Probing Interfacial Magnetic Anisotropy in \texorpdfstring{CoV2_{2}O4_{4}}{CoV2O4} using Spin Hall Magnetoresistance

Abstract

Spin Hall magnetoresistance (SMR) has emerged as a powerful probe for investigating interfacial spin transport and magnetic anisotropy in complex oxide heterostructures. In this work, we investigate the interfacial magnetic anisotropy in Pt/CVO through angle-dependent magnetotransport measurements. Unlike the bulk-sensitive magnetic measurements on both strained CVO and Pt/CVO films, which exhibit a ferrimagnetic transition at TC≈150T_{C} \approx 150 K accompanied by out-of-plane anisotropy that reorients toward in-plane anisotropy below 90 K, SMR reveals a distinct interfacial magnetic anisotropy. The rotational scans of the in-plane transverse SMR at 20 K exhibit substantial hysteresis about [100], while no hysteresis is observed along [110] and [11ˉ\bar{1}0], indicating a biaxial anisotropy with easy axes along [110] and [11ˉ\bar{1}0]. Furthermore, the absence of sharp discontinuities in both the in-plane longitudinal and transverse SMR, together with pronounced discontinuities near the in-plane [010] direction during out-of-plane rotation, strongly indicates the presence of in-plane anisotropy. This behavior persists up to 120 K. The discrepancy between the bulk-sensitive magnetic measurements and the SMR response suggests that the Pt/CVO interface retains a magnetic anisotropy distinct from the bulk, highlighting the interfacial sensitivity of SMR. Additionally, the spin mixing conductance is found to be of the order of 101410^{14} Ω−1m−2Ω^{-1}\mathrm{m}^{-2}, comparable to other oxide-based spintronic systems. These findings highlight the crucial role of interfacial effects in spin transport and establish Pt/CVO as a promising platform for spintronic applications.

Introduction

Spin Hall magnetoresistance (SMR) has emerged as a powerful electrical probe for investigating complex spin structures and magnetic anisotropy configurations across a broad range of magnetic systems, including collinear[1, 2, 3, 4, 5] and noncollinear antiferromagnets[6, 7], canted ferrimagnets[8, 9]. The SMR effect originates from the modulation of the resistivity of a heavy metal layer through spin charge interconversion processes when it is interfaced with an adjacent magnetic material. In heavy metals with strong spin-orbit coupling, such as Pt, Ta, and W, an applied charge current generates a transverse spin accumulation through the spin Hall effect, enabling efficient spin-current generation in spintronic heterostructures[10, 11, 12]. Owing to its interface-sensitive nature, SMR plays a pivotal role in the Rashba Edelstein effect[13], the spin-momentum locking of topological surface states[14], the orbital Hall and Rashba-Edelstein effects[15], while serving as a complementary approach to sophisticated techniques such as synchrotron radiation and neutron diffraction[16]. Furthermore, SMR enables extraction of the interfacial spin-mixing conductance, a key parameter governing spin transport efficiency and spin-current transfer across interfaces[18, 19] [17]. SMR has been extensively investigated in heavy metal/magnetic insulator bilayers, particularly Pt/Y3_3Fe5_5O12_{12} (YIG), owing to the exceptionally low Gilbert damping parameter of YIG. Although garnets have been widely explored for spin transport studies, their integration with existing microelectronics remains challenging. In contrast, complex oxide spinel magnetic insulators such as Ni0.65_{0.65}Zn0.35_{0.35}Al0.8_{0.8}Fe1.2_{1.2}O4_4 (NZAFO) and MgAl0.5_{0.5}Fe1.5_{1.5}O4_4 (MAFO)[20, 21, 22] are compatible with silicon-based technologies[23, 24] and have shown efficient spin pumping and electrical spin-current detection in bilayers[22], making spinel oxides attractive for spintronic devices.

In the family of spinel oxides, vanadates with the general formula AV2_2O4_4 constitute a compelling class of materials in which the interplay of strong electronic correlations, geometric frustration, orbital ordering, gives rise to a wide variety of emergent phenomena[25, 26, 27]. CoV2O4\mathrm{CoV}_{2}\mathrm{O}_{4} (CVO) stands out among spinel vanadates due to its proximity to itinerant behavior, arising from the short V–V distance near the critical limit for metallicity[28, 29]. Bulk CVO crystallises in a cubic spinel structure, where Co2+\mathrm{Co}^{2+} (3d73d^{7}) ions occupy the tetrahedral A-sites, while V3+\mathrm{V}^{3+} (3d23d^{2}) ions reside at the octahedral B-sites. Magnetically, cubic bulk CoV2_2O4_4 (CVO) exhibits a nearly collinear ferrimagnetic (CF) ground state below TC∼150T_{\mathrm{C}} \sim150 K and undergoes a subtle first-order structural transition near ∼90\sim90 K, accompanied by the emergence of spin canting[30] whereas CVO thin films exhibit pronounced strain-dependent magnetic anisotropy and spin reorientation behavior. Under compressive strain [SrTiO3_3 (STO) and MgAl2_2O4_4 (MAO)], the magnetization below ∼150\sim150 K (∼160\sim160 K for MAO) favours along the out-of-plane direction below ∼150\sim150 K (∼160\sim160 K for MAO) and subsequently reorients toward the in-plane direction near ∼90\sim90 K (∼160\sim160 K for MAO)[31, 32, 33]. While under the tensile strain (MgO), magnetization switches from an in-plane at ∼127\sim127 K to an out-of-plane easy axis below ∼45\sim45 K[31, 32, 33]. Further, CVO grown on SrTiO3_3 exhibits a field-driven spin reorientation below ∼75\sim75 K, where the easy axis changes from [110] at low fields to [100] above ∼3\sim3 T, accompanied by V-site spin canting[34]. The temperature and field-dependent evolution of magnetic anisotropy in CVO/STO is summarised in the phase diagram shown in Figure 1. Complementarily, Kim et al. investigated CVO/STO using torque magnetometry to probe its magnetic anisotropy. Interestingly, while earlier zero-field neutron measurements identified the low-temperature easy axis along [110], torque magnetometry under applied magnetic fields revealed that the in-plane ⟨100⟩\langle100\rangle directions are energetically favourable[35]. These contrasting observations point toward a complex evolution of magnetic anisotropy in CVO. Such tunable magnetic anisotropy, together with the temperature-driven spin reorientation in CVO, makes it an attractive platform for spintronic applications, as it can facilitate efficient manipulation of spin configurations.

Figure 1. (a) Crystal structure of CoV2_2O4_4 (CVO), illustrating the arrangement of CoO4_4 tetrahedra and VO6_6 octahedra along with their corresponding electronic configurations and spin states of Co2+^{2+} and V3+^{3+} ions. (b) Schematic magnetic phase diagram of CVO, illustrating the evolution of magnetic anisotropy and spin configurations with temperature. The red and blue arrows represent the spin orientations of Co and V ions, respectively, while the dotted arrows indicate the canting of V spins in the spin-reoriented phase. (c) θ\theta–2θ2\theta X-ray diffraction patterns of the Pt/CVO bilayer and bare CVO thin films grown on STO(001), showing the CVO (00ll) reflections and the additional Pt diffraction peak from the overlayer. Insets show the Pt (6 nm)/CVO (26 nm) and bare CVO (26 nm) thin-film heterostructures grown on SrTiO3_3 (001) substrates.

Although the temperature and field dependent magnetic anisotropy of bulk CVO has been extensively studied, its interfacial magnetic behaviour remains largely unexplored. To gain insight into interfacial magnetic anisotropy and spin transport in CVO, SMR measurements were carried out on Pt/CVO heterostructures. Prior to the SMR studies, magnetic measurements performed on bare CVO/STO and Pt/CVO/STO samples revealed similar anisotropic behavior, suggesting that Pt deposition does not significantly affect the intrinsic anisotropy of CVO. Subsequently, SMR measurements were performed under both in-plane and out-of-plane magnetic field configurations to investigate interfacial magnetic behavior and spin transport. The low-temperature in-plane SMR response at 20 K reveals the presence of biaxial anisotropy with easy axes along the [110] and [11ˉ0][1\bar{1}0] directions. Furthermore, the SMR results confirm the persistence of in-plane anisotropy up to 110 K, unlike the magnetic measurements on Pt/CVO, likely due to the presence of distinct surface anisotropy in CVO. Given the interface-sensitive nature of SMR, the measured response likely reflects the surface magnetic behavior rather than the bulk. Moreover, the spin mixing conductance parameter estimated from the SMR measurements, is on the order of 2×1014 Ω−1 m−22 \times10^{14}\ \Omega^{-1}\,\mathrm{m}^{-2}, indicating that the Pt/CVO interface is highly transparent to spin currents. Overall, these results demonstrate that SMR provides valuable insight into the interfacial magnetic and spin transport properties of CVO heterostructures.

Experimental Methods

CVO thin films were grown on STO(001) substrates using PLD, with a KrF excimer laser (λ=248\lambda= 248 nm), operating at a repetition rate of 4 Hz and a laser fluence of 1.8 J/cm2^2. A CoV2_2O6_6 target was used, and the substrate temperature was maintained at 650∘^\circ C under a base pressure of 2×10−62 \times10^{-6} mbar. Subsequently, a Pt layer was deposited on top of the CoV2_2O4_4 layer by sputtering at room temperature to avoid interdiffusion. The structural characterization of the films was carried out using a Rigaku SmartLab high-resolution X-ray diffractometer (HR-XRD) with a Cu Kα1\alpha_1 radiation source (λ=1.54\lambda= 1.54 Å). θ\theta–2θ2\theta scans were performed to confirm the phase, while X-ray reflectivity (XRR) measurements were carried out to determine the film thickness. DC magnetization measurements were carried out using a superconducting quantum interference device-based magnetometer (Quantum Design SQUID-VSM). The films were then patterned into Hall bars using UV photolithography. Electrical contacts were made by using wire-bonded with Au–Cr wires. For SMR measurements, The sample was mounted in a modified closed-cycle refrigerator equipped with a rotating magnet arrangement. The angular dependence of SMR was measured by rotating the sample in both clockwise and counterclockwise directions at various constant magnetic fields in the range of 150 Oe to 3.5 kOe. An AC current (IP−P=2I_{\mathrm{P-P}} = 2 mA, 333 Hz) was applied using a Keithley 6221 DC/AC current source, and the transverse voltage was measured using a Stanford Research SR830 lock-in amplifier.

Results and Discussion:

Figure 1(b) shows the θ\theta–2θ2\theta scan of representative bare CoV2_2O4_4 (26 nm) and Pt (6 nm)/CoV2_2O4_4 (26 nm) thin films. The (001) diffraction peaks corresponding to the CVO layer are clearly observed in both samples, indicating oriented growth, while the Pt/CVO sample exhibits an additional peak arising from the Pt overlayer. No impurity phases are detected, confirming that the crystallographic structure of CVO remains preserved after Pt deposition.

Figure 2(a) shows the temperature-dependent magnetisation measured under zero-field-cooled (ZFC) and field-cooled (FC) conditions in an applied field of 100 Oe over the temperature range 5 to 300 K, with the magnetic field applied along the in-plane (IP) and out-of-plane (OP) directions of CVO/STO (001). Consistent with previous reports, the system undergoes a paramagnetic-to-ferrimagnetic transition near ∼150\sim150 K (TcT_\mathrm{c})[31, 36]. A spin reorientation from the out-of-plane (OP) to the in-plane (IP) direction occurs near ∼90\sim90 K (T1T_1), accompanied by a decrease in OP magnetization and a corresponding increase in IP magnetization.

Figure 2(b) and 2(c) present the field-dependent magnetization measured in both IP and OOP configurations at 20 K and 110 K, respectively, to probe the anisotropy across different magnetic phases. At T=20T = 20 K, the sample exhibits a larger coercive field along inplane compared to out of plane ([1]), indicating a stronger anisotropy along the inplane direction. In contrast within the ferrimagnetic phase at 110 K, the coercive field becomes nearly negligible, while the comparatively lower field required to saturate the magnetization along [1] indicates that the [1] direction is the easy axis compared to [100] at 110 K. The temperature-dependent evolution of the magnetic easy axis from out of plane along [1] at high temperatures to inplane at low temperatures, as confirmed by the MM–HH measurements, is indicative of a spin reorientation transition. These observations are consistent with evolution of magnetic anisotropy of CVO/STO, as reported earlier[34]. To further examine whether the Pt overlayer induces any substantial modification in the magnetic response, magnetization measurements were performed on Pt/CVO/STO, as shown in Figure 2(d). The magnetization exhibits anisotropic behavior similar to that of bare CVO/STO, with all characteristic magnetic transitions occurring at nearly identical temperatures. Although the MM–HH curves at 20 K and 110 K exhibit some variation in the coercive field values following Pt deposition, the overall anisotropic characteristics and the temperature-driven spin reorientation behavior remain essentially unchanged in Pt/CVO/STO. These results demonstrate that the deposition of Pt overlayer does not significantly affect the overall magnetic anisotropy of CVO, as confirmed by our magnetization measurements. However, previous neutron studies have reported that below ∼75\sim75 K, CoV2O4\mathrm{CoV}_2\mathrm{O}_4 undergoes spin canting accompanied by a reorientation of spins toward the [110] direction[34]. In the present case, the magnetization measurements are limited to the [100] and [1] orientations, the anisotropy between the [110] and [100] directions could not be conclusively resolved, thereby necessitating complementary angle-sensitive probes such as SMR, capable of detecting in-plane anisotropic variations.

Figure 2. Temperature- and field-dependent magnetic properties of bare CVO and Pt/CVO heterostructures. The upper panel [(a)–(c)] corresponds to bare CVO, while the lower panel [(d)–(f)] represents Pt/CVO. Panels (a) and (d) show the temperature dependence of the magnetization measured under zero-field-cooled (ZFC), field-cooled cooling (FCC), and field-cooled warming (FCW) protocols. Panels (b), (c), (e), and (f) display the magnetic field dependence of magnetization, M(H)M(H), measured at different temperatures, highlighting the evolution of magnetic hysteresis and saturation behavior in both systems.

Therefore to illucidate the underlying anisotropy, SMR measurements were carried out on Pt/CVO using angle-dependent magnetoresistance (ADMR). In the Pt/CoV2O4\mathrm{CoV}_2\mathrm{O}_4 device, when a charge current is applied along the xx-direction in the Pt Hall bar, the spin Hall effect (SHE) generates a transverse spin current, leading to spin accumulation (μs\mu_s) at the Pt/CoV2O4\mathrm{CoV}_2\mathrm{O}_4 interface. The relative orientation between the spin polarization (ss) in Pt and the magnetization M\mathbf{M} in CoV2O4\mathrm{CoV}_2\mathrm{O}_4 governs the absorption of the spin current mediated by spin-transfer torque at the interface. This results in a modulation of the spin current in the Pt layer and, consequently, a change in charge current via the inverse spin Hall effect (ISHE), thereby producing a modulation in the resistance of the Pt layer upon rotation of the applied magnetic field. The longitudinal resistivity (ρxx\rho_{xx}) and the transverse resistivity (ρxy\rho_{xy}) measured in the Pt exhibits an angular dependence as [16, 37, 38]:

ρxx=ρ0+Δρ1(my2)(1)\rho_{xx} = \rho_0 + \Delta\rho_1(m_y^2) \tag*{(1)}
ρxy=ρ2mz+ρ1mxmy(2)\rho_{xy} = \rho_2m_z + \rho_1m_xm_y \tag*{(2)}

where m(mx,my,mz)=m/msm(m_x,m_y,m_z) = m/m_s are the direction cosines of magnetizations along x,y,zx,y,z. Here ρ0\rho_0 is the base line resistivity, ρ1ρ0\frac{\rho_1}{\rho_0} is SMR, and ρ2\rho_2 is an anomalous Hall like contribution.

At a fixed magnetic field HH, angular-dependent measurements were performed by rotating the field in both forward and reverse directions within the in-plane (xyxy-plane) configuration. The corresponding transverse (ρxy\rho_{xy}) and longitudinal (ρxx\rho_{xx}) resistivities were recorded for both α\alpha and −α-\alpha rotation scans. Figure 3 shows the in-plane transverse resistivity (ρxy\rho_{xy}) as a function of rotation angle α\alpha measured at 150 Oe for different temperatures. The magnetic field is initially aligned along the current direction (B∥j∥x\mathbf{B} \parallel\mathbf{j} \parallel x axis) and is then rotated continuously within the film plane toward the yy axis. The transverse SMR qualitatively follows a sin⁡(2α)\sin(2\alpha) dependence; however, significant deviations from this behavior are observed at all temperatures. Notably, at 20 K, a clear hysteresis between the forward and reverse scans emerges when the applied field is oriented along the [100] direction. The observed hysteresis reflects the presence of hard-axis anisotropy.[39]

Figure 3. Angular dependence of the transverse resistivity, ρxy\rho_{xy}, measured under positive and negative magnetic field sweeps at different temperatures for the Pt/CVO heterostructure under an applied magnetic field of 150 Oe. Panels (a)–(d) correspond to measurements performed at 20 K, 70 K, 85 K, and 120 K, respectively. The sinusoidal variation in ρxy\rho_{xy} with rotation angle α\alpha reflects the anisotropic magnetotransport response and its evolution with temperature.

As the magnetization approaches along the hard axis direction, it undergoes abrupt switching between orientations on either side of the hard axis. On the other hand, the absence of hysteresis corresponds to smooth rotation of magnetization along an easy axis. Thus, the absence of hysteresis along the symmetry-equivalent ⟨110⟩\langle110\rangle directions, namely [110], and [1ˉ1ˉ0][\bar{1}\bar{1}0] together with the orthogonal pair [1ˉ10][\bar{1}10] and [11ˉ0][1\bar{1}0], indicate the presence of biaxial in-plane anisotropy at 20 K. Further, the hysteresis progressively diminishes with increasing the applied field at 20 K, indicating that the Zeeman energy overcomes the magnetic anisotropy, resulting in field-driven magnetization rotation. (See Supplementary material.)

Upon increasing the temperature from 20 K to 110 K in the in-plane transverse measurements, the angular dependence progressively deviates from the expected sin⁡(2α)\sin(2\alpha) behaviour, accompanied by a substantial decrease in the hysteresis around the [10] and [01ˉ0][0\bar{1}0] directions. At these elevated temperatures, the anisotropy along the [100] and [110] directions becomes nearly comparable, making it difficult to clearly distinguish the magnetic easy axis. Furthermore, the absence of sharp discontinuities or abrupt transitions in the rotational transverse measurements indicates the persistence of an in-plane anisotropy. Consistently, no discernible change is observed in the rotational transverse SMR response between 70 K, 85 K, and 110 K, suggesting that the in-plane anisotropic behavior persists up to 110 K. However, the magnetic measurements on Pt/CVO suggest that the system remains in the ferrimagnetic phase with an out-of-plane easy axis at 110 K, while a distinct in-plane anisotropy emerges below 90 K. This discrepancy between the bulk magnetic response and the SMR response could be further examined by performing both transverse and longitudinal SMR measurements in the out-of-plane rotational and in-plane geometries, as shown in Figure 4.

Figure 4. Angular-dependent magnetoresistance measurements of the Pt/CVO heterostructure under different magnetic field rotation geometries at various temperatures. The left panel shows the angular dependence of the longitudinal resistivity, ρxx\rho_{xx}, measured during in-plane magnetic field rotation, while the right panel presents measurements obtained under out-of-plane field rotation. Data are shown for temperatures ranging from 20 K to 120 K. The corresponding schematics at the bottom illustrate the measurement configurations, including the current direction (JJ), magnetic field orientation (BB), and crystallographic axes of the Pt/CVO/STO(001) heterostructure. The observed angular modulation in ρxx\rho_{xx} demonstrates the anisotropic magnetotransport response and its dependence on temperature and magnetic field orientation.

Figures 4(a) and 4(b) display the angular dependence of the transverse resistivity, ρxy\rho_{xy}, and longitudinal resistivity, ρxx\rho_{xx}, respectively, as a function of the rotation angle α\alpha under an applied magnetic field of 1000 Oe at different temperatures. Both ρxy\rho_{xy} and ρxx\rho_{xx} exhibit a clear periodic modulation with a period of 180∘180^\circ. The longitudinal resistivity shows maxima when the magnetic field is aligned parallel or antiparallel to the current direction (α=0∘\alpha= 0^\circ and 180∘180^\circ) and minima when the field is oriented perpendicular to the current direction (α=90∘\alpha= 90^\circ and 270∘270^\circ). Such behavior is consistent with the expected cos⁡2α\cos^{2}\alpha dependence of the longitudinal SMR contribution (ρxx=ρ0+ρ1cos⁡2α\rho_{xx} = \rho_{0} + \rho_{1}\cos^{2}\alpha), indicating that the spin-dependent scattering at the interface is governed by the projection of magnetization relative to the spin polarization direction. Simultaneously, the in-plane transverse component, ρxySMR\rho_{xy}^{\mathrm{SMR}}, exhibits the characteristic sin⁡αcos⁡α\sin\alpha\cos\alpha angular dependence expected for transverse spin Hall magnetoresistance. The extrema in ρxySMR\rho_{xy}^{\mathrm{SMR}} occur near α=45∘\alpha= 45^\circ and 135∘135^\circ for the positive maxima, while minima are observed close to α=−45∘\alpha= -45^\circ and 225∘225^\circ. Interestingly, the longitudinal and transverse SMR responses remain nearly unchanged under the applied magnetic field across all measured temperatures up to 120120 K, suggesting that the in-plane anisotropy observed at 2020 K likely persists up to 120120 K. Figure 4 (c) and Figure 4 (d) illustrate the out-of-plane transverse (ρxy\rho_{xy}) and longitudinal resistivity (ρxx\rho_{xx}) as a function of rotation angle β\beta, measured at 10001000 Oe for different temperatures. This configuration is chosen such that the signal predominantly contains the SMR contribution, with minimal contribution from anisotropic magnetoresistance (AMR). In this configuration, the magnetic field is initially aligned along the yy axis and is rotated toward the zz axis, reaching 90∘90^\circ at H∥z\mathbf{H} \parallel z. For both the transverse and longitudinal out of plane resistivity responses, sharp discontinuities are observed when the applied field is approaching towards the in-plane directions at [10] and [01ˉ00\bar{1}0], indicating the presence of strong in-plane anisotropy. Notably, this behavior is observed across all measured temperatures up to 120120 K. Altogether, the absence of sharp discontinuities in the in-plane transverse and longitudinal responses, together with the presence of pronounced discontinuities when approaching the in-plane [10] orientation in the out-of-plane rotational configuration, clearly indicates the existence of in-plane anisotropy. Thus, the ADMR measurements performed in both configurations confirm the presence of a pronounced in-plane magnetic anisotropy that persists up to 120120 K. However, this observation contrasts with our bulk sensitive magnetic measurements, which suggest that the Pt/CVO likely develops an out-of-plane anisotropy at temperatures above 9090 K. Since SMR predominantly probes the magnetization at the Pt/CoV2_2O4_4 interface, the persistence of in-plane anisotropic features in the SMR response up to higher temperatures suggests that the surface magnetization of CVO may possess a magnetic anisotropy distinct from that of the bulk. Thus, although bulk-sensitive measurements indicate the emergence of out-of-plane anisotropy, the SMR response exhibits a contrasting behaviour dominated by interfacial in-plane anisotropy. Similar interfacial anisotropy-dominated SMR behavior has previously been reported in CoFe2_2O4_4-based heterostructures[40].

Further, we estimated the spin conductance across the Pt/CVO using the eqn.3[38]

∣ΔρSMRρ0∣=θSH2(2λsρPt)tPt−1Grtanh⁡2(tPt2λs)1+2λsρPtGrcoth⁡(tPtλs).(3)\left|\frac{\Delta\rho_{\mathrm{SMR}}}{\rho_{0}}\right| = \frac{\theta_{\mathrm{SH}}^{2}(2\lambda_{\mathrm{s}}\rho_{\mathrm{Pt}})t_{\mathrm{Pt}}^{-1}G_{\mathrm{r}}\tanh^{2}\left(\frac{t_{\mathrm{Pt}}}{2\lambda_{\mathrm{s}}}\right)}{1+2\lambda_{\mathrm{s}}\rho_{\mathrm{Pt}}G_{\mathrm{r}}\coth\left(\frac{t_{\mathrm{Pt}}}{\lambda_{\mathrm{s}}}\right)}. \tag*{(3)}

In the analysis, the spin Hall angle of Pt, θSH\theta_{\mathrm{SH}}, was assumed to lie in the range of 0.070.07–0.1240.124[41], while the spin diffusion length, λs\lambda_{\mathrm{s}}, was taken to be ∼2.0\sim2.0–2.32.3 nm based on previous reports on insulating spinel systems within the Dyakonov–Perel (DP) extrinsic scattering framework[42, 43, 44, 45]. Using these parameters, the effective spin mixing conductance was determined to be in the range of

Gr≈(1.2–3.5)×1014 Ω−1m−2.G_{\mathrm{r}} \approx(1.2\text{–}3.5) \times10^{14}\ \Omega^{-1}\mathrm{m}^{-2}.

The obtained values are comparable to those reported from spin-pumping and damping enhancement measurements in several insulating spinel-based heterostructures[42]. In particular, previous studies on MAFO/Pt and MAFO/β\beta-W bilayers have demonstrated spin mixing conductance values of the order of ∼2×1014 Ω−1m−2\sim2 \times10^{14}\ \Omega^{-1}\mathrm{m}^{-2}, exceeding many of the reported values for YIG/Pt systems. The comparable magnitude of GrG_{\mathrm{r}} obtained in the present Pt/CVO heterostructure highlights the high transparency of the Pt/CVO interface to spin currents and confirms the suitability of CVO-based heterostructures for efficient spin-current generation, transmission, and manipulation. These results further establish spinel oxide heterostructures as promising candidates for pure spin-current-based spintronic applications employing magnetic insulating platforms.

