betaFeedback

WorksPhysics and Astronomy

Controllable dimensionality conversion between 1D and 2D CrCl3 magnetic nanostructures

Abstract

The fabrication of one-dimensional (1D) magnetic systems on solid surfaces, although of high fundamental interest, has yet to be achieved for a crossover between two-dimensional (2D) magnetic layers and their associated 1D spin chain systems. In this study, we report the fabrication of 1D single-unit-cell-width CrCl3 atomic wires and their stacked few-wire arrays on the surface of a van der Waals (vdW) superconductor NbSe2. Scanning tunneling microscopy/spectroscopy and first-principles calculations jointly revealed that the single wire shows an antiferromagnetic large-bandgap semiconducting state in an unexplored structure different from the well-known 2D CrCl3 phase. Competition among the total energies and nanostructure-substrate interfacial interactions of these two phases result in the appearance of the 1D phase. This phase was transformable to the 2D phase either prior to or after the growth for in situ or ex situ manipulations, in which the electronic interactions at the vdW interface play a nontrivial role that could regulate the dimensionality conversion and structural transformation between the 1D-2D CrCl3 phases.

Tailoring two-dimensional (2D) materials into one-dimensional (1D) structures such as nanoribbons and nanowires has been a prevailing approach for the manufacture of emergent properties in van der Waals (vdW) structures. Extensive attempts have been made to achieve controlled fabrication of the 1D counterparts of graphene [1, 2, 3] and semiconducting transition metal chalcogenides [4, 5, 6], which have exhibited rich electron correlated behaviors [5, 6]. The recent discovery of long-range magnetism in atomically thin vdW materials, e.g., chromium trihalides, is a major breakthrough in the field of 2D materials. This discovery has opened up a new avenue for the applications of vdW structures in spintronics [7, 8, 9, 10, 11, 12, 13, 14]. The integration of 1D and 2D magnetic nanostructures appears to be a promising strategy for minimizing the size of spintronic devices [15, 16]. The direct growth of 1D nanostructures on 2D layers is a straightforward strategy for 1D-2D vdW integration, which naturally raises the question of whether the 1D counterparts of these emerging 2D magnetic materials can be obtained on 2D substrates.

One-dimensional magnetic systems, usually in the form of spin chains, are themselves a thriving field of research and have been used to illustrate many key concepts in many-body quantum physics [17] and even triggered the recent search for new phases of matter (such as the Majorana fermion) [18, 19, 20, 21]. Note that in a practical prototypic system, spin-chain excitations strongly depend on the coupling with the environment, mostly the holding substrate. Various ways exist to create physical realizations of spin chains on solid surfaces, based on either compound solids, molecular self-assembly, or trapped atoms [21, 22, 23, 24, 25]. However, a spin chain with vdW nature, which offers considerably magnetic exchange interactions within the chain and minimizes undesired interactions with the supporting substrate, has yet to be realized.

Here, our scanning tunneling microscopy/spectroscopy (STM/S) measurements and density functional theory (DFT) calculations jointly showed an exceptional category of 1D1\mathrm{D} CrCl3\mathrm{CrCl}_3 atomic wires in a previously unobserved form. It was grown solely on an isotropic NbSe2\mathrm{NbSe}_2 vdW surface and was different from the nanoribbons of the 2D2\mathrm{D} CrCl3\mathrm{CrCl}_3 phase that were also prepared in this work. Such a 1D1\mathrm{D} wire, consisting of a single row of face-sharing CrCl6\mathrm{CrCl}_6 octahedra, is a large-gap semiconductor exhibiting a Néel-type antiferromagnetic (AFM) coupling. The narrowest 1D1\mathrm{D} wire had a single unit-cell-width (denoted as a single-wire, SW) and could be stacked in parallel, forming vdW wire arrays. Interestingly, we observed that the STM tip triggered 1D1\mathrm{D}-2D2\mathrm{D} dimensional conversion, accompanied by a polymorphic phase transformation, in quad- or wider wires arrays. Our theory, along with experimental inputs, aided the understanding of the reason for the presence of the 1D1\mathrm{D} phase and the subsequent 1D1\mathrm{D}-2D2\mathrm{D} conversion. The ability of the substrate to stabilize 1D1\mathrm{D}-wire ends or 2D2\mathrm{D}-flake edges by donating electrons through vdW couplings was of critical importance in controlling the dimensionality conversion and the phase transformation. Our findings refresh the understanding of vdW epitaxy and established an alternative idea for the vdW interface engineering of 1D1\mathrm{D} nanostructures.

Figure 1a shows a typical STM image of CrCl3\mathrm{CrCl}_3 grown on a bulk NbSe2\mathrm{NbSe}_2 substrate with ∼0.15\sim0.15 ML coverage (see the Methods Section for experimental details). The figure clearly indicates an anisotropic growth mode in which subnanometer-width or fewnanometer-width 1D structures developed along the armchair directions of the NbSe2\mathrm{NbSe}_2 lattice and were jointed at small 2D flakes. This 1D-2D coexisting feature appeared to be unique on the NbSe2\mathrm{NbSe}_2 substrate, in that an attempt of growth of CrCl3\mathrm{CrCl}_3 on a bilayer graphene (BLG) surface solely led to hexagonal-like flakes (Fig. 1e). These flakes showed the lattice of the well-known 2D CrCl3\mathrm{CrCl}_3 monolayer (Fig. 1f), namely, periodically spaced trimers of top-layer Cl atoms (marked by the dashed triangles) [12] with a separation of 6.0 A˚6.0\,\AA, which denoted the 2D phase.

In terms of the 1D-2D complexes formed on the NbSe2\mathrm{NbSe}_2 substrate, the small flakes were also in the 2D phase (Supplementary Fig. S1), but the 1D wires seemed to be in a different phase. A close-up look at the wires (Fig. 1b) explicitly illustrates their composition of parallelly stacked integer numbers of single atomic wires. A further zoomed-in constant-current image of a single wire is shown in Fig. 1c. The figure exhibits a zigzag chain of protrusions with an apparent height of ∼6.2 A˚\sim6.2\,\AA (Supplementary Fig. S2a, b), a periodicity (cc) of 6.0 A˚6.0\,\AA, and a separation of 1.8 A˚1.8\,\AA (labelled as dd in Fig. 1c) between two rows of the zigzag chain. All these remarkable features of the observed 1D phase differentiated it from simply an ultranarrow ribbon of the 2D CrCl3\mathrm{CrCl}_3 monolayer, which was, again, confirmed by the higher topographic heights of the wires than those of the 2D flakes at certain sample bias (Supplementary Fig. S2c, d).

Thus, this unknown 1D CrCl3\mathrm{CrCl}_3 structure was referred to as the 1D phase. Its STM topographic features were analogous to those of the formerly predicted 1D polymorphic phase of CrBr3\mathrm{CrBr}_3 [26]. We thus proposed that the 1D phase structure (Fig. 2a) consisted of a single Cr3+\mathrm{Cr}^{3+} row encapsulated by face-sharing CrCl6\mathrm{CrCl}_6 octahedra along the wire axis, showing a tube-like structure with six Cl lobes in the cross-sectional view (Fig. 2d).

The 2D phase also contained the same individual octahedral units, but these units were connected to each other in an edge-sharing manner, as seen in the schematic model superposed in Fig. 1f. Therefore, the two phases have very different structural parameters, e.g., the Cr-Cr spacing (2.95 Å vs. 3.44 Å), the Cr-Cr-Cr angle (180° vs. 120°), and the Cr-Cl-Cr bond angle (77° vs. 94°). Thus, discrepancies would likely exist in the exchange interactions and the magnetic ground states between these two structures.

The DFT calculated phonon spectra of the free-standing 1D CrCl3\mathrm{CrCl}_{3} wire array (Fig. 2e) and the CrCl3\mathrm{CrCl}_{3} single wire (Supplementary Fig. S3a) show no imaginary frequency, manifesting the structural stability. Upon the adsorption on the NbSe2\mathrm{NbSe}_{2} surface, the wire prefers to sit on the surface through two Cl lobes at the site shown in Fig. 2b, leading to another two Cl atomic rows being directed towards the vacuum (Fig. 2d). These two Cl atoms made dominant contributions to the STM imaging, and the image therefore yielded a zigzag appearance like that shown in Fig. 1c. In addition, our calculations revealed the lattice constant c=5.96c = 5.96 Å, the Cl-Cl separation d=1.85d = 1.85 Å, and the apparent height of 6.20 Å, which were very consistent with the experimental values of 6.0 Å, 1.8 Å, and 6.2 Å. This good consistency was maintained in the wider wire arrays, e.g., bi-wires (Fig. 1d and Fig. 2c, d). When two wires were stacked together, the experimental image (Fig. 1d) showed a different morphology from that of the single wire presented above, in that two rows of atoms in each zigzag chain appeared to have an apparent difference in height. This was consistent with the small tilt angle predicted by our calculations, as illustrated in the cross-sectional view (Fig. 2d, details in Supplementary Fig. S2e, f). In addition, for the interwire atomic registry, it was clearly seen in both the experimental and theoretical results that there was no shift along the wire axis between the two nearby zig-zag chains, and a rectangular unit-cell with an interwire separation of ∼6.1 A˚\sim6.1\ \mathring{\mathrm{A}} was thus formed.

Figure 2f shows typical differential conductivity (dI/dVdI/dV) spectra taken for 1D SW/NbSe2_2 and 2D flake/NbSe2_2. The SW had an experimental bandgap of 2.32 eV, smaller than that of the 2D flake (2.68 eV). Our DFT calculations revealed that the SW prefers a Néel AFM state (Supplementary Figs. S3b and S4), showing a magnetic moment of ∼2.8 μB\sim2.8\ \mu_{\mathrm{B}} primarily on each Cr atom and a bandgap of 1.25 eV (six-Cr finite wire) – 2.81 eV (infinite wire) depending on the wire length. Details of the band gap calculations are seen in Supplementary Table S1. The larger bandgap in the 2D monolayer was reproduced by our calculation in that the infinite form of the 2D phase gave a bandgap of 3.08 eV and the six-Cr 2D-phase flake gave a bandgap of 1.52 eV. The systematically smaller experimental values could be ascribed to the finite sizes of the 1D and 2D CrCl3_3 structures measured in our experiments. The easy axis of the magnetic moments was perpendicular to the wire axis direction with a magnetic anisotropic energy of 0.02 meV/Cr, as extensively discussed in Supplementary Fig. S6.

The ABAB AFM order was examined by spin-polarized STM (SP-STM) measurements [27, 28]. With out-of-plane magnetic fields, the bulk Ni tip was in-situ magnetized to be spin-up (spin-down) state before scanning [Methods]. The observations shown below were reproducible in our experiments using different Ni tips.

Figure 2h shows the constant current images of the same area taken with the spin-up (upper panel) and spin-down (middle panel) tip states. The bias here was chosen to be near the conduction band edge, which hosts the maximum polarization in the density of states (DOS) (Fig. S7). It is apparent in both images that a contrast appears between adjacent Cr sites. In addition, we observed that such contrast is reversed under flipping of the tip magnetization (up/down). For comparison, we show a spin-averaged image (lower panel in Fig. 2h) derived by adding the intensities of the two spin-resolved images, which resembles the topographic image taken with a Pt-Ir tip (Fig. 1c). The DFT simulated SP-STM images (Fig. 2i) are composed of dumbbell-shaped protrusions centred at alternate Cr atoms and oriented along the two nearest top-layer Cl atoms, which well reproduce the experimental results. Note that both the SP-STM imaging and the DFT calculations indicate the antiferromagnetic coupling in the SW. Our calculation results do not support the existence of spiral magnetism in the classical magnetism picture and at the DFT level (Fig. S4). However, the inherent quantum (thermal) fluctuation in quasi-1D systems and the small MAE of 0.02 meV between the yy and zz directions (arising from vdW adsorption) could result in complex magnetic long-range ordering, which appears to be another elusive topic that requires further exploration.

The formation of the 1D phase differentiated the NbSe2_2 substrate from the others. Thus, it was interesting to more carefully examine the competition between the 1D and 2D phases on NbSe2_2. Figure 3a–d illustrate a sequence of topographic images of CrCl3_3/NbSe2_2 as a function of the total coverage (NtotalN_{\mathrm{total}}) ranging from 0.035 ML to 0.36 ML, which showed that the 1D phase was dominant at a lower coverage (0.035 ML, Fig. 3a and that the 2D phase became predominant for higher coverages (from 0.12 to 0.36 ML, Fig. 3b–d). This trend is more clearly depicted by a plot of the ratio (R1DR_{\mathrm{1D}}) between the partial coverage of the 1D wires NwireN_{\mathrm{wire}} and NtotalN_{\mathrm{total}} as a function of NtotalN_{\mathrm{total}} (black dotted line in Fig. 3e) in which R1DR_{\mathrm{1D}} continuously decrease. The plot of NwireN_{\mathrm{wire}} (red dashed line) also supports the dominance of the 2D phase at higher coverages, because it first reaches a maximum at Ntotal=0.12N_{\mathrm{total}} = 0.12 ML and then decreases with further deposition of CrCl₃. The reduced NwireN_{\mathrm{wire}} is also accompanied by a narrowed average width of the 1D wires. Figure 3f plots the statistical width (ww) distribution of the multi-wire arrays (MW) at two typical NtotalN_{\mathrm{total}} values, namely, 0.12 and 0.36 ML. Interestingly, an increase in NtotalN_{\mathrm{total}} reduced the most-probable width of the MW from w=4w = 4 to w=2w = 2, implying a likely spontaneous transformation of the 1D phase into the 2D phase when the MW width exceeded a threshold (wTw_{\mathrm{T}}).

Furthermore, such 1D-2D dimensionality conversion and the threshold width wTw_{\mathrm{T}} were directly visualized in tip-controlled postgrowth transformations. Figure 3g shows that a moderate tip stimulus precisely induced a transformation from 1D wire-array to 2D nanoribbon (NR) at the nanometre scale (Methods Section). Through substantive experimental attempts, we found that the wider the array was, the more readily the transformation occurred, and the transformation never occurred for w<4w < 4. For instance, in the right-most region of Fig. 3g, the MW with w=3w = 3 could retain their structure under all the considered tunneling conditions. Combining the as-grown and postgrowth transformations, the wTw_{\mathrm{T}} was estimated to be approximately three, which was well reproduced in our calculations as shown in Fig. S8. This threshold width represents the crossover of the formation energies of the two phases; hence, is crucial for comprehending the growth mechanism, as we will discuss in the following. Note that as the 2D phase was predicted to be in an XY FM state, the tip-induced structural transformations are, most likely, accompanied with changes of magnetism between 1D AFM and 2D FM states [14].

Our DFT results showed that the infinite 2D form of the CrCl3\mathrm{CrCl}_{3} was 0.34 eV/Cr more stable than the infinite 1D form, which indicated that the edge-bulk energy competition of the 1D and 2D phases might play an essential role in stabilizing the 1D phase on the NbSe2\mathrm{NbSe}_{2} substrate in the early growth stage. We thus focused on the relative stabilities of the SW and the 2D hexagonal flake (HF) containing the same finite number of Cr atoms, nCrn_{\mathrm{Cr}} (see Supplementary Fig. S9 for their atomic models). We found that the bulk unit indeed has lower energy than the edge (end) unit in both phases (Supplementary Table S2). Note that the ratio between the numbers of end (edge) and bulk units in the SW is generally smaller than that in the HF, and the discrepancies in the ratio are nCrn_{\mathrm{Cr}} dependent. For instance, with the smallest nCr=6n_{\mathrm{Cr}}=6 (Figure 4a, Figure 4b), SW-6 contains two end units while all six Cr atoms in HF-6 are edge units, yielding the largest difference in the edge(end)/bulk ratio. This might have accounted for the superior stability of the SW in the early growth stage.

Image not extracted

Figure 4. Theoretical understanding of the 1D phase growth and the 1D-2D transformation. a, Side view of SW-6. b, Top view of HF-6. The upper and lower surface Cl atoms are represented by yellow and green balls, respectively. c, Plot of ΔH\Delta H between the free-standing SW and HF at the Cl-rich (green square) and Cl-deficient (green circle) extremes as a function of nCrn_{\mathrm{Cr}}. The HFs with zigzag (ZZ) edges (nCr=6n_{\mathrm{Cr}} = 6, 24 and 54) are more stable than the arm-chair (AC) ones (nCr=12n_{\mathrm{Cr}} = 12 and 36). d, e, Plots of the charge variations for each individual Cl atom in SW-6 (d) and HF-6 (e) on the NbSe2_2 (orange) and graphene (blue) substrates. The indices of the Cl atoms are labelled in a and b. The edge atoms are marked by grey shadows. f, ΔH\Delta H between SWs and HFs (at nCr=6n_{\mathrm{Cr}} = 6 and 12) with the substrates involved. The colour-filled bars represent the estimated range of experimental μCl\mu_{\mathrm{Cl}}. The circle and square symbols represent the results at the Cl-deficient and Cl-rich limits, respectively. g, h, Atomic structures of multi-wire array (MW, w=3w = 3) on NbSe2_2 and its corresponding nanoribbon (NR). i, Phase diagram of ΔH\Delta H as functions of ww and μCl\mu_{\mathrm{Cl}}. The contour line of ΔH=0\Delta H = 0 is plotted as the dashed line. The shadow region corresponds to the experimental observation of wT=2w_{\mathrm{T}} = 2–4.

However, the inferred superior stability of SWs could not be illustrated by directly comparing the total energies of HF-6 and SW-6 because of the unequal numbers of Cl atoms. The introduction of the formation enthalpies, i.e., the consideration of the difference in the Cl number and the Cl chemical potential μCl\mu_{\mathrm{Cl}}, solved this issue (see the Methods Section for details of the formation enthalpy HH and the total energies). Figure 4c plots the difference in the formation enthalpies of the HFs and their corresponding SWs for the Cl-rich (μCl=0.08\mu_{\mathrm{Cl}} = 0.08 eV) and Cl-deficient (μCl=−2.27\mu_{\mathrm{Cl}} = -2.27 eV) limits (Methods Section). The SW was found to be more stable (with a positive ΔH\Delta H value) for both limits when nCr=6n_{\mathrm{Cr}} = 6. With increasing nCrn_{\mathrm{Cr}}, ΔH\Delta H showed an overall declining tendency towards the negative regime. Although this declining trend implied a growth mode transformation from 1D wires to 2D flakes, these results could not explain the fact that the SW was solely formed on NbSe2_2.

With the adsorption on both the NbSe2_2 and BLG substrates, substantial charge transfer was identified in our calculation, especially at the ends (CrCl4.5_{4.5} units, Figure 4d) or edges (CrCl4_4 units, Figure 4e). A total amount of 1.86 ee was transferred from NbSe2_2 to SW-6, primarily at the six end Cl atoms (~0.3 ee/Cl, Figure 4d), which stabilized the end unit with a larger adsorption energy (Supplementary Table S2-S3). The delocalized π\pi-orbital nature of the graphene electrons, along with the graphene work function and the energy levels of the SW (or HF) (Supplementary Fig. S10), led to an additional donated charge of 0.48 ee for SW-6, further lowering its energy of the end unit (Supplementary Table S2). In comparison with the SWs, the HFs had a stronger ability to accept electrons, and 0.42 ee and 0.50 ee more electrons were transferred from the NbSe2_2 and graphene substrates to HF-6, respectively, mainly around the outermost Cl edge atoms. These additionally transferred electrons provided extra stabilization for the 2D edges of the HF on the graphene substrate (Figure 4e), on which EedgeHF=−10.42E_{\mathrm{edge}}^{\mathrm{HF}} = -10.42 eV/Cr was surprisingly lower than EbulkSW=−10.13E_{\mathrm{bulk}}^{\mathrm{SW}} = -10.13 eV/Cr (Supplementary Table S2). This partially, or even fully broke the superior stability of the freestanding 1D phase in the early growth stage. Note that on the NbSe2_2 substrate, the EedgeHF=−10.13E_{\mathrm{edge}}^{\mathrm{HF}} = -10.13 eV/Cr remained higher than the EbulkSW=−10.23E_{\mathrm{bulk}}^{\mathrm{SW}} = -10.23 eV/Cr, which favoured the possibility of 1D phase growth. See Supplementary Table S2 for comprehensive results. The stronger charge transfer at the end (edge) results from their electron acceptor nature (valence of 3+ for Cr), while the structural relaxation plays a minor and passive role (Fig. S11).

This inferred favoured growth was indeed reflected in the plot of ΔH\Delta H between the HF and SW for nCr=6n_{\mathrm{Cr}} = 6 and 12 upon adsorption on the two substrates (Figure 4f) for an experimentally estimated μCl\mu_{\mathrm{Cl}}. In the following, we first discuss this estimation of μCl\mu_{\mathrm{Cl}}.

In practical experiments, the phase transformation mostly occurred from 1D MW to 2D NR, rather than directly to hexagonal flakes. We compared the ΔH\Delta Hs between the MW and NR that formed on NbSe2_2 with the equivalent width ww (see Figure 4g and h for their atomic models with w=3w = 3 Cr rows). The phase diagram as functions of ww and μCl\mu_{\mathrm{Cl}} is displayed in Figure 4i, where a black dotted line represents the contour line of ΔH=0\Delta H = 0. According to the experimental fact that the most-probable width varied between wT=2w_{\mathrm{T}} = 2 and 4 (Fig. 3f and 3g), we can estimate a range of experimental μCl=−0.803\mu_{\mathrm{Cl}} = -0.803 to −0.217-0.217 eV/Cl (shadow region in Figure 4i).

In Figure 4f, the colour-filled bars represent the ranges of ΔH\Delta H for the experimental range of μCl\mu_{\mathrm{Cl}}. It is indeed shown that the 1D phase retained more stability throughout the whole experimental range of μCl\mu_{\mathrm{Cl}} on the NbSe2_2, while on graphene, the possibility of favouring the 2D growth appeared. These results demonstrated that the selective choice of a substrate with a proper ability to donate electrons could tune the 1D and 2D growth modes of CrCl3_3 on the substrate. This new mechanism is significantly distinct from the common notion of vdW epitaxy, in which the structure of the epilayer is nearly unrelated to the substrate [15].

In conclusion, we demonstrated the first experimental realization of single-unit-cell-width CrCl3_3 atomic wires and their stacked few-wire arrays on the surface of NbSe2_2. The single CrCl3_3 wire was identified as a new 1D polymorphic phase of the 2D magnetic material CrCl3_3 with a large bandgap and an antiferromagnetic ground state. Rich emergent quantum phenomena are anticipated in this unprecedented hybrid system consisting of vdW integrated 1D spin chain/2D superconductor. Moreover, a thorough understanding of the underlying growth mechanism revealed the elegant role of the electronic interactions at the vdW interface in controlling the dimensionality conversion and polymorphic phase transformation in epitaxial growth. This study expands the application scope of vdW interface engineering, offering an easy and flexible means to fabricate exotic 1D nanostructures.

Methods Section

Growth of CrCl3_3: The CrCl3_3 were grown on a freshly cleaved NbSe2_2 substrate with compound source molecular beam epitaxy (MBE). Anhydrous CrCl3_3 powder of 99% purity was evaporated from a Knudsen cell. The growth speed of ~0.02 ML/min was determined by checking the coverages of the as-grown samples. The NbSe2_2 substrate was kept at room temperature during growth. The BLG/SiC substrate was synthesized by silicon sublimation from the (0001) plane (Si face) of n-type 6H-SiC [29]. The optimal substrate temperature for the growth of the CrCl3_3 monolayer flakes was ~500 K. Below this temperature, the CrCl3_3 tended to form 2D fractal structures features on the bilayer graphene surface (for details, see Supplementary Fig. S12).

STM/S Measurements: After sample preparation, the sample was inserted into a low-temperature scanning tunneling microscope (STM, Unisoku USM-1300) housed in the same ultra-high vacuum system. Polycrystalline Pt-Ir STM tip was used in our experiments. The bias voltage was applied to the sample. All STM images presented in this article were taken at 4.3 K. The dI/dVdI/dV spectra were measured by using the lock-in technique with reference signal at 963 Hz. The modulation amplitudes were set as 50 μ\muV (Fig. 2e) and 10 mV for all other spectra. The SP-STM measurements were carried out via electrochemically etched Ni tips in a constant-current mode [30, 31]. The spin-polarization of the Ni tip was calibrated on Co/Cu(111) (Supplementary Fig. S13). Following the procedure reported in ref. [32, 33, 34], perpendicular magnetic fields of + 0.7 T (− 0.7 T) were used to magnetize the ferromagnetic Ni tip acquiring the spin-up (spin-down) tip state. The external fields were usually held for five minutes and then slowly reduced to zero. The magnetized tip was then used to perform STM imaging at 0 T on the same location.

Tip-induced Phase Transformation: The structural phase of the stacked wire arrays was not affected by imaging using a sample bias 0 V >VB>−2.5> V_{\mathrm{B}} > -2.5 V. Once the sample bias was in excess of ∼−2.8\sim-2.8 V, the transformation to the 2D phase could easily occur. The practical procedure we adopted for Fig. 3g was as follows: running continuous scanning of the selected region at the constant height mode with the initial scanning parameters of VB=−2.9V_{\mathrm{B}} = -2.9 V, I=3I = 3 pA until an abrupt drop of II (usually down to zero) was observed (since the 2D phase was slightly lower in terms of the topographic height).

DFT Calculations: Calculations were performed using the generalized gradient approximation in the Perdew-Burke-Ernzerhof (PBE) form [35] for the exchange-correlation potential, the projector augmented wave method [36], and a plane-wave basis set as implemented in the Vienna ab-initio simulation package (VASP) [37]. Dispersion corrections were made at the van der Waals density functional (vdW-DF) level [38] with the optB86b functional for the exchange potential (optB86b-vdW) [39] in all structural relaxations. The structures were fully relaxed until the residual force per atom was less than 0.005 (0.02) eV/A˚\mathrm{eV}/\mathrm{\AA} for free-standing (substrate-supported) SWs and HFs. On-site Coulomb interactions on the Cr dd orbitals were considered using a DFT+UU method [40] with U=3.9U=3.9 eV and J=1.1J=1.1 eV, consistent with the values used in the literature [41]. A vacuum layer larger than 15 A˚\mathrm{\AA} was used in all supercells to avoid interactions between the slabs of adjacent supercells. An energy cut-off of 700 (400) eV was used for the plane wave basis set in calculating free-standing (substrate-supported) structures. A kk-mesh of 14×1×114 \times1 \times1 was used to sample the first Brillouin zone of freestanding infinite SWs while the Gamma point was used in other calculations.

The PBE functional was used in comparison of relative energies of individual configurations based on the atomic structures optimized using the optB86b-vdW functional. Spin-orbit coupling was considered in all energy comparisons. The accuracy of such set of methods were well tested in calculations on many 2D magnets [42, 43, 44, 45, 46, 47, 48, 49]

The charge transfer between the SWs (HFs) and the substrate was evaluated using the Bader charge analysis method [50]. The charge variation of a Cl atom was defined as the Bader charge of the Cl atom in SW-6 (HF-6) being placed on the substrate minus the that in the free-standing form. The phonon dispersion was calculated using the density functional perturbation theory, as implemented in the PHONOPY code [51].

The periodic direction of the multi-wires array (zig-zag direction of corresponding nanoribbon) is oriented along the arm-chair direction of NbSe2_2, which was consistent with the experimental observation. For the finite SWs and HFs with a NbSe2_2 or graphene substrate, we used the same relative orientations as the periodic case. Two-layer NbSe2_2 (graphene) was used to model the substrate, in which the bottom layer was kept fixed and the top layer was allowed to fully relax.

Calculation of formation enthalpy HH: The formation enthalpy HH for finite SW and HF is defined as H=(EtotalHF/SW−nClμCl−nClμCl)/nCrH = (E_{\mathrm{total}}^{\mathrm{HF/SW}} - n_{\mathrm{Cl}}\mu_{\mathrm{Cl}} - n_{\mathrm{Cl}}\mu_{\mathrm{Cl}})/n_{\mathrm{Cr}}. EtotalHF/SWE_{\mathrm{total}}^{\mathrm{HF/SW}} is the total energy of SW or HF, nCr(nCl)n_{\mathrm{Cr}}(n_{\mathrm{Cl}}) is the number of Cr (Cl) atoms. Chemical potentials of Cr and Cl in CrCl3_3 fulfill the equation μCr+3μCl=μCr∗+3μCl∗+ΔHCrCl3\mu_{\mathrm{Cr}}+3\mu_{\mathrm{Cl}}=\mu_{\mathrm{Cr}}^{*}+3\mu_{\mathrm{Cl}}^{*}+\Delta H_{\mathrm{CrCl}_3}, where μCr∗\mu_{\mathrm{Cr}}^{*} is the chemical potential of Cr in the bulk form, μCl∗\mu_{\mathrm{Cl}}^{*} is the chemical potential of Cl2_2 and ΔHCrCl3\Delta H_{\mathrm{CrCl}_3} is the formation energy of CrCl3_3. At the Cl rich limit, one gets μCl=μCl∗\mu_{\mathrm{Cl}}=\mu_{\mathrm{Cl}}^{*}, while at Cl deficient limit, μCl=μCl∗+ΔHCrCl3/3\mu_{\mathrm{Cl}}=\mu_{\mathrm{Cl}}^{*}+\Delta H_{\mathrm{CrCl}_3}/3.

The total energy reads EtotalHF/SW=nedgeHF/SW×(Eedge−fsHF/SW+Eedge−adHF/SW)+nbulkHF/SW×(Ebulk−fsHF/SW+Ebulk−adHF/SW)+ESECHF/SWE_{\mathrm{total}}^{\mathrm{HF/SW}} = n_{\mathrm{edge}}^{\mathrm{HF/SW}} \times(E_{\mathrm{edge-fs}}^{\mathrm{HF/SW}} + E_{\mathrm{edge-ad}}^{\mathrm{HF/SW}}) + n_{\mathrm{bulk}}^{\mathrm{HF/SW}} \times(E_{\mathrm{bulk-fs}}^{\mathrm{HF/SW}} + E_{\mathrm{bulk-ad}}^{\mathrm{HF/SW}}) + E_{\mathrm{SEC}}^{\mathrm{HF/SW}}. If we set EedgeHF/SW=Eedge−fsHF/SW+Eedge−adHF/SWE_{\mathrm{edge}}^{\mathrm{HF/SW}} = E_{\mathrm{edge-fs}}^{\mathrm{HF/SW}} + E_{\mathrm{edge-ad}}^{\mathrm{HF/SW}} and EbulkHF/SW=Ebulk−fsHF/SW+Ebulk−adHF/SWE_{\mathrm{bulk}}^{\mathrm{HF/SW}} = E_{\mathrm{bulk-fs}}^{\mathrm{HF/SW}} + E_{\mathrm{bulk-ad}}^{\mathrm{HF/SW}}, it further reads EtotalHF/SW=nedgeHF/SW×EedgeHF/SW+nbulkHF/SW×EbulkHF/SW+ESECHF/SWE_{\mathrm{total}}^{\mathrm{HF/SW}} = n_{\mathrm{edge}}^{\mathrm{HF/SW}} \times E_{\mathrm{edge}}^{\mathrm{HF/SW}} + n_{\mathrm{bulk}}^{\mathrm{HF/SW}} \times E_{\mathrm{bulk}}^{\mathrm{HF/SW}} + E_{\mathrm{SEC}}^{\mathrm{HF/SW}}, where subscripts “edge” and “bulk” refer to edge and bulk units of SW and HF, postfixes “-fs” and “-ad” denote free-standing and adsorbed forms of the CrClx_x units, nn is the number of CrClx_x units in a finite size SW or HF, subscript “SEC” stands for spinexchange coupling.

In order to determine the relative stability of the SW and HF phases with the same nCrn_{\mathrm{Cr}}, we could examine the difference of normalized enthalpy ΔHHF−SW=\Delta H_{\mathrm{HF-SW}}=

[(nedgeHF×EedgeHF+nbulkHF×EbulkHF)−(nedgeSW×EedgeSW+nbulkSW×EbulkSW)+(ESECHF−ESECSW)+ΔnClμCl]nCr\frac{\left[\left(n_{\mathrm{edge}}^{\mathrm{HF}} \times E_{\mathrm{edge}}^{\mathrm{HF}} + n_{\mathrm{bulk}}^{\mathrm{HF}} \times E_{\mathrm{bulk}}^{\mathrm{HF}}\right) - \left(n_{\mathrm{edge}}^{\mathrm{SW}} \times E_{\mathrm{edge}}^{\mathrm{SW}} + n_{\mathrm{bulk}}^{\mathrm{SW}} \times E_{\mathrm{bulk}}^{\mathrm{SW}}\right) + \left(E_{\mathrm{SEC}}^{\mathrm{HF}}-E_{\mathrm{SEC}}^{\mathrm{SW}}\right) + \Delta n_{\mathrm{Cl}}\mu_{\mathrm{Cl}}\right]}{n_{\mathrm{Cr}}}

where ΔnCl\Delta n_{\mathrm{Cl}} indicates the number difference of Cl atoms between the SW and HF phases. A ΔHHF−SW\Delta H_{\mathrm{HF-SW}} value larger (smaller) than zero indicates the superior stability of SW (HF). Here, the magnetic term is considerably smaller than other terms and is thus negligible in comparing relative energy of SW and HF. Number nedgeSWn_{\mathrm{edge}}^{\mathrm{SW}} always equals to 2 in a finite SW and number nbulkHFn_{\mathrm{bulk}}^{\mathrm{HF}} is often smaller than nedgeHFn_{\mathrm{edge}}^{\mathrm{HF}} or even approaches to zero in a small-size HF. We could consider a simplified and qualitative relation

ΔHHF−SW∼EedgeHF−EbulkSW+ΔnCl⋅μClnCr\Delta H_{\mathrm{HF-SW}} \sim E_{\mathrm{edge}}^{\mathrm{HF}}-E_{\mathrm{bulk}}^{\mathrm{SW}}+\frac{\Delta n_{\mathrm{Cl}}\cdot\mu_{\mathrm{Cl}}}{n_{\mathrm{Cr}}}

to judge the relative stability of SW and HF by assuming EedgeHF≈EbulkHFE_{\mathrm{edge}}^{\mathrm{HF}} \approx E_{\mathrm{bulk}}^{\mathrm{HF}} and EbulkSW≈EedgeSWE_{\mathrm{bulk}}^{\mathrm{SW}} \approx E_{\mathrm{edge}}^{\mathrm{SW}}. Thus, if EbulkSWE_{\mathrm{bulk}}^{\mathrm{SW}} is lower than EedgeHFE_{\mathrm{edge}}^{\mathrm{HF}}, we could have chance to obtain a positive ΔHHF−SW\Delta H_{\mathrm{HF-SW}} and thus more stable SW in a certain μCl\mu_{\mathrm{Cl}} range as derived from the experiments.

Data availability

The data that support the findings of this study are available within the article and its Supplementary Information. The source data are available from the corresponding authors upon request.

Code availability

The code that supports the findings of this study is available from the corresponding author upon reasonable request.

Acknowledgments

We thank the supports from the National Key R&D Program of China (Grant No. 2018FYA0305800, 2018YFA0703700 and No. 2018YFE0202700), the National Natural Science Foundation of China (Grant No. 11974012, 12134011, 61888102, 21802165, 11974422 and 12104504), the Strategic Priority Research Program of Chinese Academy of Sciences (Grant No. XDB30000000), the Fundamental Research Funds for the Central Universities, China, and the Research Funds of Renmin University of China [22XNKJ30 (W.J.)]. D.P.G. was supported by the Outstanding Innovative Talents Cultivation Funded Programs 2022 of Renmin University of China. S.Z.L. and C.W were supported by the China Postdoctoral Science Foundation (2019M652694 and 2021M693479). Calculations were performed at the Physics Lab of High-Performance Computing of Renmin University of China, Shanghai Supercomputer Center.

Author Contributions

S.Z.L., Z.B.C. and Y.P.G. carried out the MBE growth and STM/S measurements. D.P.G. and J.W. performed the first-principles calculations. J.H.D. and Y.S.B. contributed to the sample preparation and STM measurements. Z.B.C. completed the SP-STM characterization. C.T. and Y.G.S coordinated the preparations of NbSe2_2. C.W. and L.W.Z participated in discussions of theoretical calculations. J.H. and C.D.Z. initiated and coordinated the work, participated in the experiments, analyzed data. W.J. conceived the theoretical calculations and analysis. S.Z.L., D.P.G., J.H., J.W. and C.D.Z. wrote the manuscript with inputs from the other co-authors.

Competing interests

The authors declare no competing financial interests.

Additional information

Supplementary information The online version contains supplementary material available at https://doi.org/

Figure Captions

Figure 2 | STM images of 1D CrCl3\mathrm{CrCl}_3 wires on NbSe2\mathrm{NbSe}_2 and 2D CrCl3\mathrm{CrCl}_3 flakes on BLG. a, STM image of CrCl3\mathrm{CrCl}_3 grown on a bulk NbSe2\mathrm{NbSe}_2 surface (1.1 V, 10 pA). The inset shows the atomically resolved STM image taken on the nearby NbSe2\mathrm{NbSe}_2. The prime vector asub\mathbf{a}_{\mathrm{sub}} of the NbSe2\mathrm{NbSe}_2 lattice is marked as shown. b, Close-up image (1.1 V, 10 pA) showing that the as-grown 1D structures consisted of integer numbers of atomic wires, which were jointed at the small flakes. c, d, Atomically resolved images (0.5 V, 100 pA) of the isolated CrCl3\mathrm{CrCl}_3 single wire and bi-wires. The schematics of the atomic models are superposed on the images. Only the topmost Cl atoms (yellow in the model) were imaged, with the formation of the zigzag chains marked by the red dashed lines. The rectangular unit cell of the bi-wires is marked by black dashed lines. e, Typical image (1.6 V, 5 pA) of the sample grown on BLG showing only 2D flakes with a monolayer thickness. f, Atomically resolved image of the 2D CrCl3\mathrm{CrCl}_3 phase in e with an overlaid schematic model. The dashed black triangles indicate the Cl trimers. The small 2D flakes in a show the same 2D phase (Supplementary Fig. S1).

Image not extracted

Figure 2.

fig:2 | Atomic, electronic, and magnetic structures of 1D CrCl3\mathrm{CrCl}_3 wires. a, Perspective view of a single CrCl3\mathrm{CrCl}_3 wire composed of face-sharing CrCl6\mathrm{CrCl}_6 octahedra (shadowed). b, c, Top views of the most stable configurations of the single wire and bi-wires on the adsorbed NbSe2\mathrm{NbSe}_2 obtained in our DFT calculations. The corresponding cross-sectional views are shown in d. The Cr atoms are displayed in blue, and the Cl atoms are displayed in yellow (for the top-most ones) and green. e, Calculated phonon spectrum of the CrCl3\mathrm{CrCl}_3 wire array with an infinite width. f, Typical dI/dVdI/dV spectra (on a logarithmic scale) of a single wire (orange) and a 2D CrCl3\mathrm{CrCl}_3 flake (blue). The bandgap values are labelled. g, Schematics of the spin configuration in a single wire. A total energy comparison among various magnetic configurations indicates that the most stable configuration is the Néel AFM (ABAB) state (Supplementary Fig. S4). The arrows represent the spin directions. The lower panel shows the visual spin density distribution. (red: spin-up; blue: spin-down) h, Constant current images taken with a spin-polarized Ni tip. The upper and middle panels show the same area imaged by the tip magnetized with +0.7 T and -0.7 T magnetic fields, respectively. Both images were acquired at +1.5 V and 5 pA. Cross-check of the contrast reversal is seen in Supplementary Fig. S5. The lower panel is a sum of the above two panels. Scale bars are 0.5 nm. The vertical grid lines represent the Cr sites (blue dots), and atomic models are superimposed on each panel. i, Simulations of STM images with pure spin-up/down sample DOS at +1.0 V.

fig:3 | Coverage-dependent and tip-manipulated 1D-to-2D transformations. a–d, Coverage-dependent topographic images of CrCl3\mathrm{CrCl}_3 grown on NbSe2\mathrm{NbSe}_2 with the total coverage ranging from 0.035 ML to 0.36 ML. Scale bars are 50 nm. e, Plot of the coverage NwireN_{\mathrm{wire}} of the 1D wires and the coverage ratio R1D=Nwire/NtotalR_{\mathrm{1D}} = N_{\mathrm{wire}}/N_{\mathrm{total}} as functions of NtotalN_{\mathrm{total}}. f, Statistical analysis of the widths of the wire arrays at Ntotal=0.12N_{\mathrm{total}} = 0.12 ML and 0.36 ML. g, Tip-manipulated transformations from the 1D multi-wire arrays (MWs) to 2D nanoribbons (NRs). The technical details are discussed in the Methods Section. Images were taken at −0.6 V and 10 pA; scale bars are 2 nm.

Panels showing crystal structures, phonon spectrum, transport characteristics, magnetic configurations, and spin density

Figure 1 (PDF p. 23).

Image not extracted

Figure 1 (PDF p. 24).

Multi-panel figure showing Cr atom configurations and calculated charge variations. Panels (a) SW-6: Cr$_6$Cl$_{?}$; (b) HF-6: Cr$_6$Cl$_{?}$; (c) $\Delta H$ versus numbers of Cr atom ($n_{\mathrm{Cr}}$), comparing Cl deficient and Cl rich configurations, with labels AC, ZZ, SW, HF, and $\Delta H = H_{\mathrm{HF}} - H_{\mathrm{SW}}$; (d) SW-6 charge variation for configurations with NbSe$_2$ and Gr; (e) HF-6 charge variation for configurations with NbSe$_2$ and Gr; (f) $\Delta H$ versus numbers of Cr atom ($n_{\mathrm{Cr}}$), comparing Cl deficient and Cl rich configurations with NbSe$_2$ and Gr; (g) MW structure; (h) NR structure; (i) heat map of $\Delta H$ (eV) versus width ($w$), with regions labelled MW, expt., and NR.

Figure 3 (PDF p. 25).

References

  1. [1]Karakachian, H. et al. One-dimensional confinement and width-dependent bandgap formation in epitaxial graphene nanoribbons. Nat. Commun. 11, 6380 (2020).DOI
  2. [2]Chen, Y.-C. et al. Tuning the band gap of graphene nanoribbons synthesized from molecular precursors. ACS Nano 7, 6123–6128 (2013).
  3. [3]Yan, L. & Liljeroth, P. Engineered electronic states in atomically precise artificial lattices and graphene nanoribbons. Adv. Phys.-X 4, 1651672 (2019).
  4. [4]Yu, Y. et al. Phase-controlled growth of one-dimensional Mo₆Te₆ nanowires and two-dimensional MoTe₂ ultrathin films heterostructures. Nano Lett. 18, 675–681 (2018).DOI
  5. [5]Xia, Y. et al. Quantum confined Tomonaga–Luttinger liquid in Mo₆Se₆ nanowires converted from an epitaxial MoSe₂ monolayer. Nano Lett. 20, 2094–2099 (2020).DOI
  6. [6]Deng, J. et al. Precise tuning of band structures and electron correlations by van der Waals stacking of one-dimensional W₆Te₆ wires. Nano Lett. 20, 8866–8873 (2020).DOI
  7. [7]Huang, B. et al. Layer-dependent ferromagnetism in a van der Waals crystal down to the monolayer limit. Nature 546, 270–273 (2017).DOI
  8. [8]Gong, C. et al. Discovery of intrinsic ferromagnetism in two-dimensional van der Waals crystals. Nature 546, 265–269 (2017).
  9. [9]Deng, Y. et al. Gate-tunable room-temperature ferromagnetism in two-dimensional Fe₃GeTe₂. Nature 563, 94–99 (2018).DOI
  10. [10]Fei, Z. et al. Two-dimensional itinerant ferromagnetism in atomically thin Fe₃GeTe₂. Nat. Mater. 17, 778–782 (2018).DOI
  11. [11]O’Hara, D. J. et al. Room temperature intrinsic ferromagnetism in epitaxial manganese selenide films in the monolayer limit. Nano Lett. 18, 3125–3131 (2018).DOI
  12. [12]Chen, W. et al. Direct observation of van der Waals stacking–dependent interlayer magnetism. Science 366, 983–987 (2019).DOI
  13. [13]Kezilebieke, S. et al. Topological superconductivity in a van der Waals heterostructure. Nature 588, 424–428 (2020).
  14. [14]Bedoya-Pinto, A. et al. Intrinsic 2D-XY ferromagnetism in a van der Waals monolayer. Science 374, 616–620 (2021).
  15. [15]Liu, Y., Huang, Y. & Duan, X. Van der Waals integration before and beyond two-dimensional materials. Nature 567, 323–333 (2019).DOI
  16. [16]Fu, L., Shang, C., Zhou, S., Guo, Y. & Zhao, J. Transition metal halide nanowires: A family of one-dimensional multifunctional building blocks. App. Phys. Lett. 120, 023103 (2022).DOI
  17. [17]Choi, D.-J. et al. Colloquium: Atomic spin chains on surfaces. Rev. Mod. Phys. 91, 041001 (2019).DOI
  18. [18]Nadj-Perge, S. et al. Observation of Majorana fermions in ferromagnetic atomic chains on a superconductor. Science 346, 602–607 (2014).
  19. [19]Jeon, S. et al. Distinguishing a Majorana zero mode using spin-resolved measurements. Science 358, 772–776 (2017).DOI
  20. [20]Jack, B., Xie, Y. L. & Yazdani, A. Detecting and distinguishing Majorana zero modes with the scanning tunnelling microscope. Nat. Rev. Phys. 3, 541–554 (2021).DOI
  21. [21]Kim, H. et al. Toward tailoring Majorana bound states in artificially constructed magnetic atom chains on elemental superconductors. Sci. Adv. 4, eaar5251 (2018).DOI
  22. [22]Renard, J.-P., L.-P. Regnault, and M. Verdaguer, 2002, Magnetism: Molecules to Materials I: Models and Experiments (Wiley-VCH, Weinheim, Germany).
  23. [23]Sahling, S. et al. Experimental realization of long-distance entanglement between spins in antiferromagnetic quantum spin chains. Nat. Phys. 11, 255–260 (2015).DOI
  24. [24]Simon, J. et al. Quantum simulation of antiferromagnetic spin chains in an optical lattice. Nature 472, 307–312 (2011).DOI
  25. [25]Zhang, W. et al. Flat epitaxial quasi-1D phosphorene chains. Nat. Commun. 12, 5160 (2021).DOI
  26. [26]26.Li, S. et al. Robust half-metallicity in transition metal tribromide nanowires. Nanoscale 10, 15545–15552 (2018).DOI
  27. [27]Wiesendanger, R. Spin mapping at the nanoscale and atomic scale. Rev. Mod. Phys. 81,1495-1550 (2009).DOI
  28. [28]Bode, M. et al. Chiral magnetic order at surfaces driven by inversion asymmetry. Nature 447, 190–193 (2007).pubmed.ncbi.nlm.nih.gov/17495922
  29. [29]Wang, Q. et al. Large-scale uniform bilayer graphene prepared by vacuum graphitization of 6H-SiC(0001) substrates. J. Phys. Condens. Matter 25, 095002 (2013).DOI
  30. [30]Cavallini, M. & Biscarini, F. Electrochemically etched nickel tips for spin polarized scanning tunneling microscopy. Rev. Sci. Instrum. 71, 4457–4460 (2000).DOI
  31. [31]Chen, H., Xiao, W., Wu, X., Yang, K. & Gao, H.-J. Electrochemically etched Ni tips in a constant-current mode for spin-polarized scanning tunneling microscopy. J. Vac. Sci. Technol. B 32, 061801 (2014).DOI
  32. [32]Xing, Y., Shen, J., Chen, H. et al. Localized spin-orbit polaron in magnetic Weyl semimetal Co₃Sn₂S₂. Nat. Commun. 11, 5613 (2020).DOI
  33. [33]H. H., Zhang, et al. Majorana zero mode detected with spin selective Andreev reflection in the vortex of a topological superconductor. Phys. Rev. Lett., 116, 257003 (2016).
  34. [34]Jeon S, Xie Y, et al. Distinguishing a Majorana zero mode using spin-resolved measurements. Science, 358: 772-776 (2017).DOI
  35. [35]Perdew, J. P., Burke, K. & Ernzerhof, M. Generalized gradient approximation made simple. Phys. Rev. Lett. 77, 3865–3868 (1996).pubmed.ncbi.nlm.nih.gov/10062328
  36. [36]Blöchl, P. E. Projector augmented-wave method. Phys. Rev. B 50, 17953–17979 (1994).pubmed.ncbi.nlm.nih.gov/9976227
  37. [37]Kresse, G. and J. Furthmüller. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set. Phys. Rev. B 54, 11169–11186 (1996).pubmed.ncbi.nlm.nih.gov/9984901
  38. [38]Dion, M., et al. Van der Waals Density Functional for General Geometries. Phys. Rev. Lett. 92, 246401 (2004).DOI
  39. [39]Klimeš, J., et al. Van der Waals density functionals applied to solids. Phys. Rev. B 83, 195131 (2011).
  40. [40]Anisimov, V. I., et al. First-principles calculations of the electronic structure and spectra of strongly correlated systems: the LDA+U method. J. Phys. Condens. Matter 9, 767–808 (1997).
  41. [41]Li, P., et al. Single-layer CrI₃ grown by molecular beam epitaxy. Sci. Bull. 65, 1064–1071 (2020).DOI
  42. [42]Wang, C., et al. Layer and doping tunable ferromagnetic order in two-dimensional CrS₂ layers. Phys. Rev. B 97, 245409 (2018).DOI
  43. [43]Wang, C., Zhou X., et al. A family of high-temperature ferromagnetic monolayers with locked spin-dichroism-mobility anisotropy: MnNX and CrCX (X = Cl, Br, I; C = S, Se, Te). Sci. Bull. 64, 293(2019).DOI
  44. [44]Jiang P., Wang C., Chen D., et al. Stacking tunable interlayer magnetism in bilayer CrI₃. Phys. Rev. B 99, 144401 (2019).DOI
  45. [45]Wang C., Zhou X., Zhou L., et al. Bethe-Slater-curve-like behavior and interlayer spin-exchange coupling mechanisms in two-dimensional magnetic bilayers. Phys. Rev. B 102, 020402 (2020).DOI
  46. [46]Cheng, X., Cheng, Z., Wang, C., et al. Light helicity detector based on 2D magnetic semiconductor CrI₃. Nat. Commun. 12, 6874 (2021).DOI
  47. [47]Li, B., Wan, Z., Wang, C. et al. Van der Waals epitaxial growth of air-stable CrSe₂ nanosheets with thickness-tunable magnetic order. Nat. Mater. 20, 818–825 (2021).DOI
  48. [48]Xian, J., Wang, C., Nie, J. et al. Spin mapping of intralayer antiferromagnetism and field-induced spin reorientation in monolayer CrTe₂. Nat. Commun. 13, 257 (2022).DOI
  49. [49]Gu, P., et al. Magnetic Phase Transitions and Magnetoelastic Coupling in a Two-Dimensional Stripy Antiferromagnet. Nano Lett. 22,1233 (2022).DOI
  50. [50]Henkelman, G., et al. A fast and robust algorithm for Bader decomposition of charge density. Comput. Mater. Sci. 36, 354–360 (2006).DOI
  51. [51]Togo, A. and I. Tanaka. First principles phonon calculations in materials science. Scripta Mater. 108: 1–5 (2015).arxiv.org/abs/1506.08498

Paper details

vlnc:W_za3euurh
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents