We report on the low-energy electron irradiated 4H-SiC material studied by means of deep-level transient spectroscopy (DLTS) and Laplace-DLTS. Electron irradiation has introduced the following deep level defects: EH1 and EH3 previously assigned to carbon interstitial-related defects, and M-center, a metastable defect also recently assigned to carbon interstitial defects. We propose that EH1 and EH3 are identical to M1 and M3 and assign them to C_i^(= ) (h) and C_i^(0 ) (h), respectively. Moreover, we provide direct evidence that Laplace-DLTS can be used as an excellent tool to distinguish otherwise identical DLTS signals associated with S1 (VSi) and EH1 (Ci).

Electrically active defects in n-type 4H-SiC have been studied in detail for decades. Piece by piece, the puzzle behind the most common and dominant defect traps such as VC_{\mathrm{C}}(= /0), VC_{\mathrm{C}}(0/++), and VSi_{\mathrm{Si}} has been solved. Part of the puzzle that has kept researchers busy for several years is the study of silicon vacancy and carbon interstitial defects (VSi_{\mathrm{Si}} and Ci_{\mathrm{i}}), introduced by radiation. It was well known that electron irradiation[1, 2, 3], proton irradiation[4, 5, 6], neutron irradiation[7, 8], and ion implantation[9, 10] introduce two deep level defects in n-type 4H-SiC material. These levels are located at 0.40 and 0.70 eV below the conduction band and have been labeled either as S1/2_{1/2} or EH1/3_{1/3}. Recently, Bathen et al.[6] have provided conclusive evidence that S1/2_{1/2} deep level defects are related to VSi_{\mathrm{Si}}, while Alfieri et al.[3] have shown that EH1/3_{1/3} deep level defects are related to Ci_{\mathrm{i}}. The EH1/3_{1/3} deep level defects are introduced only in the case of the low-energy electron irradiation (<200< 200 keV), since under such conditions silicon atoms cannot be displaced[1, 2].

The VSi_{\mathrm{Si}} has attracted much attention in recent years due to its physical properties and its potential application for quantum sensing[6, 11, 12, 13]. The S1_1 and S2_2 are identified as VSi_{\mathrm{Si}} (−3/=) and VSi_{\mathrm{Si}} (=/−) charge transitions, respectively. Bathen et al.[6] have shown that S1_1 (in proton irradiated 4H-SiC samples) has two emission lines originating from VSi_{\mathrm{Si}} sitting at -k and -h lattice sites. These findings were later confirmed by Capan et al.[8] when studying 4H-SiC material irradiated with fast neutrons.

Despite their technological importance, Ci_{\mathrm{i}} defects are not yet fully understood. Coutinho et al.[14] have recently shown that a bi-stable defect in 4H4H-SiC, known as M-center, is carbon interstitial. Accordingly, the defect is responsible for two pairs of first and second acceptor transitions[4, 5, 10, 14, 15],

Configuration A→{M1(=/−)=Ec−0.42 eV; M3(−/0)=Ec−0.74 eV}\text{Configuration A} \rightarrow\{M_{1}(=/-) = E_{c} - 0.42\ \text{eV};\ M_{3}(-/0) = E_{c} - 0.74\ \text{eV}\}
Configuration B→{M2(=/−)=Ec−0.65 eV; M4(−/0)=Ec−0.86 eV}\text{Configuration B} \rightarrow\{M_{2}(=/-) = E_{c} - 0.65\ \text{eV};\ M_{4}(-/0) = E_{c} - 0.86\ \text{eV}\}

where configurations A and B were assigned to a carbon interstitial at the hexagonal and cubic sub-lattice sites, Ci(h)C_{\mathrm{i}(h)} and Ci(k)C_{\mathrm{i}(k)}, respectively. The two configurations can be interchanged by annealing and applying a reverse bias voltage. Configuration A is obtained when the measurement is performed after annealing the sample just above room temperature under reverse bias voltage. The defect jumps to configuration B after the sample is annealed at ∼450\sim450 K without bias.

The evident similarities between M1/3M_{1/3} and EH1/3EH_{1/3} traps, including their location within the band gap and their formation conditions, are so striking that we must hypothesize that they may ultimately arise from the same defect. Therefore, the main goal of this work is twofold. By using low energy electrons and low fluence, we intend to introduce only the EH1/3EH_{1/3} deep level defects and verify if there is evidence for bi-stability and the formation of M1/3M_{1/3}. Moreover, since we displace only the carbon atoms, resulting in a very clear EH1EH_{1} signal, Laplace-DLTS was used to investigate possible superposition of EH1EH_{1} and M1M_{1} signals.

In this work, n-type Schottky barrier diodes (SBDs) were fabricated on nitrogen-doped (∼4.7×1014 cm−3\sim4.7 \times10^{14}\ \text{cm}^{-3}) 4H4H-SiC epitaxial layers, with a thickness of approximately 25 μm25\ \mu\text{m}. The epi-layer was grown on an 8∘8^\circ off-cut silicon face of a 350 μm350\ \mu\text{m} thick 4H4H-SiC (0001) wafer without a buffer layer by chemical vapor deposition. The Schottky barriers were formed by thermal evaporation of nickel through a metal mask with a patterned squared aperture of 11 mm edge length, while the Ohmic contacts were formed on the backside of the silicon carbide substrate by nickel sintering at 950 ∘C950\,^\circ\text{C} in an Ar atmosphere.

Low-energy electron irradiations were performed at NHV, Kyoto, Japan. The electron energy was 150150 keV and the total fluence was 1×1015 cm−21 \times10^{15}\ \text{cm}^{-2}.

DLTS measurements were performed using a Boonton 7200 capacitance meter (Boonton Electronics, New Jersey, USA) and an NI PCI-6521 data acquisition device (NI, Austin, USA). Conventional DLTS measurements were carried out in the temperature range of 100100 to 450450 K with a temperature ramp rate of 22 K/min. Reverse voltage, pulse voltage, and pulse width were VR=−4V_{\mathrm{R}}=-4 V, VP=0V_{\mathrm{P}}=0 V, and tP=10t_{\mathrm{P}}=10 ms, respectively. For the Laplace-DLTS measurements the following acquisition settings were used: the number of samples 3×1043 \times10^{4}, the sampling rate 1010–8080 kHz, and the number of averaged scans 100100–800800. The numerical routine FLOGI[16] was used to calculate Laplace-DLTS spectra.

M-center was transformed to configuration B and configuration A by annealing at 450 K (for 20 min) and cooling the SBD without applying a bias voltage (0 V), or by annealing at 340 K for 20 min and cooling down the SBD with an applied bias voltage of −30 V, respectively.

Figure 1 shows the DLTS spectrum for the n-type 4H-SiC SBD irradiated with low-energy electrons in configurations A and B. It should be noted that the DLTS spectrum for the as-grown 4H-SiC SBD is not shown here, as it has been already reported in several previous studies[17, 18]. In the as-grown sample, only the Z1/2Z_{1/2} peak is present. The Z1/2Z_{1/2} has already been assigned to VC(=/0)V_\mathrm{C}(=/0)[19].

DLTS spectra for the 4H-SiC sample irradiated with low-energy electrons, measured in configurations A and B

Figure 1. DLTS spectra for the 4H-SiC sample irradiated with low-energy electrons, measured in configurations A and B.

Irradiation with low-energy electrons introduced two deep-level defects, whose positions (0.41 and 0.70 eV) are close to those that are usually labeled as EH1\mathrm{EH}_1 and EH3\mathrm{EH}_3. However, the observed peaks are also metastable and consistent with the properties of the M-center[4, 5, 10, 14, 15]. The spectra depend on the applied bias voltage and annealing. The M-center introduces four deep-level defects. M1\mathrm{M}_1 and M3\mathrm{M}_3 overlap with EH1\mathrm{EH}_1 and EH3\mathrm{EH}_3 in configuration A, while M2\mathrm{M}_2 overlaps with Z1/2Z_{1/2} in configuration B (Figure 1). M-states and their bi-stability are more clearly observed if the DLTS signal difference (configuration A – configuration B) is plotted, as shown in Figure 2. As previously reported, it is not possible to observe the M4M_4 with DLTS due to the technical limitations, but M4M_4 has been observed in ion-implanted[10] and neutron-irradiated[8] 4H\mathit{4H}-SiC using the isothermal DLTS.

DLTS signal difference showing M1, M2, and M3 peaks

Figure 2. The DLTS signal difference (configuration A – configuration B) for the 4H\mathit{4H}-SiC sample irradiated with low-energy electrons.

We have estimated the activation energies for M1M_1, M2M_2, and M3M_3 and obtained the following values 0.42, 0.73, and 0.90 eV, which are consistent with previously reported values[4, 5, 10, 14, 15].

The DLTS data obtained in this study are in perfect agreement with previous results from DLTS studies on low-energy electron irradiated 4H\mathit{4H}-SiC samples[1]. However, triggered by the recent advancements in understanding and identifying the MM-center[14], accompanied by the recent progress in understanding the EH1/3\mathrm{EH}_{1/3} and S1/2\mathrm{S}_{1/2} defects[3, 6], we have applied the Laplace-DLTS technique to study the EH1\mathrm{EH}_1 in more details and to investigate the correlation between the EHs defects and the MM-states.

Figure 3 shows Laplace-DLTS spectra in configurations A and B, measured at the temperature of the EH1\mathrm{EH}_1 DLTS peak (T = 200 K). The Laplace-DLTS results clearly indicate that EH1\mathrm{EH}_1 is a single defect, with no splitting of the emission line due to the different lattice sites (−h-h and −k-k) as is the case for S1\mathrm{S}_1 and/or Z1/2\mathrm{Z}_{1/2} (EH6/7\mathrm{EH}_{6/7})[6, 8, 17, 18, 20]. Thus, our results clearly show that Laplace-DLTS can be used as a tool to distinguish S1\mathrm{S}_1 and EH1\mathrm{EH}_1, which give identical signals in the DLTS spectrum. To our knowledge, this is the first time that EH1\mathrm{EH}_1 has been directly measured with Laplace-DLTS.

Laplace DLTS spectra of the 4H-SiC samples

Figure 3. Laplace DLTS spectra of the 4H-SiC samples irradiated with low-energy electrons, measured in configurations A and B at a measurement temperature of 200 K.

According to the recent findings of Coutinho [14], the M-center was assigned to CiC_i. The four states arising from the M-center are assigned to different charge states located at the different lattice sites. M1M_1 and M3M_3 are assigned to Ci−(h)C_i^{-}(h) and Ci0(h)C_i^{0}(h), while M2M_2 and M4M_4 are assigned to Ci−(k)C_i^{-}(k) and Ci0(k)C_i^{0}(k). The occupancy of the -hh or -kk lattice sites is controlled by the reverse bias voltage anneals. For example, if we perform zero bias annealing (configuration B), the -kk sites will be dominantly occupied, leading to the appearance of M2M_2 and M4M_4 in the DLTS spectra. However, if we perform reverse bias annealing (configuration A), then the occupation of the -hh sites prevail, which gives rise to M1M_1 and M3M_3 in the DLTS spectra.

According to the Laplace-DLTS measurements at temperatures around 200 K (i.e. temperature at which EH1EH_1 has the peak maximum in the DLTS spectrum), only one emission line is observed in both configurations, A and B. There is no convincing evidence or even suggestions for two overlapping defects with identical emission lines, that are unresolved by Laplace-DLTS. Let us assume that M1M_1 is indeed EH1EH_1. The difference in the intensity of EH1EH_1 peak (DLTS spectra) in configurations A and B is not due to the overlap of an additional defect such as M1M_1, but to the different occupancy of Ci−(h)C_i^{-}(h) sites. For configuration A, as explained above, this is more favorable than -kk sites. Therefore, we can speculate that EH1EH_1 is the same defect as M1M_1, and assigned to Ci−(h)C_i^{-}(h).

Based on the difference signal (configuration A − configuration B), as shown in Figure 2, the concentrations of M1M_1 and M2M_2 are identical within the measurements error margin. M2M_2 has been recently assigned to Ci−(k)C_i^{-}(k)[7]. This leads us to conclusion that conversion Ci−(h)↔Ci−(k)C_i^{-}(h) \leftrightarrow C_i^{-}(k) occurs more easily than anticipated. As mentioned above, we control the occupancy of the -hh and -kk sites by different bias voltage annealing. From isothermal annealing, the conversion from configuration A to configuration B was previously measured to be activated with a barrier of 1.4 eV, while the conversion from configuration B to configuration A is activated with a lower barrier of 0.9 eV[4]. It should be noted that these values were estimated in the study of MeV proton implanted 4H-SiC material. The MeV implantations result in the introduction of the S1/2S_{1/2} defects (VSiV_{\mathrm{Si}}). By varying the filling pulse length while maintaining the measurement temperature at the S1/M1S_1/M_1 peak position, Martin et al.[4] have clearly shown that contributions from at least two different defects, S1S_1 and M1M_1, are present in configuration B. These results were recently confirmed by Capan et al.[8] as S1S_1 and M1M_1 have directly been measured with Laplace-DLTS. Not only do we have contributions from S1S_1 and M1M_1, but S1S_1 is additionally resolved into two components. Although the analysis of the conversion barriers (configuration A ↔\leftrightarrow configuration B) has been done using the “difference” DLTS signal (presumably this is the case where the signal is only due to the M-center)[4], we should not completely underestimate the fact that the conversion barriers were not determined under conditions equivalent to those reported in this study. The conversion barriers Ci−(h)↔Ci−(k)C_i^{-}(h) \leftrightarrow C_i^{-}(k) could be lower than previously assumed.

All these results imply that EH1/3_{1/3} and M-center are indeed carbon interstitials, and they are all arising from the same defects.

Thus, we conclude that EH1_1 and EH3_3 are identical to M1 and M3, and assign them to Ci−(h)C_i^{-}(h) and Ci0(h)C_i^{0}(h), respectively.

Unfortunately, Laplace-DLTS cannot provide conclusive information about EH3_3 as is the case with EH1, since the EH3_3 is too close to Z1_1(≠0\ne0) and Z2_2(≠0\ne0) in the Laplace DLTS spectrum, and they overlap. The conversion Ci0(h)↔Ci0(k)C_i^{0}(h) \leftrightarrow C_i^{0}(k) should follow the same path. Further studies with isothermal DLTS are needed since this is the only way to measure M4_4 directly.

In this work, we have provided direct evidence that Laplace-DLTS can be used as an excellent and practical tool to distinguish otherwise identical DLTS signals associated with S1_1 (VSi_{\mathrm{Si}}) and EH1_1 (Ci_i). These signals have caused much confusion in the labeling and identification of irradiation-induced deep level defects located at 0.40 and 0.70 eV below the conduction band. Moreover, based on the results obtained in this study, we propose that EH1_1 and EH3_3 are identical to M1_1 and M3_3, and assign them to Ci−(h)C_i^{-}(h) and Ci0(h)C_i^{0}(h), respectively.

ACKNOWLEDGMENTS

This work was supported by the NATO SPS Programme through Project No. G5674.

AUTHOR DECLARATIONS

Conflict of Interest

The authors have no conflicts to disclose.

DATA AVAILABILITY

The data that support the findings of this study are available from the corresponding authors upon reasonable request.

References

  1. [1]¹ F.C. Beyer, C. Hemmingsson, H. Pedersen, A. Henry, E. Janzén, J. Isoya, N. Morishita, and T. Ohshima, J. Appl. Phys. 109, 103703 (2011).
  2. [2]² G. Alfieri, E.V.Monakhov, B.G.Svensson, M.K.Linnarsson, J. Appl. Phys. 98, 043518 (2005).
  3. [3]³ G. Alfieri and A. Mihaila, J. Phys. Condens. Matter 32, 46 (2020).
  4. [4]⁴ M.L.David, G.Alfieri, E.M.Monakhov, A.Hallén, C.Blanchard,B.G.Svensson, J.F.Barbot, J. Appl. Phys. 95, 4728 (2004).
  5. [5]⁵ D.M. Martin, H. Kortegaard Nielsen, P. Lévêque, A. Hallén, G. Alfieri, and B.G. Svensson, Appl. Phys. Lett. 84, 1704 (2004).
  6. [6]⁶ M.E. Bathen, A. Galeckas, J. Müting, H.M. Ayedh, U. Grossner, J. Coutinho, Y.K. Frodason, and L. Vines, Npj Quantum Inf. 5, (2019).
  7. [7]⁷ I.Capan, T.Brodar, Y.Yamazaki, Y.Oki, T.Ohshima, Y.Chiba, Y.Hijikata, L.Snoj, V.Radulović, Nucl. Instrum. Methods Phys. Res. Sect. B Beam Interact. Mater. Atoms. 478, 224 (2020).
  8. [8]⁸ I.Capan, T.Brodar, T.Makino, V.Radulovic, L.Snoj, Crystals 11, 1404 (2021).
  9. [9]⁹ Z.Pastuović, R.SiegeIe, I.Capan, T.Brodar, S.Sato, T.Ohshima, J. Phys. Condens. Matter 29, 475701 (2017).
  10. [10]¹⁰ I.Capan, T.Brodar, R.Bernat, Ž.Pastuović, T.Makino, T.Ohshima, J.D.Gouveia, J.Coutinho, J. Appl. Phys. 130, 125703 (2021).
  11. [11]¹¹ J.Wang, Y.Zhou, X.Zhang, F.Liu, Y.Li, K.Li, Z.Liu, G.Wang, W. Gao, Phys. Rev. Appl. 7, 064021 (2017).
  12. [12]¹² M.Widmann, S.Y.Lee, T.Rendler, N.T.Son, H.Fedder, S.Paik, L.P.Yang, N.Zhao, S.Yang, I.Booker et al. Nat. Mater. 14, 164 (2015).
  13. [13]¹³ F.Fuchs, B.Stender, M.Trupke, D.Simin, J.Pflaum, V.Dyakonov,G.V.Astakhov, Nat. Commun. 6, 1 (2015).
  14. [14]¹⁴ J. Coutinho, J.D. Gouveia, T. Makino, T. Ohshima, Ž. Pastuović, L. Bakrač, T. Brodar, and I. Capan, Phys. Rev. B 103, L180102 (2021).
  15. [15]H.K. Nielsen, A. Hallén, and B.G. Svensson, Phys. Rev. B 72, 085208 (2005).
  16. [16]L.Dobaczewski, A.R.Peaker, K.B.Nielsen, J. Appl. Phys. 96, 4689 (2004).
  17. [17]I. Capan, T. Brodar, Z. Pastuović, R. Siegele, T. Ohshima, S.I. Sato, T. Makino, L. Snoj, V. Radulović, J. Coutinho, V.J.B. Torres, and K. Demmouche, J. Appl. Phys. 123, (2018).
  18. [18]I. Capan, T. Brodar, J. Coutinho, T. Ohshima, V.P. Markevich, and A.R. Peaker, J. Appl. Phys. 124, 245701 (2018).
  19. [19]N.T. Son, X.T. Trinh, L.S. Løvlie, B.G. Svensson, K. Kawahara, J. Suda, T. Kimoto, T. Umeda, J. Isoya, T. Makino, T. Ohshima, and E. Janzén, Phys. Rev. Lett. 109, 187603 (2012).
  20. [20]G.Alfieri, T. Kimoto, Appl. Phys. Lett. 102, 152108 (2013).

Paper details

vlnc:W_ubp3p9x4
Version
v1 · latest
Published
Fresh — added to the Hub within the last 30 days
Added
License
CC BY 4.0
Usage

views · 0

downloads · 0

A view counts once per browser per day, a download each time the PDF is requested.

  • Physics and Astronomy

Not recorded for this paper

View statement
Looking for related papers…
Contents