Spontaneous Circular Dichroism and Memory Effect from Surface Defects in Altermagnetic MnTe
Abstract
Altermagnetism has emerged as a new class of magnetism with vanishing magnetization and macroscopic time reversal symmetry breaking. Hexagonal MnTe is a g-wave altermagnet with a 307 K Néel temperature, large spin splitting, and an anomalous Hall effect. However, the relationship between altermagnetism and the anomalous Hall effect in MnTe remains debated. Here, using optical magnetic circular dichroism, we observe hysteresis and a memory effect in a MnTe bulk crystal below 250 K. No hysteresis is seen after polishing the bulk crystal and in thin films. We conclude that the hysteresis in magnetic circular dichroism in the bulk crystal is from surface defects. The similar temperature dependence and a sign change between circular dichroism and the anomalous Hall effect indicate that the origin of the anomalous Hall effect in transport is likely not intrinsic.
Altermagnetism (AM) is a recently identified class of compensated magnetic materials that host spin-dependent transport phenomena, typically associated with ferromagnets (FM), despite vanishing net magnetization, typically associated with antiferromagnets (AFM) [1, 2, 3, 4, 5, 6, 7]. In AMs, two opposite spin sublattices are related by time reversal combined with a lattice rotation, rotoinversion, or a mirror symmetry. This symmetry combination causes a nonrelativistic spin-splitting of the electronic bands with d-, g-, or i-wave symmetry, even in the absence of spin-orbit coupling. The spin-split band structure enables AMs to exhibit spin-dependent transport phenomena including spin currents and an anomalous Hall effect (AHE) despite the nearly vanishing net magnetization. The AHE in altermagnets is particularly notable because it provides a route for electronic readout of time-reversed magnetic domains, directly addressing a significant obstacle for conventional AFM spintronics [4, 5, 8, 9].
Hexagonal MnTe (–MnTe) has emerged as a textbook semiconducting altermagnet. –MnTe crystallizes in the NiAs-type structure (space group ), with stacked triangular layers of Mn and Te atoms and a band gap of 1.4 eV. A magnetic transition occurs at K [10]. In the magnetic state Mn atoms display ferromagnetic order in the ab plane with an AFM-like vertical stacking. Nonrelativistic spin splitting (ARPES) [11, 12, 13] and chiral magnons [14, 15] have both been observed in –MnTe, providing direct evidence of AM order and experimentally establishing the field of altermagnetism. The observation of the anomalous Hall effect (AHE) [16, 17, 18, 19, 20, 21, 22] provides in the indirect evidence, but demonstrates the excitement for electric read-out of 180 degree Néel vector switching.
Prior reports of the AHE in -MnTe show several significant discrepancies between the AHE and the AM order parameter. First, the AHE often turns on around 280 K, noticeably below the AM transition temperature [16, 18, 19, 20, 21, 22]. Second, the hysteresis loop changes sign around 200 K with no shrinking of the coercive field. This sign change remains poorly understood but is thought to be driven by changes in the Berry curvature instead of changes in the real-space-magnetization [19, 20]. Lastly, the exact temperature dependence shows significant variation among samples [16, 17, 18, 19, 20, 21, 22] with Ref. [19] reporting that the AHE occurs only when the thermal activation energy is 15–18 meV. These puzzling results have received different interpretations, raising questions about the relationship between the AHE and AM order in MnTe and motivating further investigation of how the magnetic state couples to the electronic transport properties.
Optical probes, such as magnetic circular dichroism (MCD), can study magnetic domains with micrometer spatial resolution [23, 24, 25, 26, 27, 28]. MCD is the difference in absorption of left- and right-hand circularly polarized light. MCD is proportional to the index of refraction difference for right-hand and left-hand circularly polarized light, where and are the transverse and longitudinal dielectric tensor components at a given photon energy [29, 30]. The dielectric constants are related to the optical conductivity. MCD probes the off-diagonal elements of the conductivity tensor making MCD an optical analogue to the AHE [31]. Both x-ray MCD and magnetic linear dichroism have been previously employed to image AM domains in −MnTe thin films [32, 33].
A non-zero static magneto-optical Kerr effect (MOKE) was predicted in −MnTe [34], time-resolved magneto-optical effects were observed in MnTe thin films [35], and static MOKE was recently reported at infrared wavelengths [36, 37], but the origin was not clear.
Here we observe spontaneous optical MCD hysteresis in a MnTe bulk crystal with an onset of around 250 K, well below the 307 K Néel temperature. We also observe a magnetic memory effect that shifts the center of the hysteresis loop away from 0 T. Field cooling the sample shifts hysteresis in the direction of the applied field. After polishing the sample no hysteresis or spontaneous MCD was observed. Thin films grown using molecular beam epitaxy (MBE) on InP (111) also showed no hysteresis. We attribute the hysteresis to a surface-defect state and the shift to a magnetic memory effect. Our results suggest the MCD in MnTe originates from surface defects rather than bulk altermagnetic order.
Our main MnTe bulk crystal was grown using a Bi-Te flux method. Under an argon atmosphere, Mn, Te, and Bi were mixed in a molar ratio of 1:16:10 and loaded into an alumina crucible. The crucible was then sealed in an evacuated quartz tube and heated to 900 °C over 3 hours where it was held for 12 hours to promote homogeneous melting. Subsequently, the temperature was lowered to 610 °C over 12 hours, followed by a slower cooling to 595 °C over 200 hours to promote single-crystal growth. Finally, the Bi-Te flux was removed by centrifugation. Measurements were initially preformed on shiny regions of the naturally formed facet without additional surface preparation.
The field-dependent CD from this bulk crystal is shown in Figure 1a. The CD was measured with a 633 nm continuous wave HeNe laser. Both the laser and applied magnetic field are normal to the sample surface. The sample was cooled from 300 K to the lowest temperature (50 K or 75 K) with no applied magnetic field and the hysteresis loop was measured. Then the sample was warmed with no applied field and the next loop was measured, until the highest temperature hysteresis loop was measured.

Figure 1. a, b) Temperature dependent circular dichroism hysteresis loops after consecutive zero field coolings from 300 K. Hysteresis turns on below 225–250 K and changes sign below 200 K. At lower temperatures, the hysteresis loop shifts to negative fields. c) Hysteresis loops after cooling the sample with a +3 T field from 300 K. The sign of the hysteresis does not change, but loop now shifts to positive fields. Hysteresis loops in a-c were taken when warming after cooling the sample. No field was applied when changing temperature. d) CD mapping of the bulk crystal taken at +1 T and at 200 K. Red and blue regions show time-reversed domains are simultaneously present. e) The anomalous component of the CD loops after zero field cooling as a function of temperature. Values are extracted from the data in Figure 1b. The anomalous component is taken at the field the hysteresis loop is centered on. The anomalous component is defined as half the difference between the two domains at this field where refers to when sweeping from positive field (+) and negative (−) to .
Despite cooling with no magnetic field, the hysteresis loops are shifted and not centered at 0 T. At low temperatures the hysteresis loops are shifted towards negative fields. As the sample warms, the hysteresis loop reverses sign between 150 K and 200 K and becomes positively shifted. Hysteresis then disappears above 225 K. A second temperature sweep at the same spot is shown in Figure 1b. The second run was taken after zero field cooling the sample from 300 K. Once again the hysteresis loop is shifted and then changes sign between 150 K and 200 K. However, we observe that loops at the same temperature (100 K, 150 K, and 200 K for examples) are different in these two runs. A mapping taken at 200 K is shown in Figure 1d. The presence of red and blue regions, showing opposite CD signs, means time-reversal domains spontaneously form upon zero field cooling the sample.
The onset of hysteresis below the 307 K Néel temperature and the sign change around 200 K are consistent with prior AHE measurements on MnTe thin films and bulk crystals [16, 17, 18, 19, 20, 21, 22]. The temperature dependence suggests the observed hysteresis has the same microscopic origin as the AHE in MnTe. We attribute the shift to a magnetic memory effect, as discussed later. The temperature dependent spontaneous component of the CD signal is shown in Figure 1e. The spontaneous component is defined as half the difference between the two domains at the center of the hysteresis loop, , where refers to the field halfway between the two coercive fields when swept from the maximum positive (+) or negative field (−). After the hysteresis sign change, the spontaneous component, within experimental uncertainty, shows no clear temperature dependence. To further probe the shift of the hysteresis, we field-cooled the crystal with T and remeasured the hysteresis loops while warming the sample. As seen in Figure 1c, field cooling the bulk crystal does not change the sign of hysteresis, but it shifts the hysteresis loop in the positive field direction. This is further shown in Figure 2a. Hysteresis loops at 200 K were measured immediately after cooling the sample with the noted magnetic field. Switching the direction of the applied cooling field switches the direction in which the hysteresis loop is shifted.
Figure 2. a) Field sweeps at 200 K after cooling the sample with ±3 T and 0 T cooling. Switching the sign of the field when cooling the sample switches the direction the hysteresis loop shifts. b) Consecutive field sweeps at 100 K immediately after cooling the sample with a +5 T field from 250 K. The coercive field becomes slightly larger after the first hysteresis loop.
The shift in the hysteresis loop is reminiscent of exchange bias at FM-AFM interfaces. Based on the observed temperature dependence, we hypothesize that the MCD hysteresis shares a microscopic origin with the AHE in MnTe, while an additional magnetic system is needed to pin domains and shift the hysteresis loop. Since we observe one shifted hysteresis loop the second spin system is not switched during our measurement and does not contribute to the observed MCD. If the second spin system were also switched, we expect it would keep the hysteresis loop centered at zero field. This second system either has a spin configuration that does not couple to the applied magnetic field and produce a CD signal, or is not optically accessible and has a coercive field above T.
Figure 2b shows five consecutive field sweeps at 100 K after field cooling the sample with T. The hysteresis loop widens by 0.5 T after the first loop, then narrow by 0.1 T each on the third and fourth loops, and widens by 0.16 T on the fifth loop. These changes are larger than the approximate 0.02 T steps between data points, suggesting that the hysteresis depends, in part, on the history of the applied magnetic field. Training effects in conventional exchange bias cause the shift to decrease and is typically absent when the AFM is a single crystal [38]. Another deviation from conventional exchange bias is that we are measuring a single material bulk crystal and lack a known FM-AFM interface.
A field-tunable "positive exchange bias" in a single material bulk crystal was previously reported in the ferromagnetic Weyl semimetal [39, 40, 41] and recently attributed to a magnetic memory effect [41]. The memory effect caused the shape, saturation, and shift of the magnetization and AHE hysteresis loops to depend on temperature, maximum applied magnetic field, and the previously applied magnetic field. Microscopically the memory effect originates from a dilute secondary spin population distinct from the ferromagnetic moments on the Co atoms. In addition to the 175 K Curie temperature [42], was known to have another sample-dependent temperature scale of 125–150 K [40, 41, 43, 44]. Above this additional temperature scale hysteresis loops typically form a "bow tie" shape, where the magnetization shows a sudden partial jump then scales linearly with the applied magnetic field [40, 41, 43]. At higher temperatures, the "soft" magnetic anisotropy may cause a multi-domain configuration to be stable. The external magnetic field may not be enough to completely overcome the energy barrier between domains making switching incomplete. At lower temperatures, the magnetic anisotropy "hardens," causing domain switching to be complete and a rectangular hysteresis loop. However, the secondary spin population does not flip, causing the two coercive fields to be unequal and shifting the center of the hysteresis loop from 0 T. Ref. [41] proposes the secondary spin population resides at either the sample surface or stoichiometric off-sites, but to our knowledge the microscopic origin remains unknown. A dilute secondary spin system in our MnTe bulk crystal would explain the shifted hysteresis loop in the absence of a magnetic interface. Field cooling would set the secondary spin direction thus changing the direction the hysteresis loop is shifted in.
To better probe the connection between bulk AM order and the observed hysteresis, we polished the MnTe bulk crystal and repeated the MCD measurements. Polishing the sample should not remove a bulk AM contribution as demonstrated by MOKE measurements of hematite [45, 46, 47]. Polishing the bulk crystal removes microcraters from the sample surface, much greater than the optical penetration depth typically around 50 nm for doped semiconductors above the gap, allowing us to probe freshly exposed crystallographic planes. As shown in Figure 3c all hysteresis disappears after polishing the bulk crystal. Figure 3 shows no MCD hysteresis in a MBE-grown thin film on InP, despite showing an AHE in dc transport [18]. The thin film was grown using the procedure described in Refs. [18] and [48]. We also measured two separate bulk crystals grown using chemical vapor transport described in Refs. [19]. Both additional bulk crystals showed an AHE in dc transport, but no spontaneous MCD. The disappearance of spontaneous MCD hysteresis upon polishing and its absence in samples that exhibit an AHE indicate a non-robust surface effect, potentially arising from surface defects.
Figure 3. Microscope images of the MnTe bulk crystal with a 5x microscope objective a) before polishing and b) after polishing. Each image is about 3 mm by 3 mm. c) Hysteresis loops taken at select temperatures of a) polished MnTe bulk crystal and d) capped thin film on InP. Neither sample shows MCD hysteresis. The absence of hysteresis suggests the observed hysteresis above and exchange bias is sensitive to the surface of the bulk crystal.
The absence of MCD despite an AHE in dc transport was previously reported in MnTe thin films grown on InP and GaAs [18, 22]. Both studies also reported multiple distinct spin populations in their films, suggesting multiple distinct spin populations, but gave different interpretations. Magnetization curves in Ref. [18] showed exchange bias, which was attributed to ferromagnetic impurities pinned by an altermagnet. If the spontaneous MCD and the AHE originate from magnetic impurities, as proposed in Ref. [18], then a lower impurity concentration could reduce the spontaneous MCD below our optical sensitivity limit.
Since MnTe is a self-doped semiconductor [18, 19, 49], the narrow thermal activation energy window to observe an AHE, reported in Ref. [19], is consistent with variable-range hopping type transport due to disorder. Ref. [19] also found that below 80 K, the scaling exponent of the anomalous Hall conductivity was in the localized hopping regime. At higher temperatures, the measured scaling exponent is beyond our current understanding of the AHE. Defect-driven MCD hysteresis would be consistent with the impurity induced variable-range hopping regime measured in transport at low temperatures.
We expect the bulk defect density to remain relatively uniform throughout the crystal. A dominant bulk contribution contradicts our observation that spontaneous MCD disappeared after a new region of the bulk crystal was exposed by polishing. This interpretation is consistent with transport measurements on thin films reported in Ref. [22], which reported a surface state driven AHE. Surface defects may alter the electronic structure at the surface causing observable hysteresis and subsequent disappearance after polishing. Atomic defects are localized on the atomic length scale, on the order of several Å, at least one order of magnitude smaller than our laser spot size and optical penetration depth. Our measurements probe the collective effect of defects within the illuminated region and cannot resolve the nature of individual defects or quantitatively estimate the defect density. Our measurements cannot distinguish if the disappearance of spontaneous MCD is from a difference in the surface states before and after polishing or lower defect density in the bulk causing hysteresis to lie below the optical sensitivity limit.
If defects are the microscopic origin of the observed hysteresis loop, then they are unlikely to also cause the observed memory effect. The origin of the hysteresis sign change around 200 K remains unknown. However, the fact that AHE also has a change around 200 K [16, 18, 19, 20, 21, 22] suggests that the origin of the AHE might also not be intrinsic. Another evidence is that the AHE is only observed in the variable range hopping regime due to impurities [19].
In conclusion, we have observed spontaneous circular dichroism in a MnTe bulk crystal. The spontaneous MCD, an optical analogue of the AHE, emerges around 250 K, below the reported Néel temperature and changes sign around 200 K, consistent with prior AHE results. We also found that the hysteresis loop is shifted away from zero field. The direction of the shift depended on the sign of the cooling field. Both the polished bulk crystal and MBE-grown thin film showed no hysteresis, suggesting that the spontaneous MCD in MnTe is not from bulk altermagnetic order. We instead attributed the spontaneous MCD to a defect-driven surface state. More work is needed to understand the origin of the surface defects, the hysteresis sign change. Looking forward, we hope our work motivate the community to identify new systems where the AHE is intrinsic to the altermagnetic ground state.
B.M. and L.W. were sponsored by the Army Research Office under Grant No. W911NF-20-2-0166 and W911NF-25-2-0016 for the measurement and data analysis. L.W also acknowledges support from the Office of Naval Research under Grant No. N00014-24-1-2064 and from Kaufman Foundation under the award number KA2025-151542 for manuscript writing. The single crystal growth work at Rice is supported by the U.S. DOE BES DE-SC0026179 (P.D., E.M.). Part of the materials characterization work at Rice is supported by the Robert A. Welch Foundation under Grant No. C-1839 (P.D.) and C-2114 (A.J. and E.M.). Z.-J.Y and C.-Z.C were supported by the Office of Naval Research under Grant No. N000142412133. The single-crystal growth work by S.H.Y. and Z.M. was performed at the Pennsylvania State University Two-Dimensional Crystal Consortium—Materials Innovation Platform (2DCC-MIP), which is supported by NSF Cooperative Agreement No. DMR-2039351. Film growth at Oak Ridge by M.C. and M.B. was supported by the U. S. Department of Energy (DOE), Office of Science, Basic Energy Sciences (BES), Materials Sciences and Engineering Division (thin film growth). J.W.F.V. acknowledges support from the U.S. Department of Energy under Early Career Award No. DE-SC0025632.
References
References
- [1]L. Šmejkal, J. Sinova, and T. Jungwirth, Beyond conventional ferromagnetism and antiferromagnetism: A phase with nonrelativistic spin and crystal rotation symmetry, Phys. Rev. X 12, 031042 (2022).DOI
- [2]L. Šmejkal, J. Sinova, and T. Jungwirth, Emerging research landscape of altermagnetism, Phys. Rev. X 12, 040501 (2022).arxiv.org/abs/2204.10844
- [3]T. Jungwirth, J. Sinova, R. M. Fernandes, Q. Liu, H. Watanabe, S. Murakami, S. Nakatsuji, and L. Šmejkal, Symmetry, microscopy and spectroscopy signatures of altermagnetism, Nature 649, 837 (2026).
- [4]T. Jungwirth, J. Sinova, P. Wadley, D. Kriegner, H. Reichlová, F. Krizek, H. Ohno, and L. Šmejkal, Altermagnetic spintronics, Nature Physics 22, 1012 (2026).
- [5]C. Song, H. Bai, Z. Zhou, L. Han, H. Reichlova, J. H. Dil, J. Liu, X. Chen, and F. Pan, Altermagnets as a new class of functional materials, Nature Reviews Materials 10, 473 (2025).DOI
- [6]L. Bai, W. Feng, S. Liu, L. Šmejkal, Y. Mokrousov, and Y. Yao, Altermagnetism: Exploring new frontiers in magnetism and spintronics, Advanced Functional Materials 34, 2409327 (2024).
- [7]R. Tamang, S. Gurung, D. P. Rai, S. Brahimi, and S. Lounis, Altermagnetism and altermagnets: A brief review, Magnetism 5, 10.3390/magnetism5030017 (2025).DOI
- [8]T. Jungwirth, X. Marti, P. Wadley, and J. Wunderlich, Antiferromagnetic spintronics, Nature Nanotechnology 11, 231 (2016).
- [9]V. Baltz, A. Manchon, M. Tsoi, T. Moriyama, T. Ono, and Y. Tserkovnyak, Antiferromagnetic spintronics, Rev. Mod. Phys. 90, 015005 (2018)DOI
- [10]W. Szuszkiewicz, B. Hennion, B. Witkowska, E. Łusakowska, and A. Mycielski, Neutron scattering study of structural and magnetic properties of hexagonal MnTe, physica status solidi (c) 2, 1141 (2005).DOI
- [11]J. Krempaský, L. Šmejkal, S. W. D’Souza, M. Hajlaoui, G. Springholz, K. Uhliřová, F. Alararp, P. C. Constantinou, V. Strocov, D. Usanov, W. R. Pudelko, R. González-Hernández, A. Birk Hellenes, Z. Jansa, H. Reichlová, Z. Šobáň, R. D. Gonzalez Betancourt, P. Wadley, J. Sinova, D. Kriegner, J. Minár, J. H. Dil, and T. Jungwirth, Altermagnetic lifting of Kramers spin degeneracy, Nature 626, 517 (2024).DOI
- [12]S. Lee, S. Lee, S. Jung, J. Jung, D. Kim, Y. Lee, B. Seok, J. Kim, B. G. Park, L. Šmejkal, C.-J. Kang, and C. Kim, Broken Kramers degeneracy in altermagnetic MnTe, Phys. Rev. Lett. 132, 036702 (2024).
- [13]T. Osumi, S. Souma, T. Aoyama, K. Yamauchi, A. Honma, K. Nakayama, T. Takahashi, K. Ohgushi, and T. Sato, Observation of a giant band splitting in altermagnetic MnTe, Phys. Rev. B 109, 115102 (2024).DOI
- [14]Z. Liu, M. Ozeki, S. Asai, S. Itoh, and T. Masuda, Chiral split magnon in altermagnetic MnTe, Phys. Rev. Lett. 133, 156702 (2024).DOI
- [15]D. Jost, R. B. Regmi, E. G. Lomeli, S. Sahel-Schackis, M. Scheufele, M. Neuhaus, R. Nickel, F. Yakhou, K. Kummer, N. Brookes, L. Shen, G. L. Dakovski, N. J. Ghimire, S. Geprägs, and M. F. Kling, Chiral altermagnon in MnTe (2025), arXiv:2501.17380 [cond-mat.mtrl-sci].arxiv.org/abs/2501.17380
- [16]R. D. Gonzalez Betancourt, J. Zubáč, R. Gonzalez-Hernandez, K. Geishendorf, Z. Sobán, G. Springholz, K. Olejník, L. Šmejkal, J. Sinova, T. Jungwirth, S. T. B. Goennenwein, A. Thomas, H. Reichlová, J. Železný, and D. Kriegner, Spontaneous anomalous Hall effect arising from an unconventional compensated magnetic phase in a semiconductor, Phys. Rev. Lett. 130, 036702 (2023).DOI
- [17]K. P. Kluczyk, K. Gas, M. J. Grzybowski, P. Skupiński, M. A. Borysiewicz, T. Fąs, J. Suffczyński, J. Z. Domagała, K. Grasza, A. Mycielski, M. Baj, K. H. Ahn, K. Výborný, M. Sawicki, and M. Gryglas-Borysiewicz, Coexistence of anomalous Hall effect and weak magnetization in a nominally collinear antiferromagnet MnTe, Phys. Rev. B 110, 155201 (2024).DOI
- [18]M. Chilkote, A. R. Mazza, Q. Lu, I. Gray, Q. Tian, Q. Deng, D. Moseley, A.-H. Chen, J. Lapano, J. S. Gardner, G. Eres, T. Z. Ward, E. Feng, H. Cao, V. Lauter, M. A. McGuire, R. Hermann, D. Parker, M.-G. Han, A. Kayani, G. Rimal, L. Wu, T. R. Charlton, R. G. Moore, and M. Brahlek, Stoichiometry-induced ferromagnetism in altermagnetic candidate MnTe, Advanced Functional Materials 34, 2405829 (2024).
- [19]Z. Liu, S. Xu, J. M. DeStefano, E. Rosenberg, T. Zhang, J. Li, M. B. Stone, F. Ye, W. Tian, S. Edwards, R. Cong, S. Pan, C.-W. Chu, L. Deng, E. Morosan, R. M. Fernandes, J.-H. Chu, and P. Dai, Strain-tunable anomalous Hall effect in hexagonal MnTe (2026), arXiv:2509.19582 [cond-mat.str-el].DOI
- [20]S. Smolenski, N. Mao, D. Zhang, Y. Guo, A. K. M. A. Shawon, M. Xu, E. Downey, T. Musall, M. Yi, W. Xie, C. Jozwiak, A. Bostwick, N. Tamura, E. Rotenberg, L. Li, K. Sun, Y. Zhang, and N. H. Jo, Strain-tunability of the multipolar Berry curvature in altermagnet MnTe (2025), arXiv:2509.21481 [cond-mat.mtrl-sci].arxiv.org/abs/2509.21481
- [21]S. Bey, S. S. Fields, N. G. Combs, B. G. Márkus, D. Beke, J. Wang, A. V. Levlev, M. Zhukovsky, T. Orlova, L. Forró, S. P. Bennett, X. Liu, and B. A. Assaf, Unexpected tuning of the anomalous Hall effect in altermagnetic MnTe thin films (2024), arXiv:2409.04567 [cond-mat.mtrl-sci].arxiv.org/abs/2409.04567
- [22]L.-J. Zhao, Z.-J. Yan, H. Rong, Y. Zhao, P. Xiao, L.-K. Lai, Z. Xi, K. Wang, T. Adhikari, G. P. Tiwari, Z. Lin, P. Manue, F. Orlandi, D. Khalyavin, A. J. Grutter, C.-X. Liu, B. Yan, and C.-Z. Chang, Surface-state-driven anomalous Hall effect in altermagnetic MnTe films (2026), arXiv:2602.09363 [cond-mat.mtrl-sci].
- [23]M. A. Willard and G. F. Vander Voort, Microstructure and domain imaging of magnetic materials, in Metallography and Microstructures, edited by G. F. Vander Voort (ASM International, 2004) https://dl.asminternational.org/handbooks/book/chapter-pdf/486124/a0003788.pdf.
- [24]J. Wu, H. Wu, and P. Tan, Magneto-optical interactions in layered magnets, Advanced Functional Materials 34, 2312214 (2024).DOI
- [25]T. Higo, H. Man, D. B. Gopman, L. Wu, T. Koretsune, O. M. J. van ’t Erve, Y. P. Kabanov, D. Rees, Y. Li, M.-T. Suzuki, S. Patankar, M. Ikhlas, C. L. Chien, R. Arita, R. D. Shull, J. Orenstein, and S. Nakatsuji, Large magneto-optical Kerr effect and imaging of magnetic octupole domains in an antiferromagnetic metal, Nature Photonics 12, 73 (2018).DOI
- [26]X. Han, X. Liu, M. K. Kareev, J. Chackhalian, and L. Wu, Large topological magnetic optical effects and imaging of antiferromagnetic octupole domains of an altermagnet-like Weyl semimetal (2025), arXiv:2505.03713 [cond-mat.mtrl-sci].arxiv.org/abs/2505.03713
- [27]Z. Ni, H. Zhang, D. A. Hopper, A. V. Haglund, N. Huang, D. Jariwala, L. C. Bassett, D. G. Mandrus, E. J. Mele, C. L. Kane, and L. Wu, Direct imaging of antiferromagnetic domains and anomalous layer-dependent mirror symmetry breaking in atomically thin MnPS3, Phys. Rev. Lett. 127, 187201 (2021).DOI
- [28]Z. Ni, A. V. Haglund, H. Wang, B. Xu, C. Bernhard, D. G. Mandrus, X. Qian, E. J. Mele, C. L. Kane, and L. Wu, Imaging the Néel vector switching in the monolayer antiferromagnet MnPSe3 with strain-controlled ising order, Nature Nanotechnology 16, 782 (2021).DOI
- [29]T. Yokoyama, T. Nakagawa, and Y. Takagi, Magnetic circular dichroism for surface and thin film magnetism: Measurement techniques and surface chemical applications, International Reviews in Physical Chemistry 27, 449 (2008), https://doi.org/10.1080/01442350802127608.
- [30]R. Starke, R. Wimmer, G. A. H. Schober, N. Bulut, and J. Kortus, Wavevector-dependent optical properties from wavevector-independent proper conductivity tensor, The European Physical Journal B 93, 54 (2020).
- [31]N. Nagaosa, J. Sinova, S. Onoda, A. H. MacDonald, and N. P. Ong, Anomalous Hall effect, Rev. Mod. Phys. 82, 1539 (2010).DOI
- [32]O. J. Amin, A. Dal Din, E. Golias, Y. Niu, A. Zakharov, S. C. Fromage, C. J. B. Fields, S. L. Heywood, R. B. Cousins, F. Maccherozzi, J. Krempaský, J. H. Dil, D. Kriegner, B. Kiraly, R. P. Campion, A. W. Rushforth, K. W. Edmonds, S. S. Dhesi, L. Šmejkal, T. Jungwirth, and P. Wadley, Nanoscale imaging and control of altermagnetism in MnTe magnetism in MnTe, Nature 636, 348 (2024).DOI
- [33]A. Hariki, A. Dal Din, O. J. Amin, T. Yamaguchi, A. Badura, D. Kriegner, K. W. Edmonds, R. P. Campion, P. Wadley, D. Backes, L. S. I. Veiga, S. S. Dhesi, G. Springholz, L. Šmejkal, K. Výborný, T. Jungwirth, and J. Kuneš, X-ray magnetic circular dichroism in altermagnetic α−MnTe, Phys. Rev. Lett. 132, 167601 (2024).DOI
- [34]I. I. Mazin, Altermagnetism in MnTe: Origin, predicted manifestations, and routes to detwinning, Phys. Rev. B 107, L100418 (2023).
- [35]I. Gray, Q. Deng, Q. Tian, M. Chilcote, J. S. Dodge, M. Bra hlek, and L. Wu, Time-resolved magneto-optical effects in the altermagnet candidate MnTe, Applied Physics Letters 125, 212404 (2024).
- [36]G. Watanabe, S. Yamane, R. Maki, A. Ikeda, A. Kirikoshi, J. Otsuki, T. Aoyama, K. Ohgushi, and S. Yonezawa, Magneto-optical imaging of macroscopic altermagnetic domains in MnTe (2026), arXiv:2604.14947 [cond-mat.mtrl-sci].arxiv.org/abs/2604.14947
- [37]W. Yang, C. Won, C. Cress, W. Lu, X. Fang, S. Fields, N. Combs, S. Han, M. Z. Franklin, S. P. Bennett, S.-W. Cheong, and J. Xia, Giant spontaneous Kerr effect and its self-doping dependence in altermagnetic MnTe (2026), arXiv:2604.21021 [cond-mat.str-el].arxiv.org/abs/2604.21021
- [38]J. Nogués and I. K. Schuller, Exchange bias, Journal of Magnetism and Magnetic Materials 192, 203 (1999).DOI
- [39]A. Noah, F. Toric, T. D. Feld, G. Zissman, A. Gutfreund, D. Tsruya, T. R. Devidas, H. Alpern, A. Vakahi, H. Steinberg, M. E. Huber, J. G. Analytis, S. Gazit, E. Lachman, and Y. Anahory, Tunable exchange bias in the magnetic Weyl semimetal Co3Sn2S2, Phys. Rev. B 105, 144423 (2022).
- [40]E. Lachman, R. A. Murphy, N. Maksimovic, R. K. Ealhofer, S. Haley, R. D. McDonald, J. R. Long, and J. G. Analytis, Exchange biased anomalous Hall effect driven by frustration in a magnetic kagome lattice, Nature Communications 11, 560 (2020).
- [41]C. Menil, B. Leridon, A. Cavanna, U. Gennser, D. Mailly, L. Ding, X. Li, Z. Zhu, B. Fauqué, and K. Behnia, Magnetic memory and distinct spin populations in ferromagnetic Co3Sn2S2, npj Quantum Materials 10, 23 (2025).DOI
- [42]P. Vaqueiro and G. G. Sobany, A powder neutron diffraction study of the metallic ferromagnet Co3Sn2S2, Solid State Sciences 11, 513 (2009).DOI
- [43]I. Živković, R. Yadav, J.-R. Soh, C. Yi, Y. Shi, O. V. Yazyev, and H. M. Rønnow, Unraveling the origin of the peculiar transition in the magnetically ordered phase of the Weyl semimetal Co3Sn2S2, Phys. Rev. B 106, L180403 (2022).DOI
- [44]C. Lee, P. Vir, K. Manna, C. Shekhar, J. E. Moore, M. A. Kastner, C. Felser, and J. Orenstein, Observation of a phase transition within the domain walls of ferromagnetic Co3Sn2S2, Nature Communications 13, 3000 (2022).DOI
- [45]H. Pan, R.-C. Xiao, J. Han, H. Zhu, J. Li, Q. Niu, Y. Gao, and D. Hou, Experimental evidence of Néel-order-driven magneto-optical Kerr effect in an altermagnetic insulator, Phys. Rev. Lett. 136, 036701 (2026).DOI
- [46]J. Luo, X. Zhou, J. Liang, L. Wang, Q. Zhou, Y. Jiang, W. Wang, Y. Yao, L. Yang, and W. Jiang, Symmetry-driven giant magneto-optical Kerr effects in altermagnetic insulator, Chin. Phys. Lett. 43, 020713 (2026).DOI
- [47]H. Yoshimochi, K. Yoshida, R. Oiwa, T. Nomoto, N. D. Khanh, A. Kitaori, R. Takagi, R. Arita, and S. Seki, Large magneto-optical Kerr effect induced by collinear antiferromagnetic order (2026), arXiv:2601.13723 [cond-mat.str-el].
- [48]A.-H. Chen, P. R. Raghuvanshi, J. Cook, M. Chilcote, J. Lapano, A. R. Mazza, Q. Lu, S. Kim, Y.-C. Wu, T. Z. Ward, B. J. Lawrie, G. Bian, J. Burns, J. D. Poplawsky, M.-G. Han, Y. Zhu, L. Lindsay, H. Miao, Z. Gai, R. G. Moore, G. Eres, V. R. Cooper, and M. Brahl ek, Programmable phase selection between altermagnetic and noncentrosymmetric polymorphs of MnTe on InP via molecular beam epitaxy, ACS Applied Materials & Interfaces 18, 15654 (2026).DOI
- [49]I. I. Mazin and K. D. Belashchenko, Origin of the gossamer ferromagnetism in mnte, Phys. Rev. B 110, 214436 (2024).arxiv.org/abs/2407.14389