betaFeedback

WorksPhysics and Astronomy

Geometrical Confinement of Magnetic Domains and Domain Walls on Two-Dimensional Cylindrical-Shaped Ferromagnetic Surfaces

Abstract

The rolling of two-dimensional (2D) van der Waals (vdW) magnetic monolayers into cylindrical architectures provides an ideal platform for confining magnetic domain walls (DWs) without edge-pinning effects. Here, we present a combined analytical and numerical investigation of DW confinement and interaction in ferromagnetic (FM) nanotubes. Using an analytical Heisenberg model on a 2D rectangular lattice, we show that transversal curvature introduces an azimuthal exchange energy penalty that intrinsically compresses the DW width. This model demonstrates excellent quantitative agreement with atomistic Landau-Lifshitz-Gilbert (LLG) spin dynamics simulations. By extending our study to realistic CrSBr (CSB) nanotubes, we model a bound state of two interacting DWs arising from a balance between long-range dipolar attraction and short-range exchange repulsion. Micromagnetic simulations reveal a non-monotonic evolution of the inter-wall distance with the tube perimeter. These findings highlight vdW magnetic nanotubes as robust platforms for stable domain confinement in quasi-one-dimensional spintronic architectures.

Introduction

2D vdW magnetic materials have emerged at the forefront of condensed matter physics owing to their remarkable and highly tunable properties [4, 5] [1, 2, 3]. Compounds such as CSB, CrI3_3, CrGeTe3_3, Fe3_3GeTe2_2 and NiPS3_3 have attracted significant interest, as their magnetic properties can be effectively manipulated via applied strain, interlayer sliding, twisting, or magnetoelectric fields [6, 7, 8, 9, 10, 11, 12]. The fundamental drive to understand these systems is largely motivated by their potential integration into next-generation spintronic and memory devices [13, 14, 15], where the external control of their magnetic properties allows for extended functionalities beyond conventional spintronics. Among such potential applications, magnetic racetrack memories represent a highly promising architecture, encoding data within magnetic DWs that are driven by spin currents along magnetic tracks [16, 17, 18].

The inherent mechanical flexibility of these vdW monolayers suggests the possibility of their reconfiguration into cylindrical architectures (nanotubes) which may be conceptually envisioned as a 2D sheet rolled into a seamless, hollow geometry [19, 20, 21, 22]. Within the continuum framework, micromagnetic models have successfully described magnetization reversal modes and DW dynamics in magnetic nanotubes [23, 24], forming part of the rapidly expanding field of curved magnetism [25, 26, 27]. However, despite extensive research on 2D vdW magnets, the physics of magnetic nanotubes derived from these materials remains largely unexplored [28, 29, 30, 31]. In this context, vdW magnetic nanotubes could serve as promising candidates for quasi-one-dimensional racetrack memory devices [32]. Their inherently cylindrical geometry is expected to facilitate the robust confinement and seamless propagation of magnetic domains along the tube axis, offering a potential route to circumventing the deleterious edge-pinning effects that typically plague conventional flat nanostripes.

Beyond these geometric and architectural advantages, the transition from a planar flat sheet to a cylindrical geometry fundamentally alters the topology and the underlying symmetry groups of the magnetic system. The imposition of periodic boundary conditions (PBC) along the azimuthal direction inherently quantizes the allowed magnetic textures, endowing the DWs with a topological protection that is strictly tied to a non-zero winding number [33]. This topological constraint severely restricts the continuous unwinding of the magnetic texture into a uniform FM state, thereby providing remarkable robustness against thermal fluctuations and structural defects. Furthermore, the geometric rolling process explicitly breaks the continuous two-dimensional translational symmetry, reducing the system to a symmetry group governed by one-dimensional (1D) axial translations and discrete CnC_n azimuthal rotations.

It is worth noting that DWs within these FM nanotube surfaces constitute inherently metastable configurations. Consequently, a primary objective of this work is to systematically investigate the precise conditions under which this metastability ensures sufficient stability to effectively confine magnetic domains.

In this work, we focus on the study of magnetic domains and DWs confined within cylindrical FM surfaces. To this end, Section III A presents an analytical investigation of DWs in a two-dimensional rectangular lattice rolled into a nanotube geometry. Subsequently, Section III B incorporates the material-specific exchange, anisotropy, and long-range dipolar parameters of CrSBr to simulate multi-domain states, demonstrating the robust spatial confinement of magnetic domains whose equilibrium length along the zz-axis is directly governed by the nanotube diameter.

Computational Method

To investigate the magnetic configurations of the cylindrical nanostructures, we performed atomistic spin dynamics simulations using the VAMPIRE software package [34]. The time evolution of the atomic spins and the energy minimization were computed by numerically integrating the LLG equation. For all calculations, each site was assigned a Cr atomic spin moment of μS=3.0μB\mu_S = 3.0 \mu_B. Furthermore, a Gilbert damping parameter of α=0.1\alpha= 0.1 was employed and dipole-dipole interactions were included.

The simulation protocols were specifically tailored for the two distinct geometries studied in this work. For the fundamental analysis of the rectangular lattice mapped onto a cylinder (§ 3 A), the system was constructed using Open Boundary Conditions (OBC) along the longitudinal zz-axis. To nucleate a single DW, the initial magnetic state was straightforwardly divided into two distinct halves: the lower section was magnetized antiparallel to the −z-z-direction (spin-down), while the upper section was set parallel (spin-up).

Conversely, to accurately capture the interactions between two confined DWs in the realistic CSB nanotubes (§ 3 B), a more sophisticated methodology was required. PBCs were rigorously applied along the zz-direction to emulate a quasi-one-dimensional continuous system and eliminate spurious edge-pinning effects. The initial state was engineered by defining longitudinally alternating domains (spin-up, spin-down, spin-up) separated by two finite-width transition regions. Within these interfaces, the local magnetization was azimuthally discretized into uniform sectors to artificially enforce specific chiralities (left- or right-handed) for each approaching DW. Crucially, in addition to the short-range exchange and uniaxial magnetocrystalline anisotropy, macroscopic dipole-dipole (magnetostatic) interactions were explicitly included in these CSB simulations. The evaluation of this dipolar field is essential to physically capture the long-range attractive forces governing the two-wall bound state.

For both theoretical setups, the systems were allowed to dynamically relax over an extended simulation timeframe of up to 100 ns. This prolonged relaxation protocol ensures that the delicate energetic balance—whether governed strictly by curvature-induced exchange penalties or by the competition between dipolar attraction and exchange repulsion—converges into a robust metastable bound state. While the global energy minimum of the system is fundamentally a uniform FM single domain, this extensive relaxation guarantees that the system successfully bypasses transient dynamic artifacts and settles into the local minima that stabilize the confined DWs.

Results

Rectangular Lattice on a Cylindrical FM Surface

In this subsection we establish a fundamental baseline by formulating an analytical Heisenberg model on an idealized 2D rectangular lattice rolled into a cylinder. This allows us to isolate how azimuthal exchange curvature penalties intrinsically compress the DW width, validating our analytical scaling laws against atomistic LLG spin dynamics simulations. We investigate the magnetic behavior of DWs within a nanotube geometry constructed from a rectangular lattice as depicted in Figure 1 (a). The system is described by an Heisenberg Hamiltonian for unit spins localized at site ii, ei=(eix,eiy,eiz)\mathbf{e}_i = (e_i^x, e_i^y, e_i^z), incorporating FM isotropic exchange interactions up to the second-nearest neighbors (J1J_1 and J2J_2). The isotropic exchange J1J_1 couples first-nearest neighbors along the zz direction, while J2J_2 couples nearest neighbors along the azimuthal direction (see Figure 1 (b)). To define the ground-state orientation, a uniaxial anisotropy KK is imposed, constraining the magnetic easy axis along the longitudinal direction of the cylinder. The resulting Hamiltonian is given by

Image not extracted

Figure 1. Schematic representation of a Néel DW separating magnetic domains on a rectangular lattice wrapped into a cylindrical geometry. (a) Longitudinal view of the cylinder, where the yellow region highlights the azimuthal rotation of magnetization inside the DW. Cyan (orange) regions represents the spin up (down) domains. (b) Cross-sectional view of the cylinder, where NcN_c is the number of atoms forming the circumference. (c) Unrolled 2D lattice mapping of the nanotube section enclosed by the dashed box, where blue arrows represent the local spins, NDWN_{\mathrm{DW}} defines the DW width along the zz-axis, and J1J_1 (J2J_2) denotes the longitudinal (azimuthal) exchange coupling constant.

H=12∑⟨ij⟩Jijei⋅ej+∑iK(eiz)2(1)H = \frac{1}{2} \sum_{\langle ij \rangle} J_{ij} \mathbf{e}_i \cdot\mathbf{e}_j + \sum_i K(e_i^z)^2 \tag*{(1)}

We investigate the energetic cost of forming a Néel-type DW with axial symmetry. Consequently, the spin orientations are restricted to the tangent planes of the cylindrical nanostructure, possessing only longitudinal and azimuthal components. The DW is shown in Figure 1(a). To this end, we evaluate separately the three contributions to the energy formation of the DW, δEJ1\delta E^{J_1}, δEJ2\delta E^{J_2}, and δEK\delta E^K. We chose to parametrize the spin vectors using spherical coordinates ei(θi,ϕi)=(sin⁡θicos⁡ϕi,sin⁡θisin⁡ϕi,cos⁡θi)\mathbf{e}_i(\theta_i,\phi_i) = (\sin\theta_i \cos\phi_i,\sin\theta_i \sin\phi_i,\cos\theta_i) where θ\theta is measured respect to the zz-axis and ϕ\phi respect to the xx-axis. Isotropic exchange J1J_1 couples nearest neighbors along the zz axis. Spins coupled by J1J_1 have same ϕ\phi angle and it only changes θ\theta along the zz axis according to

θi=π−π(zi−1)NDW−1for zi=1…NDW,(2)\theta_i = \pi- \frac{\pi(z_i - 1)}{N_{\mathrm{DW}} - 1} \quad\text{for } z_i = 1 \ldots N_{\mathrm{DW}}, \tag*{(2)}

where NDWN_{\mathrm{DW}} is the number of spins along the DW. The energy of a bond coupled by longitudinal exchange J1J_1 is EbondJ1=−J1cos⁡(θi+1−θi)≃J1(1−δθ2/2)E_{\mathrm{bond}}^{J_1} = -J_1 \cos(\theta_{i+1} - \theta_i) \simeq J_1(1 - \delta\theta^2/2) where δθ=θi+1−θi=π/(NDW−1)\delta\theta= \theta_{i+1} - \theta_i = \pi/(N_{\mathrm{DW}} - 1). So the energy cost from the FM state is δEbondJ1=−J1δθ2/2\delta E_{\mathrm{bond}}^{J_1} = -J_1 \delta\theta^2/2. The total contribution of J1J_1 to the DW energy is simply δEbondJ1\delta E_{\mathrm{bond}}^{J_1} times (NDW−1)(N_{\mathrm{DW}} - 1) times NcN_c so it reads

δEJ1=−J1π2Nc2(NDW−1).(3)\delta E^{J_1} = -\frac{J_1\pi^2N_c}{2(N_{\mathrm{DW}}-1)}. \tag*{(3)}

Azimuthal isotropic exchange J2J_2 couples neighbors with same height zz, this means that θ\theta remains constant for spins coupled by J2J_2. As in the previous case, we focus on a bond of a ring at height ziz_i so Ebondi,J2=J2ei(θi,ϕi)⋅ei(θi,ϕi+1)=J2[sin⁡2θicos⁡δϕ+cos⁡2θi]≃J2[sin⁡2θi(1−δϕ2/2)+cos⁡2θi]E_{\mathrm{bond}}^{i,J_2}=J_2\mathbf{e}_i(\theta_i,\phi_i)\cdot\mathbf{e}_i(\theta_i,\phi_{i+1})=J_2\left[\sin^2\theta_i\cos\delta\phi+\cos^2\theta_i\right]\simeq J_2\left[\sin^2\theta_i(1-\delta\phi^2/2)+\cos^2\theta_i\right] where δϕ=ϕi+1−ϕi=2π/Nc\delta\phi=\phi_{i+1}-\phi_i=2\pi/N_c. The energy cost from the FM state is δEbondi,J2=−J2δϕ2sin⁡2θi/2\delta E_{\mathrm{bond}}^{i,J_2}=-J_2\delta\phi^2\sin^2\theta_i/2 and considering all bonds coupled by J2J_2 on the ring at height ziz_i it is obtained δEringi,J2=−J2Ncsin⁡2θiδϕ2/2\delta E_{\mathrm{ring}}^{i,J_2}=-J_2N_c\sin^2\theta_i\delta\phi^2/2. Summing over all rings within the DW, we obtain

δEJ2=∑iNDWδEringi,J2=−12J2δϕ2Nc∑iNDWsin⁡2θi.\delta E^{J_2}=\sum_i^{N_{\mathrm{DW}}}\delta E_{\mathrm{ring}}^{i,J_2}=-\frac{1}{2}J_2\delta\phi^2N_c\sum_i^{N_{\mathrm{DW}}}\sin^2\theta_i.

Using the identity ∑iNDWsin⁡2θi=(NDW−1)/2\sum_i^{N_{\mathrm{DW}}}\sin^2\theta_i=(N_{\mathrm{DW}}-1)/2 and simplifying, we obtain

δEJ2=−J2π2(NDW−1)/Nc.(4)\delta E^{J_2}=-J_2\pi^2(N_{\mathrm{DW}}-1)/N_c. \tag*{(4)}

The contribution of the on-site anisotropy energy for all spins inside the DW is given by EKDW=KNc∑iNDWcos⁡2θiE_K^{\mathrm{DW}}=KN_c\sum_i^{N_{\mathrm{DW}}}\cos^2\theta_i.

Using the identity ∑iNDWcos⁡2θi=(NDW+1)/2\sum_i^{N_{\mathrm{DW}}}\cos^2\theta_i=(N_{\mathrm{DW}}+1)/2 it reads EKDW=KNc(NDW+1)/2E_K^{\mathrm{DW}}=KN_c(N_{\mathrm{DW}}+1)/2. Subtracting the energy of the FM state, we obtain

δEK=−KNc(NDW+1)/2(5)\delta E^K=-KN_c(N_{\mathrm{DW}}+1)/2 \tag*{(5)}

So the energy cost to form the DW described above is given by

δEDW=δEJ1+δEJ2+δEK(6)\delta E_{\mathrm{DW}}=\delta E^{J_1}+\delta E^{J_2}+\delta E^K \tag*{(6)}

By minimizing δEDW\delta E_{\mathrm{DW}} with respect to NDWN_{\mathrm{DW}}, we obtain the optimal DW length given by

NDW=J12J2/Nc2+K/π2+1(7)N_{\mathrm{DW}}=\sqrt{\frac{J_1}{2J_2/N_c^2+K/\pi^2}}+1 \tag*{(7)}

This expression represents a generalization of the standard formula NDW∝J/KN_{\mathrm{DW}}\propto\sqrt{J/K} for a 1D chain [35] to a 2D curved surface. Equation (7) indicates that the DW length increases with J1J_1, analogous to the behavior of a 1D chain, but decreases with J2J_2. The latter effect arises from the cylinder’s curvature; the exchange interaction J2J_2 couples spins located in different axial planes, which are non-parallel due to the underlying geometry. Consequently, the curvature induces an exchange energy penalty that tends to compress the DW.

Figs. 2 and 3 show the agreement between the analytical model given by Eq. (7) and the VAMPIRE atomistic simulations for an anisotropy of K=−0.1K=-0.1 meV. The DW length was numerically determined from the layer-resolved magnetization profiles (MPs) ⟨ez(z)⟩\langle e_z(z)\rangle extracted from the atomistic spin dynamics simulations, using a threshold criterion of ∣⟨ez⟩∣|\langle e_z\rangle| falling below 98.5% of its saturation value to define the transition region.

The temporal stability of the magnetic domains within the nanotubes can be modeled by the Néel-Arrhenius thermal relaxation model [36, 37, 38]. For a single domain D1 of length ND1N_{\mathrm{D1}}, the characteristic time τ\tau required to thermally overcome the anisotropy energy barrier, ΔEK=KNcND1\Delta E_K=KN_cN_{\mathrm{D1}}, is given by:

τ=τ0exp⁡(ΔEKkBT),(8)\tau=\tau_0\exp\left(\frac{\Delta E_K}{k_BT}\right), \tag*{(8)}

where kBTk_BT is the thermal energy and τ0\tau_0 represents the inverse attempt frequency, typically ranging from 10−910^{-9} to 10−1210^{-12} s. Eq. (8) allows us to determine the critical domain length for stability

ND1=kBTKNclog⁡(τ/τ0).(9)N_{\mathrm{D1}}=\frac{k_BT}{KN_c}\log(\tau/\tau_0). \tag*{(9)}

For fixed parameters T=300T=300 K, K=−0.1K=-0.1 meV, and τ=1010\tau=10^{10} s, ND1N_{\mathrm{D1}} is found to range from 100 to 600 as NcN_c varies between 20 and 100. Therefore, this guarantees that the domains are robust against spontaneous thermally activated magnetization reversal.

Image not extracted

Figure 2. Dependence of the DW length NDWN_{\mathrm{DW}} on the exchange coupling constants. (a) Colormap of the DW length calculated using atomistic simulations (VAMPIRE) as a function of J1J_1 and J2J_2 for a fixed number of cells Nc=30N_{\mathrm{c}} = 30. (b) Rounded difference between the numerical results from VAMPIRE and the theoretical predictions from Eq. (7). The color scale in (b) highlights the regions of maximum deviation between the model and the simulation.

Cylindrical CSB Nanostructure

In this subsection we extend the framework shown in § 3 A to realistic vdW monolayer CSB nanotubes. By incorporating material-specific exchange parameters, easy-axis magnetocrystalline anisotropy along the tube axis, and long-range magnetostatic dipolar interactions, we investigate the stability of multi-domain configurations and the equilibrium separation between confined DWs in these quasi-one-dimensional systems. CSB is a vdW material that can be exfoliated down to the 2D limit [39]. The monolayer is FM, with the easy axis oriented along the bb-direction (see Figure 4) and a Curie temperature around 140 K [40]. For the atomistic modeling of the CSB nanotubes, we adopt the experimental in-plane lattice parameters of the monolayer, specifically a=3.507a = 3.507 Å and b=4.749b = 4.749 Å [41]. In this work, we propose to exploit this specific magnetic anisotropy to construct a magnetic nanotube where the easy axis is parallel to the cylinder axis [29]. This configuration enables the confinement of magnetic domains of varying sizes along the length of the tubes.

Image not extracted

Figure 4. (a) Top and side views of a CSB monolayer. The lattice structure is defined by parameters aa and bb, where bb corresponds to the magnetic easy-axis direction. The intralayer exchange couplings J1J_1, J2J_2, and J3J_3 between first, second, and third nearest neighbors are indicated. (b) Schematic of a CSB nanotube formed by rolling up the monolayer with the tube axis parallel to the bb direction. The top and bottom panels display the side view and the cross-section of the cylinder, respectively.

To model the magnetic behavior of these nanotubes, we consider isotropic exchange couplings up to the third nearest neighbors, adopting the values reported for the monolayer [42]. Although curvature effects may become relevant at small radii, we assume as an approximation that the variation in these couplings is sufficiently small to avoid significant qualitative changes in our results. The easy-axis anisotropy is set to K=−0.1K = -0.1 meV, a value consistent with the range reported in previous theoretical studies of this material [7, 42, 43, 44].

We investigate the stability of magnetic domains in CSB nanotubes of varying widths and a fixed length of 947.3 Å. Figure 5 illustrates the schematic representation of these domains. We initialize the system with a spin configuration characterized by distinct, alternating up-down-up domains. These domains are separated by transition regions where ez=0e_z = 0, which subsequently evolve to form the DWs. The DWs formed in CSB nanotubes are of the Néel type described in § 3 A, as can be seen in Figure 1. This implies that a right- or left-handed chirality is associated with the DW via the right-hand rule. Figure 5 shows a CSB nanotube with two DWs separating spin-up and spin-down domains. If both DWs have opposite chirality, there is no topological protection against DW propagation, as a continuous transformation of the magnetization yields a fully FM configuration, causing the DWs to annihilate each other. However, if the chiralities of both DWs are the same, the domains are topologically protected.

Image not extracted

Figure 5. Schematic illustration of the micromagnetic simulation setup for a CSB nanotube containing a spin-down domain (orange) sandwiched between two spin-up domains (blue). Starting from an initial state where spins are aligned along the zz-axis (easy axis), the intermediate regions with ez=0e_z=0 are seeded with a specific orientation to define the desired DW chirality. The system then undergoes LLG evolution until it reaches the equilibrium state, where well-defined DWs (yellow) separated by a distance dd are formed.

The interaction between two DWs confined within a quasi-one-dimensional magnetic nanotube can be phenomenologically described by the competition between long-range magnetostatic forces and short-range exchange interactions [45]. The mutual interaction may be accurately modeled by considering them as interacting dipoles, leading to an attractive potential energy profile Ud(d)=−C/d3U_d(d)=-C/d^3, where dd denotes the separation distance between the two DWs. This dipole-dipole potential yields an attractive force whose magnitude is dictated by the parameter CC, which reflects the internal magnetization profile within the DW structures. Conversely, as the DWs approach each other, the spatial overlap of their magnetization tails induces a strong repulsive potential, which we define as Ue(d)=σ0e−d/ΔU_e(d)=\sigma_0e^{-d/\Delta}. In this expression, Δ=NDWb\Delta=N_{\mathrm{DW}}b represents the characteristic DW width and σ0\sigma_0 is the exchange energy prefactor. This fundamental competition between forces gives rise to a stable DW bound state [46]. Its characteristic equilibrium distance dd is determined by the force balance condition ∂∂d(Ud+Ue)=0\frac{\partial}{\partial d}(U_d+U_e)=0, which yields the transcendental equation d4e−d/Δ=3CΔσ0d^4e^{-d/\Delta}=\frac{3C\Delta}{\sigma_0}. By introducing the dimensionless inter-wall distance x=d/Δx=d/\Delta, the stability condition can be elegantly rewritten as x4e−x=3Cσ0Δ3≡λx^4e^{-x}=\frac{3C}{\sigma_0\Delta^3}\equiv\lambda. Here, λ\lambda

emerges as the fundamental dimensionless competition parameter dictating the existence of a stable two-wall system. The explicit dependence of λ\lambda on the discrete transversal geometry of the nanotube, parametrized by the number of azimuthal cells NcN_c, reveals a complex, non-monotonic evolution of the DW separation. The macroscopic dipolar constant scales with the square of the cross-sectional area, yielding C∝Nc2C\propto N_c^2, while the exchange penalty along the perimeter dictates σ0∝Nc\sigma_0\propto N_c. Crucially, the wall width Δ\Delta is not a constant, but is strongly coupled to the transversal curvature as we studied for the square lattice in Figure 3. According to Eq. (7) for moderate values of NcN_c, it is expected that the relief of the curvature-induced exchange energy causes Δ(Nc)\Delta(N_c) to expand rapidly. This substantial broadening of the DWs significantly stretches the spatial range of the exchange repulsion, temporarily overpowering the enhanced dipolar attraction and leading to an initial increase in the physical separation dd, as observed in micromagnetic simulations. However, in the asymptotic limit of macroscopically wide tubes (Nc→∞N_c \to\infty), the DW width saturates to a constant monolayer limit Δ∞\Delta_\infty, dictated solely by the magnetic anisotropy and exchange with no curvature effects. In this macroscopic regime, the dimensionless parameter λ(Nc)∝Nc/Δ∞3\lambda(N_c) \propto N_c/\Delta_\infty^3 grows linearly without bound. Once λ\lambda systematically exceeds the critical mathematical threshold for stable roots (λc=256/e4≈4.69\lambda_c = 256/e^4 \approx4.69), the purely quadratic scaling of the dipolar attraction inevitably crushes the exchange repulsion. Upon reaching this asymptotic collapse threshold, the ultimate fate of the system is strictly governed by topology. If the approaching DWs share the same chirality, the conservation of the total winding number forbids any continuous deformation into a collinear state.

Image not extracted

Figure 3. DW length NDWN_{\mathrm{DW}} versus the number of cells NcN_{\mathrm{c}}, with exchange couplings fixed at J1=J2=10J_1 = J_2 = 10 meV. A comparison between the results obtained from atomistic spin dynamics simulations (orange line) and the analytical model derived in Eq. (7) (blue line) is shown

To corroborate the phenomenological model, Figure 6 presents the micromagnetic simulation results for the two-wall system as a function of the nanotube perimeter. Figure 6(a) displays the normalized axial MPs (⟨ez⟩\langle e_z\rangle) for increasing nanotube perimeters, ranging from Nc=20N_c = 20 to 200. The corresponding physical separation dd between the DWs is extracted and plotted in Figure 6(b). In agreement with the theoretical framework, the system exhibits a pronounced, monotonic expansion of the inter-wall distance for moderate values of NcN_c (20≤Nc≲15020 \le N_c \lesssim150). Within this regime, the relief of the curvature-induced exchange penalty causes the characteristic DW width Δ(Nc)\Delta(N_c) to expand rapidly. As predicted, this substantial structural broadening stretches the spatial range of the exchange repulsion Ue(d)U_e(d), effectively overpowering the quadratically scaling dipolar attraction Ud(d)U_d(d) and driving the walls further apart. However, as the system transitions toward the macroscopic limit (Nc≳150N_c \gtrsim150), the growth of dd noticeably decelerates, leading to a saturation plateau. This behavior precisely reflects the onset of the asymptotic regime where the DW width approaches its constant monolayer limit, Δ∞\Delta_\infty, governed solely by magnetic anisotropy and exchange. In this plateau region, the exchange repulsion no longer gains spatial reach, allowing the dimensionless parameter λ(Nc)\lambda(N_c) to grow linearly. The stabilization of dd around Nc=200N_c = 200 indicates that the system has entered the macroscopic regime but has not yet systematically exceeded the critical mathematical threshold (λc≈4.69\lambda_c \approx4.69); therefore, the purely quadratic scaling of the dipolar attraction has not yet surpassed the short-range exchange repulsion required to drive a structural collapse of the bound state.

Image not extracted

Figure 6. (a) MPs of a CSB nanotube of length L=1275L = 1275 Å obtained from LLG dynamics versus the nanotube perimeter NcN_c, for the fixed initial condition ND=L/5N_D = L/5, at T=0T = 0 K. (b) Distance dd between DWs as a function of NcN_c.

From a technological standpoint, the physical length of the confined magnetic domains (which effectively encode the data bits in potential racetrack memory applications) is highly tunable via the nanotube geometry. As evidenced by Figure 6(b), the equilibrium distance of the spin-down domain sandwiched between two spin-up regions can be systematically modulated from 148 to 375 Å for NcN_c values corresponding to nanotube diameters ranging between 22 and 220 Å, respectively. This direct correlation demonstrates that the transverse geometrical confinement provides a versatile and precise mechanism to control the bit size and, consequently, the data density in these quasi-one-dimensional magnetic architectures. It is instructive to put these figures in the context of conventional racetrack memory concepts. In state-of-the-art perpendicular magnetic anisotropy (PMA)-based racetrack, experimentally demonstrated bit lengths have been pushed down to approximately 200 Å [47, 48]. This suggests that magnetic nanotubes could, in principle, reach comparable or higher data densities than conventional PMA racetracks.

Summary and Conclusions

We have systematically investigated the geometric confinement and stabilization of magnetic domains and DWs within two-dimensional vdW FM nanotubes. By employing an analytical Heisenberg model mapped onto a cylindrical surface, alongside realistic atomistic and micromagnetic simulations parameterized for CSB, we demonstrated that the transition from a planar geometry to a closed cylindrical architecture fundamentally alters the magnetic energetic landscape and topology of the system. Our analytical model for a rectangular lattice reveals that the characteristic DW width is tightly coupled to the transversal curvature of the cylinder. Specifically, the azimuthal exchange coupling between adjacent axial planes introduces an energy penalty that intrinsically compresses the DW. This curvature-induced compression modifies the standard one-dimensional DW length, yielding a generalized functional dependence on the discrete transversal geometry (NcN_c). Furthermore, applying a Néel-Arrhenius thermal relaxation model, we verified that domains of moderate lengths within these nanostructures present a remarkable robustness against thermally activated spontaneous magnetization reversal at room temperature.

We have established that interacting domain walls can form a metastable bound state at a specific equilibrium distance, dictated by the fine balance between dipolar attraction and exchange repulsion. We modeled their dynamics through the competition between a long-range attractive dipole-dipole potential and a short-range repulsive exchange interaction. Micromagnetic simulations of CSB nanotubes corroborate this framework, revealing a complex, non-monotonic evolution of the inter-wall distance as a function of the tube perimeter. For moderate tube perimeters, the relief of the curvature-induced exchange penalty rapidly expands the DW width Δ\Delta, stretching the spatial range of the exchange repulsion and temporarily overcoming the dipolar attraction, which physically drives the walls further apart.

However, as the system transitions toward the asymptotic planar limit (Nc→∞N_c \to\infty), the DW width saturates to a constant value governed by intrinsic anisotropy and exchange. In this macroscopic regime, the purely quadratic spatial scaling of the macroscopic dipolar constant ultimately crushes the exchange repulsion. Upon reaching this collapse threshold, topological constraints determine the resulting magnetic state. If the interacting DWs are topologically protected, the conservation of the winding number prohibits continuous annihilation.

Although this study employs CSB as a prototypical system, the physical principles driving the spatial confinement of magnetic domains are essentially universal. The analytical mapping of the rolled rectangular lattice demonstrates that domain wall compression arises fundamentally from the geometric curvature, transcending specific material parameters. Similarly, the energy balance between short-range exchange and long-range dipolar interactions, which dictates the domain length, is a general property of cylindrical boundary conditions. Therefore, our theoretical framework can be directly generalized to the broader class of 2D vdW ferromagnets, offering a universal route to design stable, quasi-one-dimensional magnetic architectures for spintronic applications simply by tuning the macroscopic curvature. Altogether, our findings establish that vdW magnetic nanotubes provide an exceptional platform for confining complex magnetic textures. Furthermore, the interplay between competing magnetic interactions yields a novel self-packing mechanism, offering a versatile route to control bit density in nanoscale storage architectures. The inherent absence of edge effects, combined with the strict topological protection granted by the periodic azimuthal boundary conditions, positions these curved quasi-one-dimensional geometries as highly promising candidates for robust, next-generation racetrack memory architectures and nanoscale spintronic devices.

Acknowledgements

G. M.-C., A. G.-F. and J. F. have been funded by Ministerio de Ciencia, Innovación y Universidades, Agencia Estatal de Investigación, Fondo Europeo de Desarrollo Regional via the grant PID2022-137078NB-I00, and by Agencia SEKUENS (Asturias) under grant UONANO IDE/2024/000678 with the support of FEDER funds. This project is supported by the TRILMAX Horizon Europe consortium (Grant No. 101159646). A. H.-R. acknowledges the support of Spanish MCIN/AEI/10.13039/501100011033/ FEDER, UE under Grant PID2022-136784NB and of Agencia SEKUENS (Asturias) under grant UONANO IDE/2024/000678 with the support of FEDER funds.

References

  1. [4]Y. Li, B. Yang, S. Xu, B. Huang, and W. Duan, Emergent phenomena in magnetic two-dimensional materials and van der waals heterostructures, ACS Applied Electronic Materials 4, 3278 (2022).DOI
  2. [5]J.-G. Park, K.-X. Zhang, H. Cheong, J. H. Kim, C. A. Belvin, D. Hsieh, H. Ning, and N. Gedik, 2d van der waals magnets: From fundamental physics to applications, Rev. Mod. Phys. (2026).DOI
  3. [6]Z. Fei, B. Huang, P. Malinowski, W. Wang, T. Song, J. Sanchez, W. Yao, D. Xiao, X. Zhu, A. F. May, W. Wu, D. H. Cobden, J.-H. Chu, and X. Xu, Two-dimensional itinerant ferromagnetism in atomically thin fe3gete2, Nature Materials 17, 778 (2018).DOI
  4. [7]C. Boix-Constant, A. Rybakov, C. Miranda-Pérez, G. Martínez-Carracedo, J. Ferrer, S. Mañas-Valero, and E. Coronado, Programmable magnetic hysteresis in orthogonally-twisted 2d crsbr magnets via stacking engineering, Advanced Materials 37, 2415774 (2025).
  5. [8]D. Bennett, G. Martínez-Carracedo, X. He, J. Ferrer, P. Ghosez, R. Comin, and E. Kaxiras, Stacking-engineered ferroelectricity and multiferroic order in van der waals magnets, Physical Review Letters 133, 246703 (2024).DOI
  6. [9]N. Sivadas, S. Okamoto, X. Xu, C. J. Fennie, and D. Xiao, Stacking-dependent magnetism in bilayer cri3, Nano Letters 18, 7658 (2018).DOI
  7. [10]X. Hu, Y. Zhao, X. Shen, A. V. Krasheninnikov, Z. Chen, and L. Sun, Enhanced ferromagnetism and tunable magnetism in fe3gete2 monolayer by strain engineering, ACS Applied Materials & Interfaces 12, 26367 (2020).DOI
  8. [11]G. Martínez-Carracedo, A. García-Fuente, L. Oroszlány, L. Szunyogh, and J. Ferrer, Tuning magnetic exchange interactions in two-dimensional magnets: The case of CrGeX3 (x = se, te) and janus cr2ge2 (se,te)3 monolayers, Phys. Rev. B 110, 184406 (2024).
  9. [12]C.-Y. Cheon, V. Multian, K. Watanabe, T. Taniguchi, A. F. Morpurgo, and D. Lebedev, Nature of 2d xy antiferromagnetism in a van der waals monolayer, Nature Communications 17, 60 (2025).DOI
  10. [13]A. Fert, R. Ramesh, V. Garcia, F. Casanova, and M. Bibes, Electrical control of magnetism by electric field and current-induced torques, Rev. Mod. Phys. 96, 015005 (2024).DOI
  11. [14]V. J. Borràs, R. Carpenter, L. Žaper, S. Rao, S. Couet, M. Munsch, P. Maletinsky, and P. Rickhaus, A quantum sensing metrology for magnetic memories, npj Spintronics 2, 14 (2024).DOI
  12. [15]B. Zhang, P. Lu, R. Tabrizian, P. X.-L. Feng, and Y. Wu, 2d magnetic heterostructures: spintronics and quantum future, npj Spintronics 2, 6 (2024).arxiv.org/abs/2311.03505
  13. [16]K. Gu, Y. Guan, B. K. Hazra, H. Deniz, A. Migliorini, W. Zhang, and S. S. P. Parkin, Three-dimensional race-track memory devices designed from freestanding magnetic heterostructures, Nature Nanotechnology 17, 1065 (2022).DOI
  14. [17]R. Tomasello, E. Martinez, R. Zivieri, L. Torres, M. Carpentieri, and G. Finocchio, A strategy for the design of skyrmion racetrack memories, Scientific Reports 4, 6784 (2014).arxiv.org/abs/1409.6491
  15. [18]M. G. Morshed, H. Vakili, and A. W. Ghosh, Positional stability of skyrmions in a racetrack memory with notched geometry, Phys. Rev. Appl. 17, 064019 (2022).DOI
  16. [19]I. Caha, A. u. Ahmad, and F. L. Deepak, Confinement-controlled morphology and stability of one-dimensional
  17. [20]X. Lan, L. Geng, Z. Zhang, Y. Li, J. Yuan, C.-X. Zhou, S. Huang, Z. Hu, J. Li, C. Yang, Y. Zhang, Z. Fan, D. Tian, X. Zhao, Q. Li, and L. Kang, Tunable synthesis of atomic one-dimensional xtey magnets within single-walled carbon nanotubes, Nature Communications 16, 6300 (2025).DOI
  18. [21]R. Rao, G. Chen, L. M. R. Arava, K. Kalaga, M. Ishigami, T. F. Heinz, P. M. Ajayan, and A. R. Harutyunyan, Graphene as an atomically thin interface for growth of vertically aligned carbon nanotubes, Scientific Reports 3, 1891 (2013).DOI
  19. [22]J. Li, Z. Zhang, Y. Li, H. Zhang, Y. Zhong, A. Li, Y. Teng, J. Yao, C. Zhou, Z. Fan, L. Geng, and L. Kang, Quantum spin dynamics of one-dimensional magnetic van der waals heterostructures, Journal of the American Chemical Society 147, 23972 (2025).DOI
  20. [23]P. Landeros, S. Allende, J. Escrig, E. Salcedo, D. Altbir, and E. E. Vogel, Reversal modes in magnetic nanotubes, Applied Physics Letters 90, 102501 (2007).
  21. [24]P. Landeros and Á. S. Núñez, Domain wall motion on magnetic nanotubes, Journal of Applied Physics 108, 033917 (2010).DOI
  22. [25]R. Streubel, P. Fischer, F. Kronast, V. P. Kravchuk, D. D. Sheka, Y. Gaididei, O. G. Schmidt, and D. Makarov, Magnetism in curved geometries, Journal of Physics D: Applied Physics 49, 363001 (2016).
  23. [26]K. V. Yershov, S. Kondovych, and D. D. Sheka, Chiral breakdown engineered by mesoscale dzyaloshinskii-moriya interaction in biaxial magnetic nanotubes, Phys. Rev. B 111, 184419 (2025).DOI
  24. [27]D. A. Dugato, W. B. F. Jalil, R. Cardias, M. Albuquerque, M. Costa, T. P. Almeida, K. Fallon, A. Kovács, S. McVitie, R. E. Dunin-Borkowski, and F. Garcia, Curved nanomagnets: An archetype for the skyrmionic states at ambient conditions, Nano Letters 25, 8901 (2025).DOI
  25. [28]A. Edström, D. Amoroso, S. Picozzi, P. Barone, and M. Stengel, Curved magnetism in cri3, Phys. Rev. Lett. 128, 177202 (2022).DOI
  26. [29]X. Zhang, X. Chen, and J. Qi, Curvature-induced magnetic anisotropy in two-dimensional magnetic semiconductor crsbr, Applied Physics Letters 127, 052407 (2025).
  27. [30]J. Huang and Y.-J. Zhao, Theoretical study of the stability and magnetic anisotropy of cr3x (x = cl, br, i) nanotubes, Journal of Physics D: Applied Physics 59, 095003 (2026).DOI
  28. [31]A. ul Ahmad, I. Çāha, T. Ahmad, A. N. Enyashin, J. H. Belo, W. Bin, P. Gargiani, M. Valvidares, and F. L. Deepak, Curvature-engineered magnetism and interfacial charge transfer in 1d crcl3@mwcnts heterostructures, Nanoscale 18, 17598 (2026).DOI
  29. [32]Y. Guan, Y. Wu, Y. Zhang, J.-C. Jeon, W. Zhang, K. Xiao, and S. S. P. Parkin, Highly efficient current-induced domain wall motion in a room temperature van der waals magnet, Nature Communications 16, 10790 (2025).DOI
  30. [33]M. Nakahara, Geometry, Topology and Physics (CRC Press, 2003).
  31. [34]R. F. L. Evans, W. J. Fan, P. Chureemart, T. A. Ostler, M. O. A. Ellis, and R. W. Chantrell, Atomistic spin model simulations of magnetic nanomaterials, Journal of Physics: Condensed Matter 26, 103202 (2014).
  32. [35]S. H. Simon, The Oxford Solid State Basics (Oxford University Press, Oxford, UK, 2013).
  33. [36]L. Néel, Théorie du traînage magnétique des ferromagnétiques en grains fins avec applications aux terres cuites, Ann. Géophys. 5, 99 (1949).
  34. [37]W. F. Brown, Thermal fluctuations of a single-domain ferromagnetic particle, Phys. Rev. 130, 1677 (1963).
  35. [38]A. R. Chalifour, J. C. Davidson, N. R. Anderson, T. M. Crawford, and K. L. Livesey, Magnetic relaxation time for an ensemble of nanoparticles with randomly aligned easy axes: A simple expression, Phys. Rev. B 104, 094433 (2021).DOI
  36. [39]Y. Zur, A. Noah, C. Boix-Constant, S. Mañas-Valero, N. Fridman, R. Rama-Eiroa, M. E. Huber, E. J. G. Santos, E. Coronado, and Y. Anahory, Magnetic imaging and domain nucleation in crsbr down to the 2d limit, Advanced Materials 35, 2307195 (2023), https://advanced.onlinelibrary.wiley.com/doi/pdf/10.1002/adma.202307195DOI
  37. [40]K. Lee, A. H. Dismukes, E. J. Telford, R. A. Wiscons, J. Wang, X. Xu, C. Nuckolls, C. R. Dean, X. Roy, and X. Zhu, Magnetic order and symmetry in the 2d semiconductor crsbr, Nano Letters 21, 3511 (2021).DOI
  38. [41]S. A. López-Paz, Z. Guguchia, V. Y. Pomjakushin, C. Witteveen, A. Cervellino, H. Luetkens, N. Casati, A. F. M. Mourgou, and F. O. von Rohr, Dynamic magnetic crossover at the origin of the hidden-order in van der waals antiferromagnet crsbr, Nature Communications 13, 4745 (2022).
  39. [42]S. Dey, D. L. Esteras, and J. J. Baldoví, Tailoring the properties of the 2d ferromagnet crsbr by lanthanide doping, Journal of Physics: Materials 8, 025013 (2025).arxiv.org/abs/2412.17682
  40. [43]A. N. Rudenko, M. Rösner, and M. I. Katsnelson, Dielectric tunability of magnetic properties in orthorhombic ferromagnetic monolayer crsbr, npj Computational Materials 9, 83 (2023).DOI
  41. [44]B. Wang, Y. Wu, Y. Bai, P. Shi, G. Zhang, Y. Zhang, and C. Liu, Origin and regulation of triaxial magnetic anisotropy in the ferromagnetic semiconductor crsbr monolayer, Nanoscale 15, 13402 (2023).DOI
  42. [45]A. Kunz, Field-induced domain wall motion in magnetic nanowires, Journal of Applied Physics 99, 08G107 (2006).
  43. [46]L. Thomas, M. Hayashi, R. Moriya, C. Rettner, and S. Parkin, Topological repulsion between domain walls in magnetic nanowires leading to the formation of bound domain walls, Nature Communications 3, 810 (2012).DOI
  44. [47]S. Fukami, M. Yamanouchi, K. J. Kim, T. Suzuki, N. Sakimura, D. Chiba, S. Ieda, T. Sugibayashi, N. Kasai, T. Ono, and H. Ohno, 20-nm magnetic domain wall motion memory with ultralow-power operation, in 2013 IEEE International Electron Devices Meeting, 2013 IEEE International Electron Devices Meeting (2013) pp. 3.5.1–3.5.4.DOI
  45. [48]S. Parkin and S.-H. Yang, Memory on the racetrack, Nature Nanotechnology 10, 195 (2015).DOI

Paper details

vlnc:W_fx9hwwub
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents