Unprecedented superionicity of ultra-low barrier in A0.5CoO2 (A=Li, Zn)

Abstract

The ion conductivity of a solid-state ion conductor generally increases exponentially upon reduction in ion migration barrier. For prevalent cathode material LiCoO2, the room-temperature ion conductivity and migration barrier are respectively around 10-4 S/cm and 0.3 eV. In this paper, through first-principles calculations we predict the existence of 1D superionicity as the Li ions in O2 LiCoO2 are transformed to Zn0.5CoO2 or Li0.5CoO2 via cation-exchange reaction or deintercalation. The ion migration barriers (0.01-0.02 eV) even lower than room-temperature ~kBT are reduced by more than an order of magnitude compared with LiCoO2, which are facilitated by facile transition of mobile ions between two coordination configurations. The room-temperature ion conductivity is estimated to be over 50 S/cm, enhanced by 2-3 orders of magnitude compared with current highest reported value. Such unprecedented superionicity may also exist in other similar layered ion conductors, which may render technical advances and exotic effects such as ultrafast ion batteries and quantized ferroelectricity.

Solid-state ion conductors exhibiting fast ion transport have been widely used in energy-storage devices like batteries.[1, 2, 3, 4, 5, 6, 7, 8] In particular, lithium-ion batteries have emerged as an essential component of modern portable power sources. LiCoO2\mathrm{LiCoO}_{2} is one of the most extensively studied cathode materials due to its high energy density and long cyclability,[9] where the layered structure is formed by Co3+\mathrm{Co}^{3+}-based edge-sharing CoO6\mathrm{CoO}_{6} octahedrons separated by lithium layers, facilitating the intercalation/deintercalation of Li ions. However, its low room-temperature ion conductivity (∼10−4\sim10^{-4} S/cm) [10] due to high migration barrier (∼\sim0.3–0.4 eV) [11, 12, 13] would cause not only a sluggish transport of Li ions, but also a large polarization at the cathode-electrolyte interface. The ion conductivity is proportional to exp⁡(−ΔkBT)\exp\left(-\frac{\Delta}{k_{\mathrm{B}}T}\right), which can be greatly enhanced even when the barrier Δ\Delta is only slightly reduced. For example, the room-temperature ion conductivity and migration barrier for LiNbOCl4\mathrm{LiNbOCl}_{4} have been respectively estimated to be 10.4 mS/cm and 0.205 eV[14], which are 24 mS/cm and 0.155 eV for Li5.3PS4.3ClBr0.7\mathrm{Li}_{5.3}\mathrm{PS}_{4.3}\mathrm{ClBr}_{0.7} with disorder between Cl−\mathrm{Cl}^{-}, Br−\mathrm{Br}^{-} and S2−\mathrm{S}^{2-} sites[15]. In 2023, Ryoji Kanno et al. synthesized Li9.54[Si1−δMδ]1.74P1.44S11.1Br0.3O0.6\mathrm{Li}_{9.54}[\mathrm{Si}_{1-\delta}\mathrm{M}_{\delta}]_{1.74}\mathrm{P}_{1.44}\mathrm{S}_{11.1}\mathrm{Br}_{0.3}\mathrm{O}_{0.6} (M=Ge,Sn\mathrm{M}=\mathrm{Ge},\mathrm{Sn}) with a high room-temperature conductivity of 32 mS/cm and low migration barrier of 0.09 eV, surpassing all previous records for inorganic Li-ion conductors[16]. However, even such a low barrier still corresponds to kBTk_{\mathrm{B}}T of a high temperature over 1000K, surpassing the melting points of many solid-state ion conductors. If the barrier can be reduced below ∼kBT\sim k_{\mathrm{B}}T, ion can move as quasi-free particle and the potential wells provide scattering instead of localization, which may give rise to various exotic effects described in lattice gas model.[17]

Additionally, some solid-state ion conductors with ion vacancies may exhibit unconventional ferroelectricity with quantized polarizations.[18] It has also been proposed that such quantized ferroelectricity may even emerge in monovalent ion conductors with non-ferroelectric crystal lattices if their mobile monovalent cations are substituted by multivalent cations (e.g., Mg2+\mathrm{Mg}^{2+}, Al3+\mathrm{Al}^{3+}[19]) via cation-exchange reaction, based on previous experimental reports on topotactic reaction with an aliovalent cation between trigonal layers of ion conductors.[20, 21] However, the experimental realization of such quantized ferroelectricity is also hindered by the high migration barriers of those ion conductors (e.g., 0.31 eV per Na ion for Na4SnS4\mathrm{Na_4SnS_4},[18] and 0.29 eV per Mg ion for Mg0.5CrS2\mathrm{Mg_{0.5}CrS_2},[19] much higher than the switching barrier of BaTiO3\mathrm{BaTiO_3} around 0.1 eV). In this paper, we predict by ab initio calculations that when the Li ions in O2O_2 LiCoO2\mathrm{LiCoO_2} are substituted by half number of divalent Zn2+\mathrm{Zn^{2+}} by cation-exchange reaction, or half of them are deintercalated, arrays of 1D ion conduction channels with ultra-low migration barriers (0.01-0.02 eV) will be formed, giving rise to unprecedented room-temperature ion conductivity over 50 S/cm. The ultralow migration barrier can be attributed to the existence of two interconvertible states with different coordinate configurations that are almost degenerate in energy, making the intercalated ions behave like 1D liquids at ambient conditions.

Our theoretical calculations are performed based on density-functional-theory (DFT) methods implemented in the Vienna Ab initio Simulation Package (VASP) code[22, 23]. The generalized gradient approximation (GGA) in the form of Perdew-Burke-Ernzerhof functional (PBE)[24] and the projector augmented wave (PAW)[25] method are applied to describe the exchange-correlation and the core electrons, respectively. PBE+U method with an effective UU value (UeffU_{\mathrm{eff}}) of 4.9 eV[26] is used to account for strong correlation. The kinetic energy cutoff was set at 500 eV, and the Brillouin zone was sampled by 7×5×37 \times5 \times3 K points for O2O_2-state and 5×7×55 \times7 \times5 K points for O3O_3-state using the Monkhorst−Pack scheme[27]. The convergence threshold for self-consistent-field iteration is set to 10−610^{-6} eV and all structures are fully optimized until the forces are smaller than 0.01 eV/Å. The Berry phase method was employed to evaluate crystalline polarizations, and the ion migration pathways were obtained by using the solid-state nudged elastic band (SSNEB)[28] method.

The experimentally verified O3 and O2 phase LiCoO2\mathrm{LiCoO_2} respectively with parallel and antiparallel CoO2\mathrm{CoO_2} layers are displayed in Figure 1, where the Li ions are intercalated into the interstitial octahedral sites.[29, 30, 31, 32] As the Li ions are substituted by half number of Zn ions, the CoO2\mathrm{CoO_2} layers in O2 phase Zn0.5CoO2\mathrm{Zn_{0.5}CoO_2} become buckled in the ground state (see the comparison in energy between different configurations in Fig. S1), which are still planar in O3 phase. Two configurations may form in O2 Zn0.5CoO2\mathrm{Zn_{0.5}CoO_2}, where each Zn ion can either bond with 6 O atoms in a ZnO6\mathrm{ZnO_6} octahedron (denoted as Oct-state), or 4 O atoms in a ZnO4\mathrm{ZnO_4} tetrahedron (denoted as Tet-state, only 2 meV/f.u. higher in energy compared with Oct-state). The bonding configurations of Zn ions in two phases are shown in Figure 1(b), where the Zn-O bond lengths in Tet-state range from 1.998 to 2.018 Å (dZn−O1=dZn−O3=1.998d_{\mathrm{Zn-O1}} = d_{\mathrm{Zn-O3}} = 1.998 Å, dZn−O2=dZn−O4=2.018d_{\mathrm{Zn-O2}} = d_{\mathrm{Zn-O4}} = 2.018 Å), mostly shorter compared with Oct-state (dZn−O1=dZn−O2=2.226d_{\mathrm{Zn-O1}} = d_{\mathrm{Zn-O2}} = 2.226 Å, dZn−O5=dZn−O6=2.195d_{\mathrm{Zn-O5}} = d_{\mathrm{Zn-O6}} = 2.195 Å, dZn−O3=2.015d_{\mathrm{Zn-O3}} = 2.015 Å, dZn−O4=2.043d_{\mathrm{Zn-O4}} = 2.043 Å), and the differences between those bond lengths reveal the distortions of octahedrons and tetrahedrons.

Transformation of O3 and O2 state LiCoO2 to Zn0.5CoO2

Figure 1. (a) Transformation from O3 state LiCoO2\mathrm{LiCoO_2} to Zn0.5CoO2\mathrm{Zn_{0.5}CoO_2} upon cation-exchange reaction. (b) Transformation from O2 state LiCoO2\mathrm{LiCoO_2} to Oct and Tet state Zn0.5CoO2\mathrm{Zn_{0.5}CoO_2}, respectively with distorted ZnO6\mathrm{ZnO_6} octahedrons and ZnO4\mathrm{ZnO_4} tetrahedrons.

As shown in Figure 2 where adjacent in-plane O atoms of each layer are linked, each Zn cation in LiCoO2\mathrm{LiCoO}_{2} is located between two antiparallel oxygen triangles of adjacent layers respectively marked in red and blue, with overlapping centers from the overview. As Li ions are substituted by half number of Zn ions, the deviations between the centers of two triangles upon slightly interlayer sliding make them staggered in Oct phase Zn0.5CoO2\mathrm{Zn}_{0.5}\mathrm{CoO}_{2}, accompanied by the distortions of ZnO6\mathrm{ZnO}_{6} octahedrons. According to our NEB calculations, the transition barrier between Oct and Tet-phase upon displacements of Zn ions (accompanied by slightly interlayer sliding) is only around 20 meV/f.u..

Side views, overviews, and transition pathways for O2 LiCoO2, Oct and Tet states

Figure 2. The side view and overview of O2 LiCoO2\mathrm{LiCoO}_{2}, Oct and Tet state of ZnCo2O4\mathrm{ZnCo}_{2}\mathrm{O}_{4}, and Oct-Tet phase transition pathways for ZnCo2O4\mathrm{ZnCo}_{2}\mathrm{O}_{4} and LiCoO2\mathrm{LiCoO}_{2}, where the upper and lower oxygen triangles are marked in red and blue, respectively.

It is noteworthy that when half of Li ions in O2 LiCoO2\mathrm{LiCoO}_{2} are deintercalated, similar Oct and Tet-phase for Li0.5CoO2\mathrm{Li}_{0.5}\mathrm{CoO}_{2} may emerge with a small energy difference around 5 meV/f.u. between them, and their transition barrier of 13 meV/f.u. is even lower, although it is metallic compared with insulating Zn0.5CoO2\mathrm{Zn}_{0.5}\mathrm{CoO}_{2} with a bandgap of 1.27 eV. Similar low migration barrier may also exist in some other layered ion conductors like Zn0.5NiO2\mathrm{Zn}_{0.5}\mathrm{NiO}_{2} (see the estimated value around 33 meV in Fig. S2). Compared with the ground state with pyrochlore lattices, such layered structures are respectively 64 and 36 meV/atom for Zn0.5CoO2\mathrm{Zn}_{0.5}\mathrm{CoO}_{2} and Zn0.5CoO2\mathrm{Zn}_{0.5}\mathrm{CoO}_{2}, so their stable formations via cation-exchange reaction from O2 LiCoO2\mathrm{LiCoO}_{2} should be still possible. According to our ab initio molecular dynamic (AIMD) simulations in the canonical ensemble with the temperature being controlled at 600 K in Fig. S3, the robust integrity of layered structure suggests good thermal stability.

The migration barrier of Li ions in O3 LiCoO2_2 are typically ∼\sim0.3-0.4 eV according to previous studies, [11, 12] which is reduced to ∼\sim0.2-0.3eV per Zn ion upon cation-exchange reaction, as shown in Figure 3(a). In the anti-parallel stacking configuration, the migration of Zn ions along −-x direction can be greatly facilitated by the low barrier of Oct-Tet phase transition where the Zn ions are displaced by half lattice constant ∣a∣/2|\mathbf{a}|/2, and the migration for one lattice constant ∣a∣|\mathbf{a}| is equivalent to Oct-Tet-Oct phase transition. As shown in Figure 3(b), the migration barrier along the conduction channel is just the Oct-Tet phase transition barrier, even lower than ∼kBT\sim k_{\mathrm{B}}T at ambient conditions and more than an order of magnitude lower compared with migration barrier in O3 phase. Meanwhile the migration barriers along other two directions (marked as path 2 and 3 in Figure 3(b)) are much higher (all over 0.4 eV). Such anisotropy should clarify the formations of confined 1D ion liquids in Fig. S3, where the displacements of Zn ions along −y-y direction at elevated temperature are negligible compared with −x-x direction.

Sideview and overview structures of O3-ZnCo2O4 and O2-ZnCo2O4 with ion migration pathways and migration barriers

Figure 3. (a) The sideview and overview structure of O3-ZnCo2_2O4_4 and two ion migration pathways. (b) The sideview and overview structure of O2-ZnCo2_2O4_4 and three ion migration pathways, where the migration along path1 also gives ultralow barrier for O2-LiCo2_2O4_4.

A coarse estimation of ion conductivity (δion\delta_{\mathrm{ion}})[33] can be formulated as

δion=(γcνZ2e2a02kBT)exp⁡(−ΔGmkBT)\delta_{\mathrm{ion}} = \left(\frac{\gamma c \nu Z^{2} e^{2} a_{0}^{2}}{k_{\mathrm{B}}T}\right) \exp\left(-\frac{\Delta G_{\mathrm{m}}}{k_{\mathrm{B}}T}\right)

where Z=2Z = 2 is the charge number of Zn ion, a0=3.03×10−8 cma_{0} = 3.03 \times10^{-8}\,\mathrm{cm} and ΔGm=0.02 eV\Delta G_{\mathrm{m}} = 0.02\,\mathrm{eV} are respectively the transfer distance and migration barrier of each Zn ion. c=0.012×1024 cm−3c = 0.012 \times10^{24}\,\mathrm{cm}^{-3} is its ion density, ν=1013 s−1\nu= 10^{13}\,\mathrm{s}^{-1} is the frequency and γ=1\gamma= 1 represents the 1D Zn ion conduction channel. Given the parameters above, δion\delta_{\mathrm{ion}} is estimated to be 55.6 S/cm for ZnCo2_{2}O4_{4}. Similarly, the Li ion conductivity in O2 LiCo2_{2}O4_{4} estimated to be 27.3 S/cm is not only 5 orders of magnitude larger than δ\delta in O3 LiCoO2_{2}[10] (10−410^{-4} S/cm), but also much higher than all superionic crystals currently known, like lithium argyrodites[34] (∼\sim10 mS/cm), α\alpha-RbAg4_{4}I5_{5}[35] (0.3 S/cm) and α\alpha-KAg4_{4}I5_{5} (0.221 S/cm)[36]. However, such ultrahigh conductivity is highly anisotropic since the migration barrier is much higher along two other directions, where the coordination phase transition is not involved.

We use the following equation for a rough estimation of the specific capacity of ZnCo2_{2}O4_{4} as a cathode material:

C=nZF3.6mC = \frac{nZF}{3.6m}

where n=1n = 1 is the mole number of Zn ion, Z=2Z = 2 is the charge number of Zn ion, FF is the Faraday constant (F=96485F = 96485 C⋅\cdotmol−1^{-1}), and m=247.24m = 247.24 g⋅\cdotmol−1^{-1} is the mole mass of ZnCo2_2O4_4. Given the parameters above, CC is estimated to be 216.44 mAh/g. The open-circuit voltage (OCV) of ZnCo2_2O4_4 in Figure 4(a) estimated to be 4.88V is larger than most Li-ion cathode materials such as LiCoO2_2 (3.75 V) and LiFePO4_4 (3.47 V)[11], and the estimated energy density of 1056.3 Wh/kg is also higher (LiCoO2_2:760 /1027.5 Wh/kg in experimental/theoretical reports; LiFePO4_4: 476 /590 Wh/kg in experimental/theoretical reports) [37]. With high energy density and ultra-low migration barrier, ZnCo2_2O4_4 could be a promising material for ultra-fast rechargeable ion battery.

Calculated open-circuit voltage and polarization quantum evolution

Figure 4. (a) Calculated open-circuit voltage (OCV) as a function of Zn-ion concentration x in Znx_xCo2_2O4_4. (b) The polarization quantum evolution upon the migration of Zn ions along −x-x direction for one lattice constant ∣a∣\lvert\mathbf{a}\rvert, where Δn=ΩΔP/e∣a∣\Delta n=\Omega\Delta\mathbf{P}/e\lvert\mathbf{a}\rvert.

Finally, the low ion migration barrier of ZnCo2_2O4_4 should facilitate the realization of unconventional ferroelectricity with quantized polarization, considering the unattainable voltage required for switching due to the high barriers over 0.3 eV in previous predicted systems.[18, 19] Upon migration of Zn ions for one lattice constant along -xx direction corresponding to 1 ion vacancy at each channel, the change of polarization quanta (Δn=4\Delta n=4 in Figure 4(b)) is 63.6 μC/cm2^2, already two times larger compared with BaTiO3_3. In a ZnCo2_2O4_4 crystal with size ~1 μm and a density of only 1 vacancy per 100 Zn ions, the migration distance in each channel will be orders of magnitude larger, giving rise to an immense ferroelectric polarization around ~1000 μC/cm2^2, with barriers comparable to the lowest values of current ferroelectrics.[38, 39]

In summary, we predict the existence of superionicity in antiparallel stacking ZnCo2_2O4_4 and LiCo2_2O4_4 based on O2 LiCoO2_2. The ultralow transition barriers (0.01-0.02 eV) between Oct and Tet states are also the ion migration barrier along the 1D conduction channels, leading to the highest solid-state ion conductivity known to date. Similar superionicity may also exist in some other layered ion conductors like ZnNi2_2O4_4. Considering the technical advances and various exotic effects[17] that may be brought by such elusive superionicity with barrier lower than room-temperature ∼kBT\sim k_{\mathrm B}T, our prediction should deserve further experimental efforts.

Acknowledgement

This work is supported by National Natural Science Foundation of China (Nos. 22073034).

Supporting Information

References

  1. [1]Rickert H 1978 Solid Ionic Conductors: Principles and Applications Angewandte Chemie International Edition in English 17 37-46DOI
  2. [2]Sebti E, Evans H A, Chen H, Richardson P M, White K M, Giovine R, Koirala K P, Xu Y, Gonzalez-Correa E, Wang C, Brown C M, Cheetham A K, Canepa P and Clément R J 2022 Stacking Faults Assist Lithium-Ion Conduction in a Halide-Based Superionic Conductor Journal of the American Chemical Society 144 5795-811DOI
  3. [3]Zhang Z, Roy P-N, Li H, Avdeev M and Nazar L F 2019 Coupled Cation–Anion Dynamics Enhances Cation Mobility in Room-Temperature Superionic Solid-State Electrolytes Journal of the American Chemical Society 141 19360-72DOI
  4. [4]Li M, Pietrowski M J, De Souza R A, Zhang H, Reaney I M, Cook S N, Kilner J A and Sinclair D C 2014 A family of oxide ion conductors based on the ferroelectric perovskite Na0.5Bi0.5TiO3 Nature Materials 13 31-5DOI
  5. [5]Peng J, Liu Y, Pan Y, Wu J, Su Y, Guo Y, Wu X, Wu C and Xie Y 2020 Fast Lithium Ion Conductivity in Layered (Li–Ag)CrS2 Journal of the American Chemical Society 142 18645-51DOI
  6. [6]Nishijima M, Ootani T, Kamimura Y, Sueki T, Esaki S, Murai S, Fujita K, Tanaka K, Ohira K, Koyama Y and Tanaka I 2014 Accelerated discovery of cathode materials with prolonged cycle life for lithium-ion battery Nature Communications 5 4553DOI
  7. [7]Jun K, Sun Y, Xiao Y, Zeng Y, Kim R, Kim H, Miara L J, Im D, Wang Y and Ceder G 2022 Lithium superionic conductors with corner-sharing frameworks Nature Materials 21 924-31DOI
  8. [8]Jun K, Chen Y, Wei G, Yang X and Ceder G 2024 Diffusion mechanisms of fast lithium-ion conductors Nature Reviews MaterialsDOI
  9. [9]Lyu Y, Wu X, Wang K, Feng Z, Cheng T, Liu Y, Wang M, Chen R, Xu L, Zhou J, Lyu Y and Guo B 2021 An Overview on the Advances of LiCoO2 Cathodes for Lithium-Ion Batteries Advanced Energy Materials 11 2000982
  10. [10]Slima I B, Karoui K and Rhaïem A B 2023 Ionic conduction, structural and optical properties of LiCoO2 compound Ionics 29 1731-9
  11. [11]Zhang T, Li D, Tao Z and Chen J 2013 Understanding electrode materials of rechargeable lithium batteries via DFT calculations Progress in Natural Science: Materials International 23 256-72DOI
  12. [12]Ning F, Li S, Xu B and Ouyang C 2014 Strain tuned Li diffusion in LiCoO2 material for Li ion batteries: A first principles study Solid State Ionics 263 46-8DOI
  13. [13]Aydinol M K, Kohan A F, Ceder G, Cho K and Joannopoulos J 1997 Ab initio study of lithium intercalation in metal oxides and metal dichalcogenides Physical Review B 56 1354-65DOI
  14. [14]Tanaka Y, Ueno K, Mizuno K, Takeuchi K, Asano T and Sakai A 2023 New Oxyhalide Solid Electrolytes with High Lithium Ionic Conductivity >10 mS cm−1 for All-Solid-State Batteries Angewandte Chemie International Edition 62 e202217581DOI
  15. [15]Patel S V, Banerjee S, Liu H, Wang P, Chien P-H, Feng X, Liu J, Ong S P and Hu Y-Y 2021 Tunable Lithium-Ion Transport in Mixed-Halide Argyrodites Li6−xPS5−xClBrx: An Unusual Compositional Space Chemistry of Materials 33 1435-43
  16. [16]Li Y, Song S, Kim H, Nomoto K, Kim H, Sun X, Hori S, Suzuki K, Matsui N, Hirayama M, Mizoguchi T, Saito T, Kamiyama T and Kanno R 2023 A lithium superionic conductor for millimeter-thick battery electrode Science 381 50-3DOI
  17. [17]Dieterich W, Fulde P and Peschel I 1980 Theoretical models for superionic conductors Advances in Physics 29 527-605DOI
  18. [18]Wang X, Ren Y and Wu M 2022 Unconventional Ferroelectricity with Quantized Polarizations in Ionic Conductors: High-Throughput Screening The Journal of Physical Chemistry Letters 13 9552-7DOI
  19. [19]Wang X and Wu M 2024 Quantized ferroelectricity in multivalent ion conductors with non-polar point groups Materials Horizons 11 3885-91DOI
  20. [20]Heubner C, Lein T, Schneider M and Michaelis A 2020 Intercalation materials for secondary batteries based on alkali metal exchange: developments and perspectives Journal of Materials Chemistry A 8 16854-83DOI
  21. [21]Miura A, Takei T and Kumada N 2013 Synthesis and crystal structure of Mg0.5NbO2: An ion-exchange reaction with Mg2+ between trigonal [NbO2]− layers Journal of Solid State Chemistry 197 471-4DOI
  22. [22]Kresse G and Furthmüller J 1996 Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set Computational Materials Science 6 15-50DOI
  23. [23]Kresse G and Furthmüller J 1996 Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set Physical review B 54 11169pubmed.ncbi.nlm.nih.gov/9984901
  24. [24]Perdew J P, Ruzsinszky A, Csonka G I, Vydrov O A, Scuseria G E, Constantin L A, Zhou X and Burke K 2008 Restoring the density-gradient expansion for exchange in solids and surfaces Physical review letters 100 136406pubmed.ncbi.nlm.nih.gov/18517979
  25. [25]Blöchl P E 1994 Projector augmented-wave method Physical review B 50 17953pubmed.ncbi.nlm.nih.gov/9976227
  26. [26]Zhou F, Cococcioni M, Marianetti C, Morgan D and Ceder G 2004 First-principles prediction of redox potentials in transition-metal compounds with LDA+U Physical Review B 70DOI
  27. [27]Monkhorst H J and Pack J D 1976 Special points for Brillouin-zone integrations Physical Review B 13 5188-92DOI
  28. [28]Henkelman G, Uberuaga B P and Jónsson H 2000 A climbing image nudged elastic band method for finding saddle points and minimum energy paths The Journal of Chemical Physics 113 9901-4
  29. [29]Li S, Sun Y, Gao A, Zhang Q, Lu X and Lu X 2022 Sustainable LiCoO2 by collective glide of CoO6 slabs upon charge/discharge Proceedings of the National Academy of Sciences 119 e2120060119DOI
  30. [30]Yabuuchi N, Kawamoto Y, Hara R, Ishigaki T, Hoshikawa A, Yonemura M, Kamiyama T and Komaba S 2013 A Comparative Study of LiCoO2 Polymorphs: Structural and Electrochemical Characterization of O2-, O3-, and O4-type Phases Inorganic Chemistry 52 9131-42DOI
  31. [31]Carlier D, Van der Ven A, Delmas C and Ceder G 2003 First-Principles Investigation of Phase Stability in the O2-LiCoO2 System Chemistry of Materials 15 2651-60DOI
  32. [32]Carlier D, Saadoune I, Croguennec L, Ménétrier M, Suard E and Delmas C 2001 On the metastable O2-type LiCoO2 Solid State Ionics 144 263-76DOI
  33. [33]Ohno S, Banik A, Dewald G F, Kraft M A, Krauskopf T, Minafra N, Till P, Weiss M and Zeier W G 2020 Materials design of ionic conductors for solid state batteries Progress in Energy 2 022001DOI
  34. [34]Zhou L, Assoud A, Zhang Q, Wu X and Nazar L F J J o t A C S 2019 New family of argyrodite thioantimonate lithium superionic conductors 141 19002-13DOI
  35. [35]Shabanov O M, Kachaev R T and Kazieva L A 2012 High-voltage conductivity of [alpha]-RB [Ag. sub. 4][I. sub. 5],[alpha]-K [Ag. sub. 4][I. sub. 5], and [alpha]-K [Cu. sub. 4][I. sub. 5] superionic conductors Technical Physics 57 1157-62
  36. [36]Andreeva A V and Despotuli A L 2005 Interface design in nanosystems of advanced superionic conductors Ionics 11 152-60DOI
  37. [37]Yu Q, Tang W, Hu Y, Gao J, Wang M, Liu S, Lai H, Xu L and Fan C 2021 Novel low-cost, high-energy-density (>700 Wh kg − 1) Li-rich organic cathodes for Li-ion batteries Chemical Engineering Journal 415 128509DOI
  38. [38]Li L and Wu M 2017 Binary Compound Bilayer and Multilayer with Vertical Polarizations: Two-Dimensional Ferroelectrics, Multiferroics, and Nanogenerators ACS Nano 11 6382-8DOI
  39. [39]Wu M and Zeng X C 2016 Intrinsic Ferroelasticity and/or Multiferroicity in Two-Dimensional Phosphorene and Phosphorene Analogues Nano Letters 16 3236-41DOI

Paper details

vlnc:W_nt84mfwq
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents