betaFeedback

WorksPhysics and Astronomy

Engineering antiferromagnetic (LaVO3)m/(PrVO3)n superlattices

Abstract

In this study, we demonstrate the atomic-scale engineering of antiferromagnetic (LaVO3)m/(PrVO3)n superlattices grown by MBE on (001)-oriented SrTiO3 substrates. Our work achieved a precise layer-by-layer control, revealing how interface-driven structural distortions can be systematically tuned. X-ray diffraction and reciprocal space mapping confirm both the epitaxial strain state and the high crystalline quality of the superlattices. High-resolution scanning transmission electron microscopy further uncovers layer-resolved atomic displacements, where La3+ and Pr3+ exhibit antipolar motions modulated by the superlattice periodicity. The alternate stackings of LaVO3 and PrVO3 yield a unique antiferromagnetic transition temperature, which can be tuned by adjusting their relative proportions. This behavior exists despite the distinct spin ordering temperatures observed in the constituent materials. Layer-resolved spectroscopic measurements reveal that the hybridization of La and Pr 5d orbitals with O 2p orbitals is also modulated and directly correlated to the oxygen octahedra rotations. By determining the orbital hybridization and mapping the cation displacements as proxies, we can visualize indirectly the trilinear coupling between oxygen octahedra rotations and antipolar rare earth displacements. Notably, the interfacial oxygen octahedra connectivity between cubic SrTiO3 substrate and orthorhombic vanadate layers significantly influences the structural distortions. These distortions, almost quenched near the interface, relax over few unit cells, demonstrating how strain and interfacial effects propagate through the superlattice. This study illustrates how artificial superlattices can be engineered to control structural distortions at the atomic scale, offering a pathway to tune the magnetic properties through strain-distortion relationships in perovskite oxides.

Introduction

Antiferromagnetic materials have emerged as a leading alternative to ferromagnetic materials in spintronics [1]. As in ferromagnets, information can be written in antiferromagnets via spin reorientations between antiferromagnetic states, achieved by using current-induced spin transfer torques [2] or a short laser pulse [3]. Likewise, information stored in antiferromagnets can be read out either by converting their antiferromagnetic configuration into a measurable voltage via spin orbit torque [4], or by imaging it through magneto-optical [5] or polarization-dependent spectroscopic [6] techniques. While both antiferromagnetic and ferromagnetic spintronics rely on the spin of the electron rather than its charge, antiferromagnetic materials overcome some limitations inherent to ferromagnetic materials, such as magnetic stray fields, low dynamic frequencies or Joule heating. Furthermore, antiferromagnets are more abundant than ferromagnets, and among them chemically stable antiferromagnetic transition metal oxides standout as particularly promising candidates for future devices. Their zero net magnetic moment implies the absence of stray fields, their dynamics fall into the THz range, and most are insulators. Therefore, antiferromagnetic oxides enable a paradigm shift toward higher storage densities, ultrafast operations, and lower power consumption in spintronic devices [7].

In oxide insulators, magnetic orders can be manipulated by an electric field (rather than an electrical current). This magnetoelectric property can be found in some transition metal oxides, especially those having a ABO3_{3} perovskite structure, where electrons’ degrees of freedom give rise to correlated electronic states driven by the strong interplay among spin, orbital, and charge orders [8, 9]. The crystalline structure plays also an important role in the coupling mechanisms, thereby motivating the systematic consideration of structural distortions in perovskites. In proper ferroelectric materials like BaTiO3_{3}, the spontaneous polarization appears as the compound undergoes a structural phase transition. On the contrary, in materials such as TbMnO3_{3}, ferroelectricity is magnetically driven, arising from canted antiferromagnetic spins that break inversion symmetries [10]. This improper ferroelectric character results in a strong magnetoelectric coupling, inspiring the search for materials whereby ferroelectricity and antiferromagnetism are intimately coupled to the lattice distortions. In PbnmPbnm orthorhombic perovskites, non-polar BO6BO_6 oxygen octahedra rotations and anti-polar A-site displacements are trilinearly coupled, leading theoretically to a hybrid improper ferroelectric character in AA′BO3AA'BO_3 double-perovskites or in designed short-period (ABO3)1/(A′BO3)1(ABO_3)_1/(A'BO_3)_1 superlattices [11, 12, 13]. In these artificially designed materials, another trilinearly coupled term, involving Jahn-Teller (JT) and A-site motions, can also induce a ferroelectric state [14]. In RVO3RVO_3 (RR = rare earth or yttrium), JT distortions lift the degeneracy of the V3+V^{3+} 3d3d–t2gt_{2g} orbitals resulting in either in-phase or anti-phase orbital ordering. Consequently, the overlap between orbitals at neighboring V-sites favors different antiferromagnetic spin order, determined by specific orbital arrangements [15]. This spin-orbital-distortion coupling underpins the design principles for artificial magnetoelectric materials.

Here, in the pursuit of developing an artificial multiferroic system, we have investigated the magnetic properties of symmetry-broken RVO3RVO_3-based superlattices. To this end, we have precisely engineered superlattices made of alternating layers of LaVO3_3 and PrVO3_3 with an atomic-level precision. Both LaVO3_3 and PrVO3_3 are antiferromagnetic Mott insulators that adopt an orthorhombic PbnmPbnm structure at room temperature. At the orbital ordering temperature TOOT_{\mathrm{OO}}, the 3d3d–t2gt_{2g} V3+V^{3+} orbitals undergo a G-type order (GOOG_{\mathrm{OO}}) transition, accompanied by a structural phase transition from orthorhombic PbnmPbnm to monoclinic P21/mP2_1/m symmetry. Close to or below this temperature, superexchange interactions stabilize a C-type antiferromagnetic spin order (CSOC_{\mathrm{SO}}) of the V3+V^{3+} spins at the spin ordering temperature TSOT_{\mathrm{SO}}. For bulk LaVO3_3, these transitions occur at TOO≈140T_{\mathrm{OO}} \approx140 K and TSO≈142T_{\mathrm{SO}} \approx142 K, and for bulk PrVO3_3, they take place at TOO≈180T_{\mathrm{OO}} \approx180 K and TSO≈135T_{\mathrm{SO}} \approx135 K [16]. After characterizing the structural and chemical properties of the superlattices down to the atomic scale at interfaces, we investigated the magnetic properties of the superlattices and found that they exhibit a unique, composition-dependent TSOT_{\mathrm{SO}}, whose value can be tuned by controlling the relative proportions of PrVO3_3 (PVO) and LaVO3_3 (LVO). Finally, we quantified the La- and Pr-displacements throughout the thickness and correlated the rare-earth atomic positions with the oxygen octahedra rotations. These lattice distortions, initially almost quenched near the interface, relax over 5–6 unit cells, demonstrating how strain and interfacial effects propagate through the superlattice (SL).

Results and Discussion

Growth and design of the superlattices.