Conclusion:

In summary, spin Hall magnetoresistance (SMR) measurements on Pt/CoV2_2O4_4 reveal a robust in-plane magnetic anisotropy that persists across a wide temperature range up to 110110 K. Angular-dependent measurements demonstrate clear hysteresis at low fields, identifying an in-plane easy axis along the ⟨110⟩\langle110\rangle directions, while high-field measurements confirm that the magnetization undergoes field-driven rotation consistent with the SMR framework. Notably, both in-plane and out-of-plane rotation geometries consistently exhibit signatures of in-plane anisotropy even at temperatures where bulk magnetization measurements indicate a transition to out-of-plane anisotropy. This apparent discrepancy highlights the interfacial sensitivity of SMR, suggesting that the Pt/CoV2_2O4_4 interface retains a distinct magnetic anisotropy compared to the bulk. The persistence of interfacial in-plane anisotropy, despite bulk reorientation, points to a decoupling between surface and bulk magnetic behavior. These findings underscore the importance of interface-driven effects in spin transport and establish Pt/CoV2_2O4_4 as a compelling platform for studying anisotropy engineering and interfacial magnetism in complex oxide heterostructures.

Acknowledgment

D.S. acknowledges the funding from Max Planck Partner Group and SERB, Government of India (Grant No. CRG/2019/005144). S.I. thanks Priya Lekshmi, Vikram, and Pranjul for assistance during the measurements.

Data Availability Statement

The data that support the findings of this study are available from the corresponding author upon reasonable request.

References

  1. [1]Y. Ji, J. Miao, K. Meng, Z. Ren, B. Dong, X. Xu, Y. Wu, and Y. Jiang, Spin Hall magnetoresistance in an antiferromagnetic magnetoelectric Cr₂O₃/heavy-metal W heterostructure, Applied Physics Letters 110 (2017).DOI
  2. [2]W. Lin and C. Chien, Electrical Detection of Spin Backflow from an Antiferromagnetic Insulator/Y₃Fe₅O₁₂ interface, Physical Review Letters 118, 067202 (2017).DOI
  3. [3]D. Hou, Z. Qiu, J. Barker, K. Sato, K. Yamamoto, S. Vélez, J. M. Gomez-Perez, L. E. Hueso, F. Casanova, and E. Saitoh, Tunable Sign Change of Spin Hall Magnetoresistance in Pt/NiO/Y₃Fe₅O₁₂ Structures, Physical Review Letters 118, 147202 (2017).
  4. [4]J. Fischer, M. Althammer, N. Vlіеstra, H. Huebl, S. T. Goennenwein, R. Gross, S. Sprägпs, and M. Opel, Large Spin Hall Magnetoresistance in Antiferromagnetic α-Fe₂O₃/Pt Heterostructures, Physical Review Applied 13, 014019 (2020).DOI
  5. [5]T. Ishikawa, M. Matsuo, and T. Kato, Spin Hall magnetoresistance in quasi-two-dimensional antiferromagnetic-insulator/metal bilayer systems, Physical Review B 107, 054426 (2023).DOI
  6. [6]K. Oda, T. Moriyama, and T. Ono, Magnetoresistance in bilayers of heavy metal and non-collinear antiferromagnet, Journal of the Magnetics Society of Japan 43, 1901R001 (2019).
  7. [7]T. Uchimura, J. Han, P. Tang, J.-Y. Yoon, Y. Takeuchi, Y. Yamane, S. Kanai, G. E. Bauer, H. Ohno, and S. Fukami, Unconventional Spin Hall Magnetoresistance in Noncollinear Antiferromagnet/Heavy-Metal Stacks, Physical Review Letters 134, 096701 (2025).DOI
  8. [8]K. Ganzhorn, J. Barker, R. Schlitz, B. A. Piot, K. Ollefs, F. Guillou, F. Wilhelm, A. Rogalev, M. Opel, M. Althammer, et al., Spin Hall magnetoresistance in a canted ferrimagnet, Physical Review B 94, 094401 (2016).DOI
  9. [9]B.-W. Dong, J. Cramer, K. Ganzhorn, H. Yuan, E.-J. Guo, S. T. Goennenwein, and M. Kläui, Spin Hall magnetoresistance in the non-collinear ferrimagnet GdIG close to the compensation temperature, Journal of Physics: Condensed Matter 30, 035802 (2018).DOI
  10. [10]L. Vila, T. Kimura, and Y. Otani, Evolution of the Spin Hall effect in Pt Nanowires: Size and Temperature Effects, Physical Review Letters 99, 226604 (2007).DOI
  11. [11]R. Liu, C.-F. Pai, Y. Li, H. Tseng, D. Ralph, and R. Buhrman, Spin-Torque Switching with the Giant Spin Hall Effect of Tantalum, Science 336, 555 (2012).DOI
  12. [12]Q. Hao and G. Xiao, Giant spin hall effect and switching induced by spin-transfer torque in a W/Co₄₀Fe₄₀B₂₀/MgO structure with perpendicular magnetic anisotropy, Phys. Rev. Appl. 3, 034009 (2015).
  13. [13]H. Nakayama, Y. Kanno, H. An, T. Tashiro, S. Haku, A. Nomura, and K. Ando, Rashba-Edelstein Magnetoresistance in Metallic Heterostructures, Physical Review Letters 117, 116602 (2016).DOI
  14. [14]X. Chen, H. Bai, Y. Ji, Y. Zhou, L. Liao, Y. You, W. Zhu, Q. Wang, L. Han, X. Liu, et al., Control of spin current and antiferromagnetic moments via topological surface state, Nature Electronics 5, 574 (2022).DOI
  15. [15]S. Ding, A. Ross, D. Go, L. Baldrati, Z. Ren, F. Freimuth, S. Becker, F. Kammerbauer, J. Yang, G. Jakob, et al., Harnessing Orbital-to-Spin Conversion of Interfacial Orbital Currents for Efficient Spin-Orbit Torques, Physical Review Letters 125, 177201 (2020).DOI
  16. [16]Y.-T. Chen, S. Takahashi, H. Nakayama, M. Althammer, S. T. Goennenwein, E. Saitoh, and G. E. Bauer, Theory of spin hall magnetoresistance (smr) and related phenomena, Journal of Physics: Con- M. Onbasli, A. Kehlberger, D. H. Kim, G. Jakob, M. Kläui, A. V. Chumak, B. Hillebrands, and C. A. Ross, Pulsed laser deposition of epitaxial yttrium iron garnet films with low Gilbert damping and bulk-like magnetization, APL Materials 2 (2014).
  17. [18]Z. Qiu, K. Ando, K. Uchida, Y. Kajiwara, R. Takahashi, H. Nakayama, T. An, Y. Fujikawa, and E. Saitoh, Spin pumping conductance at a well-controlled platinum/yttrium iron garnet interface, Applied Physics Letters 103 (2013).DOI
  18. [19]H. Wang, C. Du, Y. P. R. Adu, P. C. Hammel, and F. Yang, Scaling of Spin Hall Angle in 3d, 4d, and 5d Metals from Y3Fe5O12/Metal Spin Pumping, Physical Review Letters 112, 197201 (2014).DOI
  19. [20]S. Emori, B. A. Gray, H.-M. Jeon, J. Peoples, M. Schmitt, K. Mahalingam, M. Hill, M. E. McConney, M. T. Gray, U. S. Alaan, et al., Coexistence of Low Damping and Strong Magnetoelastic Coupling in Epitaxial Spinel Ferrite Thin Films, Advanced Materials 29, 1701130 (2017).DOI
  20. [21]S. Emori, D. Yi, S. Crossley, J. J. Wisser, P. P. Balakrishnan, B. Khodadadi, P. Shafer, C. Klewe, A. T. N’Diaye, B. T. Urwin, et al., Ultralow Damping in Nanometer-Thick Epitaxial Spinel Ferrite Thin Films, Nano letters 18, 4273 (2018).DOI
  21. [22]M. Gray, S. Emori, B. Gray, H. Jeon, O. van’t Erve, B. Jonker, S. Kim, M. Suzuki, T. Ono, B. Howe, et al., Spin-Current Generation in Low-Damping Ni0.65Zn0.35Al0.8Fe1.2O4 Spinel Ferrite, Physical Review Applied 9, 064039 (2018).
  22. [23]L. Kang, J. Gao, H. Xu, S. Zhao, H. Chen, and P. Wu, Epitaxial Mg2SiO4 thin films with a spinel structure grown on Si substrates, Journal of Crystal Growth 297, 100 (2006).
  23. [24]M. P. Warusawithana, C. Cen, C. R. Sleasman, J. C. Woicik, Y. Li, L. F. Kourkoutis, J. A. Klug, H. Li, P. Ryan, L-P. Wang, et al., A Ferroelectric Oxide Made Directly on Silicon, Science 324, 367 (2009).DOI
  24. [25]S. Kawaguchi, H. Ishibashi, S. Nishihara, S. Mori, J. Campo, F. Porcher, O. Fabelo, K. Sugimoto, J. Kim, K. Kato, et al., Orthorhombic distortion and orbital order in the vanadium spinel FeV2O4, Physical Review B 93, 024108 (2016).
  25. [26]S. Niitaka, H. Ohsumi, K. Sugimoto, S. Lee, Y. Oshima, K. Kato, D. Hashizume, T. Arima, M. Takata, and H. Takagi, A-Type Antiferro-Orbital Ordering with I41/a Symmetry and Geometrical Frustration in the Spinel Vanadate MgV2O4, Physical Review Letters 111, 267201 (2013).
  26. [27]T. Suzuki, M. Katsumura, K. Taniguchi, T. Arima, and T. Katsufuji, Orbital Ordering and Magnetic Field Effect in MnV2O4, Physical Review Letters 98, 127203 (2007).pubmed.ncbi.nlm.nih.gov/17501154
  27. [28]A. Kismarahardja, J. Brooks, A. Kiswandhi, K. Matsubayashi, R. Yamanaka, Y. Uwatoko, J. Whalen, T. Siegrist, and H. Zhou, CuO2: A Spinel Approaching the Itinerant Electron Limit, Physical Review Letters 106, 056602 (2011).
  28. [29]A. Kiswandhi, J. Brooks, J. Lu, J. Whalen, T. Siegrist, and H. Zhou, Chemical pressure effects on structural, magnetic, and transport properties of Mn1−xCoxV2O4, Physical Review B 84, 205138 (2011).
  29. [30]D. Reig-i Plessis, D. Casavant, V. O. Garlea, A. A. Aczel, M. Feygenson, J. Neufeld, H. Zhou, S. E. Nagler, and G. J. MacDougall, Structural transition and orbital glass physics in near-itinerant CoV2O4, Physical Review B 93, 014437 (2016).
  30. [31]B. C. Behera, G. Sabat, S. G. Bhat, S. N. Sarangi, B. R. Sekhar, and D. Samal, Tailoring magnetism in spinel vanadate CoV2O4 epitaxial thin films, Journal of Physics: Condensed Matter 33, 365801 (2021).DOI
  31. [32]L. El Khabchi, L. Schlur, J. Robert, M. Lenertz, C. Leuvrey, G. Versini, F. Roulland, G. Chahine, N. Blanc, D. Preziosi, C. Lefèvre, and N. Viart, Strain-driven magnetic anisotropy and spin reorientation in epitaxial CoV2O4 spinel oxide thin films, Physical Review Materials 10, 014408 (2026).
  32. [33]L. Liu, C. Zhen, J. Feng, X. Wang, L. Ma, G. Li, D. Zhao, and D. Hou, Magnetic anisotropy in epitaxial CoV2O4 thin films under strain, Physical Review B 110, 224424 (2024).
  33. [34]C. J. Thompson, Magnetic Anisotropy and Non-collinear Spin Textures in CoV2O4 Thin Films, Ph.D. dissertation, Florida State University (2020).
  34. [35]S. Kim, C. J. Thompson, Y. Xin, and C. Beekman, Large magnetic anisotropy and magnetostriction in thin films of CoV2O4, Physical Review Materials 7, 014408 (2023).DOI
  35. [36]C. J. Thompson, D. Reig-i Plessis, L. Kish, A. A. Aczel, B. Zhang, E. Karapetrova, G. J. MacDougall, and C. Beekman, Spin canting and orbital order in spinel vanadate thin films, Physical Review Materials 2, 104411 (2018).DOI
  36. [37]M. Althammer, S. Meyer, H. Nakayama, M. Schreier, S. Altmannshofer, M. Weiler, H. Huebl, S. Geprägs, M. Opel, R. Gross, et al., Quantitative study of the spin hall magnetoresistance in ferromagnetic insulator/normal metal hybrids, Physical Review B 87, 224401 (2013).DOI
  37. [38]Y.-T. Chen, S. Takahashi, H. Nakayama, M. Althammer, S. T. Goennenwein, E. Saitoh, and G. E. Bauer, Theory of spin Hall magnetoresistance, Physical Review B 87, 144411 (2013).DOI
  38. [39]A. A. Wagh, P. Garg, A. Haldar, K. Mallick, T. Chakraborty, S. Elizabeth, and P. S. Anil Kumar, Probing magnetic anisotropy and spin-reorientation transition in 3D antiferromagnet, Ho0.5Dy0.5Fe3[Pt using spin Hall magnetoresistance, Physical Review B 106, 104426 (2022).DOI
  39. [40]M. Isasa, S. Vélez, E. Sagasta, A. Bedoya-Pinto, N. Dix, F. Sánchez, L. E. Hueso, J. Fontcuberta, and F. Casanova, Spin Hall Magnetoresistance as a Probe for Surface Magnetization in Pt/CoFe2O4 Bilayers, Physical Review Applied 6, 034007 (2016).DOI
  40. [41]M. Weiler, G. Woltersdorf, M. Althammer, H. Huebl, and S. T. B. Goennenwein, Spin pumping and spin currents in magnetic insulators, in Solid State Physics, Vol. 64 (Elsevier, 2013) pp. 123–156.DOI
  41. [42]L. J. Riddiford, J. J. Wisser, S. Emori, P. Li, D. Roy, E. Cogulu, O. van’t Erve, Y. Deng, S. Y. Wang, B. T. Jonker, et al., Efficient spin current generation in low-damping Mg(Al,Fe)₂O₄ thin films, Applied Physics Letters 115 (2019).DOI
  42. [43]J. Guo, K. Meng, T. Zhang, J. Liu, J. Chen, Y. Wu, X. Xu, and Y. Jiang, Spin Hall Magnetoresistance of CoFe₂O₄/Pt Heterostructures with Interface Non-Collinear Magnetic Configurations, Applied Physics Letters 121 (2022).DOI
  43. [44]Y.-J. Hui, W.-M. Cheng, Z.-B. Zhang, H.-K. Ji, X.-M. Cheng, L. You, and X.-S. Miao, Spin Hall Magnetoresistance in Ta/CoFe₂O₄ Nanostructures, Applied Physics Express 9, 073006 (2016).DOI
  44. [45]A. Peña Cordor, A. Anadón, L. Schlur, J. Robert, H. Damas, J.-C. Rojas-Sánchez, S. Petit-Watelot, N. Viart, D. Preziosi, and C. Lefevre, Spin Transport Properties of Spinel Vanadate-Based Heterostructures, Applied Physics Letters 123 (2023).

Paper details

vlnc:W_pam6cgh8
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents