Physical properties of RhGe and CoGe single crystals synthesized under high pressure

Abstract

Chiral topological semimetals hosting multifold fermions and exotic surface states represent a frontier in topological materials research. Among them, noncentrosymmetric cubic B20 compounds-notably transition-metal silicides and germanides-offer a unique platform for realizing symmetry-protected topological phases and unconventional optoelectronic responses. Here, we report the physical properties of RhGe and CoGe single crystals with B20 structure in detail. Transport measurements reveal metallic behavior with characteristic Fermi-liquid scaling at low temperatures, while magnetization results confirm paramagnetism in both compounds. In addition, both of materials exhibit low carrier concentrations with small electronic specific heat coefficient, indicating their semimetal feature with weak electronic correlations. Such high-quality CoGe and RhGe single crystals provide a material platform to explore the evolution of multifold fermions and the instability of helicoid-arc surface states with spin-orbit coupling and surface environment in B20 material systems.

Introduction

The existence of nontrivial band topology generates exotic quantum phenomena in condensed matter physics, establishing topological materials as a major research frontier since the discovery of topological insulators and semimetals [1, 2, 3]. Fundamental fermionic particles predicted in high-energy physics—including Dirac, Weyl, and Majorana fermions—emerge as low-energy quasiparticle excitations within these materials. Dirac semimetals host four-fold degenerate nodes exhibiting linear dispersion in all momentum directions, protected by combined inversion, time-reversal, and lattice symmetries [4, 5, 6, 7]. Breaking either inversion or time-reversal symmetry splits Dirac nodes into Weyl points (characterized by a Chern number ∣C∣=1|C| = 1), generating distinctive Fermi arc surface states [8, 9, 10, 11]. Chirality, degeneracy, and dimensionality further define diverse topological phases [12, 13, 14], while non-symmorphic symmetries enforce high-symmetry-point band crossings that produce higher-fold fermions. Recent advances reveal massless fermions beyond standard model analogues—such as spin-1 chiral fermions, double Weyl fermions, and spin-3/2 Rarita-Schwinger-Weyl (RSW) fermions—characterized by higher quantized Chern numbers [15, 16, 17, 18, 19, 20, 21, 22].

Transition metal monosilicides and monogermanides crystallizing in the cubic noncentrosymmetric B20 structure (space group P213P2_{1}3, No. 198) exhibit a rich spectrum of magnetic, topological, and transport properties [15, 16, 17, 18, 19, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40]. The inherent structural chirality in these materials dictates both electronic and magnetic behaviors, leading to some unusual phenomena in real and reciprocal spaces. On the one hand, structural chirality induces a finite spin-orbit-driven Dzyaloshinskii-Moriya interaction, which competes with the Heisenberg exchange coupling. This competition underpins unusual magnetic properties, including the observation of skyrmion phases in compounds such as MnSi, FeGe, MnGe, and solid solutions like Fe1−xCoxSi\mathrm{Fe}_{1-x}\mathrm{Co}_{x}\mathrm{Si} and Fe1−xMnxSi\mathrm{Fe}_{1-x}\mathrm{Mn}_{x}\mathrm{Si} [24, 25]. On the other hand, in nonmagnetic B20 systems, structural chirality enables chiral topological semimetal states. These states host non-symmorphic symmetry-protected multifold fermions at high-symmetry points [22, 26, 27, 28]. For example, when neglecting spin-orbit coupling (SOC), the band structures of CoSi exhibit a threefold degenerate crossing (spin-1 fermion) at the Γ\Gamma point and a four-fold degenerate crossing (double Weyl fermion) at the RR point, carrying chiral charges of +2+2 and −2-2, respectively [22, 26, 27, 28]. Such unconventional quasiparticles can give rise to novel optoelectronic responses, such as the circular photogalvanic effect [16, 29]. The surface states of CoSi and RhSi also demonstrate long Fermi arcs but they possess two different types of helicoid arc van Hove singularities [30, 31], indicating the diversity of surface states (SSs) due to distinct chemical environments of the surface and SOC. Furthermore, theoretical studies have recently substantiated the potential for topological superconductivity in B20-structured RhGe [32].

Despite their intriguing topological properties, the studies on B20 RhGe and CoGe, which are isoelectronic to RhSi and CoSi, remain scarce and controversial due to the significant challenges associated with their single-crystal synthesis, which necessitates high-pressure and high-temperature conditions [33, 34, 35, 36]. Previous study of RhGe polycrystal suggested there is a coexistence of weak itinerant ferromagnetism (TC∼140T_C \sim140 K) and superconductivity (Tc∼4.3T_c \sim4.3 K) in this material [35], but our preliminary experimental results on RhGe single crystals indicate that both behaviors are absent [37]. In contrast, CoGe exhibits a Pauli paramagnetism [38, 39]. In this work, we study the physical properties of CoGe and RhGe single crystals grown by using high-pressure and high-temperature method. Both materials exhibit paramagnetic metallic behaviors with low concentrations of electron-type charge carriers.

Methods

Single crystals of RhGe and CoGe were grown under high pressure in a cubic anvil apparatus. High-purity elemental precursors (Rh: 99.99 %, Co: 99.95 % and Ge: 99.99 %) were homogenized by grinding with stoichiometric ratios of Rh : Ge = 1 : 1.2 (excess Ge serving as solvent flux) and Co : Ge = 1 : 1, respectively, sealed in hBN capsules (Au and Pt capsules were avoided because they can react with Ge under high temperature and high pressure). They were then positioned at the center of the high-pressure cell and compressed to 5 GPa. For RhGe (CoGe), the temperature was ramped to 1250 °C (1100 °C) at 10 °C/min, maintained for 3 h (2 h), slowly cooled to 800 °C (700 °C), and finally quenched to ambient temperature prior to decompression.

The powder X-ray diffraction (PXRD) patterns of crushed RhGe and CoGe crystals were performed using a high-resolution diffractometer (Bruker D8) using Cu Kα_\alpha radiation (λ=1.5406\lambda= 1.5406 Å) at room temperature. The single-crystal orientations of the RhGe and CoGe were determined using a Laue in backscattering mode (SmartLab, Rigaku). Scanning electron microscopy (SEM) imaging and energy-dispersive X-ray (EDX) spectroscopy for chemical composition analysis were performed using a JEOL JSM-7000F field-emission scanning electron microscope. Electrical transport measurements were conducted using a superconducting magnetic system (Cryomagnetics, C-Mag Vari-9). Magnetization and heat capacity measurements were performed using a Quantum Design magnetic property measurement system (MPMS3) and physical property measurement system (PPMS-14T), respectively.

Results and Discussions

The RhGe and CoGe compounds crystallize in the non-centrosymmetric cubic chiral B20 structure (space group P213P2_{1}3, No. 198) [23, 33, 34, 35, 39], isostructural to CoSi [26, 27, 28]. This non-symmorphic chiral framework features a distorted rocksalt-type arrangement with atomic displacements along the [111] direction (Figure 1(a)). Figure 1(b) and Figure 1(c) displays the PXRD patterns for both compounds measured at room temperature and ambient pressure, accompanied by Rietveld refinement profiles, confirming the phase-pure B20 structures. The refinement parameters (RwR=7.504R_{wR} = 7.504 % for RhGe and 1.046 % for CoGe) demonstrate high model reliability. The fitted aa-axial lattice parameter is 0.4859(2) nm and 0.4640(1) nm for RhGe and CoGe, respectively, which are in agreement with the reported values in literature for polycrystalline samples [33, 35, 38, 39, 40]. The larger lattice constant of RhGe than that of CoGe can be ascribed to the larger ionic radius of Rh than Co. The B20 structure contains 8 atoms per unit cell with Rh/Co and Ge occupying Wyckoff positions 4a at fractional coordinates: (u,u,u)(u, u, u), (u+0.5,0.5−u,−u)(u + 0.5, 0.5 - u, -u), (u,0.5+u,0.5−u)(u, 0.5 + u, 0.5 - u), and (0.5−u,u,0.5+u)(0.5 - u, u, 0.5 + u). The refined positional parameter uu is 0.1086(2) for Rh and 0.9023(4) for Ge in RhGe, while CoGe shows u=0.135(4)u = 0.135(4) for Co and 0.837(2) for Ge. EDX analysis determined the composition to be Rh : Ge = 1.08(1) : 1 for RhGe, which is close to the ideal stoichiometric ratio. For CoGe, however, the measured ratio of Co : Ge was 1.25(1) : 1 suggests the presence of excess Co and related defects. Figure 1(d) and Figure 1(e) present the Laue diffraction patterns of RhGe and CoGe single crystals along the high-symmetry (100) plane, exhibiting sharp, well-indexed diffraction spots with cubic symmetry, further attesting to the high quality and structural integrity of grown single crystals.

B20 cubic crystal structures, PXRD patterns, and Laue diffraction patterns of RhGe and CoGe

Figure 1. (a) The B20 cubic crystal structure of RhGe and CoGe with origin shift (0.23, 0.23, 0.23). The blue and red balls represent Rh/Co and Ge atoms, respectively. The orange arrow in the left panel indexes the [111][111] direction. The helix arrangements are clearly visible in the top view along the [111][111]-direction (right panel). PXRD patterns of (b) RhGe and (c) CoGe along with the Rietveld refinements. The insets show the photograph of each single crystal. Laue diffraction patterns of (d) RhGe and (e) CoGe single crystal.

The temperature-dependent electrical resistivity ρxx(T)\rho_{xx}(T) of RhGe and CoGe single crystals are shown in Figs. 2(a) and 2(b). Both of them exhibit metallic behaviors in general and the residual resistivity ratios RRRRRR is about 27 and 2 for RhGe and CoGe, respectively. For RhGe, ρxx(T)\rho_{xx}(T) decreases linearly from ∼150 μΩ cm\sim150 \,\mu\Omega\,\mathrm{cm} at 300 K down to ∼70\sim70 K, indicating the dominant electron-phonon scattering at the high-temperature region. The ρxx(T)\rho_{xx}(T) can be fitted using ρxx(T)=ρ0+ATn\rho_{xx}(T) = \rho_0 + AT^n between 20 - 70 K, the obtained nn is 2.05(2), implying that the Fermi-liquid behavior appears at low-temperature region in RhGe. It is noted that superconductivity is absent in present RhGe crystals when temperature above 1.8 K, consistent with our previous results [37]. As emphasized in Ref. [35], superconductivity in RhGe is highly sensitive to sample composition and applied pressure. The EDX analysis revealed a slight compositional difference between our single crystals and the superconducting polycrystals. We therefore suggest that the absence of superconductivity in our samples may be attributed to these subtle differences in composition and/or residual strain, which can inherently arise from differences in synthesis methods. For CoGe crystal, it displays similar trends to RhGe but with lower resistivity (∼120\sim120 μΩ\mu\Omega cm at 300 K). The ρxx(T)\rho_{xx}(T) curve shows a linear behavior with lowering TT down to 180 K and changes to a T2.06(4)T^{2.06(4)} dependence between 40 - 70 K, consistent with Fermi-liquid behavior. When T<25T < 25 K, a subtle resistivity upturn can be observed. Such low-TT resistivity increase are generally attributed to three mechanisms: weak localization (WL), Kondo effect and electron-electron interaction (EEI) etc. However, WL and Kondo effect will lead to a negative MR when applying a magnetic field and are safely excluded here due to being inconsistent with the positive MR of CoGe (discuss below) [38, 39, 40]. As depicted in the inset of Fig 2(b), the upturn part in conductivity curve follows a T1/2T^{1/2} dependence, suggest the existence of EEI in the presence of disorder [38]. We propose that the disorder may arise from the excess Co defects in CoGe.

Temperature-dependent resistivity and magnetic susceptibility of RhGe and CoGe

Figure 2.

Image not extracted

Figure 2 (PDF p. 8). Temperature dependence of ρxx(T)\rho_{xx}(T) of (a) RhGe and (b) CoGe single crystals. The red solid lines show the fits using the formula ρxx(T)=ρ0+ATn\rho_{xx}(T) = \rho_0 + AT^n. Inset of (b) shows longitudinal conductivity σxx\sigma_{xx} as a function of T1/2T^{1/2} of CoGe single crystals, accompanied by a linear fit. Temperature dependence of χ(T)\chi(T) at field of 0.1 T with ZFC and FC modes for (a) RhGe and (b) CoGe single crystal, respectively. Inset of (a) shows χ(T)\chi(T) data at μ0H=1\mu_0H = 1 mT with ZFC mode. The red lines in (b) show the fits using the modified Curie-Weiss law χ=χ0+C/(T−Tθ)\chi= \chi_0 + C/(T - T_\theta).

Temperature dependence of magnetic susceptibility χ(T)\chi(T) of RhGe and CoGe at μ0H=0.1\mu_0H = 0.1 T with zero-field-cooling (ZFC) and field-cooling (FC) modes are shown in Figs. 2(c) and 2(d). For RhGe, the χ(T)\chi(T) curve exhibits a weak temperature dependence in the whole temperature range (Fig. 2(c)), suggesting a Pauli paramagnetic behavior. At low-temperature region, the absence of diamagnetic signal in χ(T)\chi(T) curve at μ0H=1\mu_0H = 1 mT with ZFC mode (inset of Fig. 2(b)) confirms there is no superconducting transition in present RhGe single crystals, consistent with resistivity data. For CoGe, the χ(T)\chi(T) curve shows a similar behavior to RhGe at T>50T > 50 K (Fig. 2(d)), implying the same Pauli paramagnetism. It is consistent with prior report on CoGe polycrystal [41, 42]. When T<50T < 50 K, however, the χ(T)\chi(T) curve of CoGe exhibits a slight upturn behavior (Fig. 2(d)), likely due to trace magnetic impurities, spin fluctuations or weak electronic correlations. The fitted Curie constant is 0.0014(3) emu K mol−1^{-1} Oe−1^{-1} using the modified Curie-Weiss law (χ=χ0+C/(T−Tθ)\chi= \chi_0 + C/(T - T_\theta)), corresponding to 0.11(2) μB\mu_{\mathrm{B}}/f.u. The observed excess Co from EDX analysis suggests that these atoms may act as magnetic impurities. If assuming these magnetic impurities originates from Co element with magnetic moment 3.87 μB\mu_{\mathrm{B}}, the estimated molar content of magnetic impurities are below 2.8(6) %.

Figure 3(a) and Figure 3(b) present the magnetoresistance (MR) of RhGe and CoGe at various temperatures. RhGe exhibits a large positive MR (∼600\sim600 %) at 2 K, which diminishes rapidly with increasing temperature. Moreover, the MR curve can be fitted well using the formula MR=A(μ0H)n\mathrm{MR} = A(\mu_{0}H)^{n} with n=1.75(2)n = 1.75(2). Such nearly parabolic field dependence suggests that there may be multiply bands with different carrier type (electron or hole) near Fermi level EFE_{\mathrm{F}}. In contrast, CoGe displays a weak positive MR <3%< 3 \% across the entire measured range (2 – 300 K, 0 – 9 T), comparable to those of CoGe polycrystal [42] and CoSi grown via the chemical vapor transport method [44].

Field dependence of MR and Hall resistivity of RhGe and CoGe

Figure 3. Field dependence of MR up to μ0H=9\mu_{0}H = 9 T at various temperatures for (a) RhGe and (b) CoGe single crystal, respectively. The color codes in (a) and (b) are the same. The red solid line in (a) is the fit of MR data at 2 K using MR=A(μ0H)n\mathrm{MR} = A(\mu_{0}H)^{n}. (c) and (d) The ρyx(μ0H)\rho_{yx}(\mu_{0}H) of RhGe and CoGe as a function of μ0H\mu_{0}H between 2 K and 300 K. The color codes in (c) and (d) are the same. (e) Temperature dependences of na(T)n_{a}(T) for RhGe and CoGe derived from the linear fits of ρyx(μ0H)\rho_{yx}(\mu_{0}H) curves at high-field region (4–9 T). (f) Derived temperature dependences of μ(T)\mu(T) of RhGe and CoGe. Inset: enlarged part of μ(T)\mu(T) below 50 K for CoGe.

The Hall resistivity ρyx(μ0H)\rho_{yx}(\mu_{0}H) as a function of magnetic field at various temperatures is shown in Figure 3(c) and Figure 3(d) for both materials. All curves exhibit negative slopes, indicating the dominance of electron-type carriers in the transport properties. By linearly fitting the ρyx(μ0H)\rho_{yx}(\mu_{0}H) curves at high-field region (4 – 9 T) and combining them with zero-field ρxx(T)\rho_{xx}(T) data, the temperature dependence of apparent carrier concentration na(T)n_{a}(T) and mobility μ(T)\mu(T) can be determined based on single-band model (RH=ρyx(μ0H)/μ0H=1/naeR_{\mathrm{H}} = \rho_{yx}(\mu_{0}H)/\mu_{0}H = 1/n_{a}e and ρxx=neμ\rho_{xx} = n e \mu, where RHR_{\mathrm{H}} is Hall coefficient and ee is elementary charge). As shown in Figure 3(e), the carrier concentrations of both compounds at 2 K are comparable: na∼4.5×1020 cm−3n_{a} \sim4.5 \times10^{20}\ \mathrm{cm}^{-3} and 3.5×1020 cm−33.5 \times10^{20}\ \mathrm{cm}^{-3} for RhGe and CoGe, respectively. Moreover, these values of nan_{a} are also close to that in CoSi [44, 45]. With increasing temperature TT, the nan_{a} of RhGe increases rapidly, reaching a maximum at T∼160T \sim160 K, and then starts to decrease gradually. It implies that at high temperature there may have more thermal activated hole-type carriers mainly from the band at MM point in Brillouin zone, which leads to the decrease of nan_{a}. In contrast, CoGe shows a monotonic mild increase of nan_{a} with increasing TT. For RhGe, it exhibits a significantly higher mobility (μ∼2366 cm2 V−1 s−1\mu\sim2366\ \mathrm{cm}^{2}\ \mathrm{V}^{-1}\ \mathrm{s}^{-1}) than that of CoGe (μ∼359 cm2 V−1 s−1\mu\sim359\ \mathrm{cm}^{2}\ \mathrm{V}^{-1}\ \mathrm{s}^{-1}) at 2 K (Figure 3(f)). At high TT, The μ\mu of RhGe undergoes a rapid decay to ∼350 cm2 V−1 s−1\sim350\ \mathrm{cm}^{2}\ \mathrm{V}^{-1}\ \mathrm{s}^{-1} at T=50T = 50 K and finally deceases to ∼25 cm2 V−1 s−1\sim25\ \mathrm{cm}^{2}\ \mathrm{V}^{-1}\ \mathrm{s}^{-1} at 300 K. For CoGe, its μ\mu peaks at ∼370 cm2 V−1 s−1\sim370\ \mathrm{cm}^{2}\ \mathrm{V}^{-1}\ \mathrm{s}^{-1} near 25 K (inset of Figure 3(f)) before declining to ∼47 cm2 V−1 s−1\sim47\ \mathrm{cm}^{2}\ \mathrm{V}^{-1}\ \mathrm{s}^{-1} at 300 K slowly. Such behavior explains the more obvious low-temperature MR of RhGe when compared to CoGe and its rapid suppression with TT. It also suggests that the upturn feature of ρxx(T)\rho_{xx}(T) for CoGe at T∼25T \sim25 K (Figure 1(c)) originates from the non-monotonic behavior of μ\mu not the evolution of nan_{a}.

RhGe and (b) CoGe, respectively. Insets of (a) and (b) show the relationship between Cp/TC_p/T and T2T^2. The red solid lines represent the fits using the formula Cp/T=γ+βT2C_p/T = \gamma+ \beta T^2.

Specific heat measurements of RhGe and CoGe single crystals, shown in Figure 4(a) and (Figure 4b), reveal their thermodynamic properties across 2 – 300 K. For RhGe single crystal, no anomaly (e.g., specific heat jump) at specific heat Cp(T)C_p(T) curve is observed at 2.6 K (Figure 4(a)), consistent with above resistivity and magnetic susceptibility results. It confirms the absence of superconductivity in present RhGe single crystal. The high-temperature Cp(T)C_p(T) for both compounds approaches the Dulong-Petit limit (~ 57 J mol−1^{-1} K−1^{-1} at 300 K), consistent with the classical value 3NR3NR (N=2N = 2 atoms per formula unit, R=8.314R = 8.314 J mol−1^{-1} K−1^{-1}). At low-temperature region, the Cp(T)C_p(T) data can be fitted well using the formula Cp/T=γ+βT2C_p/T = \gamma+ \beta T^2, where γ\gamma represents the electronic specific heat coefficient and β\beta the lattice contribution (insets in Figure 4(a) and (Figure 4b)). The fitted γ\gamma of RhGe is 0.40(1) mJ mol−1^{-1} K−2^{-2} and β=0.084(9)\beta= 0.084(9) mJ mol−1^{-1} K−4^{-4}, yielding a Debye temperature ΘD=357(6)\Theta_{\mathrm{D}} = 357(6) K via ΘD=(12π4NR/5β)1/3\Theta_{\mathrm{D}} = (12\pi^4NR/5\beta)^{1/3}. CoGe shows a comparable value of γ\gamma with RhGe (~ 0.24(1) mJ mol−1^{-1} K−2^{-2}) and a larger ΘD=403(4)\Theta_{\mathrm{D}} = 403(4) K, derived from the value of β=0.059(2)\beta= 0.059(2) mJ mol−1^{-1} K−4^{-4}. The latter can be explained by the smaller atomic weight of Co than that of Rh. The values of γ\gamma in both RhGe and CoGe is similar to that of CoSi (γ\gamma ~ 0.5 – 1.2 mJ mol−1^{-1} K−2^{-2}) [46], but much smaller than MnGe (γ\gamma = 16 - 20 mJ mol−1^{-1} K−2^{-2}) [41, 42] and FeGe (γ\gamma = 9 mJ mol−1^{-1} K−2^{-2}) [42] (summarized in Table 1 with other related B20 materials). It demonstrate that the electron correlations in nonmagnetic RhGe, CoGe and CoSi are weaker than those of magnetic B20 systems.

Temperature dependence of heat capacity for RhGe and CoGe

Figure 4. Temperature dependence of Cp(T)C_{p}(T) from 2 K to 300 K at zero field for (a)

RRRMR (%)nn (102010^{20} cm−3^{-3})μ\mu (cm2^{2} V−1^{-1} s−1^{-1})γ\gamma (mJ mol−1^{-1} K−2^{-2})Properties2Ref.
CoSi1–30-1–4001–3200–73000.5-1.2PM, UCF[26, 28, 41, 43, 51]
CoGe2<32.53590.24PMThis work
CoGe1.8<0.160–3PM, UCF[38, 39, 40, 46]
RhSiPM, UCF[15, 16]
RhGe276004.523660.40(1)PMThis work
RhGe102.9SC (Tc=4T_c = 4 K), UCF[32, 35]
RhSn244504.6PM, UCF[19] [52]
FeGe14-0.52/3 carrier/f.u.9HM (TC=280T_C = 280 K), Sky[25, 39]
MnGe9.3<51/2 carrier/f.u.16–20HM (TC=275T_C = 275 K), Sky[25, 38, 39]

Table 1. Summary of physical parameters of some silicide and germanide materials with B20 structure.

A comparison of the physical parameters of RhGe and CoGe with other silicide and germanide materials with B20 structure is presented in Table 1. Theoretical calculations indicate that RhGe and CoGe are nonmagnetic, and they exhibit remarkably similar electronic band structures, well-described within the rigid band approximation framework. States within 5 eV of the Fermi energy (EFE_F) originate predominantly from transition metal dd-orbitals, which are understood to govern many of the intriguing properties in these compounds. Specifically, the Fermi surfaces of CoGe and RhGe comprise electron pockets centered at the Brillouin zone center (Γ\Gamma point) and corner (RR point), alongside a hole pocket at the MM point. Additional, very small hole pockets may exist along the Γ\Gamma-RR direction. All the Fermi surface pockets are rather small and resemble those of semimetals [22, 42, 47, 48, 49, 50]. Our magnetic and electrical transport measurements corroborate the theoretical predictions, confirming that both RhGe and CoGe single crystals are paramagnetic metals with low charge carrier density, similar to CoSi. These features likely arises from a significantly reduced density of states (DOS) at EFE_F when compared to itinerant ferromagnets like FeGe or MnGe. More importantly, because CoGe and RhGe are isoelectronic to CoSi and RhSi, they should exhibit similar band topology, especially long Fermi arcs. But different strength of SOC and subtle surface environment could lead to different connectivity and instability of SSs. Thus, RhGe and CoGe provide a novel platform to study surface-dominant correlation effects in topological semimetals.

Conclusion

In summary, we successfully grew the high-quality RhGe and CoGe single crystals up to millimeter size under high pressure and high temperature. Transport measurement reveals the metallic behaviors of RhGe and CoGe single crystals at low temperature, while magnetic measurements indicate that both RhGe and CoGe are paramagnets. Neither superconductivity nor ferromagnetism are observed down to 2 K. These high-quality RhGe and CoGe single crystals are prerequisite for further investigation of their novel topological properties using angle-resolved photoemission spectroscopy (APRES). Moreover, this study highlights the ongoing challenges of discovering superconductivity in B20-structured materials.

Acknowledgments

This work was supported by National Key R&D Program of China (Grants No. 2022YFA1403800 and No. 2023YFA1406500), National Natural Science Foundation of China (Grants No. 12274459, 12474002 and 22171283), and China Postdoctoral Science Foundation (Grant Nos. 2023M730011). This work was supported by the Synergetic Extreme Condition User Facility (SECUF, https://cstr.cn/31123.02.SECUF).

References

  1. [1]Vergniory M, Elcoro L, Felser C, Regnault N, Bernevig B A, and Wang Z 2019 Nature 566 480
  2. [2]Zhang T, Jiang Y, Song Z, Huang H, He Y, Fang Z, Weng H, and Fang C 2019 Nature 566 475
  3. [3]Cano J, Bradlyn B, and Vergniory M 2019 APL Mater. 7 101125
  4. [4]Bradlyn B, Cano J, Wang Z, Vergniory M, Felser C, Cava R J, and Bernevig B A 2016 Science 353 aaf5037
  5. [5]Liu Z, Zhou B, Zhang Y, Wang Z, Weng H, Prabhakaran D, Mo S-K, Shen Z, Fang Z, Dai X, Hussain Z, and Chen Y L 2014 Science 343 864
  6. [6]Kushwaha S K, Krizan J W, Feldman B E, Gyenis A, Randeria M T, Xiong J, Xu S-Y, Alidoust N, Belopol ski I, Liang T, Hasan M Z, Ong N P, Yazdani A, and Cava R J 2015 APL Mater. 3 041504
  7. [7]Wang Z, Weng H, Wu Q, Dai X, and Fang Z 2013 Phys. Rev. B 88 125427
  8. [8]Lv B, Xu N, Weng H, Ma J, Richard P, Huang X, Zhao L, Chen G, Matt C, Bisti F, Strocov V N, Mesot J, Fang Z, Dai X, Qian T, Shi M, and Ding H 2015 Nat. Phys. 11 724
  9. [9]Sun Y, Wu S-C, and Yan B 2015 Phys. Rev. B 92 115428
  10. [10]Xu S-Y, Belopolski I, Sanchez D S, Zhang C, Chang G, Guo C, Bian G, Yuan Z, Lu H, Chang T-R, Shibayev P P, Prokopovych M L, Alidoust N, Zheng H, Lee C- C, Huang S-M, Sankar R, Chou F, Hsu C-H, Jeng H-T, Bansil A, Neupert T, Strocov V N, Lin H, Jia S, and Hasan M Z 2015 Sci. Adv. 1 e1501092
  11. [11]Xu S-Y, Alidoust N, Chang G, Lu H, Singh B, Belopolsky I, Sanchez D S, Zhang X, Bian G, Zheng H, Husanu M-A, Bian Y, Huang S-M, Hsu C-H, Chang T-R, Jeng H-T, Bansil A, Neupert T, Strocov V N, Lin H, Jia S, and Hasan M Z 2017 Sci. Adv. 3 e1603266
  12. [12]Chiu C-K, Teo J C, Schnyder A P, and Ryu S 2016 Rev. Mod. Phys. 88 035005
  13. [13]Senthil T 2015 Annu. Rev. Condens. Matter Phys. 6 299
  14. [14]Mardanya S, Singh B, Huang S-M, Chang T-R, Su C, Lin H, Agarwal A, and Bansil A 2019 Phys. Rev. Mater. 3 071201(R)
  15. [15]Rees D, Manna K, Lu B, Morimoto T, Borrmann H, Felser C, Moore J, Torchinsky D H, and Orenstein J 2020 Sci. Adv. 6 eaba0509
  16. [16]Chang G, Xu S-Y, Wieder B J, Sanchez D S, Huang S-M, Belopolsky I, Chang T-R, Zhang S, Bansil A, Lin H, and Hasan M Z 2017 Phys. Rev. Lett. 119 206401
  17. [17]Sessi P, Fan F-R, Küster F, Manna K, Schröter N B, Ji J-R, Stolz S, Krieger J A, Pei D, Kim T K, Dudin P, Cacho C, Widmer R, Borrmann H, Shi W, Chang K, Sun Y, Felser C, and Parkin S S P 2020 Nat. Commun. 11 3507
  18. [18]Yao M, Manna K, Yang Q, Fedorov A, Voroshinin V, Schwarze B V, Hornung J, Chattopadhyay S, Sun Z, Guin S N, Wosnitza J, Borrmann H, Shekhar C, Kumar N, Fink J, Sun Y, and Felser C 2020 Nat. Commun. 11 20333
  19. [19]Li H, Xu S, Rao Z-C, Zhou L-Q, Wang Z-J, Zhou S-M, Tian S-J, Gao S-Y, Li J-J, Huang Y-B, Lei H-C, Weng H-M, Sun Y-J, Xia T-L, Qian T, and Ding H 2019 Nat. Commun. 10 5505
  20. [20]Gao H, Vanderbos J W, Kim Y, and Rappe A M 2019 Annu. Rev. Mater. Res. 49 153
  21. [21]Chang G, Wieder B J, Schindler F, Sanchez D S, Belopolsky I, Huang S-M, Singh B, Wu D, Chang T-R, Neupert T, Xu S-Y, Lin H, and Hasan M Z 2018 Nat. Mater. 17 978
  22. [22]Tang P, Zhou Q, and Zhang S-C 2017 Phys. Rev. Lett. 119 206402
  23. [23]Pshenay-Severin D A, and Burkov A T 2019 Materials 12 2710
  24. [24]Mulbauer S, Binz B, Jonietz F, Pfleiderer C, Rosch A, Neubauer A, Georgii R, and Böni P 2009 Science 323 915
  25. [25]Tokura Y, and Kanazawa N 2021 Chem. Rev. 121 2857
  26. [26]Rao Z, Li H, Zhang T, Tian S, Li C, Fu B, Tang C, Wang L, Li Z, Fan W, Li J, Huang Y, Liu Z, Long Y, Fang C, Weng H, Shi Y, Lei H, Sun Y, Qian T et al. 2019 Nature 567 496
  27. [27]Sanchez D S, Belopolsky I, Cochran T A, Xu X, Yin J-X, Chang G, Xie W, Manna K, Süß V, Huang C-Y, Alidoust N, Multer D, Zhang S S, Shumiya N, Wang X, Wang G-Q, Chang T-R, Felser C, Xu S-Y, Jia S, Lin H, and Hasan M Z 2019 Nature 567 500
  28. [28]Takane D, Wang Z, Souma S, Nakayama K, Nakamura T, Oinuma H, Nakata Y, Iwasawa H, Cacho C, Kim T, Horiba K, Kumagishira K, Takahashi T, Ando Y, and Sato T 2019 Phys. Rev. Lett. 122 076402
  29. [29]Ni Z, Wang K, Zhang Y, Pozo O, Xu B, Han X, Manna K, Paglione J, Felser C, Grushin A G, de Juan F, Mele E J, and Wu L 2021 Nat. Commun. 12, 154 (2021).
  30. [30]Rao Z-C, Tian S-J, Gao S-Y, Hu Q-X, Fan W-H, Huang J-R, Tang C-Y, Huang Y-B, Lei H-C, Sun Y-J, Qian T, and Ding H 2022 Sci. China Phys. Mech. Astron. 65 257013
  31. [31]Sanchez D S, Cochran T A, BelopolskI I, Cheng Z-J, Yang X P, Liu Y, Hou T, Xu X, Manna K, Shekhar C, Yin J-X, Borrmann H, Chikina A, Denlinger J D, Strocov V N, Xie W, Felser C, Jia S, Chang G, and Hasan M Z 2023 Nat. Phys. 19 682
  32. [32]Mardanya S, Kargarian M, Verma R, Chang T-R, Chowdhury S, Lin H, BansiI A, Agarwal A, and Singh B 2024 Phys. Rev. Mater. 8 L091801
  33. [33]Larchev V I, and Popova S V 1982 J. Less-Common Met. 87 53
  34. [34]Takizawa H, Sato T, Endo T, and Shimada M 1988 J. Solid State Chem. 73 40
  35. [35]Tsvyashchenko A V, Sidorov V A, Petrova A E, Fomicheva L N, Zibrov I P, and Dmitrienko V E 2016 J. Alloys Compd. 686 431
  36. [36]Kamaeva L V, Magnitskaya M V, Suslov A A, Tsvyashchenko A V, and Chtchelkatchev N M 2022 J. Phys.: Condens. Matter 34 424001
  37. [37]Dong X, Zhang B, Ye X, Wei P, Lian L, Sun N, Long Y, Tian S, Wang S, Lei H, and Yu R 2025 Chin. Phys. B 34 088101
  38. [38]Lee P A, and Ramakrishnan T V 1985 Rev. Mod. Phys. 57 287
  39. [39]Kondo J 1964 Progr. Theoret. Phys. 32 37
  40. [40]Wang Y, Xie C, Li J, Du Z, Cao L, Han Y, Zu L, Zhang H, Zhu H, Zhang X, Xiong Y, and Zhao W 2021 Phys. Rev. B 103 174418
  41. [41]Tsvyashchenko A, Sidorov V, Fomicheva L, Krasnorussky V, Sadykov R, Thompson J, Gofryk K, Ronning F, and Ivanov V 2012 SSP 190 225
  42. [42]DiTusa J F, Zhang S B, Yamaura K, Xiong Y, Prestigiacomo J C, Fulfer B W, Adams P W, Brickson M I, Browne D A, Capan C, Fisk Z, and Chan J Y 2014 Phys. Rev. B 90 144404
  43. [43]Baek S-H, Sidorov V A, Nikolaev A V, Klimczuk T, Ronning F, and Tsvyashchenko A V 2022 Phys. Rev. B 105 165132
  44. [44]Xu X, Wang X, Cochran T A, Sanchez D S, Chang G, BelopolskI I, Wang G, Liu Y, Tien H-J, Gui X, Xie W, Hasan M Z, Chang T-R, and Jia S 2019 Phys. Rev. B 100 045104
  45. [45]Wu D S, Mi Z Y, Li Y J, Wu W, Li P L, Song Y T, Liu G T, Li G, and Luo J L 2019 Chin. Phys. Lett. 36 077102
  46. [46]Stishov S M, Petrova A E, Sidorov V A, and Menzel D 2012 Phys. Rev. B 86 064433
  47. [47]Magnitskaya M, Chtchelkatchev N, Tsvyashchenko A, Salamatin D, Lepeshkin S, Fomicheva L, and Budzynski M 2019 J. Magn. Magn. Mater. 470 127
  48. [48]Chtchelkatchev N M, Magnitskaya M V, and Tsvyashchenko A V 2020 Eur. Phys. J. Special Topics 229 167
  49. [49]Kanazawa N, Onose Y, Shiomi Y, Ishiwata S, and Tokura Y 2012 Appl. Phys. Lett. 100 093902
  50. [50]Basak S, Kobiakka A, Sternik M, Łażewski J, Jochym P T, Oleś A M, Piekarz P, and Ptok A 2024 Comput. Mater. Sci. 244 113149
  51. [51]Elastic, thermodynamic, and electronic properties of MnSi, FeSi, and CoSi 2010 Phys. Rev. B 82 155124

Paper details

vlnc:W_kmt5c5f7
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents