure of STO. Consistently, ellipsometry measurements show that the dielectric response of annealed membranes approaches that of bulk STO (Figure S3). Figure 3e summarizes the evolution of the absorption coefficient and band gap with annealing temperature. While the absorption coefficient increases monotonically, the optical band gap remains essentially unchanged, showing that structural recovery is accompanied by enhanced optical transitions without substantial modification of the underlying electronic structure.

To further examine the annealing-induced structural recovery and the membrane-substrate interface at the atomic scale, we performed cross-sectional high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) on as-transferred and annealed m-STO on SiO2\mathrm{SiO}_2/Si, viewed along the STO [110][110] zone axis. The as-transferred m-STO exhibits pronounced structural non-uniformity, including local bending and spatially varying contrast, indicating that the local orientation deviates from the [110][110] zone axis by varying amounts across the membrane (Figure 4a, top). At higher magnification, the top and bottom membrane boundaries appear visibly curved, accompanied by region-to-region contrast variations indicating local membrane distortion after transfer (Figure 4a, bottom). In contrast, after thermal annealing at 600 °C, the m-STO becomes significantly flatter showing uniform contrast across a wide field of view (Figure 4b, top), and the corresponding high-magnification image reveals uniform atomic-column contrast, indicating that the membrane is no longer locally tilted (Figure 4b, bottom). These observations show that thermal annealing suppresses bending and improves the structural uniformity of m-STO on SiO2\mathrm{SiO}_2/Si, resulting in a substantially flatter and more conformal membrane-substrate interface. This atomic-scale picture is consistent with the XRD and XRR results (Figure 2d), which reveal reduced mosaicity and interfacial roughness after annealing.

Cross-sectional STEM analysis of annealing-induced structural enhancements

Figure 4. Cross-sectional STEM analysis of annealing-induced structural enhancements in m-STO on SiO2\mathrm{SiO}_{2}/Si and at twisted m-STO/STO interfaces. (a) Low-magnification (top) and high-magnification (bottom) cross-sectional HAADF-STEM images of as-transferred m-STO on SiO2\mathrm{SiO}_{2}/Si viewed along the STO [110] zone axis, showing region-to-region contrast variations that suggest local membrane bending. (b) Low-magnification (top) and high-magnification (bottom) cross-sectional HAADF-STEM images of annealed m-STO on SiO2\mathrm{SiO}_{2}/Si. After annealing, the membrane exhibits a flatter morphology with uniform lattice contrast, indicating reduced local bending. (c) HAADF-STEM images and corresponding EDS elemental maps of Sr, Ti, and Sr+Ti for an annealed, twisted m-STO sample on an STO substrate with a twist angle (ϕTwist\phi_{\mathrm{Twist}}) of ∼11.1∘\sim11.1^\circ. The EDS maps show a uniform, atomically flat interface without gaps. (d) Ti and Sr intensity profiles acquired across the interface along the region indicated in (c). The red arrow marks the m-STO/STO interface.

Having established that thermal annealing suppresses structural inhomogeneities in oxide membranes, we next examine whether this structural recovery extends to interfaces in twisted oxide geometries. In such structures, residual interfacial gaps weaken interlayer coupling and may hinder moiré-driven emergent quantum phenomena[30, 31, 33, 39, 40]. To investigate this, we transferred an m-STO sample onto an STO substrate with a twist angle of ϕTwist≈11.1∘\phi_{Twist} \approx11.1^\circ and subsequently annealed at 600 °C (Figure S4). Cross-sectional HAADF-STEM shown in Figure 4c reveals a uniform, atomically flat m-STO/STO interface without discernible interfacial gaps. Higher-magnification imaging, together with Sr and Ti elemental maps acquired by energy-dispersive spectroscopy (EDS), resolves the atomic structure and elemental connection across the twisted interface. The corresponding Sr and Ti intensity profiles, extracted along the direction indicated by the white arrow in Figure 4c, show an abrupt transition across the m-STO/STO boundary (Figure 4d), further confirming the formation of a well-defined atomic-scale interface. These results demonstrate that thermal annealing can establish conformal interfacial contact even between crystallographically twisted oxide layers, providing a structural basis for constructing stacked and twisted oxide heterostructures with atomically well-defined interfaces.

Conclusion and outlook

In summary, we demonstrate that thermal annealing enables transferred freestanding oxide membranes to recover structural uniformity and form atomically flat, conformal interfaces with the underlying substrate. X-ray diffraction and cross-sectional STEM measurements reveal a substantial reduction in membrane curvature, lattice mosaicity, and interfacial roughness, accompanied by enhanced membrane–substrate contact. This structural recovery restores the intrinsic optical response of STO membranes without introducing detectable low-energy in-gap states. We further demonstrate thermal “ironing” as the critical step to twist-oxide membranes with with no discernible interfacial gaps, thereby, creating atomically conformal interfaces. Such control over membrane–substrate conformity and interfacial uniformity provides an important foundation for stacked, twisted, and heterogeneous oxide architectures, in which well-defined interfaces and structural coherence are critical for enabling emergent quantum phenomena.

Methods

Growth of epitaxial oxide heterostructure

Epitaxial SrTiO3\mathrm{SrTiO}_{3} (STO)/Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} heterostructures were grown on (001) STO substrates using pulsed laser deposition. A single-crystalline STO target was used, while for Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} thin films, a sintered polycrystalline Sr3Al2O6\mathrm{Sr}_{3}\mathrm{Al}_{2}\mathrm{O}_{6} target was used. Before deposition, (001)-oriented STO single-crystal substrates (Crystec GmbH, dimensions of 5×5×1 mm35 \times5 \times1\ \mathrm{mm}^{3}) were treated with the buffered oxide etcher followed by annealing at 1100 ∘C1100\,^{\circ}\mathrm{C} to obtain a TiO2\mathrm{TiO}_{2}-terminated surface.

Film growth was performed using a KrF excimer laser (Coherent LPXpro 305 F, λ=248 nm\lambda= 248\ \mathrm{nm}) with a laser fluence fixed at 1.0 Jcm−21.0\ \mathrm{J}\mathrm{cm}^{-2}. A 20 nm20\ \mathrm{nm} water-soluble Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} sacrificial layer was first deposited at 750 ∘C750\,^{\circ}\mathrm{C} under oxygen partial pressure of 15 mTorr15\ \mathrm{mTorr}. Subsequently, STO films were grown epitaxially on Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} films at 700 ∘C700\,^{\circ}\mathrm{C} and 15 mTorr15\ \mathrm{mTorr} of oxygen. The growth process was monitored real time using in situ reflection high-energy electron diffraction.

Release and transfer of freestanding SrTiO3 membranes

To provide mechanical support for the membrane during the selective etching of the Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} sacrificial layer in water, 2 μL2\ \mu\mathrm{L} of a poly(propylene carbonate) (PPC; Sigma-Aldrich) solution, prepared by dissolving 10 g10\ \mathrm{g} of PPC in 100 mL100\ \mathrm{mL} of anisole, was drop-cast onto the epitaxial heterostructures. The PPC coating was then cured on a hot plate at 70 ∘C70\,^{\circ}\mathrm{C} for 10 min10\ \mathrm{min}. The sample was subsequently immersed in deionized water at room temperature, allowing the Sr4Al2O7\mathrm{Sr}_{4}\mathrm{Al}_{2}\mathrm{O}_{7} sacrificial layer to dissolve selectively. After dissolution, the PPC-supported membranes were detached from the parent substrate and transferred onto a desired substrate. Finally, the PPC support layer was removed by thermal decomposition in air at 250 ∘C250\,^{\circ}\mathrm{C} for 1 h1\ \mathrm{h}, yielding freestanding STO membranes.

Structural characterization of freestanding oxide membranes

X-ray diffraction (XRD) using a four-circle high-resolution X-ray diffractometer (X’Pert Pro, PANalytical; Cu Kα1K\alpha_1 radiation) was used to confirm the structural properties of the crystalline films. To investigate the atomic structure of the freestanding membranes, atomic-resolution imaging was performed using HAADF-STEM. Cross-sectional STEM lamellae oriented along the STO [110] zone axis were prepared using a focused ion beam (FIB) system (FEI Helios G4). Prior to milling, about 15 nm-thick carbon layer was deposited by electron beam-induced deposition using a gas injection system in the SEM to protect the surface. STEM imaging was carried out using an aberration-corrected, monochromated microscope (Thermo Fisher Scientific Themis Z) operated at an accelerating voltage of 300 kV, with a convergence semi-angle of 18 mrad and a HAADF collection semi-angle of 50-200 mrad. Energy-dispersive X-ray spectroscopy (EDS) was performed on the same instrument using a probe current of 100 pA and a pixel dwell time of 2 μ\mus, with acquisition of 300 frames for integration.

Optical measurement on freestanding SrTiO3\mathrm{SrTiO_3} membranes

Transmission measurement

Transmission spectra were obtained using a PerkinElmer Lamda 950, equipped with tungsten-halogen and deuterium lamps and PMT and PbS detectors, covering the spectral range from 175 to 3300 nm. The absorption coefficient was calculated using the membrane thickness and substrate transmission. Samples were mounted on a 1 mm pinhole holder.

Ellipsometry measurement

Spectroscopic ellipsometry was performed using an M-2000 ellipsometer (J.A. Woollam Co.) to obtain the real (ε1\varepsilon_1) and imaginary (ε2\varepsilon_2) parts of the dielectric function. Prior to all measurements, the instrument was calibrated at 300 K using a 25 nm SiO2\mathrm{SiO_2}/Si wafer to minimize the mean square error (MSE) of the optical signal. Ellipsometric spectra were acquired at an incident angle of 70∘70^\circ, yielding Ψ\Psi and Δ\Delta over the photon-energy range of 0.74 - 6.46 eV.

Acknowledgments

This work was sponsored by the U.S. Department of Energy, Office of Science, Basic Energy Sciences, Materials Sciences and Engineering Division. Part of optical spectroscopy and data analysis work at University of Kentucky was supported by the National Science Foundation Grant No. DMR-2426874. Cross-sectional microscopy work was supported by the National Research Foundation of Korea (NRF) grant funded by the Korean government (MSIT) (No. RS-2021-NR060087).

Author contributions

J. S. and H. N. L. conceived the idea and designed the experiments; J. S. and H. N. L. performed freestanding membrane fabrication, characterization, and data analysis with the help of T. J. S., Y.-H. K., H. M., and J. Y.; K.-Y. P. and C. S. C. performed the STEM measurements; K. K. and A. S., performed optical transmission measurement and related analysis; J. S. and H. N. L. wrote the manuscript with contributions from all authors.

Additional information

Supplementary Information is available in the online version of the paper. Correspondence and requests for materials should be addressed to H-. N-. L.

Data availability

The data supporting the findings of this study are available from the corresponding author upon request.

Competing financial interests

The authors declare no competing financial interests.

References

  1. [1]Manzeli, S.; Ovchinnikov, D.; Pasquier, D.; Yazyev, O. V.; Kis, A. 2D transition metal dichalcogenides. Nature Reviews Materials 2017, 2 (8), 17033. DOI: 10.1038/natrevmats.2017.33.DOI
  2. [2]Castro Neto, A. H.; Guinea, F.; Peres, N. M. R.; Novoselov, K. S.; Geim, A. K. The electronic properties of graphene. Reviews of Modern Physics 2009, 81 (1), 109-162. DOI: 10.1103/RevModPhys.81.109.DOI
  3. [3]Novoselov, K. S.; Mishchenko, A.; Carvalho, A.; Castro Neto, A. H. 2D materials and van der Waals heterostructures. Science 2016, 353 (6298), aac9439. DOI: 10.1126/science.aac9439.DOI
  4. [4]Jariwala, D.; Marks, T. J.; Hersam, M. C. Mixed-dimensional van der Waals heterostructures. Nature Materials 2017, 16 (2), 170-181. DOI: 10.1038/nmat4703.DOI
  5. [5]Geim, A. K.; Grigorieva, I. V. Van der Waals heterostructures. Nature 2013, 499 (7459), 419-425. DOI: 10.1038/nature12385.DOI
  6. [6]Oh, M.; Nuckolls, K. P.; Wong, D.; Lee, R. L.; Liu, X.; Watanabe, K.; Taniguchi, T.; Yazdani, A. Evidence for unconventional superconductivity in twisted bilayer graphene. Nature 2021, 600 (7888), 240-245. DOI: 10.1038/s41586-021-04121-x.DOI
  7. [7]Cao, Y.; Fatemi, V.; Fang, S.; Watanabe, K.; Taniguchi, T.; Kaxiras, E.; Jarillo-Herrero, P. Unconventional superconductivity in magic-angle graphene superlattices. Nature 2018, 556 (7699), 43-50.DOI
  8. [8]Hwang, H. Y.; Iwasa, Y.; Kawasaki, M.; Keimer, B.; Nagaosa, N.; Tokura, Y. Emergent phenomena at oxide interfaces. Nature materials 2012, 11 (2), 103-113.
  9. [9]Bednorz, J. G.; Müller, K. A. Perovskite-type oxides---The new approach to high-${T}_{c}$ superconductivity. Reviews of Modern Physics 1988, 60 (3), 585-600. DOI: 10.1103/RevModPhys.60.585.DOI
  10. [10]Kalisky, B.; Bert, J. A.; Klöper, B. B.; Bell, C.; Sato, H. K.; Hosoda, M.; Hikita, Y.; Hwang, H. Y.; Moler, K. A. Critical thickness for ferromagnetism in LaAlO3/SrTiO3 heterostructures. Nature Communications 2012, 3 (1), 922. DOI: 10.1038/ncomms1931.DOI
  11. [11]Lee, D.; Lu, H.; Gu, Y.; Choi, S. Y.; Li, S. D.; Ryu, S.; Paudel, T. R.; Song, K.; Mikhееv, E.; Lee, S.; et al. Emergence of room-temperature ferroelectricity at reduced dimensions. Science 2015, 349 (6254), 1314-1317. DOI: 10.1126/science.aaa6442.DOI
  12. [12]Park, D. S.; Hadad, M.; Riemer, L. M.; Ignatans, R.; Spirito, D.; Esposito, V.; Tileli, V.; Gauquelin, N.; Chezganov, D.; Jannis, D.; et al. Induced giant piezoelectricity in centrosymmetric oxides. Science 2022, 375 (6581), 653-657. DOI: 10.1126/science.abm7497.DOI
  13. [13]Tokura, Y.; Nagaosa, N. Orbital Physics in Transition-Metal Oxides. Science 2000, 288 (5465), 462-468. DOI: 10.1126/science.288.5465.462.DOI
  14. [14]Lee, H. N.; Christen, H. M.; Chisholm, M. F.; Rouleau, C. M.; Lowndes, D. H. Strong polarization enhancement in asymmetric three-component ferroelectric superlattices. Nature 2005, 433 (7024), 395-399. DOI: 10.1038/nature03261.DOI
  15. [15]Van Tendeloo, G.; Lebedev, O.; Hervieu, M.; Raveau, B. Structure and microstructure of colossal magnetoresistant materials. Reports on Progress in Physics 2004, 67 (8), 1315-1365.
  16. [16]Bakaul, S. R.; Serrao, C. R.; Lee, M.; Yeung, C. W.; Sarker, A.; Hsu, S.-L.; Yadav, A. K.; Dedon, L.; You, L.; Khan, A. I. Single crystal functional oxides on silicon. Nature communications 2016, 7 (1), 10547.DOI
  17. [17]Lu, H.; Lipatov, A.; Ryu, S.; Kim, D. J.; Lee, H.; Zhuravlev, M. Y.; Eom, C. B.; Tsymbal, E. Y.; Sinitskii, A.; Gruverman, A. Ferroelectric tunnel junctions with graphene electrodes. Nature Communications 2014, 5 (1), 5518. DOI: 10.1038/ncomms6518.DOI
  18. [18]Chiabrera, F. M.; Yun, S.; Li, Y.; Dahm, R. T.; Zhang, H.; Kirchert, C. K.; Christensen, D. V.; Trier, F.; Jespersen, T. S.; Pryds, N. Freestanding perovskite oxide films: Synthesis, challenges, and properties. Annalen der Physik 2022, 534 (9), 2200084.
  19. [19]Choo, S.; Varshney, S.; Liu, H.; Sharma, S.; James, R. D.; Jalan, B. From oxide epitaxy to freestanding membranes: Opportunities and challenges. Science Advances 10 (50), eadg8561. DOI: 10.1126/sciadv.adg8561.DOI
  20. [20]Nian, L.; Sun, H.; Wang, Z.; Xu, D.; Hao, B.; Yan, S.; Li, Y.; Zhou, J.; Deng, Y.; Hao, Y. Sr4Al2O7: A new sacrificial layer with high water dissolution rate for the synthesis of freestanding oxide membranes. Advanced Materials 2024, 36 (15), 2307682.DOI
  21. [21]Zhang, J.; Lin, T.; Wang, A.; Wang, X.; He, Q.; Ye, H.; Lu, J.; Wang, Q.; Liang, Z.; Jin, F.; et al. Super-tetragonal Sr4Al2O7 as a sacrificial layer for high-integrity freestanding oxide membranes. Science 2024, 383 (6681), 388-394. DOI: 10.1126/science.adi6620.DOI
  22. [22]Lu, D.; Baek, D. J.; Hong, S. S.; Kourkoutis, L. F.; Hikita, Y.; Hwang, Harold Y. Synthesis of freestanding single-crystal perovskite films and heterostructures by etching of sacrificial water-soluble layers. Nature Materials 2016, 15 (12), 1255-1260. DOI: 10.1038/nmat4749.DOI
  23. [23]Kim, Y.; Cruz, S. S.; Lee, K.; Alawode, B. O.; Choi, C.; Song, Y.; Johnson, J. M.; Heidelberger, C.; Kong, W.; Choi, S.; et al. Remote epitaxy through graphene enables two-dimensional material-based layer transfer. Nature 2017, 544 (7650), 340-343. DOI: 10.1038/nature22053.DOI
  24. [24]Hong, S. S.; Gu, M.; Verma, M.; Harbola, V.; Wang, B. Y.; Lu, D.; Vailionis, A.; Hikita, Y.; Pentcheva, R.; Rondinelli, J. M.; et al. Extreme tensile strain states in La0.7Ca0.3MnO3 membranes. Science 2020, 368 (6486), 71-76. DOI: 10.1126/science.aax9753.DOI
  25. [25]Xu, R.; Huang, J.; Barnard, E. S.; Hong, S. S.; Singh, P.; Wong, E. K.; Jansen, T.; Harbola, V.; Xiao, J.; Wang, B. Y. Strain-induced room-temperature ferroelectricity in SrTiO3 membranes. Nature communications 2020, 11 (1), 3141.
  26. [26]Harbola, V.; Crossley, S.; Hong, S. S.; Lu, D.; Birkholzer, Y. A.; Hikita, Y.; Hwang, H. Y. Strain gradient elasticity in SrTiO3 membranes: bending versus stretching. Nano letters 2021, 21 (6), 2470-2475.DOI
  27. [27]Sánchez-Santolino, G.; Rouco, V.; Puebla, S.; Aramberri, H.; Zamora, V.; Cabero, M.; Cuellar, F. A.; Munuera, C.; Mompean, F.; Garcia-Hernandez, M.; et al. A 2D ferroelectric vortex pattern in twisted BaTiO3 freestanding layers. Nature 2024, 626 (7999), 529-534. DOI: 10.1038/s41586-023-06978-6.
  28. [28]Kim, M.-S.; Lee, K.; Ishikawa, R.; Song, K.; Shahed, N. A.; Eom, K.-T.; Rzechowski, M. S.; Tsymbal, E. Y.; Shibata, N.; Mizoguchi, T. Charge Density Proportionation at Twisted SrTiO3 Bilayer Interface Driven by Local Atomic Registry. ACS nano 2025, 19 (46), 39714-39724.DOI
  29. [29]Tenreiro, I.; Aramberri, H.; Rouco, V.; Sánchez-Santolino, G.; Cabero, M.; Gallego, F.; Sánchez-Manzano, D.; González-Calbet, J. M.; Mompeán, F.; García-Hernández, M. Flexoelectrically Induced Polar Topology in Twisted SrTiO3 Membranes. Advanced Materials 2026, e12969.DOI
  30. [30]Kp, H.; Wei, X.; Lee, C. H.; Yoon, D.; Lee, Y.; Crust, K. J.; Shao, Y. T.; Xu, R.; Kang, J. H.; Liang, C. Mind the Gap—Imaging Buried Interfaces in Twisted Oxide Moirés. Advanced Materials 2026, e21189.DOI
  31. [31]Kim, Y.-H.; Ghanbari, R.; Jung, M.-H.; Zhang, Y.; Kim, Y.-M.; Xu, R.; Chi, M. Establishing Atomic Coherence in Twisted Oxide Membranes Containing Volatile Elements. Advanced Materials 2026, n/a (n/a), e74365. DOI: https://doi.org/10.1002/adma.74365.
  32. [32]Kinoshita, K.; Moriya, R.; Onodera, M.; Wakafuji, Y.; Samubuchi, S.; Watanabe, K.; Taniguchi, T.; Machida, T. Dry release transfer of graphene and few-layer h-BN by utilizing thermoplasticity of polypropylene carbonate. npj 2D Materials and Applications 2019, 3 (1), 22. DOI: 10.1038/s41699-019-0104-8.
  33. [33]Wang, H.; Harbola, V.; Wu, Y. J.; van Aken, P. A.; Mannhart, J. Interface Design beyond Epitaxy: Oxide Heterostructures Comprising Symmetry-Forbidden Interfaces. Advanced Materials 2024, 36 (32), 2405065.arxiv.org/abs/2403.08736
  34. [34]Segantini, G.; Hsu, C.-Y.; Rischau, C. W.; Blah, P.; Matthiesen, M.; Gargilio, S.; Triscone, J.-M.; Alexander, D. T. L.; Caviglia, A. D. Electron-Beam Writing of Atomic-Scale Reconstructions at Oxide Interfaces. Nano Letters 2024, 24 (45), 14191-14197. DOI: 10.1021/acs.nanolett.4c02913.DOI
  35. [35]Varshney, S.; Choo, S.; Thompson, L.; Yang, Z.; Shah, J.; Wen, J.; Koester, S. J.; Mkhoyan, K. A.; McLeod, A. S.; Jalan, B. Hybrid molecular beam epitaxy for single-crystalline oxide membranes with binary oxide sacrificial layers. ACS nano 2024, 18 (8), 6348-6358.DOI
  36. [36]van Benthem, K.; Elsässer, C.; French, R. H. Bulk electronic structure of SrTiO3: Experiment and theory. Journal of Applied Physics 2001, 90 (12), 6156-6164. DOI: 10.1063/1.1415766.DOI
  37. [37]Kok, D. J.; Irmscher, K.; Naumann, M.; Guguschev, C.; Galazka, Z.; Uecker, R. Temperature-dependent optical absorption of SrTiO3. physica status solidi (a) 2015, 212 (9), 1880-1887. DOI: https://doi.org/10.1002/pssa.201431836.
  38. [38]Lee, H. N.; Ambrose Seo, S. S.; Choi, W. S.; Rouleau, C. M. Growth control of oxygen stoichiometry in homoepitaxial SrTiO3 films by pulsed laser epitaxy in high vacuum. Scientific Reports 2016, 6 (1), 19941. DOI: 10.1038/srep19941.DOI
  39. [39]Moon, J.-Y.; Bae, S.; Ryu, J.; Kim, S.-I.; Han, S.; Kim, J. S.; Choi, J.; Kim, S.; Lee, J.-H.; Choi, S.-G.; et al. Crack-Free Transfer of Wafer-Scale Freestanding Single-Crystalline Nanomembranes Enabled by Elastically Graded Polymer. Advanced Materials 2026, 38 (1), e13080. DOI: https://doi.org/10.1002/adma.202513080.
  40. [40]Li, Y.; Xiang, C.; Chiabrera, F. M.; Yun, S.; Zhang, H.; Kelly, D. J.; Dahm, R. T.; Kirchert, C. K. R.; Cozannet, T. E. L.; Trier, F.; et al. Stacking and Twisting of Freestanding Complex Oxide Thin Films. Advanced Materials 2022, 34 (38), 2203187. DOI: https://doi.org/10.1002/adma.202203187.

Paper details

vlnc:W_r7hd9223
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 2

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents