Noble metal free photocatalytic H2_2 generation on black TiO2_2: On the influence of crystal facets vs. crystal damage

Abstract

In this study, we investigate noble metal free photocatalytic water splitting on natural anatase single crystal facets and on wafer slices of the [001] plane before and after these surfaces have been modified by high pressure hydrogenation (HPH) and hydrogen ion-implantation. We find that on the natural, intact low index planes photocatalytic H2_2 evolution (in absence of noble metal co-catalyst) can only be achieved when the hydrogenation treatment is accompanied by the introduction of crystal damage, such as simple scratching, miscut in the wafer or by implantation damage. X-ray reflectivity (XRR), Raman, and optical reflection measurements show that plain hydrogenation leads to a ~ 1 nm thick black titania surface layer without activity, while a colorless, density modified and ~ 7 nm thick layer with broken crystal symmetry is present in the ion implanted surface. These results demonstrate that i) the H-treatment of an intact anatase surface needs to be combined with defect formation for catalytic activation, and ii) activation does not necessarily coincide with the presence of black color.

Paper details

vlnc:W_wh39twd9
Version
v1 · latest
Published
Added
License
arXiv nonexclusive license
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…