At room temperature, the bulk lattice parameters are aoPVO=5.487a_o^{\mathrm{PVO}} = 5.487 Å, boPVO=5.564b_o^{\mathrm{PVO}} = 5.564 Å, coPVO=7.779c_o^{\mathrm{PVO}} = 7.779 Å for PVO and aoLVO=5.555a_o^{\mathrm{LVO}} = 5.555 Å, boLVO=5.553b_o^{\mathrm{LVO}} = 5.553 Å, coLVO=7.847c_o^{\mathrm{LVO}} = 7.847 Å for LVO (oo stands for orthorhombic) [17]. Considering a pseudo-cubic (pcpc) unit cell approximation, where apc≈ao/2≈bo/2≈co/2a_{pc} \approx a_o/\sqrt{2} \approx b_o/\sqrt{2} \approx c_o/2, the averaged subcell parameters are 3.901 Å for PVO and 3.926 Å for LVO. When epitaxially grown on (001)-oriented SrTiO3_3 (STO) (aSTO=3.905a_{\mathrm{STO}} = 3.905 Å), stoichiometric and (110)o_o-oriented LVO and PVO thin films experience a compressive (−0.5%-0.5\%) and tensile (+0.1%+0.1\%) strain state, respectively [18]. Based on this previous work, we have grown epitaxial SLs consisting of pp repetition of a (LVO)m_m/(PVO)n_n motif (mm and nn pseudocubic unit cells) on (001)-oriented STO cubic substrates. The mm LVO and nn PVO layers were deposited under optimized conditions using molecular beam epitaxy (MBE) in a background pressure of distilled ozone (see Methods and Ref. [18]). A layer-by-layer growth mode was monitored by in situ reflective high energy electron diffraction (RHEED), with diffraction patterns along the [100]pc_{pc} and [110]pc_{pc} surface directions confirming the epitaxial growth of the SL (see Fig. S1 in Supporting Information, SI). Additionally, we performed in situ X-ray photoelectron spectroscopy (XPS) to probe the rare earths 3d3/23d_{3/2} and 3d5/23d_{5/2} core-level states. Due to the surface sensitivity of XPS, we observed that for m=5m = 5, the intensity of the Pr 3d3d states increases with nn, while that of the La 3d3d states decreases (see Fig. S1 in SI), confirming the layered structure of the deposited materials. For conciseness, these SLs are denoted by their compositional parameters as [m/n]p[m/n]_p.

Figure 1 presents the results of high-resolution X-ray diffraction (XRD) measurements performed on the SLs grown under optimized conditions. Figure 1(a) illustrates the SL motif or supercell, where mm and nn are the number of LVO and PVO layers, respectively. During the growth, the motif is repeated pp times, with pp adjusted according to mm and nn to maintain the same total thickness (∼80\sim80 nm) across the SL series. In Figure 1(b), we show the symmetric 2θ2\theta–ω\omega diffraction patterns around the (002) Bragg peak for various [m/n]p[m/n]_p SLs. The presence of Laue fringes on the main peak (labelled 0) confirms the high crystallinity of the SLs and a well defined interface with the substrate. Additionally, the presence of satellite peaks (labelled −1-1 and +1+1) indicates a superstructure along the growth direction, characteristic of the SL with well-defined interfaces separated by a superperiod (Λ\Lambda, in Å). We point out that (±2\pm2) satellite peaks were also observed for the thickest Λ\Lambda (see Fig. S2 in SI). The full-width at half-maximum of the main Bragg peak rocking curves (not shown) is approximately 0.05∘0.05^\circ for the SLs and 0.02∘0.02^\circ for the substrate, reflecting the high structural quality of the samples.

Figure 1. (a) Sketch of (LaVO3)m/(PrVO3)n(\mathrm{LaVO}_3)_m/(\mathrm{PrVO}_3)_n motif repeated pp times. (b) 2θ−ω2\theta-\omega XRD measurements of [m/n]p[m/n]_p SLs close to the (001) STO Bragg peak (indicated by a star). The SL main and satellite peaks are labelled by 0 and ±1\pm1, respectively. (c)–(g) RSMs of the asymmetric (1ˉ03)(\bar{1}03) Bragg peaks for the [1/5]36[1/5]_{36}, [3/5]27[3/5]_{27}, [5/5]22[5/5]_{22}, [7/5]18[7/5]_{18} and [9/5]16[9/5]_{16} superlattices, respectively. The red and black dotted lines indicate the position of the STO and SL Bragg peaks, respectively. The SL peak width is marked between arrows. (h) 1/cˉ1/\bar{c} and (c/a)(c/a) as a function of m×cLVO/Λm \times c_{\mathrm{LVO}}/\Lambda, representing the LVO proportion in the motif. The solid lines are the calculated values considering the lattice parameters of LVO and PVO thin films.

Figure 1(c)–(Figure 1g) display the reciprocal space maps around the asymmetrical (103) Bragg peaks of the SLs and the substrate for different [m/5]p[m/5]_p compositions (with 5 PVO unit cells in the supercells). Firstly, we observe that the SL and substrate peaks are vertically aligned at the same q∥q_{\parallel} value, indicating that the SLs are fully strained by STO, which imposes its in-plane lattice parameter aSTOa_{\mathrm{STO}}. Secondly, as the thickness of the LVO layer increases with mm, we observe that the q⊥q_{\perp} value of the SL peak decreases, indicating an elongation of the out-of-plane superlattice parameter. This behavior corresponds to the increasing contribution of the LVO layers to the average cˉ\bar{c} lattice parameter (see below). Hence, the SL and substrate Bragg peaks are nearly superimposed in Figure 1(c) when m=1m=1, where the 5 PVO layers dominate, similar to PVO thin films [18]. Then, as mm increases, the SL and substrate Bragg peaks split vertically. We note that the surface topography of LVO and PVO thin films, observed by atomic force microscopy (AFM), revealed a surface roughness of approximately 1 unit cell [18]. Consequently, the interfaces are expected to be better defined as mm and nn deviate from 1. This is indeed confirmed by examining the width of the SL Bragg peaks along q∥q_{\parallel} in Figure 1(c)–(Figure 1g): as mm increases, the width decreases, indicating an improved lateral correlation or reduced mosaicity.

From the 2θ−ω2\theta-\omega measurements, we determine the pseudo-cubic out-of-plane lattice parameter (cˉ\bar{c}), which represents a weighted average of the interplanar distance in the LVO and PVO layers (cLVOc_{\mathrm{LVO}} and cPVOc_{\mathrm{PVO}}). cˉ\bar{c} is expressed as [19, 20]:

cˉ=m×cLVO+n×cPVOm+n=Λntot(1)\bar{c}=\frac{m \times c_{\mathrm{LVO}}+n \times c_{\mathrm{PVO}}}{m+n}=\frac{\Lambda}{n_{\mathrm{tot}}} \tag*{(1)}

The analysis of the main (002)pc_{\mathrm{pc}} Bragg peaks enables the determination of cˉ\bar{c} for each epitaxially strained SL. Considering cLVOc_{\mathrm{LVO}} and cPVOc_{\mathrm{PVO}} out-of-plane interplanar distances are similar to optimized thin films grown under identical conditions [18], mm, nn and ntotn_{\mathrm{tot}} (m+nm+n) are input growth parameters, which are monitored by the RHEED intensity oscillations. Thereby, we derive:

1cˉ=m×cLVOΛ(1cLVO−1cPVO)+1cPVO(2)\frac{1}{\bar{c}}=\frac{m \times c_{\mathrm{LVO}}}{\Lambda}\left(\frac{1}{c_{\mathrm{LVO}}}-\frac{1}{c_{\mathrm{PVO}}}\right)+\frac{1}{c_{\mathrm{PVO}}} \tag*{(2)}

In Figure 1(h), we present 1/cˉ1/\bar{c} as a function m×cLVO/Λm \times c_{\mathrm{LVO}}/\Lambda. Furthermore, since the SLs are constrained by STO, we also plot the (cˉ/a)(\bar{c}/a) ratio as a function of m×cLVO/Λm \times c_{\mathrm{LVO}}/\Lambda, where aa (equal to aSTOa_{\mathrm{STO}}) is the in-plane lattice parameter. These relationships describe how the SL structure depends on the LVO composition, treated here as a common variable. The solid lines represent the theoretical relationships for the targeted compositions, while the points are derived from fitting the main peak positions. The very good agreement between the calculated and experimental data demonstrates the precise control over the layer composition and, consequently, the atomic-level design of the SLs grown by MBE. To achieve a macroscopic electric polarization, the alternate stacking of the LVO and PVO layers breaks the inversion symmetry along the growth direction. But, mm and nn must be odd to ensure that the antipolar displacements of La3+^{3+} and Pr3+^{3+} remain uncompensated. Ultimately, we designed a [3/3]36_{36} SL exhibiting well defined satellite peaks (see Fig. S2 in SI).

The microstructural and compositional details of the interfaces were further investigated using a combination of scanning transmission electron microscopy (STEM) and electron energy-loss spectroscopy (EELS). In Figure 2 (top), we show a high-angle annular dark field (HAADF) cross-section image of a [5/9]16_{16} SL, observed along the [10]pc_{\mathrm{pc}} zone axis of STO (see Fig. S3 in for a broader view of the same region). The STEM-HAADF image confirms that the SL is epitaxially strained by the substrate. Although the interface between the substrate and the first layer is sharp, the close La and Pr atomic numbers (ZZ) obscure the interfaces between PVO and LVO layers in the HAADF image. In contrast, the EELS elemental maps from the same region reveal that these interfaces are atomically sharp, without cationic intermixing between the layers within our experimental resolution.

Figure 2. (top) HAADF-STEM image of the cross-section of a [5/9]16_{16} SL viewed along the [10]pc_{\mathrm{pc}} zone axis (top). Below, EELS compositional maps (Sr-L edges, La-M edges, and Pr-M edges) obtained from the simultaneously acquired HAADF-STEM image. (bottom) SL map together with the composition profile across the SL close to the STO interface.

This holds true throughout the SL thickness (see Fig. S4 in SI). Overall, the interfaces between the mm LVO and nn PVO layers are well defined when mm and nn are odd integers, meaning there is no significant intermixing of La and Pr cations between the layers. Together with the characteristic superstructure peaks observed in Figure 1(b), our chemical analysis further exemplifies the controlled design of the LVO/PVO SLs with sharp interfaces.

Engineering the magnetic phase transitions.

Figure 3 displays the results of the paramagnetic-to-antiferromagnetic phase transition, characterized using SQUID magnetometry (see Methods). In Figure 3(a), we show the temperature dependence of the magnetization for various SLs, alongside reference PVO and LVO thin films 3. The inset of Figure 3(a) displays the corresponding derivative (dM/dT) curves. By analyzing the high temperature onset in the magnetization curves and the local minimum in the derivatives, we identified three temperatures: TSO_{\mathrm{SO}}, T′SO_{\mathrm{SO}} and TS_{\mathrm{S}}. TSO_{\mathrm{SO}} and T′SO_{\mathrm{SO}}, albeit separated by ∼\sim20 K, follow the same trend and both are associated with the V3+^{3+} spin ordering. A single magnetic transition is thus observed at TSO_{\mathrm{SO}} for all SLs. At lower temperature, an additional magnetic transition occurs at TS_{\mathrm{S}}. In Figure 3(b), we show the composition dependence of these temperatures, expressed as a function of the LVO layer content (m×cLVO/Λm \times c_{\mathrm{LVO}}/\Lambda) within the SL motif. We see that the antiferromagnetic transition temperature scales with the composition, ranging between the reference PVO and LVO thin films. We point out that the same TSO_{\mathrm{SO}} is observed for the [5/5]22_{22} and [3/3]36_{36} superlattices (see Fig. S2 in SI), i.e. having the same relative concentration of LVO and PVO. In contrast, TS_{\mathrm{S}} remains at 20 K for all periodicities and compositions, except in the reference LVO thin film, where no corresponding transition is observed in the dM/dT curve. This feature is attributed to changes in the magnetic properties of the PVO layer, as further confirmed in the dM/dT curves [inset of the Figure 3(a)], where the local minimum at 20 K becomes more visible as the proportion of PVO increases in the SLs. As seen in PVO thin films using X-ray magnetic circular dichroism (XMCD), the magnetic properties of the Pr3+^{3+} sublattice can couple to the V3+^{3+} sublattice 4. A spin/orbital reordering at the V sites, from CSO_{\mathrm{SO}}/GOO_{\mathrm{OO}} to GSO_{\mathrm{SO}}/COO_{\mathrm{OO}}, induces a magnetic transition of the Pr 4f24f^{2} electron, which are polarized by the V3+^{3+} sublattice. Similar to TSO_{\mathrm{SO}}, the onset of this low-temperature Pr3+^{3+} magnetic transition is expected at higher temperature (∼\sim40 K) than the local minimum in the dM/dT curve, consistent with a remanent magnetic signal of Pr3+^{3+} observed by XMCD, which persists up to 40 K in PVO thin film 4.

Figure 3. (a) Temperature dependence of various [m/n]p[m/n]_{p} SLs (with the same color code as in 1) magnetization (dotted lines are guide for the eyes). The measurements were performed with an in-plane applied magnetic field of 50 Oe while heating up from 10 K to 300 K. Inset: corresponding dM/dT derivatives of the magnetization curves (lines are guide for the eyes). (b) Magnetic ordering temperature as a function of the LVO composition m×cLVO/Λm \times c_{\mathrm{LVO}}/\Lambda, representing the V3+^{3+} spin ordering and the Pr3+^{3+} magnetic transition (lines are guide for the eyes). Inset: TSOT_{\mathrm{SO}} versus mm (red) and nn (blue) for n=5n = 5 and m=5m = 5, respectively. The solid lines are guide for the eyes.

Our results demonstrate that the precise growth control of these heterostructures enables tuning the magnetic phase transitions, resulting in a unique paramagnetic-to-antiferromagnetic transition at TSO_{\mathrm{SO}}, despite alternating RVO3_{3} layers with distinct spin ordering temperatures in thin films (132 K for PVO and 150 K for LVO) 3. In the inset of Figure 3(b), we show TSOT_{\mathrm{SO}} either as a function of mm LVO layers (for n=5n = 5 PVO layers) or as a function of nn PVO layers (for m=5m = 5 LVO layers). As expected, TSOT_{\mathrm{SO}} increases with mm and decreases with nn. However, while the data points for n=5n = 5 align nearly perfectly along a straight line (red line), those for m=5m = 5 are exhibit greater scatter (blue line). The red case corresponds to a monotonous improvement in the lateral correlation as mm increases with n=5n = 5, as evidenced in RSMs in Figure 1(c)-(Figure 1g). On the contrary, the blue case corresponds to SLs, whose lateral correlation in RSMs is worse (see Fig. S5 in SI). This probably emphasizes the importance of the interfacial quality, where even a slight variation in cationic composition or disorder can destabilize the spin ordering, as observed in bulk doped RVO3_3 [22]. Nonetheless, we show here that the RVO3_3-based SL can be designed beyond simple solid solutions, forming a new layered system, where separated constituent materials exhibit a unique magnetic behavior from TSOT_{\mathrm{SO}}. As evidenced in PVO [23] and LVO [24] thin films, chemical and/or epitaxial strain engineering could provide additional parameters for further tuning the magnetic properties. This approach could also contribute to a deeper understanding of the interfacial mechanisms governing the coupling between the PVO and LVO layers.

Engineering the structural distortions.

Contrary to solid solutions, SLs have interfaces between the constituent materials, thereby introducing new degrees of freedom. Perovskite oxides with a PbmnP bmn orthorhombic structure, such as RVO3_3, are characterized by cooperative octahedral-site rotations around the ⟨100⟩pc\langle100\rangle_{\mathrm{pc}} axes. These tilts and rotations can be described using the Glazer notation [25] as the a−a−c+a^{-}a^{-}c^{+} tilting system. In these materials, such octahedral tilts result in a deviation of the V–O–V bond angle from the ideal 180∘180^\circ observed in a cubic structure. This deviation increases as the ionic radius of R3+^{3+} decreases, leading to a progressive reduction of the bond angle. The antipolar motion of R3+^{3+} (X5−X_{5}^{-}) and the out-of-phase (φx+φy=φxy\varphi_{x} + \varphi_{y} = \varphi_{xy}), in-phase (φz+\varphi_{z}^{+}) oxygen octahedra rotations are coupled [26, 27], as described by the trilinear energetic term φxyφz+X5−\varphi_{xy}\varphi_{z}^{+}X_{5}^{-}. Consequently, an increase in the oxygen octahedra rotation angle pushes R3+^{3+} away from its position in an ideal cubic symmetry, thereby enhancing the amplitude of the R3+^{3+} displacements.

To gain insights on the local atomic displacements, i.e. lattice distortions, we show in Figure 4 high-resolution STEM-HAADF images of the [5/9]16[5/9]_{16}, [5/5]22[5/5]_{22} and [9/5]16[9/5]_{16} SLs, in Figure 4(a), (d) and (g), respectively. Again, these images reveal a sharp film/substrate interface. The brighter pixels correspond to the La and Pr columns, and a numerical analysis of the STEM images allows us to map their atomic positions relative to an undistorted reference (see Methods and Ref. [18]). By highlighting the La3+^{3+} and Pr3+^{3+} displacements, we characterize the X5−X_{5}^{-} antipolar displacement mode, which manifests as vertical atomic displacement maps across the SLs, as shown in Figure 4(b), Figure 4(e) and Figure 4(h) for the [5/9]16[5/9]_{16}, [5/5]22[5/5]_{22}

Figure 4. STEM-HAADF images of a cross-section, viewed along the [10] zone axis direction of STO, for (a) [5/9]16_{16}, (d) [5/5]22_{22} and (g) [9/5]16_{16} SLs. The STO/LVO interface is indicated by a solid white line. Corresponding vertical R-displacement maps displayed in (b), (e) and (h), respectively. Corresponding quantified R-displacement amplitude along the growth direction displayed in (c), (f) and (i), respectively. The lines are guide for the eyes and the error bars represent the standard deviation of the Sr-displacements in STO.

and [9/5]16[9/5]_{16} superlattices, respectively. The X5−X_{5}^{-} mode is projected along the growth direction, parallel to the [110]o[110]_{\mathrm{o}} direction, while the in-phase oxygen octahedra rotation, parallel to the [001]o[001]_{\mathrm{o}} direction, lies within the substrate plane. The resulting tilt pattern can be described as a−b+c−a^{-}b^{+}c^{-} or a+b−c−a^{+}b^{-}c^{-}.

These distortions double the periodicity along the long orthorhombic direction, as evidence by half-order Bragg reflection measured via XRD (see Fig. S6 in SI). The measured intensities of the (0121)pc(0\frac{1}{2}1)_{\mathrm{pc}} and (1201)pc(\frac{1}{2}01)_{\mathrm{pc}} peaks indicate that the long orthorhombic axis aligns along the (100)pc(100)_{\mathrm{pc}} or (010)pc(010)_{\mathrm{pc}} substrate direction, with equal proportion. A minor fraction of the SL exhibits a long orthorhombic axis parallel to the growth direction, as revealed by the (1012)pc(10\frac{1}{2})_{\mathrm{pc}} peak. This fraction, with [001]o[001]_{\mathrm{o}} parallel to the growth direction, seems to depend on both

the relative LVO and PVO composition in the supercell and the number of repetitions within the SLs. The alternate stacking of mm LVO and nn PVO layers is likely introducing interfacial strain (±0.6%\pm0.6\%) between the mismatched layers, whose role needs further investigation. We assume in the following that the SLs are primarily (110)o(110)_{\mathrm{o}}-oriented, with the [001]o[001]_{\mathrm{o}} lying in the substrate plane.

At the local scale, we extracted the distance between two cations from the displacement maps in Figure 4(b), (e) and (h) and quantified the R-displacement along the growth direction in Figure 4(c), (f) and (i). The SLs exhibit a clear modulation of the R3+\mathrm{R}^{3+} displacements, with amplitudes corresponding to the alternation of the LVO and PVO layers. Specifically, the cation displacements gives around 35 pm for La3+\mathrm{La}^{3+} and 48 pm for Pr3+\mathrm{Pr}^{3+} in the [5/5]22_{22} and [9/5]16_{16} SLs [see Figure 4(f) and (i)] but only around 15 pm for La3+\mathrm{La}^{3+} and 27 pm for Pr3+\mathrm{Pr}^{3+} for the [5/9]16_{16} SL [see Figure 4(c)]. This discrepancy and the lower R-displacements found in LVO (30 pm) and PVO (36 pm) thin films [18] may indicate that interfacial quality and strain are critical. The quantified line profile shows that the interfacial coupling length scale is around 4 unit cells between the LVO and PVO layers (i.e. 2 unit cells in each layer side). Conversely, the amplitude of the La3+\mathrm{La}^{3+} displacement is almost suppressed in the vicinity of the substrate interface but increases over 6-8 unit cells into the first LVO layer. This behavior is in agreement with the interfacial coupling length scale in the vicinity of the substrate in LVO/STO heterostructures grown by MBE [18, 28]. With regards to structural distortions, there are two length scales depending on whether the vanadate layer is juxtaposed with a compound having the same tilt pattern (a−a−c+a^{-}a^{-}c^{+}) or with another one having a different tilt pattern (a0a0a0a^{0}a^{0}a^{0}). This raises the question of why only a single TSO_{\mathrm{SO}} is observed for each superlattice. The phase diagram of the spin ordering temperature for bulk Pr1−x_{1-x}Lax_{x}VO3_{3} shows that TSO_{\mathrm{SO}} changes continuously from Pr to La [29]. However, we can exclude any chemical origin as the intermixing region is less than 1 unit cell wide in our superlattice. Still, the spin ordering temperature TSO_{\mathrm{SO}} decreases when increasing the orthorhombic lattice distortions in RVO3_{3}. Hence, the interfacial structural coupling could propagate between the PVO and LVO layers but given the coupling length-scale between them (2 unit cells) we should see two magnetic transition temperatures for Λ>4\Lambda> 4. On the contrary, we see a single temperature (TSO_{\mathrm{SO}}) for the entire series. A third possibility could be that the coupling mechanism between layers is determined neither by chemistry nor by interfacial distortions but rather by an energy balance at the interface between a paramagnetic and an antiferromagnetic phase. As demonstrated for the metal-to-insulator transition in (SmNiO3_{3})m_{m}/(NdNiO3_{3})n_{n} superlattices, this would allow larger coupling length-scales [30].

Going from LVO to PVO induces changes in the oxygen octahedra rotations (V–O–V bond angles), which increase in PVO and decrease in LVO owing to the different ionic radii of La3+^{3+} and Pr3+^{3+}. Consequently, the amplitude of the X5−X^{-}_{5} antipolar displacement is smaller in the LVO layers than in the PVO layers, in excellent agreement with our observations. These results provide an indirect path to visualizing the amplitude of the in-phase oxygen octahedra rotation. In order to investigate the coupling between the rotational mode of the oxygen atoms and the shift mode of the rare earth atoms, we have analyzed the RR–O chemical bonds and hybridization at the atomic scale. We carried out STEM-EELS experiments to characterize the layer-resolved electronic states across the SLs. In Figure 5(a), we present the STEM cross section image of a [9/5]16\left[9/5\right]_{16} SL. In Figure 5(b), we show a 2D intensity plot of the EEL spectra recorded at the V-L2,3L_{2,3} and O-K edges (horizontal axis), measured throughout the SL (vertical axis). In Figure 5(c), we display the averaged spectra along the vertical axis of Figure 5(b). Overall, the fine structures at the V-L2,3L_{2,3} are consistent with the V3+^{3+} valence state. The features observed at the O-K edge correspond to the electronic excitations from the O 1ss core level to the O 2pp empty states, which hybridize with the empty orbital states of the cations, making them sensitive to the surrounding environment. The broad peak around 547.5 eV and the peaks around

Figure 5. (a) STEM-HAADF image, simultaneously recorded with spectral data, of a cross-section of a [9/5]16\left[9/5\right]_{16} SL viewed along the [10] zone axis of STO. (b) 2D intensity plot of the EEL spectra recorded at the V-L2,3L_{2,3} and O-K edges (horizontal axis), measured throughout the SL (vertical axis) region in (a). Modulation of the RR 5dd – O 2pp peak energy position is represented by a horizontal arrows and black line fit of the peak position (see text). (c) Averaged spectra along the vertical axis in (b). (d) and (e) Peak energy (left axis) of the RR 5dd – O 2pp hybridized orbitals along the growth direction of a [9/5]16\left[9/5\right]_{16} SL and a [5/5]22\left[5/5\right]_{22} SL, respectively. The corresponding mean RR-displacements profiled of Figure 4 are also displayed for comparison (right axis). The lines are guide for the eyes.

537 eV correspond to the V 4spsp and RR (La or Pr) 5dd hybridized orbitals, respectively. The peaks around 533 eV and 534 eV arise from the O 2pp overlap with the crystal-field-split V 3dd t2gt_{2g} and ege_g orbitals, respectively. To probe the structural coupling between the oxygen atoms and the rare earths, we focused on the RR 5dd peak. We determined its energy position across the LVO and PVO layers by fitting the peak to a Gaussian profile in the layer-resolved EEL spectra. We display, in Figure 5(d) and (e), the O 2pp – RR 5dd hybridized peak position profiles as a function of the distance from the interface for the [9/5]16\left[9/5\right]_{16} and [5/5]22\left[5/5\right]_{22} SLs, respectively. We point out that we excluded energy instabilities or offsets by determining the position of the rather narrow V-L3L_{3} edge peak and larger O 2pp – V 4spsp hybridized peak, which display no significant variation within our experimental accuracy (remaining at 516.34 ±\pm0.02 eV and 543.50 ±\pm0.1 eV, respectively). In contrast, we observed that the RR 5dd peak shifts to lower (higher) energy in the PVO (LVO) layer within the SLs. Remarkably, this modulated spectral shift follows the period alternation of the LVO and PVO layers as it is also represented in Figure 5(b). Additional results obtained from another dataset for each SL show the same trends (see Fig. S7 in SI). These shifts arise from changes in the O 2p2p − R 5d5d hybridization, driven by the variations of the oxygen octahedra rotation amplitude between the two different layers. Indeed, the structural distortions modify the cuboctahedral environment surrounding the R3+^{3+} cation, changing the electron transfer integral between neighboring atoms, as observed using X-ray absorption at the O-K edge [21, 31]. Consequently, Pr3+^{3+} 5d5d electrons have a lower energy than the La3+^{3+} 5d5d electrons since the O 2p2p − R 5d5d overlap is reduced due to the octahedra rotational distortion, resulting in less repulsion for Pr3+^{3+} electrons from the oxygen orbitals than for La3+^{3+} electrons. In Figure 5(d) and (e), we show also the corresponding R-displacement profile, both following the periodic alternation of the LVO and PVO layers [the fit in Figure 5(d) is reproduced in the 2D intensity plot in Figure 5(b)]. This provide a direct evidence of the correspondence between the oxygen octahedral rotation and the R3+^{3+} shift.

The coupling between the two distortion modes is further demonstrated when looking at the vicinity of the STO/LVO interface, where the corner-sharing octahedra of both must maintain their connectivity [32]. However, STO and LVO have different tilt patterns. An interfacial effect confined within few unit cells shall accommodate the a0a0a0a^{0}a^{0}a^{0} in STO tilt system and the a−b+c−a^{-}b^{+}c^{-} (or a+b−c−a^{+}b^{-}c^{-}) tilt system in LVO (considering the [110]o[110]_{o} growth direction [28]). Consequently, the in-plane oxygen octahedra rotations in LVO are initially quenched (a0a0c−a^{0}a^{0}c^{-}) due to the absence of rotation in STO. Moving away from the interface, the influence of the substrate decays, thereby releasing the rotations in the first LaVO3_3 layer, which then adopts the a−b+c−a^{-}b^{+}c^{-} (or a+b−c−a^{+}b^{-}c^{-}) tilt system. In the quenched interfacial LVO region, the La3+^{3+} cations experience more repulsion from the oxygen orbitals. This likely corresponds to the higher energy of O 2p2p − La 5d5d hybridized peak near the substrate in Figure 5(d) and (e). As the oxygen octahedra rotations are released in LVO, the peak shifts towards lower energy within 5-6 unit cells for [9/5]16_{16} SL, where the O 2p2p − La 5d5d peak energy matches the local maximum of the La-displacement. For [5/5]22_{22} SL, the periodicity is too narrow and the energy position of the peak decreases from the STO/LVO interface down to the first PVO layer. Moreover, the in-phase and out-of-phase oxygen octahedra rotations and R-site displacements are coupled through a trilinear coupling term. Consequently, the X5−X_{5}^{-} shift mode should be suppressed near the STO/LVO interface due to the absence of in-phase rotations and should gradually stabilize as the in-phase rotations are released. This behavior is indeed observed in Figure 4(c), (f) and (i) and in Figure 5(d), (e), providing an important cross-check for the internal consistency of our analysis. These results show that the oxygen octahedra connectivity, between the first LVO layer and the STO substrate, and subsequently between the LVO and PVO layers within the SLs, promotes modulation of the oxygen octahedra rotation angles. Interfacial engineering thus enables the control of the octahedral tilts and rotations

within few unit cells, which in turn allows for the tuning of the properties of transition metal oxide thin films [33]. The modulation of the R-displacement occurs over a coupling length scale of 5-6 unit cells within LVO close to STO and within 4 unit cells between LVO and PVO layers. Designing superlattices with mm and nn being even might be helpful in clarifying the behavior of interfacial structural coupling as superlattices with larger Λ\Lambda might stimulate further studies regarding the energetic cost of magnetic interfaces in vanadates, analogous to the electronic interface in nickelates [30]. We emphasize that the growth along the [110]o[110]_{o} direction is not the ideal orientation to expect improper hybrid ferroelectricity, since X5−X_{5}^{-} is an antipolar distortion mode. Hence, any built-in electrical polarization should be cancelled out within a single unit cell or monolayer of the [110]o[110]_{o}-oriented SL. Nevertheless, given the R-displacement gradient and the gradual release of the oxygen octahedra rotations, we speculate whether a possible flexoelectric response [34] could induce unbalanced electric dipoles. Furthermore, the distribution of the positive (cations) and the negative (oxygen) charges could also be influenced by the deformation of the oxygen octahedra [35, 36] including the cooperative Jahn-Teller distortions. Besides potential polar instabilities, the modulated response of the layered heterostructure to the oxygen octahedra connectivity mismatch could also affect the spin-orbital phase diagram of the V3+^{3+} t2gt_{2g} electrons [16], and modify the magnetic properties through interface engineering near STO and/or between the LVO and PVO layers.

Conclusion

We have shown how the precise control over layer-by-layer growth of (LaVO3_3)m_m/(PrVO3_3)n_n superlattices by MBE enables tuning interface-driven structural distortions. The designed alternate stackings of LaVO3_3 and PrVO3_3 exhibit a unique antiferromagnetic transition temperature (TSO_{\mathrm{SO}}), tunable by adjusting the relative proportions of LaVO3_3 and PrVO3_3, despite the distinct spin ordering temperatures of the constituent materials in epitaxial thin films. Layer-resolved spectroscopic measurements show that the hybridization of La/Pr 5d5d orbitals with O 2p2p orbitals is modulated and directly correlated to the oxygen octahedra rotations and R-displacements, illustrating the trilinear coupling between antiferrodistortive and antipolar distortions. Notably, the interfacial oxygen octahedra connectivity between the cubic SrTiO3_3 substrate and the vanadate layers influences significantly the structural distortions with possible consequences on the positive and negative charge distribution. Besides these potential polar instabilities, the modulated response of the layered heterostructure to the oxygen octahedra connectivity mismatch could also affect the spin-orbital phase diagram of RVO3_3 based systems. Our study illustrates how artificial superlattices are a precise and relevant approach to engineer structural distortions and octahedral modulations at the atomic scale, offering a pathway to tune the magnetic properties and inspiring routes to promote possible polar instabilities through strain-distortion relationships in perovskite oxide. Recently, some works have shown that [1]o_{\mathrm{o}}-oriented films [37, 38] and layered structures [39] can be synthesized, thereby revitalizing the design of artificial superlattices as a compelling strategy for realizing novel multiferroic materials.

Methods

Thin film growth. The superlattices have been grown in a molecular beam epitaxy (MBE) chamber with a base pressure of 6×10−116 \times10^{-11} mbar. The atoms are evaporated on a (001)-oriented SrTiO3_3 substrate using high temperature Knudsen cells, whose atomic fluxes are calibrated using a quartz crystal microbalance before and after the deposition. The Pr, La and V atomic fluxes were fixed to 1.5×10131.5 \times10^{13} atom.cm−2^{-2}.s−1^{-1} with 5% accuracy. The growth conditions were optimized beforehand so that high-quality single-phase films could be obtained [18]. To get the proper oxygen stoichiometry, an oxidant gas (O3_3+O2_2) was introduced at a pressure fixed in the 55-7×10−77 \times10^{-7} mbar range in the chamber. During the growth, the substrate temperature was kept at 850°C. The film growth was monitored using in situ reflection high-energy electron diffraction (RHEED).

X-ray photoelectron spectroscopy. The X-ray photoelectron spectra were measured in situ using the non-monochromatized Al Kα1_1 radiation at 1486.6 eV. The photoelectrons were collected by an Omicron EA 125 hemispherical analyzer with an overall resolution of about 1 eV. The spectra were taken in normal emission geometry. The XPS and MBE chambers are connected by a high-vacuum transfer tube that prevents any surface contamination from the air.

X-ray diffraction. The crystallinity and the structure were characterized by X-ray diffraction (XRD) with a PANalytical X’pert Pro MRD diffractometer using monochromatic Cu Kα1_1 radiation (λ = 1.54056 Å). Half-Bragg’s peaks were measured in skew diffraction geometry.

Magnetic characterization. The magnetization measurements were performed using a Quantum Design SQUID magnetometer (MPMS3). They are carried out with an in-plane applied magnetic field of 50 Oe, after cooling down from room temperature with a field of 5000 Oe. The diamagnetic substrate contribution is corrected to the raw magnetization curve.

Scanning transmission electron microscopy. The atomically resolved microstructure was determined by cross-sectional high angle annular dark field (HAADF) scanning transmission electron microscopy (STEM). The cross-section lamella were prepared by focus ion beam with Ga+^{+} ion milling (FEI-Helios Nanolab 600i) and observed with a JEOL JEM-ARM 200F Cold FEG TEM/STEM operating at 200 kV and equipped with a spherical aberration (Cs) probe and image correctors. The pixel intensity analysis of the single-frame STEM-HAADF images consists in the determination of the nodes of a grid, each node corresponds to an atom. The distances to the first neighbors are then calculated yielding to the local average positions of the neighboring atom. These distances between neighboring R cations are converted to picometer (pm) using the STO substrate grid as a reference atoms. The out-of-plane local average positions of the neighboring atoms are thus calculated and yield out-of-plane displacements [18].

Electron Energy-Loss Spectroscopy. For elemental maps at atomic resolution, electron energy-loss spectroscopy (EELS) experiments at IJL were performed in STEM mode at 200 kV, using a Quantum ER Gatan 965 Energy filter coupled with ADF/BF detectors, and a Gatan USC1000 camera. The dataset shown in Figure 2 was acquired in an area of 2.17×202.17 \times20 nm2^{2}, with a step of 0.11 nm (20×18420 \times184 pixels2^{2}), a dwell time of 0.1 s/pixel. The convergence and collection angles were 20.4 and 52 mrad, respectively. For near-edge fine structure analysis, EELS experiments were performed at SuperSTEM using a NION HERMES 100MC, equipped with a NION ground-potential monochromator, a C5_5 NION QO corrector, and a GATAN Enfinium ER spectrometer. The experiments were performed at 60 kV, with the monochromator turned on (energy resolution of 160 meV) or off (energy resolution of 300 meV), and at a dispersion of 0.05-0.1 eV/channel, a dwell time of 0.05-0.1s/channel. The effect of the monochromator was found to be negligible on the V-L2,3_{2,3} and O-K ELNES, and the spectra shown in the article were acquired with a native energy resolution of 300 meV. For each EELS spectrum, the background before the V-L2,3_{2,3} edges was subtracted by a power-law fit and then the spectrum was normalized after the O-K edge (at 580 eV). The dataset shown in Figure 5 was acquired in an area of 2.6×13.16252.6 \times13.1625 nm2^{2}, with a step of 0.08125 nm (32×16232 \times162 pixels2^{2}), with 16×1616 \times16 sub-pixel scanning for the HAADF image. As an example, the position of the O 2p−2p - R 5d5d hybridization peak was determined by fitting each spectrum in the SI (corresponding to the 2D intensity plot in Figure 5) using a Gaussian function, with the energy of the O-K edge of STO as an absolute reference.

Acknowledgments

The authors thank I. C. Infante and S. Andrieu for fruitful discussions. This work is supported by the Région Grand Est projects RHUM (AAP-013-075) and DECOX (23-JC-004), the France 2030 government investment plan under the ANR grant PEPR SPIN - SPINMAT (ANR-22-EXSP-0007), and the ANR project CITRON (ANR-21-CE09-0032). The work has benefited of the resources of experimental platforms at IJL: the Tube Davm, 3M (funded by FEDER EU, ANR, Région Grand Est, and Métropole Grand Nancy), and XGamma, all supported by the LUE-N4S project, part of the French PIA project Lorraine Université d’Excellence (ANR-15IDEX-04-LUE), and by FEDER-FSE Lorraine et Massif Vosges 2014-2020, an EU program. M. B. is grateful for support from a visiting associate professorship from the School of Chemical and Process Engineering at the University of Leeds. SuperSTEM is the National Research Facility for Advanced Electron Microscopy, supported by the Engineering and Physical Sciences Research Council under award EP/W021080/1.

Supplementary Information

RHEED patterns and RHEED intensity oscillations recorded during the deposition of a [7/5]18[7/5]_{18} superlattice. XPS spectra of the rare earths 3d3/23d_{3/2} and 3d5/23d_{5/2} core-level states for various [m/n]p[m/n]_p superlattices. High-resolution XRD 2θ−ω2\theta-\omega measurements performed on all [m/n]p[m/n]_p superlattices mentioned in this study, close to the (002) STO Bragg peak. Magnetic results for the [3/3]36[3/3]_{36} superlattice. HAADF cross-section image showing the spectrum image region from which the EELS elemental maps in Figure 2 were taken from. Larger scale HAADF cross-section image and spectrum image region with EELS elemental maps. RSMs around the asymmetrical (103)pc_{pc} Bragg peak of different [5/n]p[5/n]_p superlattices. 2θ2\theta-scans of (1201)pc(\frac{1}{2}01)_{pc}, (0121)pc(0\frac{1}{2}1)_{pc} and (1012)pc(10\frac{1}{2})_{pc} Bragg reflections for [m/5]p[m/5]_p and [5/n]p[5/n]_p superlattices. Results of the determination of the O 2p2p − R 5d5d hybridized peak position for the [9/5]16[9/5]_{16} and [5/5]22[5/5]_{22} with additional datasets.

References

  1. [1]V. Baltz, A. Manchon, M. Tsoi, T. Moriyama, T. Ono, and Y. Tserkovnyak, Rev. Mod. Phys. 90, 015005 (2018).
  2. [2]P. Wadley, B. Howells, J. Železný, C. Andrews, V. Hills, R. P. Campion, V. Novák, K. Olejník, F. Maccherozzi, S. S. Dhesi, S. Y. Martin, T. Wagner, J. Wunderlich, F. Freimuth, Y. Mokrousov, J. Kuneš, J. S. Chauhan, M. J. Grzybowski, A. W. Rushforth, K. W. Edmonds, B. L. Gallagher, and T. Jungwirth, Science 351, 587 (2016).
  3. [3]A. V. Kimel, A. Kirilyuk, A. Tsvekov, R. V. Pisarev, and Th. Rasing, Nature 429, 850 (2004).
  4. [4]R. Lebrun, A. Ross, S. A. Bender, A. Qaiumzadeh, L. Bald­rati, J. Cramer, A. Brataas, R. A. Duine, and M. Kläui, Nature 561, 222 (2018).
  5. [5]T. Higo, H. Man, D. B. Gopman, L. Wu, T. Koretsune, O. M. J. van’t Erve, Y. P. Kabanov, D. Rees, Y. Li, M.-T. Suzuki, S. Patankar, M. Ikhlas, C. L. Chien, R. Arita, R. D. Shull, J. Orenstein, and S. Nakatsuji, Nat. Photon. 12, 73 (2018).
  6. [6]F. Nolting, A. Scholl, J. Stöhr, J. W. Seo, J. Fompeyrine, H. Siegwart, J.-P. Locquet, S. Anders, J. Lüning, E. E. Fullerton, M. F. Toney, M. R. Scheinfeink, and H. A. Padmore, Nature 415, 767 (2000).
  7. [7]H. Yan, Z. Feng, P. Qin, X. Zhou, H. Guo, X. Wang, H. Chen, X. Zhang, H. Wu, C. Jiang, and Z. Liu, Adv. Mater. 32, 1905603 (2020).
  8. [8]M. Imada, A. Fujimori, and Y. Tokura, Rev. Mod. Phys. 70, 1039 (1998).
  9. [9]Y. Tokura, and N. Nagaosa, Science 288, 462 (2000).
  10. [10]T. Kimura, T. Goto, H. Shintani, K. Ishizaka, T. Arima, and Y. Tokura, Nature 426, 55 (2003).
  11. [11]N. A. Benedek, A. T. Mulder, and C. J. Fennie, Phys. Rev. Lett. 105, 11 (2012).
  12. [12]N. A. Benedek and C. J. Fennie, J. Solid State Chem. 106, 107204 (2011).
  13. [13]J. M. Rondinelli and C. J. Fennie, Adv. Mater. 24, 1961 (2012).
  14. [14]J. Varignon, N. C. Bristowe, E. Bousquet, Ph. Ghosez, Sci. Rep. 5, 15364 (2015).
  15. [15]K. I. Kügel, D. I. Khomskii, Zh. Eksp. Teor. Fiz 64, 1429 (1973).
  16. [16]S. Miyasaka, Y. Okimoto, M. Iwama, and Y. Tokura, Phys. Rev. B 68, 100406(R) (2003).
  17. [17]M.H. Sage, G. R. Blake, C. Marquina, and T. T. M. Palstra, Phys. Rev. B 76, 195102 (2007).
  18. [18]G. Masset, O. Copie, J. Ghanbaja, K. Dumesnil, L. Pasquier, D. Pierre, and S. Andrieu, Phys. Rev. Materials 4, 064417 (2020).
  19. [19]E. E. Fullerton, I. K Schuller, H. Vanderstraeten, and Y. Bruynseraede, Phys. Rev. B 45, 9292 (1992).
  20. [20]S. Andrieu, F. Lahratra Razafindramisa, E. Snoek, H. Revenier, A. Barbara, J.-M. Tonnerre, M. Brunel, and M. Piecuch, Phys. Rev. B 52, 9938 (1995).
  21. [21]O. Copie, J. Varignon, I. Cañero Infante, M. Martirosyan, F. Choueikani, P. Ohresser, P.-E. Janolin, A. Pautrat, A. David, Ph. Ghosez, and W. Prellier, Phys. Rev. Mater. 9, 064409 (2025).
  22. [22]J. Fujioka, S. Miyasaka, and Y. Tokura, Phys. Rev. B 72, 024460 (2005).
  23. [23]O. Copie, J. Varignon, H. Rotella, G. Steciuk, Ph. Boulay, A. Pautrat, A. David, B. Mercey, Ph. Ghosez, and W. Prellier, Adv. Mater. 29, 1604112 (2017).
  24. [24]D. Kumar, A. David, A. Fouchet, A. Pautrat, J. Varignon, C. U. Jung, U. Lüders, B. Domengès, O. Copie, Ph. Ghosez, and W. Prellier, Phys. Rev. B 99, 224405 (2019).
  25. [25]A.M. Glazer, Acta Crystallograph. B28, 3384 (1972).
  26. [26]T. Mizokawa, D. I. Khomskii, and G. A. Sawatzky, Phys. Rev. B 60, 7309 (1999).
  27. [27]S. Amisi, E. Bousquet, K. Katcho, and P. Ghosez, Phys. Rev. B 85, 064112 (2012).
  28. [28]M. Martirosyan, S. Passuti, G. Masset, J. Varignon, H. Chintakindi, J. Ghanbaja, S. Migot, E. Delacote, A. Benedit-Cárdenas, L. Pasquier, K. Dumesnil, L. Palatinus, W. Prellier, A. David, Ph. Boullay, and O. Copie, Small 43, e02538 (2025).
  29. [29]J. Fujioka, T. Yasue, S. Miyasaka, Y. Yamasaki, T. Arima, H. Sagayama, T. Inami, K. Ishii, and Y. Tokura, Phys. Rev. B 82, 144425 (2010).
  30. [30]C. Domínguez, A. B. Georgescu, M. Mundet, Y. Zhang, J. Fowlie, A. Mercy, A. Waelchli, S. Catalano, D. T. L. Alexander, P. Ghosez, A. Georges, A. J. Millis, M. Gib- ert, and J.-M. Triscone, Nat. Mater. 19, 1182 (2020).
  31. [31]S. Cao, X. Zhang, T. R. Paudel, K. Sinha, X. Wang, X. Jiang, W. Wang, S. Brutsche, J. Wang, P. J. Ryan, J.-W. Kim, X. Cheng, E. Y. Tsymbal, P. A. Dowben, and X. Xu, J. Phys.: Condens. Matter 28, 156001 (2016).
  32. [32]J. M. Rondinelli, S. J. May, and J. W. Freeland MRS Bulletin 37, 261 (2012).
  33. [33]D. Kan, R. Aso, R. Sato, M. Haruta, H. Kurata, and Y. Shimakawa, Nat. Mater. 15, 432 (2016).
  34. [34]P. Zubko, G. Catalan, and A. K. Tagantsev, Annu. Rev. Mater. Res. 43, 387 (2013).
  35. [35]J.-S. Zhou, and J. B. Goodenough, Phys. Rev. Lett. 94, 065501 (2005).
  36. [36]J.-S. Zhou, and J. B. Goodenough, Phys. Rev. Lett. 77, 132104 (2008).
  37. [37]P. Radhakrishnan, K. S. Rabinovich, A. V. Boris, K. Fürsich, M. Minola, G. Christiani, G. Logvenov, B. Keimer, and E. Benckiser, Nat. Phys. 21, 126 (2025).
  38. [38]D.T.L. Alexander, H. Meley, M. M. Schmitt, B. Mundet, Ph. Ghosez, J.-M. Triscone, and S. Gargiulo, ACS Nano 19, 10126 (2025).
  39. [39]J. Spring, N. S. Fedorova, A. Vogel, J. Herrero-Martín, E. Stylianidis, P. Zubko, J. Íñiguez-González, M. D. Rossell, M. Gibert, Adv. Mater. 38, e13458 (2026).

Paper details

vlnc:W_hnx4gdc3
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents